• Title/Summary/Keyword: Fe 회수

Search Result 230, Processing Time 0.025 seconds

Arsenic Removal Mechanism of the Residual Slag Generated after the Mineral Carbonation Process in Aqueous System (광물탄산화 공정 이후 발생하는 잔사슬래그의 수계 내 비소 제거 기작)

  • Kim, Kyeongtae;Latief, Ilham Abdul;Kim, Danu;Kim, Seonhee;Lee, Minhee
    • Economic and Environmental Geology
    • /
    • v.55 no.4
    • /
    • pp.377-388
    • /
    • 2022
  • Laboratory-scale experiments were performed to identify the As removal mechanism of the residual slag generated after the mineral carbonation process. The residual slags were manufactured from the steelmaking slag (blast oxygen furnace slag: BOF) through direct and indirect carbonation process. RDBOF (residual BOF after the direct carbonation) and RIBOF (residual BOF after the indirect carbonation) showed different physicochemical-structural characteristics compared with raw BOF such as chemical-mineralogical properties, the pH level of leachate and forming micropores on the surface of the slag. In batch experiment, 0.1 g of residual slag was added to 10 mL of As-solution (initial concentration: 203.6 mg/L) titrated at various pH levels. The RDBOF showed 99.3% of As removal efficiency at initial pH 1, while it sharply decreased with the increase of initial pH. As the initial pH of solution decreased, the dissolution of carbonate minerals covering the surface was accelerated, increasing the exposed area of Fe-oxide and promoting the adsorption of As-oxyanions on the RDBOF surface. Whereas, the As removal efficiency of RIBOF increased with the increase of initial pH levels, and it reached up to 70% at initial pH 10. Considering the PZC (point of zero charge) of the RIBOF (pH 4.5), it was hardly expected that the electrical adsorption of As-oxyanion on surface of the RIBOF at initial pH of 4-10. Nevertheless it was observed that As-oxyanion was linked to the Fe-oxide on the RIBOF surface by the cation bridge effect of divalent cations such as Ca2+, Mn2+, and Fe2+. The surface of RIBOF became stronger negatively charged, the cation bridge effect was more strictly enforced, and more As can be fixed on the RIBOF surface. However, the Ca-products start to precipitate on the surface at pH 10-11 or higher and they even prevent the surface adsorption of As-oxyanion by Fe-oxide. The TCLP test was performed to evaluate the stability of As fixed on the surface of the residual slag after the batch experiment. Results supported that RDBOF and RIBOF firmly fixed As over the wide pH levels, by considering their As desorption rate of less than 2%. From the results of this study, it was proved that both residual slags can be used as an eco-friendly and low-cost As remover with high As removal efficiency and high stability and they also overcome the pH increase in solution, which is the disadvantage of existing steelmaking slag as an As remover.

Physicochemical Properties of Colostrum by Milking Time of Gyeonggi Province (경기지역의 착유회수에 따른 초유의 이화학적 특성)

  • Jeong, Seok-Geun;Ham, Jun-Sang;Kim, Dong-Hun;Ahn, Chong-Nam;Chae, Hyun-Seok;You, Young-Mo;Jang, Ae-Ra;Kwon, Il-Kyung;Lee, Seung-Gyu
    • Food Science of Animal Resources
    • /
    • v.29 no.4
    • /
    • pp.445-456
    • /
    • 2009
  • Colostrum samples were collected from 36 dairy farms in Gyeonggi-do and one dairy farm in the National Institute of Animal Science (NIAS) for testing. Colostrum samples were analyzed for phisycochemicals (specific gravity, pH, titratable acidity), general components (fat, protein, lactose, total solid, solid non-fat (SNF)), fatty acids, amino acids, minerals, microflora, somatic cells, and Ig (Immunoglobulin). The first colostrum revealed the following data: fat contents were $6.16{\pm}2.39%$, proteins were $14.78{\pm}4.30%$, lactose $2.57{\pm}0.77%$, total solid $24.28{\pm}4.36%$, and SNF $18.12{\pm}4.08%$, whereas the 2nd (or $12^{th}$) colostrum revealed $5.56{\pm}1.76%$ fat, $3.46{\pm}0.41%$ proteins, $4.19{\pm}0.43%$ lactose, $13.90{\pm}1.76%$ total solid, and $8.34{\pm}0.81%$ SNF. Also, the first colostrum revealed the contents of major amino acids as 0.89% aspartic acid, 0.71% threonine, 0.86% serine, 1.75% glutamic acid, 0.64% valine, 0.95% leucine, 0.83% lysine, and 0.95% proline, and those in the 10th colostrum were 0.25% aspartic acid, 0.15% threonine, 0.19% serine, 0.59% glutamic acid, 0.19% valine, 0.35% leucine, 0.31% lysine, and 0.34% proine. Major amino acid contents rapidly decreased as milking times increased. In the first colostrum, the following mineral contents were observed: there were 2,168 ppm in Ca, 1,959 ppm in P, 914 ppm in K, 761 ppm in Na, 287 ppm in Mg, 1.7 ppm in Fe, 14.3 ppm in Zn, and 1.0 ppm in Cu; while in the 10th colostrum, the following ppm contents were 1,389 in Ca, 1,323 in P, 838 in K, 427 in Na, 131 in Mg, 1.0 in Fe, 4.7 in Zn, and 1.3 in Cu. The mineral contents in a colostrum rapidly decreased as milking times increased.

A Study on the Replacement of a Light Burnt Dolomite with a Waste MgO-C Refractory Material for a Steel-Making Flux in Electric Arc Furnace (폐 MgO-C계 내화재의 전기로(EAF) 제강 Flux용 경소돌로마이트 대체 사용 연구)

  • Hyun-Jong Kim;Jong-Deok Lim;Hang-Goo Kim;Jei-Pil Wang
    • Resources Recycling
    • /
    • v.31 no.6
    • /
    • pp.44-51
    • /
    • 2022
  • In the steelmaking process using an electric arc furnace (EAF), light-burnt dolomite, which is a flux containing MgO, is used to protect refractory materials and improve desulfurization ability. Furthermore, a recarburizing agent is added to reduce energy consumption via slag foaming and to induce the deoxidation effect. Herein, a waste MgO-C based refractory material was used to achieve the aforementioned effects economically. The waste MgO-C refractory materials contain a significant amount of MgO and graphite components; however, most of these materials are currently discarded instead of being recycled. The mass recycling of waste MgO-C refractory materials would be achievable if their applicability as a flux for steelmaking is proven. Therefore, experiments were performed using a target composition range similar to the commercial EAF slag composition. A pre-melted base slag was prepared by mixing SiO2, Al2O3, and FeO in an alumina crucible and heating at 1450℃ for 1 h or more. Subsequently, a mixed flux #2 (a mixture of light-burnt dolomite, waste MgO-C based refractory material, and limestone) was added to the prepared pre-melted base slag and a melting reaction test was performed. Injecting the pre-melted base slag with the flux facilitates the formation of the target EAF slag. These results were compared with that of mixed flux #1 (a mixture of light-burnt dolomite and limestone), which is a conventional steelmaking flux, and the possibility of replacement was evaluated. To obtain a reliable evaluation, characterization techniques like X-ray diffraction (XRD) analysis and X-ray fluorescence (XRF) spectrometry were used, and slag foam height, slag basicity, and Fe recovery were calculated.

Selective Phase Transformation of Arsenopyrite by Microwave Heating and their Enhancement Au Recovery by Thiocyanate Solution (마이크로웨이브 가열에 의한 황비철석의 선택적 상변환과 티오시안산염 용액에 의한 Au 회수율 향상)

  • Han, Oh-Hyung;Kim, Bong-Ju;Cho, Kang-Hee;Choi, Nag-Choul;Park, Cheon-Young
    • Journal of the Mineralogical Society of Korea
    • /
    • v.27 no.2
    • /
    • pp.73-83
    • /
    • 2014
  • In order to investigate selective phase transformations and to determine the maximum Au leaching factors from microwave treated Au-bearing complex sulfides, a microscope, SEM-EDS analysis, and thiocyanate leaching tests were performed. When the Au-bearing complex sulfides were exposed to microwave heating, increasing the microwave exposure time increased temperature and decreased weight. Arsenopyrite was first selectively transformed to hematite, which formed a concentric rim structure. In this hematite, oxygen and carbon was detected and always showed high iron content and low arsenic content due to arcing and oxidation from microwave heating. The results of the leaching test using microwave treated sample showed that the maximum Au leaching parameters was reached with 0.5 g concentration thiocyanate, 2.0 M hydrochloric acid, 0.3 M copper sulfate and leaching temperature at$60^{\circ}C$. Under the maximum Au leaching conditions, 59% to 96.69% of Au was leached from the microwave treated samples, whereas only 24.53% to 92% of the Au was leached from the untreated samples.

The study on performance of characteristics in engine oil by vehicle driving (차량 운행에 따른 엔진오일의 성능특성 평가 연구)

  • Lee, Joung-Min;Lim, Young-Kwan;Jung, Choong-Sub;Kim, Ye-Eun;Han, Kwan-Wook;Na, Byung-Ki
    • Journal of Energy Engineering
    • /
    • v.22 no.2
    • /
    • pp.237-244
    • /
    • 2013
  • The engine oil is used for lubrication of various internal combustion engines. Recently, the vehicle and engine oil manufacture usually guarantee for oil change over 15000~20000 km mileage, but the most of driver usually change engine oil every 5000 km driving in korea. It can cause to raise environmental contamination by used engine oil and increase the cost of driving by frequently oil change. In this study, we investigate the various physical properties such as flash point, pour point, kinematic viscosity, cold cranking simulator characteristics, total acid number, four-ball test and concentration of metal component for fresh engine oil and used engine oil after real vehicle driving (5000 km, 10000 km). The result showed that the total acid number, wear scar diameter by four-ball test, Fe and Cu had increased than fresh engine oil, but 2 kind of used oil (5000 km and 10000km) had similar physical values and concentration of metal component.

A Study of the Iron Production Process through the Analysis of Slags Excavated from Bupyeong-ri, Inje, Korea (인제 부평리유적 출토 슬래그 분석을 통한 제철 과정 연구)

  • Bae, Chae Rin;Cho, Nam Chul
    • Journal of Conservation Science
    • /
    • v.36 no.2
    • /
    • pp.143-151
    • /
    • 2020
  • In the present article, we have analyzed five slags excavated from the Unified Silla period iron smelting site, i.e., location 4-2 of the Inje Bupyeong-ri site, to investigate the iron smelting process. The total Fe content of the slag excavated from the Inje Bupyeong-ri site ranged between 3.65 and 23.78 wt%, lower than that of typical slag, and deoxidation agent of the slag ranged between 65.92 and 88.96 wt%, higher than that of typical slag. These results suggest that the recovery rate of iron was significantly high. Furthermore, cristobalite was detected in most of the samples, and the furnace temperature, estimated by substituting the analyzed data into the FAS and FCS state diagrams, was confirmed as 1,600℃ or more. These results suggest that the operation at the Inje Bupyeong-ri site was performed at a temperature capable of producing cast iron by completely melting the carbon-containing iron. Observation of the microstructure showed that the iron fragments excavated at the Inje Bupyeong-ri site were identified as white cast iron. Steadite from the ternary iron-carbon-phosphorus system was observed in the white cast iron structure. These results show that indirect smelting was performed when the iron smelting by-products were produced. Based on the analysis results, it was confirmed that the Inje Bupyeong-ri site was the indirect smelting site in the Unified Silla period.

Microparticulation/Air Classification of Rice Bran: Characteristics and Application (초미세분쇄/공기분급을 이용한 탈지미강 분획의 특성과 응용)

  • Park, Dong-June;Ku, Kyung-Hyung;Mok, Chul-Kyoon
    • Korean Journal of Food Science and Technology
    • /
    • v.25 no.6
    • /
    • pp.769-774
    • /
    • 1993
  • Defatted rice bran was microparticulated using fluidized bed opposed jet mill and air-classified at different air classifying wheel speed (ACWS) in Turboplex classifier. The median particle size and the standard deviation decreased, and concomitantly the specific surface area increased generally with increasing ACWS. The protein, fat and ash contents of the recovered rice bran increased with ACWS. The contents of minerals; magnesium, zinc, iron and manganese; increased positively with ACWS. The phytic acid content, however, was slightly higher at middle ACWS. The dietary fiber content was highest in the ACWS 15,000 rpm fraction showing 31.47%. Higher ACWS resulted in lighter colored powder. The water holding capacity (WHC) showed the maximum value at ACWS 12,000 rpm and decreased with increasing ACWS, while the oil holding capacity (OHC) increased with ACWS. The rheological property of the microparticulated rice bran/water suspension fitted to the linear model. The yield stress and viscosity of the suspension increased with ACWS. The shape of microparticulated rice bran at ACWS 21,000 rpm was spherical, and the median particle size was $3.7{\mu}m$. When cake was prepared with substitution of microparticulated rice bran at 5%, the cake height and volume increased remarkably.

  • PDF

Concentration of Vanadium in Jeju Groundwater Using Reverse Osmosis Processes (역삼투 공정을 이용한 제주 지하수의 바나듐 농축)

  • Lee, Ho-Won;Moon, Soo-Hyoung;Ko, Kyung-Soo
    • Membrane Journal
    • /
    • v.18 no.3
    • /
    • pp.241-249
    • /
    • 2008
  • This study is to concentrate vanadium in Jeju groundwater using reverse osmosis processes, and to utilize the concentrate for vanadium water. Groundwater samples were taken from Wahyul, Ayum, and Seogwipo groundwater wells with different in vanadium content each other. Their vanadiuln concentrations were 31.8, 44.5, and 53.0 ppb, respectively. The rejection coefficients of every component in groundwater were increased with the increase of TMP At the TMP of $8 kg_f/cm^2$, the rejection coefficients of vanadium, sodium, potassium, aluminium, iron, and barium were $97.4%{\sim}99.0%,\;97.7%{\sim}97.8%,\;98.0%{\sim}98.3%,\;94.8%{\sim}97.5%,\;88.0%{\sim}96.4.0%$, and $97.9{\sim}98.0%$, respectively. And those of magnesium, calcium, chromium, mauganese, and strontium in three groundwater were more than 99.0% at the same TMP. It was possible that vanadium contents of Wahyul, Ayum and Seogwipo groundwater were concentrated into 58.6, 118.9, and 165.1 ppb, respectively, by 6 stages treatment at the recovery ratio of 15%. And these concentrated water (vanadium water) did not exceed the permissible drinking water standards.

Studies on Ammonium Adsorption by and Desorption from Various Soils -II. Desorption of Ammonium (토양별(土壤別) 암모늄의 흡착(吸着)및 탈착(脫着)에 관한 연구 -II. 암모늄의 탈착(脫着))

  • Shim, Sang-Chil;Park, Hoon;Kim, Moo-Sung;Kim, Kwang-Rai
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.11 no.2
    • /
    • pp.75-80
    • /
    • 1979
  • Ammonium desorption from 16 soils treated with $(NH_4)_2HPO_4$ solution (2000 ppm $NH_4$) was investigated by seven extractions with 0.01M $CaCl_2$. 1. There were 2 to 4 steps alternately appeared with fast and slow mode. 2. Desorption equation, log y=b-ax where y is desorption amount, b a constant indicating adsorption maximum, a retention constant, and x extraction number, was held for each step. 3. Desorption rate (100${\times}$desorption / adsorption) was 65% for the average of 15 soils, maximum 87% in Gimcheon series, minimum 32% in Samgag series. Yongho series (a peat soil) showed 156% indicating the release of large quantity of indigenous soil ammonium. 4. Desorption rate was negatively correlated with initial adsorption and in this relation the tested soils were classified into 3 groups. 5. The cumulative desorption curve was approaching almost to maximum in all tested soils with seven extractions. The final retention amount, ranged from 25% of CEC (Gimhae series) to 502% (Samgag Series). 6. Amount and rate of desorption did not have any significant relation with Langmuir adsorption maxima of ammonium, CEC and contents of clay, available phosphorus and organic matter. 7. The above results may indicate that adsorption and desorption of ammonium is closely related with iron, aluminum silicate and adsorption and desorption characteristics of accompanied anions.

  • PDF

A study on the evaluation of metal component in automatic transmission fluid by vehicle driving (차량 운행에 따른 자동변속기유(ATF) 금속분 분석평가 연구)

  • Lee, Joung-Min;Lim, Young-Kwan;Doe, Jin-Woo;Jung, Choong-Sub;Han, Kwan-Wook;Na, Byung-Ki
    • Journal of Energy Engineering
    • /
    • v.23 no.2
    • /
    • pp.28-34
    • /
    • 2014
  • Automatic transmission fluid (ATF) is used for automatic transmissions in the vehicle as the characterized fluid. Recently, the vehicle manufacture usually guarantee for fluid change over 80000~100000 km mileage or no exchange, but most drivers usually change ATF below every 50000 km driving in Republic of Korea. It can cause to raise environmental contamination by used ATF and increase the cost of driving by frequently ATF change. In this study, we investigate the various physical properties such as flash point, fire point, pour point, kinematic viscosity, cold cranking simulator, total acid number, and metal component concentration for fresh and used ATF after driving (50000 km, 100000 km). The result showed that the total acid number, pour point, Fe, Al and Cu component had increased than fresh ATF, but 2 kind of used oil (50000 km and 100000km) had similar physical values and metal component concentration.