인버터 서지와 온도스트레스 하에서 PAI/Nano Silica 에나멜와이어의 가속절연수명 평가 (Accelerated Insulation Life Estimation for PAI/Nano Silica Enamelled Wire under Inverter Surge and Temperature Stress)

  • 박재준
    • 전기학회논문지
    • /
    • 제65권10호
    • /
    • pp.1712-1720
    • /
    • 2016
  • AC and DC insulation breakdown voltage was studied for magnet wire coated with double layers of high flexural PAI layer and high anti-corona PAI/nanosilica (15 wt%) layer. The specimens were prepared at various drying temperatures (T/D): $22^{\circ}C$, $240^{\circ}C$, and $260^{\circ}C$, respectively. The increase effects of nanosilica on AC and DC insulation breakdown voltage were not so significant compared to that of magnet wire coil coated with original PAI. And the AC and DC insulation breakdown voltage was improved by decreasing diameter of winding coil. As T/D temperature increased, AC and DC insulation breakdown voltage decreased.

인버터 서지와 온도 스트레스 하에서 Magnet Wire 절연 수명평가 (Insulation Life Estimation for Magnet Wire Under Inverter Surge and Temperature Stress)

  • 박재준
    • 한국전기전자재료학회논문지
    • /
    • 제29권10호
    • /
    • pp.641-646
    • /
    • 2016
  • Coil specimen was prepared by coating a copper wire with two varnish thin layers: the first was polyamideimide (PAI)/nanosilica (5 wt%) varnish and the second was anti-corona PAI/nanosilica (15 wt%) varnish. Insulation breakdown voltage was investigated under inverter surge condition at $20^{\circ}C$, $70^{\circ}C$, $100^{\circ}C$, $150^{\circ}C$, $200^{\circ}C$, $250^{\circ}C$, respectively. The insulation lifetime of the two layered coil was tens of times longer than that of original PAI coil. And the insulation lifetime decreased with increasing ambient temperature because there was weak binding strength between copper and varnish layer.