Role of A-TIG process in joining of martensitic and austenitic steels for ultra-supercritical power plants -a state of the art review

  • Bhanu, Vishwa;Gupta, Ankur;Pandey, Chandan
    • Nuclear Engineering and Technology
    • /
    • 제54권8호
    • /
    • pp.2755-2770
    • /
    • 2022
  • The need for Dissimilar Welded Joint (DWJ) in the power plant components arises in order to increase the overall efficiency of the plant and to avoid premature failure in the component welds. The Activated-Tungsten Inert Gas (A-TIG) welding process, which is a variant of Tungsten Inert Gas (TIG) welding, is focus of this review work concerning the DWJ of nuclear grade creep-strength enhanced ferritic/martensitic (CSEF/M) steels and austenitic steels. A-TIG DWJs are compared with Multipass-Tungsten Inert Gas (M-TIG) DWJ based on their mechanical and microstructural properties. The limitations of multipass welding have put A-TIG welding in focus as A-TIG provides a weld with increased depth of penetration (DOP) and enhanced mechanical properties. Hence, this review article covers the A-TIG welding principle and working parameters along with detailed analysis of role played by the flux in welding procedure. Further, weld characteristics of martensitic and austenitic steel DWJ developed with the A-TIG welding process and the M-TIG welding process are compared in this study as there are differences in mechanical, microstructural, creep-related, and residual stress obtained in both TIG variants. The mechanics involved in the welding process is deliberated which is revealed by microstructural changes and behavior of base metals and WFZ.

저주기 피로부하에서 F82H 강 TIG 용접 접합부의 피로손상거동 (Fatigue Damage Behavior in TIG Welded Joint of F82H Steel under Low Cycle Fatigue Loading)

  • 김동현;박기원
    • Journal of Welding and Joining
    • /
    • 제33권6호
    • /
    • pp.42-48
    • /
    • 2015
  • Reduced activation ferritic/martensitic steels are recognized as the primary candidate structural materials for fusion blanket systems. Welding is an inevitable for breeding blanket for pressure tightness and radioisotope confinement. Especially, TIG welding was chosen for sealing because it has the largest gap allowance compared to the other welding methods, and its properties are controllable by feed wire and welding conditions. In this study, the low cycle fatigue test using two-type gage such as extensometer and strain gage was applied to the TIG welded joint of F82H steel, for evaluating fatigue damage accumulation behavior of the HAZs. As the result, the over-tempered HAZ have shown a higher fatigue damage accumulation compared with other materials at all the testing conditions.

화력발전소의 장수명화를 위한 Cr 강(鋼)의 고온 $SO_2$가스 부식저감 대책 기술 (Corrosion Prevention of Cr steels in $SO_2$ Atmosphere for Electrial Power Plants)

  • 이동복;최정호
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2007년도 춘계학술발표회 초록집
    • /
    • pp.114-115
    • /
    • 2007
  • The corrosion characteristics of Cr steels were investigated to protect Cr steels from the SO2-gas corrosion in the coal-fired power plant. The samples tested were low alloy ferritic steel (ASTM T22, 23), martensitic steel (ASTM T91, 92, 122), and austenitic stainless steel (ASTM 347HFG). The corrosion tests were performed between 600oC and 1000oC in Ar + (0.2, 1)%SO2 gas for 100 hr. Chromium was quite beneficial to corrosion resistance, while iron was not. The corrosion resistance increased in the order of T22, T23, T91, T92, T122, and 347HFG.

  • PDF

스테인리스강 입계부식 (Intergranular Corrosion of Stainless Steel)

  • 김홍표;김동진
    • Corrosion Science and Technology
    • /
    • 제17권4호
    • /
    • pp.183-192
    • /
    • 2018
  • 스테인리스강은 오스테니틱 스테인리스강, 페리틱 스테인리스강과 마르텐시틱 스테인리스강으로 대별할 수 있으며, 이 고도의 안전성이 요구되는 산업계에서 스테인리스강의 입계부식, 응력부식균열과 핏팅과 같은 국부적 부식이 발생하면 대형사고로 귀결될 수 있다. 스테인리스강의 입계부식 기구와 대책 그리고 입계부식측정 방법에 대한 기술 소개를 하여 산업현장에서 흔히 접하는 스테인리스강 예민화에 대한 길잡이가 되도록 하고, 이 분야를 전문적으로 연구하려는 연구자에게 예민화 전반을 이해하는데 활용되도록 하였다.

複合組織鋼의 破壞靭性 評價와 스트렛치죤의 特性 (Estimation of fracture toughness and characteristics of stretched zone formation in dual phase steel)

  • 김정규;오재민
    • 대한기계학회논문집
    • /
    • 제10권5호
    • /
    • pp.680-688
    • /
    • 1986
  • 본 연구에서는 마르텐사이트-페라이트 복합조직강의 파괴인성평가법을 확립하 기 위하여 불균질의 대표적 인자인 페라이트 결정입경 및 마르텐사이트의 강도를 변화 시켜 R곡선법과 SZ법에 의해 파괴인성을 평가하고, SZ법에 의한 $J_{IC}$ 의 과대평가 정 도와 이에 대한 원인을 규명하기 위하여 균열선단의 미시파괴거동을 검토하였다.

Corrosion Behavior and Oxide Film Formation of T91 Steel under Different Water Chemistry Operation Conditions

  • Zhang, D.Q.;Shi, C.;Li, J.;Gao, L.X.;Lee, K.Y.
    • Corrosion Science and Technology
    • /
    • 제16권1호
    • /
    • pp.8-14
    • /
    • 2017
  • The corrosion behavior of a ferritic/martensitic steel T91 exposed to an aqueous solution containing chloride and sulfate ions is investigated depending on the stimulated all-volatile treatment (AVT) and under oxygenated treatment (OT) conditions. The corrosion of T91 steel under OT condition is severe, while the corrosion under AVT condition is not. The co-existence of chloride and sulfate ions has antagonistic effect on the corrosion of T91 steel in both AVT and OT conditions. Unlike to corrosion resistance in the aqueous solution, OT pretreatment provides T91 steel lower oxidation-resistance than VAT pretreatment. From scanning electron microscopy/energy dispersive X-ray spectroscopy (SEM/EDS) and X-ray diffraction (XRD) analysis, the lower corrosion resistance in the aqueous solution by VAT conditions possibly is due to the formation of pits. In addition, the lower oxidation resistance of T91 steel pretreated by OT conditions is explained as follows: the cracks formed during the immersion under OT conditions accelerated peeling-off rate of the oxide film.

Corrosion behavior and mechanism of CLAM and 316L steels in flowing Pb-17Li alloy under magnetic field

  • Xiao, Zunqi;Liu, Jing;Jiang, Zhizhong;Luo, Lin;Huang, Qunying
    • Nuclear Engineering and Technology
    • /
    • 제54권6호
    • /
    • pp.1962-1971
    • /
    • 2022
  • The liquid lead-lithium (Pb-17Li) blanket has many applications in fusion reactors due to its good tritium breeding performance, high heat transfer efficiency and safety. The compatibility of liquid Pb-17Li alloy with the structural material of blanket under magnetic field is one of the concerns. In this study, corrosion experiments China low activation martensitic (CLAM) steel and 316L steel were carried out in a forced convection Pb-17Li loop under 1.0 T magnetic field at 480 ℃ for 1000 h. The corrosion results on 316L steel showed the characteristic with a superficial porous layer resulted from selective leaching of high-soluble alloy elements and subsequent phase transformation from austenitic matrix to ferritic phase. Then the porous layers were eroded by high-velocity jet fluid. The main corrosion mechanism of CLAM steel was selective dissolution-base corrosion attack on the microstructure boundary regions and exclusively on high residual stress areas. CLAM steel performed a better corrosion resistance than that of 316L steel. The high Ni dissolution rate and the erosion of corroded layers are the main causes for the severe corrosion of 316L steel.

스테인리스강의 브레이징 특성 (Brazing Process of Stainless Steel)

  • 홍성철;박준규;오주희;이재훈;김원중;정재필
    • Journal of Welding and Joining
    • /
    • 제29권6호
    • /
    • pp.40-44
    • /
    • 2011
  • Brazing of a stainless steel was described in this article. Brazing is a joining technology without melting a substrate and joining temperature is higher than $450^{\circ}C$. Brazing can be broadly applicable across industries. In particular, brazing of stainless steel is widely used in aircraft parts, car engines, heat exchangers, etc. due to its excellent strength, corrosion resistance and other suitable characteristics. Characteristics of the stainless steel depend on their classification like austenitic, ferritic and martensitic stainless steels. In addition, there are many processes in brazing and various parameters such as brazing heat source, filler metals, joint design, etc. Therefore, it is necessary to know basic knowledge about brazing to achieve good brazing joint. Accordingly, properties of stainless steel and design of brazing joint and related process were described in this article.

Y2O3 입자 분산강화 9Cr 강의 상온 및 고온 파괴저항특성 (Fracture Resistances of Y2O3 Particle Dispersion Strengthened 9Cr Steel at Room Temperature and High Temperatures)

  • 윤지현;강석훈;이용복;김성수
    • 대한금속재료학회지
    • /
    • 제50권1호
    • /
    • pp.1-7
    • /
    • 2012
  • The fracture resistance and tensile properties of $Y_2O_3$ oxide dispersion strengthened steel containing 9 wt% Cr(9Cr-ODS) were measured at various temperatures up to $700^{\circ}C$. The fracture characteristics were compared with those of commercial E911 ferritic/martensitic steel. The strength of 9Cr-ODS was at least 30% higher than that of E911 steel at the test temperatures below $500^{\circ}C$. The strength difference between the two materials was almost diminished at $700^{\circ}C$. 9Cr-ODS showed cleavage fracture behavior at room temperature and unstable crack growth behaviors at $300^{\circ}C$ and $500^{\circ}C$. The J-R fracture resistance of 9Cr-ODS was much lower than that of E911 steel at all temperatures. It was deduced that the coarse $Cr_2O_3$ particles that were formed during the alloying process provided the crack initiation sites of cleavage fracture in 9Cr-ODS.

페라이트기 11Cr 저탄소강의 자기적 특성에 대한 고온 장시간 시효열화 효과 (Effect of Long-Term Aging Degradation on Magnetic Properties of Ferritic 11Cr Low-Carbon Steel)

  • 김정석;류권상
    • 비파괴검사학회지
    • /
    • 제36권5호
    • /
    • pp.377-383
    • /
    • 2016
  • 페라이트기 11Cr 저탄소강의 자기적 특성에 대한 고온 장시간 시효열화의 영향에 대해서 연구하였다. 장시간 시효시간이 증가함에 따라서 자기이력곡선으로부터 구한 보자력, 자기이력손실은 감소하였고 이들은 시효시간에 대해 2차 지수함수 관계를 나타내었다. 비커스 경도 역시 시효시간의 증가에 따라서 감소하여 기계적 물성의 연화를 나타내었다. 미세조직적 분석으로 주사전자현미경, 후방산란전자 및 X-선 회절시험을 수행하였다. 입계에서는 $Cr_{23}C_6$ 석출물의 급격한 성장과 입내의 래스 경계부에서 Laves ($Fe_2W$)상이 발달하였다. 조대한 석출물들로 인해 장시간 시효열화에 따라서 고용원소의 고갈과 래스 하부조직이 소멸되었다. 이는 자기적 물성과 기계적 물성의 연화현상과 밀접한 관련을 갖게 된다.