레이저 표면처리된 Nickel-Base 합금의 공식 저항성 연구 (A Study on the Pitting Corrosion Resistance of Laser Surface Treated Nickel-Base Alloy)

  • 송명호;김용규
    • 한국재료학회지
    • /
    • 제9권2호
    • /
    • pp.217-225
    • /
    • 1999
  • The effect on the pitting corrosion resistance of laser welding and surface treatment developed as a repair method of stream generator tubing material that was a major component of primary system at nuclear power plant was observed. Some heat-treated Alloy 600 tubing materials used at domestic nuclear power plants were laser-surface observed. Some heat-treated Alloy 600 tubing materials used at domestic nuclear power plants were laser-surface melted and the microstructural characteristics were examined. The pitting corrosion resistance was examined through Ep(pitting potential) and degree of pit generation by means of the electrochemical tests and the immersion tests respectively. The pit formation characteristics were investigated through microstructural changes and the pit initiation site and pit morphology. The test results showed that the pitting corrosion resistances was increased in the order of the followings; sensitized Alloy 600, solution annealed alloy600, and laser surface melted Alloy 600. Pits were initiated preferably at Ti-containing inclusions and their surroundings in all tested specimens and it is believed that higher pitting resistance of laser-surface treated Alloy 600 was caused by fine, homogeneous distribution of non-soluble inclusions, the disappearance of grain boundary, and the formation of dense, stable oxide film. The major element of corrosion products filled in the pit was Cr. On the other hand, Fe was enriched in the deposit formed on the pit.

  • PDF

Effects of Metalloid Elements on the Mechanical Properties of Fe-Based Bulk Amorphous Alloys

  • Kim, Yongchan;Hwang, Byoungchul
    • 한국재료학회지
    • /
    • 제26권12호
    • /
    • pp.671-675
    • /
    • 2016
  • In this study, the glass-forming ability and mechanical properties of newly developed Fe-Mn-Cr-Mo-B-C-P-Si-Al bulk amorphous alloys were investigated, and metalloid elements such as B, C, and P were found to have a strong influence on the properties of the Fe-based amorphous alloys. When the total metalloid content (B, C, and P) is less than 5 %, only the crystal phase is formed, but the addition of more than 10 % metalloid elements enhances the glass forming ability. In particular, the alloys with 10 % metalloid content exhibit the best combination of very high compressive strength (~2.8 GPa) and superior fracture elongation (~30 %) because they consist of crystal/amorphous composite phases.

복합 크롬 분말에 의한 철계 용접 오버레이의 내마모 특성 (Wear Resistance Characteristics of Iron Weld Overlays by Composite Chromium Powders)

  • 김종철;박경채;최창옥
    • Journal of Welding and Joining
    • /
    • 제19권5호
    • /
    • pp.506-511
    • /
    • 2001
  • Weld overlay has been developed to improve the property of material surface which is used in the severe environment. Weld overlay is the process which uses an arc heat and welds different composition of alloy on the substrate for the improvements of heat resistance and wear resistance. Weld overlay has a lot of advantages which are high hardness, good processing efficiency, easy controlling of layer thickness, good quality and low cost. In this study, weld overlay was performed by MAG welding on the base metal(SS400) with filler metal which contain composite powders(Cr+C+Mn+Mo+NbC) and solid wire(JIS-YGW11). Characterization of hardness and wear resistance were analyzed by EDS, EPMA, XRD and observations of microstructure were performed to investigate characteristics of overlays. The experimental results of overlaid specimens manufactured with Cr+C+Mn+Mo+NbC powders were obtained as fellows. ${\alpha}-phase$, M(Fe, Cr)3C and NbC of overlays were increased with decreasing the wire feed rates and increasing powder feed rates. Also the hardness of overlays were increased and the specific wear were decreased.

  • PDF

Cr 및 Nb 복합탄화물에 의한 철계 MAG용접 오버fp이의 내마모 특성 (Wear Resistance Characteristics of Iron System MAG Weld Overlays with Chromium and Niobium Carbide Composite)

  • 김종철;박경채
    • Journal of Welding and Joining
    • /
    • 제20권3호
    • /
    • pp.54-59
    • /
    • 2002
  • Overlays is a treatment of the surface and near-surface regions of a material to allow the surface to perform functions that are distinct from those frictions demanded far the bulk of the material. Welding, thermal spray, quenching, carburizing and nitration have been used as the surface treatment. Especially, weld overlay is a relatively thick layer of filler metal applied to a carbon or low-alloy steel base metal for the purpose of providing a wear resistant surface. In this study, weld overlay was performed by MAG welding on the base metal(SS400) with filler metal which contain composite powders($Cr_3C_2+Mn+Mo+NbC$) and solid wire(JIS-YGW11). Characteristics of hardness and wear resistance on overlays were analyzed by EDS, EPMA, XRD and microstructures. Carbide formations were $M(Cr, Fe)_7C_3$ and NbC phases. And carbide volume fraction, hardness and specific wear resistance of overlays were increased with increasing powder feed rate and decreasing wire fred rate. Hardness and wear resistance were almost proportioned to carbide volume fraction of overlay.

고에너지 볼 밀링을 이용한 Y-산화물 분산 Fe-기초내열합금 분말의 합성 및 미세조직 특성 (Synthesis and Microstructure of Fe-Base Superalloy Powders with Y-Oxide Dispersion by High Energy Ball Milling)

  • 임다미;박종관;오승탁
    • 한국재료학회지
    • /
    • 제25권8호
    • /
    • pp.386-390
    • /
    • 2015
  • Fe-base superalloy powders with $Y_2O_3$ dispersion were prepared by high energy ball milling, followed by spark plasma sintering for consolidation. High-purity elemental powders with different Fe powder sizes of 24 and 50 mm were used for the preparation of $Fe-20Cr-4.5Al-0.5Ti-O.5Y_2O_3$ powder mixtures (wt%). The milling process of the powders was carried out in a horizontal rotary ball mill using a stainless steel vial and balls. The milling times of 1 to 5 h by constant operation (350 rpm, ball-to-powder ratio of 30:1 in weight) or cycle operation (1300 rpm for 4 min and 900 rpm for 1 min, 15:1) were applied. Microstructural observation revealed that the crystalline size of Fe decreased with an increase in milling time by cyclic operation and was about 15 nm after 3 h, forming a FeCr alloy phase. The cyclic operation had an advantage over constant milling in that a smaller-agglomerated structure was obtained. The milled powders were sintered at $1100^{\circ}C$ for 30 min in vacuum. With an increase in milling time, the sintered specimen showed a more homogeneous microstructure. In addition, a homogenous distribution of Y-compound particles in the grain boundary was confirmed by EDX analysis.

Structural and Magnetic Properties of Epitaxial FexCo100-x Alloys Grown on Cr Substrate

  • Hossain, M.B.;Kim, C.G.;Chun, B.S.;Kim, W.D.;Hwang, C.
    • Journal of Magnetics
    • /
    • 제19권1호
    • /
    • pp.1-4
    • /
    • 2014
  • We report the correlation between the magnetic properties and lattice parameter of $Fe_xCo_{100-x}$ alloys as a function of constituent concentration. The saturation magnetization increases with Fe content and has a maximum value at approximately x=70 at.%. However, collapse in relative saturation magnetization is observed at approximately 30 at.% to 70 at.% of Fe in $Fe_xCo_{100-x}$ alloys. The collapse is due to the formation of Co-Co and Fe-Fe antibonding states instead of Fe-Co bonds. The lattice parameter also shrinks at approximately 30 at.% to 70 at.% of Fe. This shrinkage is due to an increase in the number of nearest neighbor antisite atoms, which then leads to a decrease in the long range order parameter.

Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N계 초내식성 스테인리스강의 생체적합성 및 부식특성에 미치는 Co함량의 영향 (Effect of Cobalt Contents on the Biocompatibility and Corrosion Properties of Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N Alloy)

  • 장순근;유영란;남희수;심규태;김정구;김영식
    • 대한금속재료학회지
    • /
    • 제46권4호
    • /
    • pp.209-216
    • /
    • 2008
  • Super austenitic stainless steels shows the high PRE (Pitting Resistance Equivalent) number and the good corrosion resistance. This work controlled the Co contents in Fe-31Cr-1.7Mo-27Ni-0.25N alloys to elucidate the effect of cobalt contents on the biocompatibility and corrosion resistance. Increasing Co contents, the hardness of the annealed alloys tends to be reduced. In aged alloys, cobalt decreased the increments of hardness by aging treatment. Cobalt decreased the critical pitting temperature (CPT) in 6% $FeCl_3$ + 1% HCl solution, but improved the anodic polarization behavior in Hanks' balanced salt solution and artificial saliva solution. Repassivation rate in artificial body solutions was improved by increasing cobalt contents, but didn't show the linear relationship to PRE number of the alloys. The experimental alloys showed the non-cytotoxicity because of its high corrosion resistance.

발전 설비용 CrMo강의 탄화물 구조와 조성 변화에 미치는 열화 및 크리프 손상의 영향 (The Effects of Thermal Degradation and Creep Damage on the Microstructure and Composition of the Carbides in the CrMo Steels for Power Plant)

  • 주연준;홍경태;이현웅;신동혁;김제원
    • 한국재료학회지
    • /
    • 제9권10호
    • /
    • pp.1018-1024
    • /
    • 1999
  • Sn-3.5Ag 무연합금을 Cu 및 Alloy42 리드프레임에 납땜접합 (solder joint)하고 미세조직, 젖음성, 전단강도, 시효효과를 측정하여 비교하였다. Cu의 경우, 땜납의 Sn기지상안에 Ag(sub)3Sn과 Cu(sub)6Sn(sub)5상이, 그리고 땜납/리드프레임의 경계면에서는 1∼2㎛ 두께의 Cu(sub)6Sn(sub)5상이 형성되었다. Alloy42의 경우, 기지상내에 있는 낮은 밀도의 Ag(sub)3Sn상만이, 그리고 계면에는 0.5∼1.5㎛ 두께의 FeSn(sub)2이 형성되었다. 한편, Cu에 비해 Alloy42 리드프레임에서 퍼짐면적은 크고 접촉각은 작아 더 우수한 젖음성을 나타내었으나, 전단강도는 35%, 연신율은 75%로 낮았다. 180℃에서 1주일간 시효처리 후, Cu 리드프레임에는 계면에 η-Cu(sub)6Sn(sub)5 층외에 ξ-Cu(sub)3Sn층이 성장하였고, Alloy42 리드프레임에는 기지상내에 Ag(sub)3Sn이 구형으로 조대하게 성장하였고, 계면에는 FeSn(sub)2층만이 약 1.5㎛로 성장하였다.

  • PDF

Ferromagnetism of thin films deposited from paramagnetic stainless steel targets by Facing Targets Sputtering

  • Matsushita, N.;Ono, N.;Naoe, M.
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 1991년도 춘계연구발표회 논문개요집
    • /
    • pp.73-74
    • /
    • 1991
  • The films with ferromagnetic fine particles dispersed in nonmagnetic matrix, such as $Fe-Al_2O_3$ and Fe-Cu have been studied for use of magnetic recording medium, optically device and sensor. Their magnetic properties depend strongly on structural parameter such as size and volume fraction of ferromagnetic particles. Fe-Cr-Ni alloy sputtered films also have microstructure with ferromagnetic -- b.c.c phase and nonmagnetic f.c.c phase grains. Magnetic properties of these films depend strongly on such a unique structure. These are depend on the ratio in volume of ferromagnetic particles to nonmagnetic ones $V_F/V_N$, the saturation magnetization Ms increased with increase of $V_F/V_N$. The coercivity Hc of the as-deposited films took maximum value of about 200 Oe at adequate $V_F/V_N$ and then Ms and Squareness S were 500 emu/cc and 0.5, respectively.(omitted)

  • PDF

Effects of Hydrogen on the PWSCC Initiation Behaviours of Alloy 182 Weld in PWR Environments

  • Kim, H.-S.;Hong, J.-D.;Lee, J.;Gokul, O.S.;Jang, C.
    • Corrosion Science and Technology
    • /
    • 제14권3호
    • /
    • pp.113-119
    • /
    • 2015
  • Alloy 82/182 weld metals had been extensively used in joining the components of the PWR primary system. Unfortunately, there have been a number of incidents of cracking caused by PWSCC in Alloy 82/182 welds during the operation of PWR worldwide. To mitigate PWSCC, optimization of water-chemistry conditions, especially dissolved hydrogen (DH) and Zn contents, is considered as the most promising and effective remedial method. In this study, the PWSCC behaviours of Alloy 182 weld were investigated in simulated PWR environments with various DH content. Both in-situ and ex-situ oxide characterizations as well as PWSCC initiation tests were performed. The results showed that PWSCC crack initiation time was shortest in PWR water (DH: 30cc/kg). Also, high stress reduced crack initiation time. Oxide layer showed multi-layered structures consisted of the outer needle-like Ni-rich oxide layer, Fe-rich crystalline oxide, and inner Cr-rich inner oxide layers, which was not altered by the level of applied stress. To analyse the multi-layer structure of oxides, EIS measurement were fitted into an equivalent circuit model. Further analyses including TEM and EDS are underway to verify appropriateness of the equivalent circuit model.