• Title/Summary/Keyword: Fiber diameter

Search Result 800, Processing Time 0.996 seconds

Properties of Reduced Polyacrylonitrile Nano Fiber (I) (폴리아크릴로니트릴 나노섬유의 환원 및 특성 (I))

  • Choi Chang-Nam;Park Won-Kyu;Lee Woong-Eui
    • Textile Coloration and Finishing
    • /
    • v.18 no.2 s.87
    • /
    • pp.1-7
    • /
    • 2006
  • In order to prepare PAN nano fiber web, PAN/DMF solution was prepared and electrospun. The diameter of fiber was depended on the polymer concentration (7.5-15wt%) and the applied voltage (10-16kV). The average diameter of fiber increased with an increase of the polymer concentration and decreased with the applied voltage. At 7.5wt% concentration, many beads were found. So, we prepared a nano PAN fiber by electrospinning at concentration of 10wt% and 16kV. PAN fibers were reduced with litium aluminium hydride and the dyeability to acid dye was checked. The reduced nano PAN fiber showed much better dyeability compared with the reduced ordinary PAN fiber. It was considered that the increase of specific surface area have an important role in dyeing with acid dye.

Effects of Short-fiber End Shape on Tensile Properties of Reinforced Rubber (단섬유 끝 형상이 강화고무의 인장 특성에 미치는 영향)

  • Ryu, Sang-Ryeol;Lee, Dong-Ju
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.6
    • /
    • pp.1023-1030
    • /
    • 2001
  • The tensile properties of short nylon6 fiber reinforced NR and SBR have been investigated as functions of diameter ratio(DR), interphase condition, fiber aspect ratio(AR), and fiber content. The short-fiber(DR=3 and AR=2) reinforced SBR did not show the dilution effect for all interphase conditions. And the short-fiber(DR=3 and AR=2) reinforced NR did not show the dilution effect except for the no-coating. The better interphase condition, the lower dilution effect at same DR. The tensile moduli are significantly improved due to fiber content and diameter ratio at same interphase condition. The pull-out force increased with the DR. The better interphase condition, the higher pull-out force at same DR. It is found that the DR and AR have an important effect on tensile properties.

Experimental Study on the Bond Properties between GFRP Reinforcements and Steel Fiber Reinforced Concrete (강섬유 보강 콘크리트와 GFRP 보강근의 부착특성에 관한 실험적 연구)

  • Choi, Yun-Cheul
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.5
    • /
    • pp.573-581
    • /
    • 2013
  • In this paper, an experimental investigation of bond properties between steel fiber reinforced concrete and glass fiber reinforced polymer reinforcements was performed. The experimental variables were diameter of reinforcements, volume fraction of steel fiber, cover thickness and compressive strength of concrete. Bond failure mainly occurred with splitting of concrete cover. Main factor for splitting of concrete is tension force occurred by the displacement difference between reinforcements and concrete. Therefore, in order to prevent the bond failure between reinforcements and concrete, capacity of tensile strength of concrete cover should be upgraded. As a results of test, volume fraction of steel fiber significantly increases the bond strength. Cover thickness changes the failure mode. Diameter of reinforcements also changes the failure mode. Generally, diameter of reinforcement also affects the bond properties but this effect is not significant as volume fraction of fiber. Increase of compressive strength increases the bond strength between concrete and reinforcement because compressive strength of concrete directly affects the tensile strength of concrete.

Estimates of Genetic Parameters and Genetic Trends for Production Traits of Inner Mongolian White Cashmere Goat

  • Bai, Junyan;Zhang, Qin;Li, Jinquan;Dao, Er-Ji;Jia, Xiaoping
    • Asian-Australasian Journal of Animal Sciences
    • /
    • v.19 no.1
    • /
    • pp.13-18
    • /
    • 2006
  • Two different animal models, which differ in whether or not taking maternal genetic effect into account, for estimating genetic parameters of cashmere weight, live body weight, cashmere thickness, staple length, fiber diameter, and fiber length in Inner Mongolia White Cashmere Goat were compared via likelihood ratio test. The results indicate that maternal genetic effect has significant influence on live body weight and cashmere thickness, but no significant influence on the other traits. Using models suitable for each trait, both genetic parameters and trends were analyzed with the MTDFREML program. Heritability estimates from single trait models for cashmere weight, live body weight, cashmere thickness, staple length, fiber diameter and fiber length were found to be 0.30, 0.07, 0.21, 0.29, 0.28 and 0.21, respectively. Genetic correlation estimates from two-trait models between live body weight and all other traits (-0.06~0.07) was negligible, as were those between fiber diameter and all other traits (-0.01~0.03) except cashmere thickness (0.19). Cashmere weight and staple length had moderate to low genetic correlations with other traits (-0.24~0.39 and -0.24~0.34, respectively) except for live body weight and fiber diameter. Cashmere thickness had a strong genetic correlation with fiber length (0.81), and low genetic correlation with other traits (0.19~0.34) except live body weight. Genetic trend analysis suggests that selection for cashmere weight was very effective, which has led to the slow genetic progress of cashmere thickness and fiber length due to their genetic correlations with cashmere weight. The selection for live body weight was not effective, which was consistent with its low inheritability.

Fiber Morphology and Physical Characteristics of Gigantochloa atter at Three Different Ages and Heights of Culms for Better Utilization

  • Marsoem, Sri Nugroho;Setiaji, Fajar;Kim, Nam-Hum;Sulistyo, Joko;Irawati, Denny;Nugroho, Widyanto Dwi;Pertiwi, Yus Andini Bekti
    • Journal of the Korean Wood Science and Technology
    • /
    • v.43 no.2
    • /
    • pp.145-155
    • /
    • 2015
  • Fiber morphology and basic characteristics of Legi bamboos (Gigantochloa atter) growing on Yogyakarta were studied considering their age and height positions in the culms. Culms of 4, 16, and 40 months were harvested, and their total lengths were measured. The length, diameter, and wall thickness of each internode were measured. All the sample culms were divided into three different parts along the height, and their fiber dimension and physical properties were observed. The data obtained were analyzed by analysis of variance. The results showed that the culms had a diameter of 5.8 to 10.8 cm. The lowest internodes always showed the shortest length and the thickest wall. The culms had an average fiber length of 2.41 mm and Runkel ratio of 0.61. Fiber length was affected by the height, while fiber diameter, lumen diameter, and fiber wall thickness were affected significantly by the age of the culms. The culms had high green moisture content (GMC) of 157.89%, and basic density (BD) of $456.67kg.m^{-3}$, a total longitudinal shrinkage of 0.35%, and relatively low R/T shrinkage ratio. The interactions between age and height were affected GMC and BD.

Measurement of Spatial Resolution in Fiber-optic Image Guides

  • Lee, Bong-Soo
    • Journal of the Optical Society of Korea
    • /
    • v.5 no.2
    • /
    • pp.33-36
    • /
    • 2001
  • Common methods of determining the spatial resolution of fiber-optic image guides are by measuring the diameter of individual microfibers or by the use of a resolution test target. However these methods cannot provide enough information of spatial resolution in ultrathin fiber-optic image guides. In this study, a simple method to measure the modulation transfer function (MTF) of an mage guide was developed. The MTFs of ultrathin image guides with 3 and 4${\mu}{\textrm}{m}$ Um diameter were measured by examining transmitted sharp edge image. This method should be especially useful for measuring spatial resolution of ultrahigh resolution image guides with less than 5 ${\mu}{\textrm}{m}$ diameter microfibers because their spatial resolution cannot be determined by individual microfiber diameter due to crosstalk and leaky ray phenomena.

Effective Utilization of Hemp Fiber for Pulp and Papermaking (I) -Morphological Characteristics of Hemp Fiber- (펄프.제지용 원료로서의 삼 섬유 이용에 관한 연구(제 1보) -대마 구성 세포의 현미경적 관찰-)

  • Yoon, Seung-Lak;Lee, Myoung-Ku
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.42 no.1
    • /
    • pp.7-12
    • /
    • 2010
  • Morphological characteristics of hemp fiber were investigated using a light microscope in order to provide fundamental data for the use of hemp as a papermaking law material. Phloem of hemp is composed of cortical parenchyma cells and bast fiber with thick walls while xylem is composed of vessel, wood fiber and ray parenchyma cells. Also there are solitary pore and radial pore multiple which exist in diffuse porous pattern. Ray cells consist of uniseriate rays and thin walled ray parenchyma cells. Wood fibers are composed of three types: a large diameter fiber with longer length; a large diameter fiber with shorter length; a small diameter fiber with medium length. Vessel elements are composed of: a medium length one; a longer length one; the one whose both end walls have ligules or tails. Parenchyma cells in xylem and pit parenchyma cells have completely different size and shape. For bast fiber, the average length is about 4.4 mm and the width is about $30.5\;{\mu}m$; for vessel element, $600.0\;{\mu}m$ in length and $493.6\;{\mu}m$ in width; for wood fiber, $1000\;{\mu}m$ and $38.9\;{\mu}m$; for parenchyma cell, $50\;{\mu}m$ and $26.4\;{\mu}m$.

Fabrication and Characterization of Thermal Expanded Core Fiber using the Flame Brushing Method (프레임 브러싱 방법을 이용한 열확산 코어 광섬유 제작 및 특성)

  • Kim, Jun-Hyong;Yang, Hoe-Young;Lee, Sang-Pil;Lee, Hyun-Yong
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.20 no.12
    • /
    • pp.1077-1081
    • /
    • 2007
  • Thermal expanded core (TEC) fiber can reduce, being advantaged from thermal diffusion technology, connection loss by expanding the tolerance in relation to axial offset and gap when making optical connection having mode field diameter (MFD) of optical fiber expanded locally. In this paper, TEC fiber fabrication system based on the frame brushing techniques using twin-torch tip was designed and developed in order to maintain a stable thermal diffusion and single-mode when manufacturing TEC fiber. We were able to obtain that varied kinds of TEC fibers of which MFD could have been extended between $20\;{\mu}m$ and $40\;{\mu}m$ by TEC fiber fabrication system. In addition, the characteristic of connection loss was measured by alignment two TEC fibers of which MFD was $30\;{\mu}m$.

Effect of Fiber Friction, Yarn Twist, and Splicing Air Pressure on Yarn Splicing Performance

  • Das A.;Ishtiaque S. M.;Parida Jyoti R.
    • Fibers and Polymers
    • /
    • v.6 no.1
    • /
    • pp.72-78
    • /
    • 2005
  • The impact of fiber friction, yarn twist, and splicing air pressure on mechanical and structural properties of spliced portion have been reported in the present paper. The mechanical properties include the tensile and bending related properties and, in the structural properties, the diameter and packing density of the splices are studied. A three variable three level facto­rial design approach proposed by Box and Behnken has been used to design the experiment. The results indicate that there is a strong correlation between retained spliced strength (RSS) and retained splice elongation (RSE) with all the experimental variables. It has been observed that RSS increases with the increase in splice air pressure and after certain level it drops, whereas it consistently increases with the increase in yarn twist. The RSE increases with the increase in both fiber friction and yarn twist. It has also been observed that the yarn twist and splicing air pressure have significant influence on splice diameter, percent increase in diameter and retained packing coefficient, but the fiber friction has negligible influence on these parame­ters. Yarn twist and splicing air pressure has a strong correlation with splice flexural rigidity, where as poor correlation with retained flexural rigidity.

The Effect of Processing Parameters on the Diameter of Electrospun Polyacrylonitrile(PAN) Nano Fibers (전기방사한 폴리아크릴니트로 나노섬유의 직경에 미치는 공정인자의 영향)

  • 강영식;김학용;류영준;이덕래;박수진
    • Polymer(Korea)
    • /
    • v.26 no.3
    • /
    • pp.360-366
    • /
    • 2002
  • The electrospinning of polyacrylonitrile dissolved in N,N-dimethyl formamide (DMF) successfully produced nano-scale fibers. The processing parameters such as charged voltage, velocity of collected roller, and tip-to-collector distance (TCD) , affected the ultimate fiber size. At TCD of 5 cm, the average tiber diameter increased with increasing charged voltage because of the more aggregation between fibers due to the remaining DMF solvent on the fiber surface. But, at TCD of 9 cm, the average fiber diameter decreased as the charged voltage was increased because of complete evaporation of DMF. Also, the fiber diameter decreased with increasing the velocity of collected roller. Cross direction width (CWD) of nonwoven mat increased with decreasing the charged voltage and with increasing TCD.