A study on the Fabrication of Copper-clad Aluminum Composite using Hydrostatic Extrusion (정수압 압출을 이용한 Copper-clad Aluminum 복합계 제조에 대한 연구)

  • 한운용;이경엽;박훈재;윤덕계;김승수
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.21 no.7
    • /
    • pp.179-184
    • /
    • 2004
  • In this work, a copper-clad aluminum composite was fabricated using hot hydrostatic extrusion with various extrusion ratios (8.5, 19, 49) and semi-die angles (30, 45, 60 degree) at a temperature of 32$0^{\circ}C$, Material characteristics of copper-clad aluminum composites were determined from compression tests and hardness tests The results showed that for ER of 8.5, the optimum semi-die angle was below or equal to 30 degree and a pressure drop was about 31%. For ER of 19, the optimum semi-die angle was in the range of 40 to 50 degree and a pressure drop was about 38%. In the case of ER=49, the optimum semi-die angle was above or equal to 60 degree and a pressure drop was about 36%. Compressive yield strength was maximum for ER of 8.5 and semi-die angle of 30 degree and the value of maximum was 155 MPa. Uniform hardness distribution was obtained as the extrusion ratio increases and the semi-die angle decreases. In the case of ER=8.5 and semi-die angle of 30 degree, the lowest extrusion pressure and the maximum compressive yield strength was obtained. Therefor, it was concluded that the optimum extrusion condition for fabricated copper-clad aluminum composites under hydrostatic pressure environment was ER of 19 and semi-die angle of 30 degree.

Effect of Die Angle in the Hydrostatic Extrusion of Copper-clad Aluminium Composites (Copper-clad Aluminium 복합재료의 정수압 압출시 다이 각이 미치는 효과)

  • 한운용;박훈재;윤덕재;정하국;김승수;김응주;이경엽
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.414-417
    • /
    • 2003
  • A copper-clad aluminium composite bar is lighter and less expressive than a commercial copper alloy bar. Copper-clad aluminium composite bar can be fabricated by hot hydrostatic extrusion process. In this work, the effect of die angle on the compressive properties of copper-clad aluminium composites fabricated using hydrostatic extrusion process was investigated experimentally. The results showed that optimum half die angle was in the range of 40$^{\circ}$ to 50$^{\circ}$ for an extrusion ratio of 19. The results also showed that the half die angle had little influence on the compressive strength of copper-clad aluminium composites. A diffusion layer increased with increasing die angle.

  • PDF

A Study on Extrusion Process of Cylindrical Product with Helical Fins Using Rotating Extrusion Die (회전압출다이를 사용한 헬리컬 핀붙이 원형단면 제품의 압출가공에 관한 연구)

  • Park S. M.;Jin I. T.
    • Transactions of Materials Processing
    • /
    • v.14 no.5 s.77
    • /
    • pp.444-451
    • /
    • 2005
  • A new extrusion process of the circular section product with helical fins could be developed by rotating extrusion die. The twisting of extruded product is caused by the twisted conical die surface connecting the die entrance section and the die exit section linearly. But, until now, because the process has used fixed extrusion die, it needs high pressure in order to twist billet and form fin shape on the surface of billet. So, during extruding billet, in order not to twist billet, the extrusion die is needed to rotate itself instead of twisting of billet. It is known that it is possible to reduce extrusion load of product with helical fins by analysis and experiments using rotating die. And it is known that, through the extrusion load analysis by $DEFORM^{TM}-3D$ software, optimal rotational velocity of rotating die can be obtained according to reduction ratio of area and twisted angle of die. And experiments and analysis using rotating extrusion die show that the twisted angle of product can be controlled by twisted angle of extrusion helical die and the rotational velocity of extrusion helical die.

Effect of the Design Parameter for Internal Spline Forming Using the Tube (중공축 내접 스플라인 성형을 위한 설계변수의 영향)

  • Wang, C.B.;Lim, S.J.;Park, Y.B.
    • Transactions of Materials Processing
    • /
    • v.15 no.7 s.88
    • /
    • pp.512-517
    • /
    • 2006
  • In this paper, the cold extrusion process for internal spline forming using a thin and long tube has been analyzed by using a rigid plastic finite element code. The internal spline consists of 10 tooths. The cold extrusion process has been focused on the comparisions of load-stroke relation and filling states of the teeth according to design parameters. The design parameters involve extrusion ratio, extrusion angle and friction factor. The internal spline forming can cause the buckling and folding during the cold extrusion process because of using a thin and long tube. The optimum design parameters have been obtained through rigid-plastic finite elements analysis. The extrusion ratio and extrusion angle have great effects on the deformation characteristics of the cold extrusion process.

Pelletizing Performance of Food Waste Compost by An Extrusion Process (음식물퇴비의 압출에 의한 펠렛화 특성)

  • Kim, Tae-Kye;Min, Young-Bong;Moon, Sung-Dong;Kim, Myung-Cheol
    • Journal of Biosystems Engineering
    • /
    • v.35 no.5
    • /
    • pp.336-342
    • /
    • 2010
  • This study was performed to develop extrusion pelletizer for pelletizing the compost waste food. The effect of water content on the shape of pellet, the relationship between diameter of pellet and of extrusion hole and the relationship between extrusion force and die angle were investigated. Considering the stable shape of compost pellet and the operation efficiency of pelletizer, the water content of 2~4% was considered as the best condition. And the compost pellet could not maintain it's shape at the water content of 10% or over. The strongest extrusion force was needs when the die angle had $90^{\circ}C$ in 6 mm extrusion hole diameter, on the other hand, the weakest extrusion force was need at the die angle of $45^{\circ}{\sim}65^{\circ}$. The compression strength of pellet shows the highest strength of 9.2Mpa when we make the compost pellet after screening the compost and make it with a size of 1.18 mm(No.16) or less.

The Characteristic of a Hydrostatic Extrusion of Magnesium Alloy(AZ31) (Mg 합금(AZ31)의 열간 정수압 압출 특성에 관한 연구(I))

  • Yoon D. J.;Seo Y. W.;Jeong H. G.;Na K. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.10a
    • /
    • pp.128-131
    • /
    • 2004
  • Magnesium alloys are being extensively used in weight-saving applications and as a potential replacement for plastics in electronic and computer applications. Magnesium alloy has some good characteristics, EMI shielding property and high specific strength. Nevertheless their high brittleness make it uneasy to process the magnesium. Magnesium alloys are extruded like aluminium alloys. The present work was done to find a characteristic of magnesium alloy(AZ31) changing the extrusion ratio 8.5, 19.1, 49 respectly and changing the die half angle $30^{\circ},\;45^{\circ},\;60^{\circ}$. Here this present done by the hydrostatic extrusion in the hot condition, $310^{\circ}$. The higher the extrusion ratio goes, the higher the extrusion force goes.

  • PDF

The Effect of Extrusion Temperature and Die Angle on Mechanical Properties of $SiC_p$/2024Al Composites Fabricated by Powder Extrusion Method (분말압출법으로 제조된 $SiC_p$/2024Al 복합재료에 있어서 압출온도와 다이각이 기계적 성질에 미치는 영향)

  • 성병진
    • Journal of Powder Materials
    • /
    • v.2 no.1
    • /
    • pp.44-52
    • /
    • 1995
  • Effects of the extrusion temperature and die angle on the tensile properties of SiCIyAl composites in powder extrusion have been investigated. SiCP/Al composites were extruded at various extrusion temperatures (450, 500, $550^{\circ}C$) under the extrusion ratio of 25 : 1. The ram speed was maintained at 13 cm/min for all the extrusion conditions. The surface of the extruded rod appeared to be smooth without tearing at 450 and 50$0^{\circ}C$, whereas it was very rough due to tearing at $550^{\circ}C$. It was found that the tensile strength and elongation of the composites extruded at $500^{\circ}C$ are greater than those of composites extruded at $450^{\circ}C$ This is due to the easier plastic deformation of composite extruded at $500^{\circ}C$, compared with the composites extruded at $450^{\circ}C$. The effect of die angle was examined under 20=60, 120, $180^{\circ}$die angles at extrusion temperature of $500^{\circ}C$ under 25:1 extrusion ratio. The tensile strength of the composites extruded with 20=$60^{\circ}$approved to be higher than that of the composties extruded with 28 : 120 and $180^{\circ}$This is attributable to the higher extrusion pressure, which mixed composite powders could be densely consolidated at elevated temperatures, resulting from high friction force between billet and sliding surface of conical die.

  • PDF

The Characteristic of a Hydrostatic Extrusion of Magnesium Alloy(AZ31) - II (Mg 합금(AZ31)의 열간 정수압 압출 특성에 관한 연구(II))

  • Seo Y. W.;Jeong H. G.;Na K. H.;Yoon D. J.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.05a
    • /
    • pp.144-147
    • /
    • 2005
  • In hydrostatic extrusion the billet in the container is extruded through a die with a liquid acting as a pressure medium, instead of by the direct application of the load by a ram. And the extrusion pressure can be affected by the flow stress and they are affected by the temperature. So in this study the temperature is the main issue with a extrusion ratio and a half die angle. As extrusion temperature goes down from $300^{\circ}C$ to $200^{\circ}C$, tensile strength goes up to 310MPa. Because velocity of extrusion is higher than the conventional extrusion, there is another characteristic in the sense of microstrure. The temperature was sotted to $300^{\circ}C,\;250^{\circ}C,\;200^{\circ}C$, respectively. There is a increase of extrusion pressure abot $15\%$.

  • PDF

The Effect of Process Parameter in Direct Extrusion of Copper Clad Aluminum Composite Materials (Cu-Al 층상 복합재료의 직접압출시 공정변수의 영향)

  • 윤여권;김희남;김용수
    • Journal of the Korean Society of Safety
    • /
    • v.15 no.4
    • /
    • pp.28-34
    • /
    • 2000
  • Copper clad aluminum composite materials are being used for economic and structural purposes, The development of an efficient production method of copper clad aluminum composite material rods by extrusion is very important. This paper describes experimental investigations in the direct extrusion of copper clad aluminum rods through conical dies. There are several parameters that have an influence on determining a sound clad extrusion. These variables are extrusion temperature, extrusion ratio, semi-cone angle of die, extrusion force, extrusion velocity, friction of between the container and billet, percentage of copper used and ratio of flow stress of copper to aluminum. In order to investigate the influence of extrusion temperature, extrusion ratio, semi-cone angle of die on the hot direct extrudability of the copper clad aluminum composite material rods, the experimental study have been performed with these variation.

  • PDF

A Study on the Forming Characteristics of Radial-Forward Extrusion Process (레이디얼-전방압출 공정의 성형특성에 관한 연구)

  • 황승규;이호용;황병복
    • Transactions of Materials Processing
    • /
    • v.11 no.1
    • /
    • pp.84-89
    • /
    • 2002
  • This study is concerned with the analysis of the forming characteristics of radial-forward extrusion. Angle between radial and forward extrusion, gap height, and friction factor are considered as important design factors to affect forming characteristics in radial-forward extrusion. The rigid-plastic finite element method is adopted to analyze the effects of design factors on forming loads. The incremental rates of loads are nearly constant except the deformation zone from radial to forward extrusion. The smaller angle induces lesser force increment, therefore forming load increases as the angle increases. Maximum load also increases as gap-height decreases and friction factor increases.