Dielectric and Piezoelectric Properties of (Na,K)$NbO3 Ceramics as a Function of SrTiO3 Substitution (SrTiO3 치환에 따른 (Na,K)NbO3계 세라믹스의 유전 및 압전특성)

  • Lee, Sang-Ho;Yoo, Ju-Hyun;Lee, Yeu-Yong;Song, Hyun-Seon;Mah, Suk-Burm;Kim, Seong-Goo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.6
    • /
    • pp.484-488
    • /
    • 2009
  • In this study, in order to develop the lead-free piezoelectric ceramics with high piezoelectric and dielectric properties, $[(K_{0.5}Na_{0.5})_{0.95}Li_{0.05}(Nb_{0.96}Sb_{0.04})]O_3$ ceramics were fabricated using $Ag_2O$ as sintering aid and a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $SrTiO_3$ substitution. $SrTiO_3$ substitution enhanced density, dielectric constant(${\varepsilon}_r$) and electromechanical coupling factor($k_p$). However, mechanical quality factor was deteriorated. And also, Curie temperature ($T_c$), and phase transition temperature($T_p$) were rapidly decreased. At the 0.5 mol% $SrTiO_3$ substitution, density, electromechanical coupling factor($k_p$), dielectric constant(${\varepsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum value of $4.437\;g/cm^3$, 0.457, 1294, 265 pC/N, respectively.

Piezoelectric Properties of Pb-free Bi(Na,K)TiO3-SrTiO3 Ceramics with the Amount of La2O3 Addition (La2O3첨가에 따른 무연 Bi(Na,K)TiO3-SrTiO3 세라믹스의 압전 특성)

  • 류주현;이현석;박창엽;정광현;이덕출;정영호;홍재일
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.8
    • /
    • pp.830-834
    • /
    • 2004
  • In this study, lead-free pirzoelectric ceramics were investigated for pressure sensor applications as a function of the amount of ${La}_2{O}_3$ addition at $Bi(Na, K)Ti{O}_3-SrTi{O}_3$system. With increasing the amount of addition, the density and dielectric constant increased up to 0.9 wt% ${La}_2{O}_3$ addition and decreased above 0.9 wt% ${La}_2{O}_3$addition. Electromechanical coupling factor( $K_{P}$) showed the maximum value at 0.2 wt% ${La}_2{O}_3$addition and decreased above 0.2 wt% ${La}_2{O}_3$ addition. Electromechanical coupling $factor{(K)}_P$, density, dielectric constant$(\varepsilon_\Gamma)$, piezoelectric constant$(d_33)$ and curie temperature$(T_C)$ showed optimum value of 0.40, 5.75 g/㎤, 768, 215 pC/N and 320 $^{\circ}C$ at 0.2 wt%${La}_2{O}_3$addition, respectively.

"Lead-free" Piezoelectric Ba(Ti0.94Zr0.06)O3 Single Crystals with Electromechanical Coupling Factor (k33) Higher Than 0.8 (0.8 이상의 전기기계결합계수(k33)를 가지는 고효율 무연 압전 Ba(Ti0.94Zr0.06)O3 단결정)

  • Lee, Jong-Yeb;Oh, Hyun-Taek;Lee, Ho-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.6
    • /
    • pp.623-628
    • /
    • 2014
  • Orthorhombic $Ba(Ti_{0.94}Zr_{0.06})O_3$ single crystals are fabricated using the cost-effective solid-state single crystal growth (SSCG) method; their dielectric and piezoelectric properties are also characterized. Measurements show that (001) $Ba(Ti_{0.94}Zr_{0.06})O_3$ single crystals have an electromechanical coupling factor ($k_{33}$) higher than 0.83, piezoelectric charge constant ($d_{33}$) of about 400 [pC/N], and piezoelectric voltage constant ($g_{33}$) higher than 50 [${\times}10^{-3}Vm/N$]. The transition temperature ($T_{OT}$) of the (001) $Ba(Ti_{0.94}Zr_{0.06})O_3$ single crystals between orthorhombic and tetragonal phases is also observed to be about $61^{\circ}C$. Because their electromechanical coupling factor ($k_{33}$) and piezoelectric voltage constant ($g_{33}$) are higher than those of soft PZT ceramics, it is expected that (001) $Ba(Ti_{0.94}Zr_{0.06})O_3$ single crystals can be used as "lead-free" piezoelectric materials in many piezoelectric applications.

A Study on the Dielectric and Piezoelectric Properties of xPb($Y_{1/2}Ta_{1/2})O_3-(1-x)Pb(Zr_{0.52}Ti_{0.48})O_3$Ceramics (xPb($Y_{1/2}Ta_{1/2})O_3-(1-x)Pb(Zr_{0.52}Ti_{0.48})O_3$ 세라믹스의 유전 및 압전 특성에 관한 연구)

  • 강도원;김태열;김범진;김명호;박태곤
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.294-296
    • /
    • 1999
  • Solid solution ceramics having various ratios between xPb( $Y_{1}$2/T $a_{1}$2/) $O_3$ and Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$were synthesized by a conventional solid state reaction for well sintered specimens, dielectric and piezoelectric prperties were studied as a function of composition. The dielectric constant of PYT-PZT ceramics of 4 mol% PYT was 1,424 at room temperature. The maximum value of electromechanical couping facotr $k_{p}$ of 51% $k_{t}$ of 30% were obtained at the composition of 4 mol% PYT, howerver mechanical quality factor( $Q_{m}$) had a minimum value of 69 at 4 mol% PYT. Also the maximum value of piezoelectric constant of $D_{33}$(310[pC/N]) and $d_{31}$(-131[pC/N]) were obtained at the composition of 4 mol% PYT content.ntent.t.t.t.

  • PDF

The Piezoelectric and Dielectric Properties of PZT-PMN Ceramics (PZT-PMN 압전 세라믹의 압전 및 유전 특성)

  • Lee, J.S.;Lee, Y.H.;Hong, J.K.;Jeong, S.H.;Chai, H.I.;Lim, K.J.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05c
    • /
    • pp.131-134
    • /
    • 2001
  • In this paper, the piezoelectric and dielectric properties as a function of x and a in $aPbZr_xTi_{1-x}O_3-(1-a)Pb(Mn_{1/3}Nb_{2/3})O_3$ + ywt%MgO is investigated. As a results, when a is 0.95 and x is 0.505, electromechanical coupling factor$(k_p)$, permittivity${\varepsilon}_33^T/{\varepsilon}_0$, piezoelectric strain constant$(d_{33})$ and mechanical quality factor$(Q_m)$ are 58 %, 1520, 272 pC/N and 1550, respectively. From XRD analysis, when x is 0.505, it is MPB which present rhombohedral and tetragonal phase in same quantity. Also, From SEM observation, when sintering temperature is $1150^{\circ}C$, grain size is about $2\;{\mu}m$. As a results added MgO dopant in the ternary piezoelectric ceramic, when MgO content is 0.1 wt%, $k_p$ increases to 63[%].

  • PDF

Piezoelectric and Dielectric Characteristics of PAN-PZT Ceramics with BaCO3Addition (BaCO3첨가량에 따른 PAN-PZI계 세라믹스의 압전 및 유전특성)

  • 박타리;이동균;최지원;강종윤;김현재;윤석진;고태국
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.4
    • /
    • pp.356-360
    • /
    • 2002
  • The piezoelectric properties of $0.05Pb(Al_{0.5}Nb_{0.5})O_3-0.95Pb(Zr_{0.52}Ti_{0.48})O_3+0.7wt%Nb_2O_5+o.5wt%MnO_2$ ceramics with the additive of BaCO$_3$were investigated. As the addition of BaCO$_3$increased from 0 to 0.4 wt%, the dielectric constant ($\epsilon^T _{33}$), piezoelectric constant ($d_33$), electromechanical coupling factor ($k_p$), and mechanical quality factor ($Q_m$) increased, while the dielectric loss ($tan\delta$) decreased. The highest piezoelectric and dielectric properties were observed at $1200^{\circ}C$ of the sintered temperature with 0.4 wt% of $BaCO_3$, and the properties of $d_33$, $k_p$, and $Q_m$ were 339 pC/N, 60% and 1754, respectively.

The Characteristics of PZ-PT PMN Piezoelectric Ceramics for Application to High Power Device (고출력 압전 디바이스 응용을 위한 PZ-PT-PMN계 압전 세라믹의 특성)

  • ;洪鍾國
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.49 no.3
    • /
    • pp.156-156
    • /
    • 2000
  • The piezoelectric properties and the doping effect for $0.95Pb(Zr_xTi_{l-x})O_3+0.O5Pb(Mn_{1/3}Nb_{2/3})O_3$compositions were studied. Also, the heat generation and the change of electromechanical characteristics, the important problem in practical usage, were investigated under high electric field driving. As a experiment results under low electric field, the value of $k_p$ and ${\varepsilon}_{33}^T$ were maximized, but $Q_m$ was minimized $(k_p=0.57, Q_m=1550)$ in the composition of x=0.51. In order to increase the values of $Q_m$, $Nb_2O_5$ was used as a dopant. As the result of that, the grain size was suppressed and the uniformity of grain was improved. Also, the values of $k_p$ decreased, and the values of $Q_m$ increased with doping concentration of $Nb_2O_5$ . As a experiment results under high electric field driving, when vibration velocity was ower than 0.6[m/s], the temperature increase was 20[℃], and the change ratio of mechanical quality factor was less than 10[%]. So, its electromechanical characteristics was very stable. Conclusively, piezoelectric ceramic composition investigated at this paper is suitable for application to high power piezoelectric devices.

Sensitivity Properties of Acoustic Emission Sensor Using NKN System Ceramics (NKN계 세라믹을 이용한 음향방출 센서의 감도 특성)

  • Hong, Jae-Il;Shin, Sang-Hoon;Yoo, Ju-Hyun;Jeong, Yeong-Ho;Lee, Sang-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.11
    • /
    • pp.696-701
    • /
    • 2014
  • In this study, in order to develop coupled vibration mode piezoelectric devices for Acoustic Emission (abbreviated as AE) sensor application with outstanding displacement and piezoelectric properties have been simulated by ATILA FEM program. And, From the results of ATILA simulation, the AE sensor specimen, obtained superior electromechanical coupling factor and displacement, when the size of specimen is $3.45mm{\Phi}{\times}3.45mm$ with ratio of diameter/thickness(${\Phi}/T$)= 1.0. Therefore, AE sensor was fabricated by (Na,K,Li)(Nb,Ta) $O_3$(abbreviated as NKL-NT) system piezoelectric ceramics using coupled vibration mode. The piezoelectric properties of NKL-NT ceramics was exhibited that piezoelectric constant($d_{33}$), piezoelectric voltage constant($g_{33}$) and electro mechanical coupling factor($k_p$) have the excellent values of 261[pC/N], 40.10[$10^{-3}Vm/N$], and 0.44, respectively. The manufactured piezoelectric device with ratio of ${\Phi}/T$= 1.0 indicated the optimum values of resonant frequency(fr)= 556.5[kHz], antiresonant frequency(fa)=631.1[kHz], and effective electromechanical coupling factor(keff)= 0.473. The maximum sensitivity of the coupled vibration mode AE sensor was 55[dB] at the resonant frequency of 75[kHz]. The results show that the coupled vibration mode piezoelectric device is a promising candidate for the application AE sensor piezoelectric device.

Dielectric and Piezoelectric Characteristics of (Na,K)NbO3 Ceramics System According to Sintering Time (소결시간변화에 따른 (Na,K)NbO3계 세라믹스의 유전 및 압전특성)

  • Kim, Do-Hyung;Yoo, Ju-Hyun;Kim, In-Sung;Song, Jae-Sung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.10
    • /
    • pp.901-905
    • /
    • 2008
  • In this study, $0.95(K_{0.5}Na_{0.5})NbO_{3}-0.05Li(Sb_{0.8}Nb_{0.2})O_{3}+0.2\;wt%Ag_{2}O$ were investigated as a variations of sintering times in order to improve dielectric and piezoelectric properties of lead-free piezoelectric ceramics. $Ag_{2}O$ were used as sintering aids and the specimens were sintered during 3, 5, 7, 9 and 11 hours, respectively. At the specimen sintered during 7 hour, Electromechanical coupling factor ($k_p$), density, dielectric constant (${\epsilon}_{\gamma}$), piezoelectric constant ($d_{33}$) and curie temperature ($T_c$) of composition ceramics showed the optimal value of 0.450, 4.274 $[g/cm^3]$, 1007, 257 [pC/N] and $396^{\circ}C$, respectively.

Characteristics of PAN-PZI Ceramics with $BaCO_3$Addition ($BaCO_3$ 첨가량에 따른 PAN-PZT계 세라믹스의 특성)

  • 박타리;이동균;최지원;김현재;윤석진;조봉희;고태국
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.981-984
    • /
    • 2001
  • The piezoelectric properties of 0.05pb(A $l_{0.5}$N $b_{0.5}$) $O_3$-0.95Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$+0.7wt%N $b_2$ $O_{5}$ +0.5wt%Mn $O_2$ceramics with the additives of BaC $O_3$were investigated. For the additions of BaC $O_3$, the dielectric constant ($\varepsilon$$^{T}$ $_{33}$ ), the piezoelectric constant ( $d_{33}$ ), the electromechanical coupling factor ( $k_{p}$ ), and . the mechanical quality factor ( $Q_{m}$ ) were increased, but dielectric loss (tan$\delta$) was decreased. The highest piezoelectric properties and dielectric properties were observed at the sintered temperature of 120$0^{\circ}C$ and 0.4 wt% of BaC $O_3$, and the properties of $d_{33}$ , $k_{p}$ , and $Q_{m}$ were 339(x10$^{-12}$ C/N), 59% and 1754, respectively.vely.y.y.