• Title/Summary/Keyword: Fail Safety Metal Filter

Search Result 3, Processing Time 0.016 seconds

The Properties of Permeability and Ash-Removal of Sintered Fail Safety Filter of Dust Collector in High Temperature (고온 집진용 Fail Safety 소결 필터의 통기도와 분진제거 특성)

  • Bae S-Y;Ahn I-S;Jung W-H;Choi J-H
    • Korean Journal of Materials Research
    • /
    • v.14 no.7
    • /
    • pp.470-476
    • /
    • 2004
  • The fail safety filter is an assistant filter element to be mounted in order to intercept the particles leaked when the main filter elements are broken. So it should have two contrary functions of being plugged easily to meet the purpose of dust sealing and a high permeability to save the space. The permeability of the metal filter elements were effectively controlled by the following factor: powder size(53-840 ${\mu}m$) and applied pressure(1000-2000 $kgf/cm^2$), and then the compact were sintered for 1 hour at $1200^{\circ}C$ in vacuum sintering furnace. The sintered metal filters was evaluated for the function of the fail safety filter in an experimental unit. The maximum allowable particle size was 420-840 ${\mu}m$, when a CIP pressure of 1500 $kgf/cm^2$ was applied reveals a permeability of about $1.2{\times}10^{10}m^2$ and pore size of about 60 ${\mu}m$. The metal filter produced with stainless steel powder of 480-840 ${\mu}m$ size, which presented excellent permeability than commercial ceramic filter element and plugged with in 3 minutes with the leak of the maximum particle size less than 3 ${\mu}m$.

Fabrication and Permeability of Stainless Steel Filter by using Filler Metal (Filler metal을 이용한 Stainless steel필터의 제조 및 통기도)

  • 배승열;안인섭;성택경;최주호
    • Journal of Powder Materials
    • /
    • v.11 no.4
    • /
    • pp.288-293
    • /
    • 2004
  • The application concept of using a fail safety filter on the filtering system is to prevent the particle leakage when the main filter element is broken at high temperature. In this study, the metal filters were fabricated by pressureless sintering method. The mixture of stainless steel powders and filler metal binder solved in the water solutions of 5% PVA was compacted to form the cylindrical filter without pressure. The compacted filter were sintered in the vacuum sintering furnace at 120$0^{\circ}C$ for 1 hour. The metal filter(produced with powder of 640-840 ${\mu}m$ size) having more than above 50% porosity, 500${\mu}m$ pore size, and permeability of 7.3${\times}$10$^{-11}$m$^{2}$ plugged within 2.5 minute to prevent the leakage of maximum slip particle size of less than 3${\mu}m$.