• 제목/요약/키워드: Equiaxed Microstructure

검색결과 130건 처리시간 0.026초

Ti-6Al-4V 합금의 조직 변화에 따른 프레팅 피로거동 (The Fretting Fatigue Behavior of Ti-6Al-4V Alloy on Change of Microstructure)

  • 배용탁;최성종;권재도
    • 대한기계학회논문집A
    • /
    • 제29권4호
    • /
    • pp.584-590
    • /
    • 2005
  • The effect of microstructure on mechanical behavior for Ti-6Al-4V alloy was studied. Two different kinds of specimens are prepared using heat treatments (rolled plate, $1050^{\circ}C)$ in order to Produce different microstructures. Various kinds of mechanical tests such as hardness, tensile, fatigue and fretting fatigue tests are performed for evaluation of mechanical properties with the changes of microstructures. Through these tests, the following conclusions are observed: 1) Microstructures are observed as equiaxed and $widmanst{\ddot{a}}ten$ microstructures respectively. 2) Impact absorbed energy is superior for the equiaxed microstructure, and the hardness and tensile strength are superior for the $widmanst{\ddot{a}}ten$ microstructure. 3) The fatigue endurance of $widmanst{\ddot{a}}ten$ microstritcture shows higher value than that of the equiaxed microstructure. 4) The fatigue endurance in fretting condition was reduced about $50{\%}$ from that of the non-fretting condition.

티타늄 합금(Ti-6Al-4V)의 조직변화에 따른 기계적 특성 평가 (The Evaluation of Mechanical properties on the Changes of Microstructure for Titanium Alloy (Ti-6Al-4V))

  • 권재도;배용탁;최성종
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.135-140
    • /
    • 2000
  • The characteristics of mechanical behavior were estimated for Ti-6Al-4V alloy with four kinds of microstructure prepared with heat treatments. For this study, impact test, tensile test and fatigue crack growth test were performed, and then compared mechanical properties on the four microstructures. Furthermore, for quantitative evaluation, fractal dimensions of crack pass were obtained using the box counting method. The main results obtained are summarized as follows. (1) The microstructures exhibited equiaxed microstructure, bimodal-microstructure and lamellar microstructure by heat treatment. (2) The impact absorbed energy and elongation is superior in the bimodal-microstructure, and the hardness and tensile strength are superior in the lamellar microstructure. (3) The fatigue crack growth rate is similar to all microstructures in the low ${\Delta}K$ region. The fatigue crack growth rate of equiaxed microstructure is fastest, and that of lamellar microstructure is lowest in the high ${\Delta}K$ region. (4) The fractal dimension D of lamellar microstructure is higher then that of the equiaxed microstructure and bimodal microstructure.

  • PDF

티타늄 합금(Ti-6Al-4V)의 조직변화에 따른 기계적 특성 평가 (The Evaluation of Mechanical Properties on the Changes of Microstructure for Titanium Alloy (Ti-6Al-4V))

  • 권재도;배용탁;최성종
    • 대한기계학회논문집A
    • /
    • 제26권4호
    • /
    • pp.609-616
    • /
    • 2002
  • The characteristics of mechanical behavior are investigated for Ti-6Al-4V alloy. Four kinds of the specimens are prepared under different heat treatments in order to produce different microstructures. In the present investigations, impact, tensile and fatigue crack growth tests are performed for each test specimen. The results obtained through the investigations are compared. Additionally fr actal dimensions of crack pass are obtained using the box counting method. The results are, 1) the microstructures shows as equiaxed, bimodal and Widmanstatten microstructures respectively, 2) the impact energy and elongation are superior fur the bimodal microstructure, and the hardness and tensile strength are superior fur the Widmanstatten microstructure, 3) the fatigue crack growth rate is similar to all microstructures in low ΔK region while that of equiaxed microstructure is the largest, and that of Widmanstatten microstructure is the lowest in high ΔK region respectively, 4) the fractal dimension D of Widmanstatten microstructure shows higher value than that of the equiaxed and bimodal microstructures under 200 magnification view of the SEM micrographs.

Ti-6Al-4V 합금의 미세조직에 따른 정적 및 동적 변형에 관한 연구 (The Effect of Microstructure on the Static and Dynamic Deformation Behavior of Ti-6Al-4V Alloy)

  • 이동근;이유환;이성학;허선무;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 추계학술대회 논문집
    • /
    • pp.277-280
    • /
    • 2001
  • The effects of a -phase morphology on the static and dynamic deformation behavior of a Ti-6Al-4V alloy was investigated in this study. Static tension test, static and dynamic tension test and hot compression test were conducted on three microstructures of Ti-6Al-4V alloy, i.e., equiaxed, widmanstatten and bimodal microstructures. Fracture surfaces of all three microstructures represented ductile fracture appearance, though the formation of adiabatic shear bands was noticed at dynamic torsion test. The susceptibility of forming adiabatic shear bands was greatest in the equiaxed microsoucture and lowest in the bimodal microstructure, which was evidenced by hot compression test.

  • PDF

Ti-6AI-4V 합금의 ECAP 가공에 따른 미세조직의 변화 (Microstructural Evolution during the Equal Channel Angular Pressing of Ti-6Al-4V Alloy)

  • 고영건;정원식;신동혁;이종수
    • 소성∙가공
    • /
    • 제11권6호
    • /
    • pp.519-528
    • /
    • 2002
  • The microstructural evolution during the equal channel angular pressing of Ti-6Al-4V alloy was investigated using the transmission electron microscopy (TEM). ECA pressing was carried out isothermally with route C at $600^{\circ}C$ for two types of initial microstructure, i.e., equiaxed and Widmanstatten microstructures. At an initial stage of ECA pressing, the equiaxed microstructure showed more uniform flow than the Widmanstatten microstructure. However, both microstructures were significantly refined revealing nearly equiaxed grains of 0.3$mu extrm{m}$ in diameter with high angle grain boundaries after 4 passes of ECA pressing. These ultrafine gains were found to be stable with little grain growth, when annealed up to $600^{\circ}C$ for 1hr.

Ti-6Al-4V 합금의 고온성형 시 미세조직 예측에 관한 연구 (Prediction of microstructure during high temperature forming of Ti-6Al-4V alloy)

  • 이유환;신태진;황상무;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 춘계학술대회논문집
    • /
    • pp.57-60
    • /
    • 2003
  • The purpose of this study is to investigate the high temperature deformation behavior of Ti-6Al-4V alloy and to predict the final microstructure under given forming conditions. Equiaxed and widmanstatten of Ti-6Al-4V alloys were prepared as initial microstructure and the compression tests were performed to obtain the flow curves at high temperatures (700∼1100$^{\circ}C$) and various strain rates (10$\^$-4/∼10$^2$/s). Form the results of compression test various parameters such as strain rate sensitivity (m) and activation energy (Q) were calculated and used to establish constitutive equations. To predict the final microstructure after forming, finite element analysis was performed considering the microstructural parameters such as the grain size and the volume fraction of second phase.

  • PDF

Ti-6A1-4V 합금의 피로거동에 미치는 온도, 주파수 및 미세조직의 영향 (The Effect of Temperature, Frequency and Microstructure on Fatigue Crack Propagation in Ti-6A1-4V Alloy)

  • 김현철;김승한;임병수;김두현;이용태
    • 한국자동차공학회논문집
    • /
    • 제4권1호
    • /
    • pp.198-207
    • /
    • 1996
  • The effect of temperature, frequency and microstructure on fatigue crack propagation property of Ti-6A1-4V alloy has been investigated. The temperatures employed were room temperature, 20$0^{\circ}C$ and 40$0^{\circ}C$. The frequencies were 20Hz and 8 Hz. The microstructures tested were equiaxed and bimodal microstructures. Mechanical properties and fatigue crack growth rates were measured in different test conditions. From the experimental results, following conclusions were obtained. Bimodal microstructure showed superior fatigue crack growth resistance to equiaxed microstructure. Under all test conditions, fatigue crack growth rate increased with test temperature. Wine the frequency decreasing from 20Hz to 8Hz, fatigue crack growth rate increased.

  • PDF

석고 몰드에서 용출된 Ca이 주입성형 알루미나 소결체의 미세구조 및 파괴인성에 미치는 영향 (Effects of Dissolved Ca from Plaster Mold During Slip Casting on the Microstructure and Fracture Toughness of Sintered Alumina)

  • 박재관;임동기;김인태;김윤호
    • 한국세라믹학회지
    • /
    • 제28권12호
    • /
    • pp.1019-1025
    • /
    • 1991
  • The effect of dissolved Ca ion from plaster mold during slip casting on the microstructure and fracture toughness of high-purity sintered alumina were investigated. When the alumina slip containing 1000 ppm MgO was casted on a calcined alumina mold, the sintered compact had a homogeneous microstructure with equiaxed grains. However, when the same slip was casted on a plaster mold, the sintered compact consisted of the mixture of equiaxed and elongated grains. This inhomogeneous microstructure was also observed in the sintered alumina doped with 100o ppm MgO and 100 ppm CaO whose compact was prepared on the calcined alumina mold indicating that the inhomogeneity was caused by CaO. It was found that the specimen containing both MgO and CaO had higher fracture toughness than that containing MgO only. The enhanced fracture toughness by CaO is probably due to the crack deflection along the boundaries of the elongated grains.

  • PDF

상압소결에 의하여 제조된 SiC-AlN 세라믹스의 상 및 미세구조 (Phase and Microstructure of SiC-AlN Ceramics Prepared by Pressureless Sintering)

  • 최웅;이종국;조덕호;김환
    • 한국세라믹학회지
    • /
    • 제32권11호
    • /
    • pp.1308-1314
    • /
    • 1995
  • Changes in phase and microstructure were investigated in the SiC-AlN ceramics prepared by pressureless sintering using yttrium aluminum garnet (YAG) as a sintering aid at 200$0^{\circ}C$ and 210$0^{\circ}C$. The SiC/AlN ratio made a remarkable difference in densification, phase relations and the morphology of grains. In the AlN-rich composition, major phase was 2H and microstructure was composed of the densified equiaxed grains irrespective of the sintering temperatures. While those sintered at 200$0^{\circ}C$ were porous with major phase being 3C, the rod-like and the equiaxed grains were coexisted when sintered at 210$0^{\circ}C$ in the SiC-rich composition.

  • PDF

Ti-6Al-4V 합금의 고온성형시 미세조직 예측에 관한 연구 (Prediction of Microstructure During High Temperature Forming of Ti-6Al-4V Alloy)

  • 이유환;신태진;황상무;박노광;심인옥;이종수
    • 소성∙가공
    • /
    • 제12권4호
    • /
    • pp.290-295
    • /
    • 2003
  • High temperature deformation behavior and prediction of final microstructure after forming of Ti-6Al-4V alloy were investigated in this study. Equiaxed and Widmanstatten microstructures of Ti-6Al-4V alloys were prepared as initial microstructures and compression tests were performed to obtain the flow curves at high temperatures (700∼110$0^{\circ}C$) and various strain rates (10$^{-4}$ ∼10$^2$/s). From the results of compression test, strain rate sensitivity (m) and activation energy (Q) were calculated and used to establish constitutive equation. To predict the final microstructure after farming, finite element analysis was performed considering the microstructural parameters such as grain size and volume fraction of second phase.