• 제목/요약/키워드: Ferroelectric properties Dielectric properties

검색결과 319건 처리시간 0.03초

Effect of Sintering Temperature on Structural and Dielectric Properties of (Ba0.54Sr0.36Ca0.10)TiO3 Thick Films

  • Noh, Hyun-Ji;Lee, Sung-Gap;Nam, Sung-Pill;Lee, Young-Hie
    • Transactions on Electrical and Electronic Materials
    • /
    • 제10권2호
    • /
    • pp.49-52
    • /
    • 2009
  • Barium strontium calcium titanate powders were prepared with the sol-gel method. Ferroelectric $(Ba_{0.54}Sr_{0.36}Ca_{0.1})TiO_3$(BSCT) thick films were fabricated by the screen-printing method on alumina substrate. Then we investigated the structural and dielectric properties of the BSCT thick films at different sintering temperatures. The thermal analysis showed that the BSCT polycrystalline perovskite phase formed at around $660^{\circ}C$. The X-ray diffraction analysis showed a cubic perovskite structure with no second phase present in all of the BSCT thick films. The average grain size and the thickness of the specimens sintered at $1450^{\circ}C$ were about $1.6{\mu}m$ and $45{\mu}m$, respectively. The relative dielectric constant increased and the dielectric loss decreased as the sintering temperature was increased; for BSCT thick films sintered at $1450^{\circ}C$ the values of the dielectric constant and the dielectric loss were 5641 and 0.4%, respectively, at 1 kHz.

펄스 레이저 증착법에 의해 제작된 Laser pulse repetition rate의 변화에 따른 $Pb(Zr_{0.48}Ti_{0.52})O_3$ (PZT) 박막의 전기적 특성 (Effect of Laser Pulse Repetition Rate on the Electrical Properties of $Pb(Zr_{0.48}Ti_{0.52})O_3$ (PZT) Thin Films grown by Pulsed Laser Deposition)

  • 이동화;이상렬
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.11-12
    • /
    • 2005
  • [ $Pb(Zr_{0.48}Ti_{0.52})O_3$ ] (PZT) thin films were deposited on Pt(111)/Ti/$SiO_2$/Si substrates by pulsed laser deposition. In order to study the effect of different laser pulse repetition rate on the dielectric and ferroelectric properties of PZT thin films,2 Hz and 5 Hz of laser pulse repetition rate were selected. We compared the results of XRD pattern, dielectric constant and hysteresis characteristics. From the experimental data, we found that the electrical properties of PZT thin films which grown ar 2 Hz of laser pulse repetition rate were better than those which grown at 5 Hz of laser pulse repetition rate.

  • PDF

Effects of annealing temperatures on the electrical properties of Metal-Ferroelectric-Insulator-Semiconductor(MFIS)structures with various insulators

  • Jeong, Shin-Woo;Kim, Kwi-Jung;Han, Dae-Hee;Jeon, Ho-Seoung;Im, Jong-Hyun;Park, Byung-Eun
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.112-112
    • /
    • 2009
  • Temperature dependence of the ferroelectric properties of poly(vinylidefluoride-trifluoroethylene) copolymer thin films are studied with various insulators such as $SrTa_2O_6$ and $La_2O_3$. Thin films of poly(vinylidene fluoridetrifluoroethylene) 75/25 copolymer were prepared by chemical solution deposition on p-Si substrate. Capacitance-voltage (C-V) and current density (J-V) behavior of the Au/P(VDF-TrFE)/Insulator/p-Si structures were studied at ($150-200\;^{\circ}C$) and dielectric constant of the each insulators were measured to be about 15 at $850\;^{\circ}C$ for 10 minutes. Memory window width at 5 V bias the MFIS(metal-ferroelectric-insulator-semiconductor) structure with as deposited films was about 0.5 V at high temperature ($200\;^{\circ}C$). And the memory window width increased as voltage increased from 1 V to 5 V.

  • PDF

Sol-gel법에 의한 $Pb(Zr_xTi_{1-x})O_3$ 강유전 박막의 전기특성 (Electrical properties of $Pb(Zr_xTi_{1-x})O_3$ferroelectric thin films prepared by sol-gel processing)

  • 백동수;박창엽
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제9권2호
    • /
    • pp.132-137
    • /
    • 1996
  • Pb(Zr$_{x}$Ti$_{1-x}$ )O$_{3}$ solutions prepared by sol-gel processing with different Zr/Ti ratio were coated on Pt/SiO$_{2}$/Si substrates using spin coating method. Coated films were annealed by rapid thermal annealing at 650.deg. C for 20sec to fabricate Pb(Zr, Ti)O$_{3}$ ferroelectric thin films. Electrical properties of the films such as dielectric constant and loss, ferroelectric hysteresis, fatigue, switching time, and leakage current were measured. Hysteresis of the films with different Zr/Ti ratio yield Pr ranging 10-21.mu.C/cm$^{2}$, E$_{c}$ ranging 37.5-137.5kV/cm. Hysteresis curve was changed from square-type to slim type according to increasing Zr contents. Switching time was faster than 180ns, and leakage current was about 20.mu.A/cm$^{2}$. The film underwent above 10$^{8}$ cycles of reversed polarization showed fatigue with increased coercive field and decreased remnant polarization.tion.

  • PDF

$YMnO_3$ 강유전 박막의 열처리 분위기가 결정화거동과 전기적 특성에 미치는 영향 (Effects of Annealing Atmosphere on Crystallization and Electrical Properties in $YMnO_3$ Ferroelectric Thin Films)

  • 윤귀영;김정석;천채일
    • 한국세라믹학회지
    • /
    • 제37권2호
    • /
    • pp.168-173
    • /
    • 2000
  • YMnO3 thin films were prepared on Pt/Ti/SiO2/Si substrate by chemical solution deposition method. The films were crystallized by heat-treatment at 85$0^{\circ}C$ for 1 hour. Effects of an annealing atmosphere(O2, Ar, vacuum) on the crystallization behavior and electridcal properties were investigated. YMnO3 thin films annealed under Ar atmosphere showed a superior crystallinity and a very strong c-aix preferred-orientation which was a polar axis. Leakage current density of the films decreased with lowering oxygen partial pressure of the annealing atmosphere. C-V and P-E ferroelectric hysteresis were observed only in the thin film heat-treated under Ar atmosphere.In order to prepare YMnO3 thin films having both low leakage current and ferroelectricity, the annealing atmsphere should be kept under a proper oxygen partial pressure which was about 1 Pa in this work. Leakage current density at 1 volt, dielectric constant($\varepsilon$r), remanent polarization(Pr), and coercive field(Ec) were 1.7$\times$10-8 A/$\textrm{cm}^2$, 25, 1.08$\mu$C/$\textrm{cm}^2$, and 100 kV/cm, respectively.

  • PDF

$MnO_2$ 첨가에 따른 Pb($Mg_{1/3}Nb_{2/3}$)$O_3$계 완화형 강유전체에서의 전기적 물성변화 (Effect of $MnO_2$ Addition on the Electric Properties in Pb($Mg_{1/3}Nb_{2/3}$)$O_3$ Relaxor Ferroelectrics)

  • 박재환
    • 한국전기전자재료학회논문지
    • /
    • 제14권7호
    • /
    • pp.562-566
    • /
    • 2001
  • The effects of MnO$_2$ addition on the properties in Pb(Mg$_{1}$3/Nb$_{2}$3/)O$_3$ relaxor ferroelectrics were studied in the phase transition temperature range from -4$0^{\circ}C$ to 11$0^{\circ}C$. Specimens were made via solid state processing method. Dielectric properties, piezoelctric properties, electric-field-induced strain were examined to clarify the effect of MnO$_2$ addition in 0.9MN-0.1PT. As the amount of MnO$_2$ increases, the maximum dielectric constant and the dielectric loss decreases. Q$_{m}$ increased by increasing the doping contents of Mn. When 0.5wt% MnO$_2$ was doped, Q$_{m}$ increased from 95 to 480. The electric-filed-induced strain and polarization decreases as the amount of MnO$_2$ increases. From the experimental results, it was suggested that Mn behaves as an ferroelectric domain pinning element.ent.

  • PDF

La치환된 PMN계 세라믹스의 유전특성에 관한 연구 (A study on Dielectric Properties using PMN Ceramics with La substitution)

  • 지승한;이능헌;김용혁;김진수;이덕출
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 C
    • /
    • pp.1242-1244
    • /
    • 1995
  • The dielectric and polarizable properties of $0.9Pb_{1-x}La_x({Mg}_{1/3}Nb_{2/3})O_3-0.1PbTiO_3$ (x=0,1,2,3,4,5) have been investigated. The temperature-dependant electrostictive characteristics of 0.9PMN-0.1PT relaxor ferroelectric system were improved by enhencing the extent of the diffuse phase transition(DPT). This was achieved using PMN-PTceramics by the partial substitution of La at the Pb site. The curie temperature and the maximum dielectric permittivity decreased by substituting La and the electric field-related hysteresis phenomena decreased with increasing La substitution amount.

  • PDF

Dielectric Properties of Ti-doped K(Ta,Nb)O3 Thin Films for Tunable Microwave Applications

  • Bae Hyung-Jin;Koo Jayl;Hong Jun-Pyo
    • Journal of Electrical Engineering and Technology
    • /
    • 제1권1호
    • /
    • pp.120-126
    • /
    • 2006
  • Ferroelectric materials have been widely investigated for high density dynamic random access memories, opto-electrics, and tunable microwave devices due to their properties. In this study, we have investigated the dielectric properties of Ti doped $K(Ta,\;Nb)O_3$ thin films. By doping Ti Into the $K(Ta,Nb)O_3$ system, Ti with a valence value of +4 will substitute Ta or Nb ions with a valence value of +5. This substitution will introduce an acceptor state. Therefore, this introduced acceptor state will reduce dielectric loss by trapping electrons. Using 3% Ti-doped $K(Ta,Nb)O_3\;targets,\;K(Ta,Nb)O_3$:Ti films were grown in MgO(001) crystals using pulsed laser deposition. First, growth conditions were optimized. A reduction in the loss tangent was observed for Ti-doped $K(Ta,Nb)O_3$ relative to undoped films, although a reduction in tunability is also seen. The crystallinity, morphology, and tunability of $K(Ta,Nb)O_3$:Ti films are reported.

Dielectric Properties of PZT(20/80)/PZT(80/20) Heterolayered Thick Films Fabricated by Screen-printing Method

  • Lee, Sung-Gap;Lee, Young-Hie
    • Transactions on Electrical and Electronic Materials
    • /
    • 제7권3호
    • /
    • pp.129-133
    • /
    • 2006
  • Ferroelectric PZT heterolayered thick films were fabricated by the alkoxide-based sol-gel method. PZT(20/80) and PZT(80/20) paste were made and alternately screen-printed on the alumina substrates. The coating and drying procedure was repeated 4 times to form the heterolayered thick films. The thickness of the PZT heterolayered thick films was approximately $60{\mu}m$. All PZT thick films showed the typical XRD patterns of a polycrystalline rhombohedral structure. And in the PZT thick films sintered at $1100^{\circ}C$, the pyrochlore phase was observed due to the evaporation of PbO. The relative dielectric constant and the dielectric loss of the PZT thick films sintered at $1050^{\circ}C$ were 445.2 and 1.90 % at 1 kHz, respectively. The remanent polarization and coercive field of the PZT thick films sintered at $1050^{\circ}C$ were $14.15{\mu}C/cm^2$ and 19.13 kV/cm, respectively.