Enhancement of delamination strength in Cu-stabilized coated conductor tapes through additional treatments under transverse tension at room temperature

  • Shin, Hyung-Seop;Bautista, Zhierwinjay;Moon, Seung-Hyun;Lee, Jae-Hun;Mean, Byoung-Jean
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제19권2호
    • /
    • pp.25-28
    • /
    • 2017
  • In superconducting coil applications particularly in wet wound coils, coated conductor (CC) tapes are subjected to different type of stresses that could affect its electromechanical transport property. These include hoop stress acting along the length of the CC tape and the Lorentz force acting perpendicular to the CC tape's surface. Since the latter is commonly associated with the delamination problem of multi-layered REBCO CC tapes, more understanding and attention on the delamination phenomena induced in the case of coil applications are needed. Difference on the coefficient of thermal expansion (CTE) of each constituent layer of the CC tape, the bobbin, and the impregnating materials is the main causes of delamination in CC tapes when subjected to thermal and mechanical cycling. In the design of degradation-free superconducting coils, therefore, characterization of the delamination behaviors including mechanism and strength in the multi-layered REBCO CC tapes becomes a critical issue. Various trials to increase the delamination strength by improving interface characteristics at interlayers have been performed. In this study, in order to investigate the influences of laser cleaning and Ag annealing treated at the substrate side surface, transverse tensile tests were conducted under different sample configurations using $4.5mm{\times}8mm$ upper anvil. The mechanical delamination strength of differently processed CC samples was examined at room temperature (RT). As a result, the Sample 1 with the additional laser cleaning and Ag annealing processes and the Sample 2 with additional Ag annealing process only showed higher mechanical delamination strength as compared to the Sample 3 without such additional treatments. Sample 3 showed quite different behavior when the loading direction is to the substrate side where the delamination strength much lower as compared to other cases.

Effect of Nb Doping on the Dielectric and Strain Properties of Lead-free 0.94(Bi1/2Na1/2)TiO3-0.06BaTiO3 Ceramics

  • Han, Hyoung-Su;Hong, In-Ki;Kong, Young-Min;Lee, Jae-Shin;Jo, Wook
    • 한국세라믹학회지
    • /
    • 제53권2호
    • /
    • pp.145-149
    • /
    • 2016
  • $(Bi_{1/2}Na_{1/2})_{0.94}Ba_{0.06}(Ti_{1-x}Nb_x)O_3$ (BNBTxNb) ceramics were investigated in terms of the crystal structure as well as the ferroelectric, dielectric, and piezoelectric properties. While little change was observed in the microstructure except for a slight decrease in the average grain size, a significant change was noticed in the temperature dependence of dielectric and piezoelectric properties. It was shown that the property changes are closely related to the downward shift in the position of the ferroelectric-to-relaxor transition temperature with increasing amount of Nb doping. A special emphasis is put on the fact that Nb doping is so effective at decreasing the ferroelectric-to-relaxor transition temperature that even at no more than 2 at.% Nb addition, the transition temperature was already brought down slightly below room temperature, resulting in the birth of a large strain at 0.46 %, equivalent to $S_{max}/E_{max}=767pm/V$.

CLN-PZT 세라믹스의 전기, 광학 특성에 관한 연구 (A Study on the Electrical and Optical Characteristics of CLN-PZT Ceramics)

  • 강원구
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1988년도 전기.전자공학 학술대회 논문집
    • /
    • pp.799-801
    • /
    • 1988
  • This paper was studied on the effects of Ca-La-Nb substitution and Zr/Ti ratio variation to Pb(Zr, Ti)$O_3$ system on structural, electrical, optical and sound level characteristics in order to develope the piezoelectric and electrooptic ceramic devices. Also the specimens were prepared by the two stage sintering technique. The molecular formular was X($CaO{\cdot}1/4La_{2}O_{3}{\cdot}1/4Nb_{2}O_{5}){\cdot}(1-X)Pb(Zr_{Y}Ti_{1-Y})O_{3}$(x=100X, y=100Y), and the variation of x was $6{\sim}12$, y was 60${\sim}$49 and second stage sintering time was 20${\sim}$40 hours. The experimental results obtained from this study are as follows : 1. The density was decreased, the grain size was increased according to increase of Ca-La-Nb substitution. 2. The crystal structure was rhombohedral in composition 6/60/40, and the crystal structure was tetragonal and cubic according to increase of Ca-La-Nb substitution. 3. The Ca substitution of PZT system enhanced the sintering property. The Pb site vacancy resulting from the substitution of La-Nb increased the dielectrical constant, the piezoelectric charge constant, the dielectric loss and decreased the coercive field. 4. The resistivity of PZT system which has the P type conduction mechanism increased according to substitution of La-Nb because of the substituent acting as donor. 5. The PZT ceramics varied from ferroelectric substance according to increase of Ca-La-Nb substituent. The coercive field and saturation remanent polarization decreased, and at last straight line according to increase of La-Nb substitution. 6. The amount of Ca-La-Nb substitution to improve the light transmittance of speciment was 10 mol%, the Zr/Ti ratio was 49/51, and the second stage sintering time was 40 hours. 7. According to Ca-La-Nb substitution, the specimens was to be transparent. The 7.5/51/49 specimen was suitable for transparent sound vibrator because it had 58% light transmittance (thick 0.2[mm], wave length 700[mm]) and 48% electromechanical coupling factor.

  • PDF