  • CoFeNi alloys are some of the most studied soft magnetic materials because of their superial properties over FeNi alloys as write head core materials in HDD and MEMS. We studied the effect of magnetic property according to size and orientation of crystal for electroplated Co-Fe-Ni alleys. In case of heat treated ternary alloy, it affect the change of crystal size and structure. In this study, it intends to improve the magnetic properties of CoFeNi thin film by heat treatment. Minimized coercivity and increased magnetization are due to heat treatment from $300^{\circ}C\;to\;400^{\circ}C$. As a bcc phase formation, it grow to amount of magnetization.

Magnetic Properties of (Fe, Co)-Al-B-Nb Nanocrystalline Alloys on Composition and Annealing Temperature ((Fe, Co)-Al-B-Nb 초미세결정립합금의 조성 및 열처리온도에 대한 자기적 특성변화)

  • 강대병;김택기;조용수
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.1
    • /
    • pp.1-7
    • /
    • 1995
  • ${(Fe_{0.85}Co_{0.15})}_{75}Al_{7}B_{18-x}Nb_{x}(x=2,\;4\;and\;6\;at%)\;and\;{(Fe_{0.85}Co_{0.15})}_{75}Al_{y}B_{21-y}Nb_{4}(y=3,\;5,\;7,\;9\;at%)$ alloys were prepared by a single-roll quenching method. Microstructure and magnetic properties of the alloys such as saturation magnetization, initial permeability, coercive force and power loss have been investigated as functions of composition and armea1ing temperature. Nanocrystallines are obtained by armealing of as-prepared amorphous alloys in all compositions except the alloy of 9 at% AI. Saturation magnetization increases after armea1ing and, decreases with Nb content. However, AI and B affects the saturation magnetization insignificantly. Initial perrreability of nanocrystallized alloy at 50 kHz is improved roore than twice compared to that of the as-prepared alloy. Coercive force and core loss reach less than half after armea1ing.

  • PDF

Microstructural Features of Multicomponent FeCoCrNiSix Alloys

  • Kong, Kyeong Ho;Kim, Kang Cheol;Kim, Won Tae;Kim, Do Hyang
    • Applied Microscopy
    • /
    • v.45 no.1
    • /
    • pp.32-36
    • /
    • 2015
  • The microstructural features of FeCoCrNi, FeCoCrNiAl and FeCoCrNiSix (x=0, 5, 10, 15, 20) alloys have been investigated in the present study. The microstructure of FeCoCrNi alloy changes dramatically with equiatomic addition of Al. The fcc irregular shaped grain structure in the as-cast FeCoCrNi alloy changes into the bcc interconnected structure with phase separation of Al-Ni rich and Cr-Fe rich phases in the as-cast FeCoCrNiAl alloy. The microstructure of FeCoCrNi alloy changes with the addition of Si. With increasing the amount of Si, the fcc structure of the grains is maintained, but new phase containing higher amount of Si forms at the grain boundary. As the amount of Si increases, the fraction the Si-rich grain boundary phase increases.

The Effect of Alloy Elements on the Damping Capacity and Plasma Ion Nitriding Characteristic of Fe-Cr-Mn-X Alloys [I Damping Capacity] (Fe-Cr-Mn-X계 합금의 감쇠능 및 플라즈마이온질화 특성에 미치는 합금원소의 영향 [I 감쇠능])

  • Son, D.U.;Jeong, S.H.;Kim, J.H.;Lee, J.M.;Kim, I.S.;Kang, C.Y.
    • Journal of Power System Engineering
    • /
    • v.9 no.1
    • /
    • pp.70-75
    • /
    • 2005
  • The damping property of Fe-12Cr-22Mn-X alloys has been investigated to develop high damping and high strength alloy. Particularly, the effect of the phase of austenite, alpha and epsilon martensite, which constitute the structure of the alloys Fe-12Cr-22Mn-X alloys, on the damping capacity at room temperature has been investigated. Various fraction of these phases were formed depending on the alloy element and cold work degree. The damping capacity is strongly affected by ${\varepsilon}$ martensite while the other phase, such as ${\alpha}'$ martensite, actually exhibit little effect on damping capacity. In case of Fe-12Cr-22Mn-3Co alloy, the large volume fraction of ${\varepsilon}$ martensite formed at about 30% cold rolling, and in case of Fe-12Cr-22Mn-1Ti alloy, formed at about 20% cold rolling and showed the highest damping capacity. Damping capacity showed higher value in Fe-12Cr-22Mn-1Ti alloy than one in Fe-12Cr-22Mn-3Co alloy.

  • PDF

Study on the HDDR Characteristics of the Nd-Fe(-Co)-B(-Ga-Zr)-type Alloys

  • Shon, S.W.;Kwon, H.W.;Kang, D.I.;Kim, Yoon.B.;Jeung, W.Y.
    • Journal of Magnetics
    • /
    • v.4 no.4
    • /
    • pp.131-135
    • /
    • 1999
  • The HDDR characteristics of the Nd-Fe-B-type isotropic and anisotropic HDDR alloys were investigated using three types of alloys: alloy A $(Nd_{12.6}Fe_{81.4}B_6), alloy B (Nd_{12.6}Fe_{81.3}B_6Zr_{0.1}), and alloy C (Nd_{12.6}Fe_{68.8}Co_{11.5}B_6Ga_{1.0}Zr_{0.1}$). The alloy A is featured with the isotropic HDDR character, while alloy B and C are featured with the anisotropic HDDR character. Hydrogenation and disproportionation characteristics of the alloys were examined using DTA under hydrogen gas. Recombination characteristics of the alloys were examined by observing the coercivity variation as a function of recombination time. The present study revealed that the alloy C exhibits slightly higher hydrogenation and disproportionation temperatures compared to the alloy A and B. Recombination of the anisotropic alloy B and C takes place more rapidly with respect to the isotropic alloy A. The intrinsic coercivities of the recombined materials rapidly increased with increasing the recombination time and then showed a peak, after which the coercivities decreased gradually. The degraded coercivity was, however, recovered significantly on prolonged recombination treatment. Compared with the isotropic HDDR alloy A the anisotropic HDDR alloy B and C are notable for their greater recovery of coercivity. The significant recovery of coercivity was accounted for the in terms of the development of well-defined smooth grain boundary between the recombined grains on prolonged recombination.

  • PDF

INFLUENCE OF B AND Nd CONTENT ON THE MAGNETIC PROPERTIES OF ${\alpha}-Fe$ BASED NdFeB MAGNETS WITH ULTRAFINE GRAINS

  • Cho, Y.S.;Kim, Y.B.;Park, W.S.;Kim, C.S.;Kim, T.K.
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.5
    • /
    • pp.427-431
    • /
    • 1995
  • The influence of Nd and B contents on the magnetic properties and structures of ${\alpha}-Fe$ based Nd-(Fe,Co)-B-Mo-Cu alloys was investigated. $Nd_{4}{(Fe_{0.9}Co_{0.1})}_{92-x}B_{x}Mo_{3}Cu_{1}$ and $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{86-x}B_{10}Mo_{3}Cu_{1}$ amorphous alloys prepared by rapid solidification process were crystallized to form nanocrystalline structure. The increase of B content in $Nd_{4}{(Fe_{0.9}Co_{0.1})}_{92-x}B_{x}Mo_{3}Cu_{1}$ nanocrystalline resulted in the change of stucture of soft phase in the sequence of ${\alpha}-Fe$->${\alpha}-Fe+Fe_{3}B$->$Fe_{3}B$. The coercivitis of the alloys were increased with increasing B content and was 263 kA/m at x=18. On the contrary, the remanence has shown an opposite trends. The increase of Nd content in $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{86-x}B_{10}Mo_{3}Cu_{1}$ nanocrystalline containing ${\alpha}-Fe$ as main phase had no effect on the structure and improved coercivity up to 256 kA/m. However, the remanence was decreased from 1.4 T to 1.15 T according to the increase of Nd content.

  • PDF

Development of Ti-Fe-X metal hydride electrode by mechanical alloying (기계적 합금화법에 의한 Ti-Fe-X계 수소 저장합금의 제조에 관한 연구)

  • Ha, Chang-Jin;Lee, Gyeong-Seop
    • Korean Journal of Materials Research
    • /
    • v.5 no.1
    • /
    • pp.112-122
    • /
    • 1995
  • Metal hydride alloys of TiFe based system have been produced by mechanical alloying(MA) method and their electrochemical characteristics have been evaluated for application for Ni/MH battery electrode. These alloys became amorphous after 36hrs ball milling and easily activated electrochemically. All MA amorphous alloys reached at the first charge/discharge cycle the maximum capacity which was 2-3 times higher than the crystalline state. But their cyclic lives were much inferior to the crystalline state. Alloying elements such as Ni, Co, Cr, Mo substituting Fe greatly improved the capacity and 180 mAh/g capacity was obtained in an alloy of TiFe_{0.6}Ni_{0.1}Co_{0.1}Cr_{0.1}Mo_{0.1}$.