Fe-35Ni-26Cr 주강 액상확산접합부의 고온기계적 특성에 미치는 접합조건의 영향 (Effect of Bonding Condition on High Temperature Mechanical Properties of TLP Bonded Joints of FE-35Ni-26Cr Alloy)

  • 김대업
    • Journal of Welding and Joining
    • /
    • 제18권4호
    • /
    • pp.96-103
    • /
    • 2000
  • This study investigated the effects of bonding temperature and bonding atmosphere on high temperature mechanical properties of transient liquid phase(TLP) bonded joints of heat resistant alloy using MBF-50 insert metal. Specimens were bonded at 1,423~1,468K for 600s. Microconstituents of {TEX}$Cr_{7}(C,B)_{3}${/TEX}were formed in the bonded region when the bonding temperature was low. The amount of microcostituents in the bonded layer decreased with increasing the bonding temperature, and the microconstituents in the bonded layer disappeared at the bonding temperature above 1,468K. The tensile strength of the joints at elevated temperatures increased with the increase the bonding temperature and was the same level as one of the base metal in the bonding temperature over 1,453K. Microstructure and alloying element distributions of the bonded region bonded in Ar and $N_2$atmosphere were similar to those of the bonded in vacuum. The creep rupture strength and rupture lives of joints were almost identical to those of base metal.

  • PDF

Ni-Cr-Fe 및 Ni-Fe-Cr-Mo계 합금의 용접부 균열특성에 관한 연구 Part II : 열영향부의 액화균열 (A Study on the Cracking Behavior in the Welds of Ni-Cr-Fe and Ni-Fe-Cr-Mo Alloys)

  • 김희봉;이창희
    • Journal of Welding and Joining
    • /
    • 제15권5호
    • /
    • pp.46-55
    • /
    • 1997
  • This study has evaluated the liquation cracking behavior in the heat affected zone of several Ni base superalloys (Incoloy 825, Inconel 718 and Inconel 600). 304 and 310S austenitic stainless steels were also included for comparison. In addition, the mechanism of liquation cracking in the HAZ was postulated based on the extensive microstructural examinations with SEM, EDAX and TEM. The liquation cracking resistance of Ni base alloys was found to be far inferior to that of austenitic stainless steels. The liquation cracking of Incoloy 825 and Inconel 718 was believed to be closely related with the Laves-austenite(Ti rich in 825 and Nb rich in 718) and MC-austenitic eutectic phases formed along the grain boundaries by constitutional liquation and incipient melting under rapid welding thermal contraction. Further, liquation cracking resistance of the HAZ was dependent not only upon the type and amount of low melting phases but also on the grain size.

  • PDF

에너지 전자상태 계산으로 도출된 이론값을 이용한 니켈 합금 설계 (Design of Nickel Alloys Using the Theoretical Values Calculated from the Electronic State Energies)

  • 백민숙;강법성;백경철;김병일;윤동주
    • 한국재료학회지
    • /
    • 제25권11호
    • /
    • pp.642-646
    • /
    • 2015
  • Super alloys, which can be divided into three categories, i.e. Ni-base, Co-base, and Fe-base alloys, are widely used for high temperature applications. Since superalloys contain many alloying elements and precipitates, their chemistry and processing parameters need to be carefully designed. In this study, we designed a new Ni alloy to prevent corrosion due to water vapor and gases at high temperatures. The new alloy was designed using the theoretical value of the resulting energy electronic state calculation($DV-X{\alpha}$ method). The components that were finally used were Cr, Mo, and Ti, with Ni as a base. For these alloys, elements were selected in order to compare their values with that of the average theoretical basis for an Inconel 625 alloy. Finally, two kinds of Ni alloy were designed: Ni-28Cr-4Mo-2Ti and Ni-20Cr-10Mo-1Ti.

Spatial Distributions of Alloying Elements Obtained from Atom Probe Tomography of the Amorphous Ribbon Fe75C11Si2B8Cr4

  • Shin, Jinkyung;Yi, Seonghoon;Pradeep, Konda Gokuldoss;Choi, Pyuck-Pa;Raabe, Dierk
    • 한국재료학회지
    • /
    • 제23권3호
    • /
    • pp.190-193
    • /
    • 2013
  • Spatial distributions of alloying elements of an Fe-based amorphous ribbon with a nominal composition of $Fe_{75}C_{11}Si_2B_8Cr_4$ were analyzed through the atom probe tomography method. The amorphous ribbon was prepared through the melt spinning method. The macroscopic amorphous natures were confirmed using an X-ray diffractometer (XRD) and a differential scanning calorimeter (DSC). Atom Probe (Cameca LEAP 3000X HR) analyses were carried out in pulsed voltage mode at a specimen base temperature of about 60 K, a pulse to base voltage ratio of 15 %, and a pulse frequency of 200 kHz. The target detection rate was set to 5 ions per 1000 pulses. Based on a statistical analyses of the data obtained from the volume of $59{\times}59{\times}33nm^3$, homogeneous distributions of alloying elements in nano-scales were concluded. Even with high carbon and strong carbide forming element contents, nano-scale segregation zones of alloying elements were not detected within the Fe-based amorphous ribbon. However, the existence of small sub-nanometer scale clusters due to short range ordering cannot be completely excluded.

신개발 Ni-3Cr-4Si-3B 삽입금속으로 액상확산접합한 내열주강 접합부의 특성 (Characteristics of Liquid Phase Diffusion Bonded Joints Using Newly Developed Ni-3Cr-4Si-3B Insert Metal of Heat Resistant Alloy)

    • Journal of Welding and Joining
    • /
    • 제18권6호
    • /
    • pp.62-67
    • /
    • 2000
  • Metallurgical characteristics of bonded region and high temperature mechanical properties of heat resistant alloy, Fe-35Ni-26Cr during liquid phase diffusion bonding were investigated employing AM17 insert metal. The insert metal for bonding, AM17 was newly developed Ni-base metal using interpolation method. Bonding of specimens were carried out at 1,403~1,463K for 600s in vacuum. The microconstituents in the bonded interlayer disappeared in the bonding temperature over 1,423K. The microstructures, alloying elements and hardness distribution in the base metal. The tensile strength and elongation of the joints at elevated temperatures were the same level as one of the base metal in the bonding temperature over 1,423K. The creep rupture strength and rupture lives of joints were almost identical to those of base metal.

  • PDF

Fe 기내열합금의 액상확상접합용 삽입금속의 개발에 관한 연구 (A Study on Development of Insert Metal for Liquid Phase Diffusion Bonding of Fe Base Heat Resistance Alloy)

  • 강정윤;김인배;이상래
    • Journal of Welding and Joining
    • /
    • 제13권3호
    • /
    • pp.147-156
    • /
    • 1995
  • The change of microstructure in the bonded interlayer and tensile properties of joints were studied for liquid phase diffusion bonding using STS-310 and Incoloy-825 as base metal and base metal+B alloy as insert inetal. Main experimental results obtained in this study are as follows. 1) The optimum amount of B addition into the insert metal was found to be about 4mass%. 2) When isothermal solidification was completed, the microstructure in the bonded interlayer was the same with that of the base metal because of the grain boundary migration in the bonded interlayer. 3) All of the tensile specimen fractured at base metal and joints bonded at optimum condition exhibited tensile properties in excess of base metal requirements. 4) It was determined that fine car-borides and bordes such as M$_{23}$(C,B)$_{6}$, Cr$_{2}$B, and CrB in STS-310S and TiB in Incoloy-825 exist at the grain boundary around bonded interlayer. These precipitates almost disappeared after homogenizing treatment at 1373K for 86.4ks.s.

  • PDF

A Study on Oxidation Mechanism in Mechanically Alloyed ODS Ni-base Alloy

  • Kim, I.H.;Kwun, S.I.;Park, J.P.;Lee, W.S.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2003년도 international symposium on advanced powder metallurgy
    • /
    • pp.65-66
    • /
    • 2003
  • 1. The oxidation resistance of $Y_{2}O_{3}$ containing Ni-base alloy is superior to that of the alloy without $Y_{2}O_{3}$. 2. The appearance of oxides of Ni-20Cr-20Fe-5Nb-$1Y_{2}O_{3}$ alloy is similar to that of oxides in commercial PM1000 and MA754 alloy. 3. The oxides in ODS alloy are grown mainly at particle boundaries.

  • PDF