$60kg/mm^2$급 조질고장력강의 용접입열량에 따른 미세조직변화 (Microstructural Changes on Weld Heat Input in $60kg/mm^2$ Quenched and Tempered High Strength Steel)

  • 김은석;정인상;박경채
    • Journal of Welding and Joining
    • /
    • 제11권4호
    • /
    • pp.79-90
    • /
    • 1993
  • Shielded metal arc welding, one-ploe and two-pole submerged arc welding were accomplished to investigate microstructure changes on phase transformation behavior in $60kg/mm^2$ quenched and tempered high strength steel. Microstructures were examined by optical micrograph and TEM. In shielded metal arc welding (oxygen 250ppm), the inclusions were small size (0.3-0.5$\mu\textrm{m}$)and small in number. In submerged arc welding (oxygen 430-529ppm), the inclusions were larger(0.7-2$\mu\textrm{m}$) than that of shielded metal arc welding and large in number. Microstructure mainly depends on number and distribution of inclusions in fusion zone of weld metal. It was noticed that a limited number of inclusions favors the formation of acicular ferrite.

  • PDF

Seed 첨가에 의한 Sr-Ferrite의 미세구조 제어 (Microstructure Control of Sr-Ferrite by Seed Addition)

  • 박준홍;신효순;이병교
    • 한국세라믹학회지
    • /
    • 제32권1호
    • /
    • pp.90-94
    • /
    • 1995
  • In Sr-ferrite system, it has been attempted to inhibit the abnormal grian growth using Sr-ferrite powders synthesized by molten salt method as the matrix and the seeds, respectively. At each sintering temperature, the addition of seed more than 15% suppressed the abnormal grain growth, and the uniform microstructure resulted. Particularly, at 12$25^{\circ}C$, it was observed that the maximum number of the abnormal grain growth nuclei was achieved since the abnormal grain growth was suppressed even by the addition of 10% seed.

  • PDF

무전극 형광램프용 페라이트에 따른 전기적 및 광학적 특성 (Electrical and Optical Characteristics by Ferrite for Electrodeless Fluorescent Lamp)

  • 백광현;양종경;이종찬;박대희
    • 한국전기전자재료학회논문지
    • /
    • 제19권2호
    • /
    • pp.200-206
    • /
    • 2006
  • An electric power efficiency of electrodeless fluorescent lamp depens on a big relative property of gas, gas pressure, lamp formation, ingredients of magnetic substance and shape and action frequency etc. in lamp. We used magnetic substance that opens self-examination material of electrodeless fluorescent lamp antenna. We used Mn-Zn type as the Ferrite. We have examined resistance, impedance and Q-factor's frequency characteristic by ferrite. Coil turns were changed from 13 to 15 turns to recognize brightness change of lamp by winding number. Optical equipment (LS-100) was used to measure brightness. We could know Q-factor's difference according to material is important part of antenna design. When an electrodeless fluorescent lamp was made using T company's PE22, it showed the highest brightness. As number of winding is increased the brightness increased, and starting characteristic became good.

3상(相) 혼합조직(混合組織) 구상흑연주철(球牀黑鉛鑄鐵)의 강인화(强引化)에 미치는 특수열처리(特殊熱處理)의 영향(影響)에 관(關)한 연구(硏究) (Effect of Special the Heat Treatment on the Strength and Toughness in a Multi-phase(Ferrite-Bainite-Martensite) Ductile Cast Iron)

  • 최현수;김석원
    • 한국주조공학회지
    • /
    • 제9권6호
    • /
    • pp.463-473
    • /
    • 1989
  • This study is aimed to investigate the effect of cyclic heat treatment which is special heat treatment on the strength and toughness in Multi-phase(Ferrite-Bainite-Martensite) Ductile cast Irons. Spceimens were austenitized at eutectoid transformation temperature range(${\alpha}+{\gamma}$) for 30min and austempered at $300^{\circ}C$ and $400^{\circ}C$ for different holding times, and then quenched in ice water to obtain the multi-phase(Ferrite-Bainite-Martensite) structure from various prior structures, which was obtained by various cyclic heat treatments. As the number of cycle in cyclic heat treatment increased, volume fraction of pearlite increased and the its morphology was refined. As the number of cycle in cyclic heat treatment increased, the multi-phase(Ferrite-Bainite-Martensite) was dispersed in whole matrix as refined island phase. Particularly, martensite among the multi-phase gradually became a spherical shape. Good combination in impact energy and tensile strength was detained in $840^{\circ}C-300^{\circ}C-15min$ condition after 10 cycles in cyclic heat treatment, and its multi-phase volume fraction is Ferrite(50%)-Martensite(l3%)-Bainite(37%).

  • PDF

무전극 형광램프용 페라이트에 따른 휘도특성 (Brightness Property by Ferrite on Electroness Flurescent Lamp)

  • 백광현;이종찬;최용성;박대희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 추계학술대회 논문집 Vol.17
    • /
    • pp.607-610
    • /
    • 2004
  • An electric power efficiency of electrodeless fluorescent lamp has big relativie propertye of gas in lamp, gas pressure, lamp formation, ingredients of magnetic substance and shape and action frequency etc. We used magnetic substance that open self-examination material of electrodeless fluorescent lamp antenna. Ferrite that is used in this experiment was Mn-Zn type. Coill turn was changed from 13th to 13th turn to recognize brightness change of lamp by winding number. Optical equipment that used in an experiment was used to measure brightness (LS-100). When an electrodeless fluorescent ]amp was made using and T company's PE22, was it showed the highest brightness. As number of winding is increased the brightness increased, and starting characteristic became good.

  • PDF

복합산화물이 형성된 API X80 라인파이프강의 용접열영향부 미세조직과 기계적 특성의 상관관계 연구 (Correlation Study of Microstructure and Mechanical Properties in Heat Affected Zones of API X80 Pipeline Steels containing Complex Oxides)

  • 신상용;오경식;이성학
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.59-70
    • /
    • 2009
  • This study is concerned with the correlation between microstructure and mechanical properties in heat affected zones (HAZs) of API X80 pipeline steels containing complex oxides. Three kinds of specimens were fabricated by varying alloying elements of Ti, Al, and Mg to form complex oxides, and their microstructures, Vickers hardness, Charpy impact properties were investigated. The number of complex oxides increased as the excess amount of Ti, Al, and Mg was included in the steels. The simulated HAZs containing a number of oxides showed a high volume fraction of acicular ferrite region because oxides acted as nucleation sites for acicular ferrite. According to the correlation study between thermal input, volume fraction of acicular ferrite region, and Charpy impact properties, the ductile fracture occurred predominantly when the volume fraction of acicular ferrite region was 65% or higher, and the Charpy absorbed energy was excellent over 200 J. When the volume fraction of acicular ferrite region was 35% or lower, the Charpy absorbed energy was poor below 50 J as the brittle cleavage fracture occurred. These findings suggested that the active nucleation of acicular ferrite in the oxide-containing steel HAZs was associated with the great improvement of Charpy impact properties of the HAZs.

API X80 라인파이프강의 용접열영향부 충격인성에 미치는 복합산화물의 영향 (Effects of Complex Oxides on HAZ Toughness of Three API X80 Linepipe Steels)

  • 신상용;오경식;강기봉;이성학
    • 대한금속재료학회지
    • /
    • 제46권4호
    • /
    • pp.199-208
    • /
    • 2008
  • This study is concerned with effects of complex oxides on Charpy impact toughness of heat affected zone (HAZ) of API X80 linepipe steels. Three kinds of steels were fabricated by varying alloying elements such as Ti, Al, and Mg and hot-rolling conditions to form complex oxides, and their microstructures and Charpy impact properties were investigated. The number of complex oxides present in the steel containing excess Ti, Al, and Mg was twice larger than that in the conventional steels, while their size ranged from 1 to $3{\mu}m$ in the three steels. After the HAZ simulation test, the steel containing a number of oxides contained about 20 vol.% of acicular ferrite in the simulated HAZ, together with bainitic ferrite and martensite, whereas the HAZ microstructure of the conventional steels consisted of bainitic ferrite and martensite with a small amount of acicular ferrite. This formation of acicular ferrite in the oxide-containing steel was associated with the nucleation of acicular ferrite at complex oxides, thereby leading to the great (five times or more) improvement of Charpy impact toughness over the conventional steels.

내열용 오버레이 12%Cr계 스테인레스강의 열피로 특성에 미치는 Cr 함량과 델타-페라이트의 영향 (Effects of Cr Content and Volume Fraction of δ-Ferrite on Thermal Cycling Fatigue Properties of Overlay Welded Heat-Resistant 12%Cr Stainless Steels)

  • 정재영
    • 소성∙가공
    • /
    • 제26권6호
    • /
    • pp.356-364
    • /
    • 2017
  • In this study, submerged arc cladded Fe-Cr-Ni-Mo-CuWNbV-C stainless steels containing various Cr contents between 11.2 wt.% and 16.7 wt.% were prepared with fixed C content at about 0.14 wt.%. Using these alloys, changes in microstructure, tensile property, and thermal fatigue property were investigated. Phase fraction of delta-ferrite was increased gradually with increasing Cr content. However, tensile strength, hardness, and thermal fatigue resistance appeared to be decreased. When the microstructure of delta-ferrite was observed, it was revealed that the mesh structure retained up to about 15% Cr content. Although thermal fatigue resistance was almost the same for Cr contents between 11.0 and 14.5 wt.%, it was significantly decreased at higher Cr contents. This was evident from mean value of crack lengths of 10 largest ones. Evaluation of thermal fatigue resistance on alloys with various Cr contents revealed the following important results. First, the reproducibility of ranking test was excellent regardless of the number of cycles. Second, thermal fatigue resistance was increased in proportion to true tensile fracture strength values of overlay materials. Finally, the number of thermal fatigue cracks per unit length was increased with increasing true tensile fracture strength.

Ferrite/varistor의 동시소성 거동에 대한 분체특성의 영향 (The effect of powder characteristics on the behavior of Co-firing of ferrite and varistor)

  • 한익현;이용현;명성재;전명표;조정호;김병익;최덕균
    • 한국결정성장학회지
    • /
    • 제17권2호
    • /
    • pp.63-68
    • /
    • 2007
  • EMI filter와 같은 적층형 세라믹 제조 시 공정 상 많은 문제점이 야기된다. 특히 표면과 계면에서의 crack, camber, delamination 같은 결함이 없는 적층체를 얻기 위해 서로 다른 두 재료의 동시 소성에 의한 수축율 조절이 필수적이다. 본 연구에서는 ferrite의 분체 특성을 통해 varistor/ferrite의 동시소성 거동을 연구하였다. ferrite 분말을 각각 24시간, 48시간, 72시간 분쇄하여 varistor와 ferrite 각각의 슬러리를 제조하고 doctor blade법으로 green sheet를 제조하였다. 슬러리는 분말 55wt(%)에 binder solution 45wt(%)로 혼합하여 제조하였다. Varistor와 ferrite green sheet는 $80 kg/cm^2$로 적층하여 $900^{\circ}C$, $1000^{\circ}C$에서 3시간 소결 하였다. 그 결과 분쇄시간과 소결온도 조절로 결함이 없는 동시 소성된 ferrite/varistor 적층체를 제조 할 수 있었다.

베이나이트강의 미세조직과 저온 충격 인성에 미치는 바나듐과 보론의 영향 (Effect of Vanadium and Boron on Microstructure and Low Temperature Impact Toughness of Bainitic Steels)

  • 황원구;이훈;조성규;서준석;권용재;이정구;신상용
    • 한국재료학회지
    • /
    • 제31권3호
    • /
    • pp.139-149
    • /
    • 2021
  • In this study, three kinds of bainitic steels are fabricated by controlling the contents of vanadium and boron. High vanadium steel has a lot of carbides and nitrides, and so, during the cooling process, acicular ferrite is well formed. Carbides and nitrides develop fine grains by inhibiting grain growth. As a result, the low temperature Charpy absorbed energy of high vanadium steel is higher than that of low vanadium steel. In boron added steel, boron segregates at the prior austenite grain boundary, so that acicular ferrite formation occurs well during the cooling process. However, the granular bainite packet size of the boron added steel is larger than that of high vanadium steel because boron cannot effectively suppress grain growth. Therefore, the low temperature Charpy absorbed energy of the boron added steel is lower than that of the low vanadium steel. HAZ (heat affected zone) microstructure formation affects not only vanadium and boron but also the prior austenite grain size. In the HAZ specimen having large prior austenite grain size, acicular ferrite is formed inside the austenite, and granular bainite, bainitic ferrite, and martensite are also formed in a complex, resulting in a mixed acicular ferrite region with a high volume fraction. On the other hand, in the HAZ specimen having small prior austenite grain size, the volume fraction of the mixed acicular ferrite region is low because granular bainite and bainitic ferrite are coarse due to the large number of prior austenite grain boundaries.