Effect of mach peening treatment on fatigue crack growth retardation in structural steel alloy (마하피닝 처리에 의한 기계구조용 합금강의 피로균열전파 지연효과)

  • Kim, Min-Gun;Lim, Bok-Kyu;Park, Hong-Ki;Hwang, Jung-Gak
    • Journal of Industrial Technology
    • /
    • v.26 no.A
    • /
    • pp.69-73
    • /
    • 2006
  • Mach peening treatment is one of the various kinds of techniques to improve the fatigue properties. The mach peening process gives high-level work hardening and compressive residual stress near the surface layer, improving the fatigue strength. In addition, this treatment reduces slip bands that initiate the fatigue cracks near the surface. During impingement, a plastic indentation surrounded by a plastic zone is formed. Mach peening treatment characteristic is less energy consumption and is an environmental friendly processing methods that is not accompanied by pollution. It is machining process that can prevent fatigue fracture beforehand in structure using already as well as process of production. The test results showed that fatigue crack propagation delay appeared by drilling type 43%, mach peening type 110%.

  • PDF

P wave Velocity Variation of the Pochon Granite due to the Cyclic Loadings (압축피로에 의한 포천화강암의 P파속도 변화 특성)

  • Kim, Yeong Hwa;Jang, Bo-An;Kim, Jae Dong;Rhee, Chan Goo;Moon, Byeung Kwan
    • Economic and Environmental Geology
    • /
    • v.30 no.3
    • /
    • pp.231-240
    • /
    • 1997
  • The behavior of rocks and microcrack development due to fatigue stresses are investigated using cyclic loading tests and ultrasonic velocity measurements. Twenty six medium-grained granite samples from the Pochon area are selected for measurements. Ultrasonic velocities are measured for samples before fatigue test to characterize the pre-existing microcracks. Then, thirteen different cycles of loadings with 70% and 80% dynamic strength are applied to the samples. The ultrasonic velocities are measured again to compare velocities after applications of fatigue stress with those before applications of fatigue stress. The results show that most microcracks are developed along the direction parallel to the axis of loading and that the amount of microcracks increases, as loading levels and numbers of cycle increase.

  • PDF

Uniaxial fatigue, creep and stress-strain responses of steel 30CrNiMo8

  • Brnic, Josip;Brcic, Marino;Krscanski, Sanjin;Lanc, Domagoj;Chen, Sijie
    • Steel and Composite Structures
    • /
    • v.31 no.4
    • /
    • pp.409-417
    • /
    • 2019
  • The choice of individual material for industrial application is primarily based on knowledge of its behavior in similar applications and similar environmental conditions. Contemporary design implies knowledge of material behavior and knowledge in the area of structural analysis supported by large capacity computers. Bearing this in mind, this paper presents and analyzes the experimental results related to the mechanical properties of the material considered (30CrNiMo8/1.6580/AISI 4340) at different temperatures as well as its creep and fatigue behavior. All experimental tests were carried out as uniaxial tests. The test results related to the mechanical properties are presented in the form of engineering stress-strain diagrams. The results related to the creep behavior of the material are shown in the form of creep curves, while the fatigue of the material is shown in the form of stress - life (S - N) diagram. Based on these experimental results, the values of the following properties are determined: ultimate tensile strength (${\sigma}_{m,20}=696MPa$), yield strength (${\sigma}_{0.2,20}=355.5MPa$), modulus of elasticity ($E_{,20}=217GPa$) and fatigue limit (${\sigma}_{f,20,R=-1}=280.4MPa$). Results related to fatigue tests were obtained at room temperature and stress ratio R = -1.

Properties of Fatigue Crack Initiation and Arrest in Structural Steel Under Acid Fog (산성안개 하의 구조용강에서 피로균열의 발생 및 정류특성)

  • Kim, Min-Geon;Kim, Jin-Hak;Kim, Myeong-Seop;Ji, Jeong-Geun;Gu, Eun-Hoe
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.2
    • /
    • pp.374-379
    • /
    • 2002
  • Corrosion fatigue tests were carried out to clarify the influence of acid fog as environmental factor on the fatigue strength of SM55C using rotary bending fatigue tester. The fatigue strength of acid fog specimen extremely decreased about 80% compared to that of distilled water specimen. In acid fog environment, a number of cracks commenced at corrosion pit and coalesced with the adjacent cracks during they propagate, and they formed a single non-propagating circumferential crack under the endurance stress of N=5$\times$10$\^$7/ cycles. Also, the depth of the crack is smaller than that of normal fatigue crack, so the crack has a veil small aspect ratio. The reason of this peculiar crack growth characteristics is that the crack opening-closure behaviors are hindered by corrosion products on the surface crack faces, and hence it is thinkable that the strong corrosion action like anodic dissolution for crack growth in depth direction is weaker compared with surface, resulting from faint pumping action of crack during loading-shedding processes.

Partial-interaction fatigue assessment of stud shear connectors in composite bridge beams

  • Seracino, Rudolf;Oehlers, Deric J.;Yeo, Michael F.
    • Structural Engineering and Mechanics
    • /
    • v.13 no.4
    • /
    • pp.455-464
    • /
    • 2002
  • There is a growing demand to assess the remaining strength and endurance of existing composite steel and concrete bridge beams due to the aging infrastructure, increases in permissible vehicle weights and increases in their frequencies. As codes are generally dedicated to the design of new structures, new procedures are required to aid in the assessment of existing bridges to ensure that they are utilised to the full. In this paper, simple expressions are presented to perform partial-interaction analyses directly from full-interaction analyses, so that the beneficial effect of partial-interaction on the shear forces on the shear connectors can be utilised in assessment to extend the fatigue life of simply supported bridge beams and to determine the effect of remedial work if necessary. Use of the assessment technique is described by way of an illustrative example.

Comparative study on the structural behavior of a transition piece for offshore wind turbine with jacket support

  • Ma, Chuan;Zi, Goangseup
    • Steel and Composite Structures
    • /
    • v.43 no.3
    • /
    • pp.363-373
    • /
    • 2022
  • As a key reinforcement connection between a tower and a substructure in offshore wind turbine system, the transition piece is inevitably subjected to cyclic dynamic environmental loads such as wind, current and wave. Therefore, well designed transition piece with high strength and good fatigue resistance is of great significance to the structural safety and reliability of offshore wind power systems. In this study, the structural behavior of the transition piece was studied by an extensive sets of finite element analyses. Three widely used types of transition piece were considered. The characteristics of stress development, fatigue life and weight depending on the type of the transition piece were investigated in the ultimate limit state (ULS) and the fatigue limit state (FLS) of a 5-MW offshore wind turbine to be placed in Korea. An optimal form of the transition piece was proposed based on this parametric study.

A Study on the Fatigue Strength of the Welded Joints in Steel Structures(I) (강구조물(鋼構造物)의 용접연결부(鎔接連結部)의 피로강도(疲勞强度)에 관한 연구(研究)(I))

  • Park, Je Seon;Chang, Dong Il;Chung, Yeong Wha
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.5 no.3
    • /
    • pp.161-175
    • /
    • 1985
  • The simplified method drawing the S-N curves in welding joints of the cover plates, the transverse stiffners and the gusset plates of the plate girders by calculation and its computer program without the direct fatigue tests, was established. And the method was applied to the Young- Dong Great Bridge, the 3 th Han River Bridge and the Kang Chon Bridge. Before this, SS 41, SS 50, SWS 50 and SWS 58 were selected, then the compact tension specimens were made by the use of these materials, the things welded by these materials transversely and the ones longitudinally to the crack propagation direction. The fatigue tests were performed by the use of these 'specimens, and the values of material constants c and m were obtained. By these results the followings were obtained. It was showed that the fatigue: strength in the case of the cover plates was much lower than in the case of other two cases. It was showed that, in the case of the cover plates with the cover plates thicker the fatigue strength was lower, but besides this the fatigue strength was not much influenced by the size of specimens. It was showed that in the difference from this the fatigue strength was sensitively influenced by the values of c and m. It was showed that in accordance with the lower values of c and m the fatigue strength was fairly higher, in accordance with the lower values of m the gradient of the S-N curves was abrupter. It was considered that if such data were accumulated continuously, in the near future the basic pattern used availably in providing the indicater of the fatigue design of the plate girders, and presuming the life-proof of the existing plate girders.

  • PDF

Performance Evaluation of Cold-Recycling Asphalt Mixtures with an Inorganic Additive (무기질 첨가제를 사용한 상온 재활용 아스팔트 혼합물의 공용성 평가)

  • Kim, kyungsoo;Kim, HyunKyum;Kim, WonJae;Park, ChangKyu;Lee, HyunJong
    • International Journal of Highway Engineering
    • /
    • v.20 no.1
    • /
    • pp.27-33
    • /
    • 2018
  • PURPOSES : The purpose of this study is to estimate the optimum content of an inorganic additive for cold-recycled asphalt mixtures and evaluate its performance. METHODS : An indirect tensile test, a tensile-strength ratio test, and an indirect tensile-fatigue test were conducted on cold-recycling asphalt mixtures with various additives. RESULTS : The laboratory performance tests indicated that granulated blast-furnace slag mixed with inorganic and cement activators provided optimum performance. The performance results of the cold-recycled asphalt pavement were similar to the inorganic and cement activators' performance in terms of the indirect tensile strength, tensile strength ratio, and indirect tensile-fatigue test. CONCLUSIONS : Overall, the performance of a cold-recycled asphalt mixture using inorganic additives and emulsion asphalt was comparable to a warm-recycled asphalt mixture. However, more experiments aimed at improving its performance and studying the effect of the inorganic additives must be conducted.

A Study on Fatigue Behavior of Two-Span Fiber Reinforced Concrete Beam (강섬유 보강 철근콘크리트 2경간 연속보의 피로거동에 관한 연구)

  • Kwak, Kae-Hwan;Cho, Seon-Jeong;Seok, In-Soo
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.2
    • /
    • pp.163-172
    • /
    • 2003
  • As concrete structures are getting larger, higher, longer, and specialized, it is more required to develop steel fiber concrete and apply to the real world. In this research, it is aimed to have fatigue strength examined, varying the steel fiber content by 0%, 0.75%, 1.00%, 1.25%, by experimental study of Two-spans Beam with Steel Fibrous with repeated loads. The ultimate load and the initial load of flexural cracking were measured by static test. In addition, the load versus strain relation, load versus strain relation, load versus deflection relation, crack pattern and fracture mode by increasing weight was observed. On the other hand, the crack propagation and the modes of fracture according to cycle number and the relation of cycle loading to deflection relation and strain relation was observed by fatigue test. As the result of fatigue test, Two-spans Beam without Steel Fibrous was failed at 60~70% of the static ultimate strength and it could be concluded that fatigue strength to two million cycle was around 67.2% by S-N curve. On the other hand, that with Steel Fibrous was failed at 65~85% of the static ultimate strength and it could be concluded fatigue strength to two million cycle around 71.7%.

A Study on Estimation of the Pavement fatigue Life by Loading (하중작용(荷重作用)에 의한 포장수명(鋪裝壽命)에 관한 연구(硏究))

  • Nam, Young Kug
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.9 no.4
    • /
    • pp.83-92
    • /
    • 1989
  • For many of the rigid pavements the observations of significantly different performances were explained to relate distress mechanisms to distress manifestation and to develope better prediction of performance. This paper summarizes the result of an investigation of the resilient elastic and fatigue behavior of inservice cement concrete pavements. Static indirect tensile tests were. conducted in order to estimate the average tensile strength of each of the projects Repeat-load indirect tensile tests were conducted to determine the fatigue and resilient elastic characteristics and the relationship between fatigue life and stress/strength ratio. Deformation measurements were taken during fatigue testing in order to determine the resilient elastic properties of the material and the changes in these properties during the test period.