• Title/Summary/Keyword: Excess MgO

Search Result 88, Processing Time 0.022 seconds

Effect of MgO Content on Microstructural Evolution and Microwave Dielectric Properties of $Ba(Mg_{1/3}Ta_{2/3})O_3$ Ceramics (MgO 변화량에 다른 $Ba(Mg_{1/3}Ta_{2/3})O_3$ [BMT]계 세라믹스의 미세조직변화와 마이크로파 유전특성)

  • 이정아;김정주;이희영;김태홍;최태구
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.11
    • /
    • pp.1299-1306
    • /
    • 1994
  • Effect of MgO content on microstructural evolution and microwave dielectric properties of Ba(Mg1/3Ta2/3)O3 system was investigated. MgO content was varied from 10 mol% deficiency to 10 mol% excess of stoichiometric composition, respectively. It was found that MgO-deficient specimen showed faster grain growth rate than stoichometric and MgO excess BMT system. Besides, sandwich type precipitates of Ba5Ta4O15 which was formed within the BMT grain, might lead to the anisotropic grain growth of BMT grain. On the contrary, in MgO excess specimen, BMT grain growth rate was retarded by precipitations of MgO phase in grain boundary. Besides, the Q values of MgO-deficient showed lower than MgO-excess due to precipitations of Ba5Ta4O15 within BMT grain.

  • PDF

Dielectric and Strain Properties of PMN-PT Ceramics Doped with $\textrm{SrTiO}^3$ and excess MgO ($\textrm{SrTiO}^3$ 와 과잉 MgO가 첨가된 $\textrm{Pb(Mg_{1/3}Nb_{2/3})O}_3$ - $\textrm{PbTiO}^3$ 계 세라믹스의 유전 및 변위 특성)

  • 이상훈
    • Journal of the Korean Institute of Telematics and Electronics T
    • /
    • v.36T no.3
    • /
    • pp.7-12
    • /
    • 1999
  • In this paper, dielectric and strain properties of (1-f-y)PMN-yPT-xST ceramics investigated with the amount of $\textrm{SrTiO}^3$(ST). The $\textrm{SrTiO}^3$ content is ranged within 1~6㏖%. Another compositions with excess MgO also investigated. As the amount of ST is increased, dielectric constant has a maximum value at 5㏖% composition. The Curie temperature is decreased linearly with increasing the amount of ST. Coercive field and ramnant polarization has a maximum value at l㏖% composition. As for the effects of excess MgO, the dielectric constant has been increased by the addition of excess MgO up to 3㏖% to a 0.8PMN-0.12PT-0.04ST specimen. But the strain has been decreased by the addition of excess MgO.

  • PDF

Effect of Excess MgO on Dielectric and Electrostrictive Properties of $0.99Pb(Mg_{1/3}Nb_{2/3})O_3-0.01Pb(Mn_{2/3}W_{1/3})O_3$ ($0.99Pb(Mg_{1/3}Nb_{2/3})O_3-0.01Pb(Mn_{2/3}W_{1/3})O_3$계의 유전 및 전왜 특성에 미치는 과잉 MgO의 영향)

  • 윤기현;김승연;남윤우;조용수;강동헌
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.8
    • /
    • pp.629-634
    • /
    • 1993
  • Dielectric and electrostrictive properties of 0.99Pb(Mg1/3Nb2/3)O3-0.01Pb(Mn2/3W1/3)O3 system using KCl-NaCl salts have been investigated as a function of the amount of excess MgO. For the specimens calcined at $700^{\circ}C$ for 1h and then sintered at 115$0^{\circ}C$ for 4h, the perovskite phase and the relative density were about 98% and 95%, respectively. With the addition of excess MgO up to 10mol%, the dielectric constant and the electrostrictive strain increased due to the increase of density and grain size, and these properties were degraded by the further addition of excess MgO. For the 10mol% excess MgO added specimen, the maximum electrostrictive strain, Xmax, and the electrostrictive coefficient, Q11, were 4.5$\times$10-4, 3.5$\times$10-2m4/C2, respectively. These results were correlated with the property of PMW and microstructure.

  • PDF

Microstructure and Dielectric Properties in $40Pb(Mg_{1/3}Nb_{2/3})O_3-30PbTiO_3-30Pb(Mg_{1/2}W_{1/2})O}3$ Ceramics with Excess $91PbO-9WO_3$ Addition ($91PbO-9WO_3$가 과잉첨가된 $40Pb(Mg_{1/3}Nb_{2/3})O_3-30PbTiO_3-30Pb(Mg_{1/2}W_{1/2})O}3$계 세라믹스의 미세구조와 유전특성)

  • 길영배;이응상
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.3
    • /
    • pp.281-288
    • /
    • 1997
  • The effects of 0 to 6 mol% excess 91PbO-9WO3 addition on the microstructure and the dielectric pro-perties in 40Pb(Mg1/3Nb2/3)O3-30PbTiO3-30Pb(Mg1/2W1/2)O3 ternary system were investigated. Excess 91PbO-9WO3 addition enhanced densification at relatively lower temperature due to the formation of liquid phase. The dielectric constant of the specimen with standard composition was 16,400 and that of specimen with 1 mol% excess additive was the maximum of 18,500. And more than 2 mol% excess addition decreased dielec-tric constant. Specimens with 2~4 mol% 91PbO-9WO3 addition showed dual peak maxima in the tem-perature dependence of dielectric constant. In the specimens which have more than 5 mol% excess addition a new phase with W-rich composition was formed at grain boundary.

  • PDF

Stbilization of Perovskite Phase and Enhanced DPT Characteristics of $Pb(Zn, Mg)_{1/3}Nb_{2/3}O_3-PbTiO_3$ Ceramics by the Additionof Excess Constituent Oxides ($Pb(Zn, Mg)_{1/3}Nb_{2/3}O_3-PbTiO_3$계에서 구성 산화물 첨가에 따른 Perovskite상 안정화 및 DPT성 증대 효과)

  • 이규만;장현명;유병두
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.11
    • /
    • pp.925-932
    • /
    • 1993
  • The perovskite phase in PZN-PMN-PT (Pb(Zn, Mg)1/3Nb2/3O3-PbTiO3) pseudoternary ceramics was stabilized by the addition of excess constituent divalent oxides (PbO, MgO and ZnO). The excess addition of 5mol% MgO or 7.5mol% PbO fully stabilized the perovskite phase. The enhanced diffuse phase transition (DPT) and the decrease in the electrical resistivity observed in the presence of excess ZnO or MgO were interpreted in terms of the additional formation of negatively charged, short-range ordered 1:1 domains with a concomitant generation of charge carriers, holes.

  • PDF

Electrical Properties of Pb(Mg1/3 Nb2/3)O3 Ceramics (Pb(Mg1/3 Nb2/3)O3 세라믹스의 전기적 특성)

  • 강동헌;윤기현
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.5
    • /
    • pp.712-718
    • /
    • 1989
  • PMN ceramics with excess MgO addition in the range of 0 to 70m/o were prepared, and their electrical properties, such as dielectric constant, tan$\delta$, diffuseness coefficient, remanent polarization, coercive field and electrical conductivity were measured. Dielectric constant and remanent polarization increased with up to 5m/o excess MgO and then decreased presumely due to the precipitation of second phase, etc. Electrical conductivity slightly increased with the addition of excess MgO.

  • PDF

Effect of Excess PbO on Grain Growth and Densification of (65)Pb(${Mg_{1/3}}{Nb_{2/3}}$)$O_3$-(35)$PbTiO_3$ Ceramics ((65)Pb(${Mg_{1/3}}{Nb_{2/3}}$)$O_3$-(35)$PbTiO_3$의 입자성장과 치밀화에 미치는 과량 PbO의 영향)

  • Lee, Jong-Bong;Hur, Tae-Moo;Lee, Ho-Yong;Choi, Kyun;Kim, Doe-Yeon
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.7
    • /
    • pp.673-680
    • /
    • 2000
  • The effect of excess PbO(0, 1, 2, 4, and 8 mol%) on grain growth and densification of (65)Pb(Mg1/3Nb2/3)O3-(35)PbTiO3 [mol%] ceramics has been investigaetd. With increasing the amount of excess PbO and sintering time, densities of sintered samples decreased gradually. The samples containing less than 1 mol% of PbO showed normal grain growth behavior, however abnormal grain growth was observed to occur in the samples with more than 2 mol% of PbO. In the samples with more than 2 mol% of PbO, the number of abnormal grains decreased and thus the average grain size became smaller with increasing the amount of excess PbO. These results demonstrated that the abnormal grain growth started to occur when a critical amount of excess PbO was added to a (65)Pb(Mg1/3Nb2/3)O3-(35)PbTiO3 sample. Since PMN-PT grains in a liquid matrix were angular, the observed abnormal grain growth was explained to proceed through the two dimensional nucleation process.

  • PDF

Microstructure and Dielectric Properties in $30Pb(Mg_{1/3}Nb_{2/3})O_3-20PbTiO_3-50Pb(Mg_{1/2}W_{1/2})O_3$ Ceramics with Excess MgO Addition (MgO가 과잉첨가된 $30Pb(Mg_{1/3}Nb_{2/3})O_3-20PbTiO_3-50Pb(Mg_{1/2}W_{1/2})O_3$계 세라믹스의 미세구조와 유전특성)

  • 길영배;이응상
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.1
    • /
    • pp.31-36
    • /
    • 1997
  • The effects of 0 to 10mol% excess MgO addition on the microstructure and dielectric properties in 30Pb(Mg1/3Nb2/3)O3-20PbTiO3-50Pb(Mg1/2W1/2)O3 ternary system were investigated. Samples were prepared by mixed oxide and precursor methods to compare the role of excess MgO. Excess MgO enhanced grain growth and increased dielectric constant. The dielectric constant and tesmperature dependence of dielectric constant of the sample sintered at 100$0^{\circ}C$ with 5mol% MgO were above 5,000 and +25% to -50% from - 55$^{\circ}C$ to 1$25^{\circ}C$, respectively. For these specimens the phases percent were mainly perovskite and Pb2WO5, which was confirmed by XRD analysis. Also the amount of cubic pyrochlore Pb3Nb4O13 and PbWO4 were de-creased with sintering temperature and MgO addition. BSE image showed the chemical inhomogeneous dis-tribution. Crystal phase formed at each sintering temperature and the chemical inhomogeneous distribution caused the decrease of the temperature dependence of dielectric constant.

  • PDF

The Study of the Properties of $Pb(Mg_{0.15} W_{0.15})Ti_{0.35}-Zr_{0.35}O_3$ Ceramics Modified with $La_2O_3$, $Nb_2O_5$ and $Al_2O_3$ (첨가제에 따른 $Pb(Mg_{1/2} W_{1/2}) O_3-PbTiO_3-ObZrO_3$ 고용체의 특성에 대한 연구)

  • 안영필;황학인;홍진녕
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.2
    • /
    • pp.17-24
    • /
    • 1985
  • In the composition of $Pb(Mg_{0.15} W_{0.15})Ti_{0.35}-Zr_{0.35}O_3$ the effect of particle size on PbO vaporization were measured, . The initial step of discontinuous vaporization of unreated PbO during the calcining process was depended on the particle size. All additives $La_2O_3Nb_2O_5$ and $Al_2O_3$ inhibited the grain growth of the composition $Pb(Mg_{0.15} W_{0.15})Ti_{0.35}-Zr_{0.35}O_3$ +2wt% excess PbO. The dielectric and piezoelectric properties of the composition $Pb(Mg_{0.15} W_{0.15})Ti_{0.35}-Zr_{0.35}O_3$ were improved by the addition of 2wt% excess PbO and proper additive. The electromechanical planar coupling factor of 0.65 and mechnical quality factor of 390 could be obtained by adding 5wt% $Nb_2O_5$ to the composition 2wt% excess PbO+$Pb(Mg_{0.15} W_{0.15})Ti_{0.35}-Zr_{0.35}O_3$.

  • PDF