• Title/Summary/Keyword: Fe(1)Cu(1)Si(3.5)

Search Result 146, Processing Time 0.03 seconds

Effect of Sc Addition on the Microstructure Modification of Al-6Si-2Cu Alloy (Sc 첨가에 따른 Al-6Si-2Cu 합금의 미세조직 개량화)

  • An, Seongbin;Kim, Chungseok
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.35 no.3
    • /
    • pp.150-158
    • /
    • 2022
  • The effects of scandium addition on the Al-6Si-2Cu Alloy were investigated. The Al-6Si-2Cu-Sc alloy was prepared by gravity die casting process. In this study, scandium was added at 0.2 wt%, 0.4 wt%, 0.8 wt%, and 1.0 wt%. The microstructure of Al-6Si-2Cu-Sc alloy was investigated using Optical Microscope, Field Emission Scanning Electron Microscope, Electron Back Scatter Diffraction, and Transmission Electron microscope. The microstructure of Al-6Si-2Cu alloy with scandium added changed from dendrite structure to equiaxed crystal structure in specimens of 0.4 wt% Sc or more, and coarse needle-shape eutectic Si and β-Al5FeSi phases were segmented and refined. The nanosized Al3Sc intermetallic compound was observed to be uniformly distributed in the modified Al matrix.

The Influence of Alloying Elements Addition on the Electrical and Mechanical Properties of Cu-Ni-Si-P Alloy (Cu-Ni-Si-P 합금의 기계적 및 전기적 성질에 미치는 첨가원소의 영향)

  • Kim, Seung-Ho;Yum, Young-Jin;Park, Dong-Hwan
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.27 no.1
    • /
    • pp.1-9
    • /
    • 2014
  • For connector material applications, the influence alloying elements of Mn, Cr, Fe, and Ti and cold rolling reduction on the mechanical property, electrical conductivity and bendiability of Cu-Ni-Si-P alloy was investigated. The hot rolled plates were solution treated at $980^{\circ}C$ for 1.5 h, quenched into water, cold rolled by 10% and 30% reduction in thickness, and then aged at $440{\sim}500^{\circ}C$ for 3, 4, 5 times. respectively. Cu-Ni-Si-P-x alloys cold rolled by 10 reduction before heat treatment have a good bendability compare to cold rolled by 30 reduction. Cu-3.4Ni-0.8Si-0.03P-0.1Ti shows the peak strength value of 759 MPa, an electrical conductivity of 39%IACS, an elongation of 10% and a hardness of 256 Hv aged at $440^{\circ}C$ for 6 hrs. Thus it is suitable for lead frame and connector.

Effect of Alloying Element Addition on the Microstructure, Tensile and Impact Toughness of the Modified Al-6.5Si Alloy (개량 Al-6.5Si 합금의 미세조직, 인장 및 충격 인성에 미치는 합금 원소 첨가의 영향)

  • Park, T.H.;Baek, M.S.;Yoon, S.I.;Kim, J.P.;Lee, K.A.
    • Transactions of Materials Processing
    • /
    • v.29 no.3
    • /
    • pp.135-143
    • /
    • 2020
  • Low-cost alloying elements were added to a modified Al-6.5Si alloy and its microstructure, tensile and impact toughness properties were investigated. The alloying elements added were Mg, Zn, and Cu, and two kinds of alloy A (Mg:0.5, Zn:1, Cu:1.5 wt.%) and alloy B (Mg:2, Zn:1.5, Cu:2 wt.%) were prepared. In the as-cast Al-6.5Si alloys, Si phases were distributed at the dendrite interfaces, and Al2Cu, Mg2Si, Al6 (Fe,Mn) and Al5 (Fe,Mn)Si precipitates were also observed. The size and fraction of casting defects were measured to be higher for alloy A than for alloy B. The secondary dendrite arm spacing of alloy B was finer than that of alloy A. It was confirmed by the JMatPro S/W that the cooling rate of alloy B could be more rapid than alloy A. The alloy B had higher hardness and strength compared to the values of alloy A. However, the alloy A showed better impact toughness than alloy B. Based on the above results, the deformation mechanism of Al-6.5Si alloy and the improving method for mechanical properties were also discussed.

Comparison of Metal Contents in Respirable Particulate Mass by Particle Size and Season in Seoul and Asan City (서울.아산지역 호흡성먼지의 금속함량에 관한 연구)

  • Choi, Yun-Na;Jeon, Yong-Taek;Jang, Bong-Ki;Yang, Won-Ho;Yom, Yoon-Ki;Son, Bu-Soon
    • Journal of environmental and Sanitary engineering
    • /
    • v.23 no.1
    • /
    • pp.33-48
    • /
    • 2008
  • The purpose of this study was to characterize background mass concentration of $PM_{10},\;PM_{2.5}$ and metallic composition from June 2004 to June 2005 in comparison with Seoul and Asan city. The results were as follows: 1. Annual mean of $PM_{10}$ concentrations in Seoul and Asan were $56.95({\pm}25.63){\mu}g/m^3,\;57.02({\pm}27.22){\mu}g/m^3$ respectly. 2. Annual mean of $PM_{2.5}$ concentrations in Seoul and Asan were $46.97({\pm}40.36){\mu}g/m^3,\;42.16({\pm}21.79){\mu}g/m^3$ respectly. 3. The average $PM_{2.5}/PM_{10}$ ratio was 0.82 in Seoul and 0.74 in Asan city. 4. The concentration of $PM_{10},\;PM_{2.5}$ were the highest in spring and the lowest in summer. Asan was higher than Seoul in spring and summer. 5. The results showed that average $PM_{10}$ composition order as Si>Fe>Pb>Zn>Mn in Seoul and Si>Fe>Zn>Pb>Mn in Asan. The concentration of metals in $PM_{10}$ of Seoul that Cr, Cu, Fe, Mn were high in spring and Zn was low in Fall. Fe, Mn were high in spring of Asan. 6. The results showed that average $PM_{2.5}$ composition order as Si>Pb>Fe>Zn>Mn in Seoul and Si>Fe>Pb>Zn>Cr in Asan. The concentration of metals in $PM_{2.5}$ of Seoul that Cr was high in spring. 7. The result showed that relation between Cr and Cu, Cu and Fe, Fe and Mn, Mn and Zn, Zn and Si in Seoul, Cr and Zn, Cu and Pb, Zn and Pb, Pb and Mn in Asan. The result showed that $PM_{10}$ concentration exceeding $50{\mu}g/m^3$(US-EPA Standard) and $PM_{2.5}$ concentration exceeding $15{\mu}g/m^3$(US-EPA Standard). In urban area, the monitoring of $PM_{2.5}$ permits the anthropogenic sources and the interference of natural sources with respect to $PM_{10}$ measurements.

Effect of Intercritical Annealing on Microstructure and Mechanical Properties of Fe-9Mn-0.2C-3Al-0.5Si Medium Manganese Steels Containing Cu and Ni (구리와 니켈이 포함된 Fe-9Mn-0.2C-3Al-0.5Si 중망간강의 미세조직과 기계적 특성에 미치는 2상역 어닐링의 영향)

  • Lee, Seung-Wan;Sin, Seung-Hyuk;Hwang, Byoungchul
    • Korean Journal of Materials Research
    • /
    • v.30 no.1
    • /
    • pp.44-49
    • /
    • 2020
  • The effect of intercritical annealing temperature on the microstructure and mechanical properties of Fe-9Mn-0.2C-3Al-0.5Si medium manganese steels containing Cu and Ni is investigated in this study. Six kinds of medium manganese steels are fabricated by varying the chemical composition and intercritical annealing temperature. Hardness and tensile tests are performed to examine the correlation of microstructure and mechanical properties for the intercritical annealed medium manganese steels containing Cu and Ni. The microstructures of all the steels are composed mostly of lath ferrite, reverted austenite and cementite, regardless of annealing temperature. The room-temperature tensile test results show that the yield and tensile strengths decrease with increasing intercritical annealing temperature due to higher volume fraction and larger thickness of reverted austenite. On the other hand, total and uniform elongations, and strain hardening exponent increase due to higher dislocation density because transformation-induced plasticity is promoted with increasing annealing temperature by reduction in reverted austenite stability.

A Study on the Microstructure and Adhesion Properties of Sn-3.5Ag/Alloy42 Lead-Frame Solder Joint (Sn-3.5Ag/Alloy42 리드프레임 땜납접합의 미세조직과 접합특성에 관한 연구)

  • Kim, Si-Jung;Bae, Gyu-Sik
    • Korean Journal of Materials Research
    • /
    • v.9 no.9
    • /
    • pp.926-931
    • /
    • 1999
  • The microstructure, wettability, shear strength and aging effect of Sn-3.5Ag/Cu and Alloy42 lead-frame solder joints were measured for comparison. In the case of Sn-3.5Ag/Cu, $Ag_3Sn and Cu_6Sn_5$ phases in the matrix Sn and $1~2\mu\textrm{m}$ thick $Cu_6Sn_5$ phase at the interface of solder/lead-frame were formed. In the case of Sn-3.5Agl Alloy42, only AgJSn phase of low density in the matrix Sn and $0.5~1.5\mu\textrm{m}$ thick $FeSn_2$, phase at the interface of solder/leadframe were formed. Comparing to Cu, Alloy42 showed wider area of spread and smaller contact angle, thus better wet­tability. But shear strength and ductility of Alloy 42 solder joints were only 33% and 75% of those of Cu, respectively After aging at $180^{\circ}C$ for 1 week, $\xi-Cu_3Sn$ layer on $\eta-Cu_6Sn_5$ layer was formed on Cu lead-frame, while coarsened cir­cular $Ag_3Sn$ phase in the matrix and thickened $FeSn_2$, at the interface were formed on Alloy42 lead- frame.

  • PDF

CRYSTALLIZATION KINETICS OF Fe-Si-B-Cu-Nb AMORPHOUS RIBBONS

  • Zhou, S.X.;Ulvensoen, J.H.;Hoier, R.
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.5
    • /
    • pp.511-514
    • /
    • 1995
  • The crystallization kinetics of $Fe_{73.5}Si_{13.5}B_{9}Cu_{1}Nb_{3}$ amorphous alloy has been investigated using differential scanning calorimetry (DSC). The crystallization process had two stages, i.e. precipitation of the $\alpha$-Fe(Si) solid solution and the tetragonal borides. The isothermal transformation data of the amorphous alloy has been fitted successfully to the generalized Johnson-Mehl-Avrami equation. The mean time exponent, n, obtained is close to 2.5. The value of n=2.5 may be interpreted as being due to a diffusion-controlled transformation process with a constant nucleation rate, one likely transformation mode for the crystallization of metallic amorphous alloys. The activation energy of the overall crystallization process deduced from the time to 50% crystallization are about 81 kcal/mole. The value is of the same order as those estimated from viscous flow.

  • PDF

Separation of Cu(II) from Metal Mixture Solution Using a Hexadecyl $NtnOenH_4$-Octadecylsilanized Silicas(ODS) in Liquid Chromatography (액체 크로마토그래피에서 Hexadecyl $NtnOenH_4$-Octadecylsilanized silicas(ODS)를 이용한 혼합금속용액으로부터 Cu(II)의 분리)

  • Shin, Young-Kook;Kim, Si-Joong;Kim, Hae-Joong
    • Analytical Science and Technology
    • /
    • v.8 no.3
    • /
    • pp.299-304
    • /
    • 1995
  • The adsorption behaviors of Ba(II), Cr(II), Fe(II) and Cu(II) on the N, N'-bispalmtoyl 1, 12-diaza-3, 4:9, 10-dibenzo-5, 8-cyclopentadecane (hexadecyl $NtnOenH_4$)-octadecylsilanized silicas(ODS) were investigated with water as the mobile phase. Binding constants for metal ions were measured in aqueous solution. The order of binding constants(K) and the degree of sorption(E) were Ba(II)$NtnOenH_4$-octadecyisiianized silicas(ODS) increased with concentration of metal ions, and the degree of adsorption was found to be affected by the cation-chelation mechanism. The experimental results showed good efficiency for separation of Cu(II) from mixtures of Ba(II), Cr(II), Fe(II) and Cu(II) in aqueous solution.

  • PDF

Studies on the Ouality of Boxthorn in Korea(Lycium chinense Miller) (한국 구기 품종의 품질에 관한 연구)

  • 이상래
    • KOREAN JOURNAL OF CROP SCIENCE
    • /
    • v.28 no.2
    • /
    • pp.267-271
    • /
    • 1983
  • The southern parts varieties have shown higher content of Oleic acid, Linoleic acid, Vitamin A, Alcaloid, Ca, P and Fe than northern parts Varieties. The $N.\;P_2O_5\;and\;K_2O content of narrow leaf were higher than wide leaf, on the other hand the Ca, Mg, Fe and $SiO_2$ content of wide leaf were higher than narrow leaf. The content of $N, \;P_2O_5, \;K_2O$ have shown higher in first yellow leaf date, the content of Ca has shown higher in first falling leaf date and the content of Mn and Cu content have shown higher in second new leaf date.

  • PDF