The Structural and Electrochemical Properties of Li[Ni0.6-xBaxCo0.1Mn0.3]O2 (x = 0, 0.01) by Barium Doping (Barium 도핑에 따른 Li[Ni0.6-xBaxCo0.1Mn0.3]O2(x=0, 0.01) 의 구조 분석 및 전기화학적 특성)

  • Jang, Byeong-Chan;Yoo, Gi-Won;Yang, Su-Bin;Min, Song-Gi;Son, Jong-Tae
    • Journal of the Korean Electrochemical Society
    • /
    • v.17 no.4
    • /
    • pp.222-228
    • /
    • 2014
  • Ni-rich system $Li[Ni_{1-x-y}Co_xMn_y]O_2$ of lithium secondary battery cathode material keep a high discharge capacity. However, by the Ni content increases, there is a problem that the electrochemical properties and stability of the structure are reduced. In order to solve these problems, research for positive ion doping is performed. The one of the cathode material, barium-doped $Li[Ni_{0.6-x}Ba_xCo_{0.1}Mn_{0.3}]O_2$ (x=0.01), was synthesized by the precursor, $Ni_{0.6}Co_{0.1}Mn_{0.3}(OH)_2$, from the co-precipitation method. The barium doped materials have studied the structural and electrochemical properties. The analysis of structural properties, results of X-ray diffraction analysis, and those results confirmed the change of the lattice from the binding energy in the structure by barium doping. Increased stability of the layered structure was observed by $I_{(006)}+I_{(102)}/I_{(101)}$(R-factor) ratio decrease. we expected that the electrochemical characteristics are improved. 23 mAh/g discharge capacity of barium-doped $Li[Ni_{0.6-x}Ba_xCo_{0.1}Mn_{0.3}]O_2$ (x=0.01) electrode is higher than discharge capacity of $Li[Ni_{0.6}Co_{0.1}Mn_{0.3}]O_2$ due to decrease overvoltage. And, through the structural stability was confirmed that improved the cycle characteristics. We caused a reduction in charge transfer resistance between the electrolyte and the electrode was confirmed that the C-rate characteristics are improved.

Synthesis and Electrochemical Performance of Mesoporous Hollow Sphere Shape LiMn2O4 using Silica Template (실리카 템플레이트를 이용하여 다공성 중공형태를 갖는 LiMn2O4 합성 및 전기화학적 특성 연구)

  • Ryu, Seong-Hyeon;Ryu, Kwang-Sun
    • Journal of the Korean Electrochemical Society
    • /
    • v.14 no.3
    • /
    • pp.184-190
    • /
    • 2011
  • $LiMn_2O_4$ with mesoporous hollow sphere shape was synthesized by precipitation method with silica template. The synthesized $LiMn_2O_4$ has nanosized first particle and mesoporous hollow sphere shape. Silica template was removed by chemical etching method using NaOH solution. When the concentration of NaOH solution was increased, first particle size of manganese oxide was decrease and confirmed mesoporous hollow shpere shape. X-ray diffraction(XRD) patterns revealed that the synthesized samples has spinel structure with Fd3m space group. In case the ratio of silica and maganese salt increased, the size of first particles was decreased. The tetragoanal $LiMn_2O_4$ with micron size was synthesized at ratio of silica and manganese salt over 1 : 9. The prepared samples were assembled as cathode materials of Li-ion battery with 2032 type coin cell and their electrochemical properties are examined by charge-discharge and cyclic performance. Electrochemical measurements show that the nano-size particles had lower capacity than micron-size particles. But, cyclic performance of nano-size particles had better than that of micron-size particles.

Influence of Annealing Temperature on Microstructure and Pitting Corrosion Behavior of the 27Cr-7Ni Hyper Duplex Stainless Steel

  • Jeon, Soon-Hyeok;Kim, Hye-Jin;Kong, Kyeong-Ho;Park, Yong-Soo
    • Corrosion Science and Technology
    • /
    • v.13 no.2
    • /
    • pp.48-55
    • /
    • 2014
  • Influence of annealing temperature on the microstructure and resistance to pitting corrosion of the hyper duplex stainless steel was investigated in acid and neutral chloride environments. The pitting corrosion resistance is strongly dependent on the microstructure, especially the presence of chromium nitrides ($Cr_2N$), elemental partitioning behavior and volume fraction of ferrite phase and austenite phase. Precipitation of deleterious chromium nitrides reduces the resistance to pitting corrosion due to the formation of Cr-depleted zone. The difference of PREN (Pitting Resistance Equivalent Number) values between the ferrite and austenite phases was the smallest when solution heat-treated at $1060^{\circ}C$. Based on the results of electrochemical tests and critical crevice temperature tests, the optimal annealing temperature is determined as $1060^{\circ}C$.

Flow-Accelerated Corrosion Behavior of SA106 Gr.C Steel in Alkaline Solution Characterized by Rotating Cylinder Electrode

  • Kim, Jun-Hwan;Kim, In-Sup
    • Nuclear Engineering and Technology
    • /
    • v.32 no.6
    • /
    • pp.595-604
    • /
    • 2000
  • Flow-Accelerated Corrosion Behavior of SA106 Gr.C steel in room temperature alkaline solution simulating the CANDU primary water condition was studied using Rotating Cylinder Electrode. Systems of RCE were set up and electrochemical parameters were applied at various rotating speeds. Corrosion current density decreased up to pH 10.4 then it increased rapidly at higher pH. This is due to the increasing tendency of cathodic and anodic exchange half-cell current. Corrosion potential shifted slightly upward with rotating velocity. Passive film was formed from pH 9.8 by the mechanism of step oxidation and the subsequent precipitation of ferrous species into hydroxyl compound. Above pH 10.4, the film formation process was active and the film became stable. Corrosion current density showed increment in pH 6.98 with the rotating velocity, while it soon saturated from 1000 rpm above pH 9.8. This seems that activation process which represents formation of passive film on the bare metal surface controls the entire corrosion process

  • PDF

The Evaluation of Materials Degradation in Modified 9Cr-1Mo Steel (Modified 9Cr-1Mo 강의 열화도 평가)

  • Hyeon, Yang-Gi;Lee, Jae-Do
    • 연구논문집
    • /
    • s.31
    • /
    • pp.157-163
    • /
    • 2001
  • Evolution of microstructure due to service exposure to high temperature has a strong effect performance of heat resistant steels. In case of modified 9Cr-1Mo steels, precipitation of $Fe_2Mo$-type laves phases and coarcening of $M_23C_6$-type carbides is the primary cause of degradation of mechanical properties such as creep resistance, tensile strength and toughness. Creep tests have been carried out on pre-aging mod. 9Cr-1Mo steels to examine the effect of pre-aging and stress on the creep strength. Based on the results, a nondestructive procedure, where electrochemical technique that quantitatively detect laves phases and $M_23C_6$-type carbides in a material is used, has been proposed to evaluate a residual creep life of mod. 9Cr-1Mo steels.

  • PDF

The effects of Si-content on the corrosion rate of Cu-al alloys (동일 알루미늄 합금의 탄식속도에 미치는 규소의 영향)

  • Ham, Dong-Ha;Kang, Tak;Kang, Choon-Sik
    • Journal of the Korean institute of surface engineering
    • /
    • v.14 no.1
    • /
    • pp.5-9
    • /
    • 1981
  • The effects of silicon content on the corrosion rates of Cu-7wt% Al alloys have been investigated by the use of electrochemical methods. The corrosion current densities of the alloys are decreased with the addition of Si up to 2wt%, and the slightly increased at 2.5%Si. This increased corrosion rates are attributed to the precipitation of more anodic gamma-2 phase. The X-ray diffraction tests reveal the dealuminumification of these alloys and mixtures of CuCl and Al2O3 formed on the surface of the specimens, which are considered to passivate the alloys at noble potentials.

  • PDF

Effects of Calcinations Temperature on the Electrochemical Properties of Li[Ni0.6Co0.2Mn0.2]O2 Lithium-ion Cathode Materials (리튬 이차전지용 양극활물질 Li[Ni0.6Co0.2Mn0.2]O2의 소성 온도가 전기화학적 특성에 미치는 영향)

  • Yoo, Gi-Won;Jeon, Hyo-Jin;Son, Jong-Tae
    • Journal of the Korean Electrochemical Society
    • /
    • v.16 no.2
    • /
    • pp.59-64
    • /
    • 2013
  • Using $Na_2CO_3$ and $MeSO_4$ (Me = Ni, Co and Mn) as starting materials, the precursor of $[Ni_{0.6}Co_{0.2}Mn_{0.2}]CO_3$ has been synthesized by carbonate co-precipitation. The precursor was mixed with $Li_2CO_3$, and calcined at 750, 850, and$950^{\circ}C$ in air. Effect of calcinations temperature on characteristics of $Li[Ni_{0.6}Co_{0.2}Mn_{0.2}]O_2$ cathode materials was investigated. The structure and characteristics of $Li[Ni_{0.6}Co_{0.2}Mn_{0.2}]O_2$ were determined by X-ray diffraction (XRD), Scanning electron microscopy (SEM) and electrochemical measurements. The X-ray diffraction (XRD) results show that the intensity ratio of $I_{(003)}/I_{(104)}$ increased and the R-factor ratio decreased with the increase of calcinations temperature. And Scanning electron microscopy (SEM) result show that the primary particle size increased. Especially, the $Li[Ni_{0.6}Co_{0.2}Mn_{0.2}]O_2$ calcined at $950^{\circ}C$ for 24 H shows excellent electrochemical performances with reversible specific capacity of $165.3mAhg^{-1}$ [cut-off voltage 2.5~4.3 V, 0.1 C($17mAhg^{-1}$)] and good capacity retention of 95.4% after 50th charge/discharge cycles[cut-off voltage 2.5~4.3 V, 1 C($170mAhg^{-1}$)].

Analyses on the Physical and Electrochemical Properties of Al2O3 Coated LiCoO2 (리튬이차전지용 양극 활물질(LiCoC2)의 표면처리의 특성 분석 및 전기화학적 특성 고찰)

  • Chang, Youn-Han;Choi, Sei-Young
    • Journal of the Korean Electrochemical Society
    • /
    • v.10 no.3
    • /
    • pp.184-189
    • /
    • 2007
  • The importance of secondary battery industry is getting excited according to the development of battery industry as a high efficiency energy supplier of electronic machine of mobile information such as mobile phone, lap-top computer, PDA. It is rasing the interest about security of safety and high efficiency of cathode material for main part of secondary lithium battery. The cathode material which has been used like $LiCoO_2,\;LiMn_2O_4,\;LiNi_xCo_yMn_zO_2,\;LiNi_xCo_yM_zO_2$ (M=Al, Zr, Mg etc.,) the most typical material is $LiCoO_2$. But it is studying the development of substitute such as efficiency amelioration of $LiCoO_2$, thetiary element, olivine element because of the capacity of $LiCoO_2$, the matter of security; especially the betterment of efficiency, security research of safety has been actively processed in domestic and overseas about surface coating treatment of active cathode which is using oxide ($M_xO_3$). This study analyses side effect of battery according to increase of surface treatment, formation of precipitation for reagent condensation, non-reagent residue of oxide ($M_xO_3$) which is remains during the surface treatment of $LiCoO_2$; conducts study of new process, the consideration of the electrochemical property to improve oxide solution of mixing rate, mixture of surface treatment, dryness, calcinations conditionetc.

A Study on the Preparation and Application of Au/TiO2 Nanofiber from AAO Template (AAO Template를 이용한 Au/TiO2 나노섬유 제조 및 응용에 관한 연구)

  • Eom, Seon-Mi;Park, Sang-Sun;Kim, Young-Deok;Kim, Yong-Rok;Shul, Yong-Gun
    • Journal of the Korean Electrochemical Society
    • /
    • v.12 no.1
    • /
    • pp.47-53
    • /
    • 2009
  • In this study, highly ordered AAO (Anodic Aluminum Oxide) with nanopores was prepared by commercial grade Al substrate containing 3.5 wt.% impurities through two step anodizing method. Nanopores of prepared AAO arrays were used as templates for preparing nanofiber. $TiO_2$ was deposited by using DP (deposition-precipitation) method into AAO pores to grow nanofiber. Au particles were loaded on this $TiO_2$ nanofiber which was grown vertically. Prepared 2 wt.% $Au/TiO_2$ nanofiber was characterized by XRD, SEM and Raman. The crystal structure was analyzed by the XRD. SEM was used to observe pore size and pore wall thickness. Photocatalytic activity of co-oxidation was compared with $TiO_2$ and $Au/TiO_2$ nanofiber on AAO arrays.

Corrosion Behaviors of Laser-welded Super Duplex Stainless Steel(UNS S32506) Tube with Post-Weld Heat Treatment Conditions (슈퍼 듀플렉스 스테인리스강(UNS S32506) 레이저 조관용접 튜브의 용접 후 열처리에 따른 부식거동)

  • Cho, Dong Min;Park, Jin-seong;Hong, Seung Gab;Hwang, Joong-Ki;Kim, Sung Jin
    • Journal of the Korean institute of surface engineering
    • /
    • v.54 no.3
    • /
    • pp.102-111
    • /
    • 2021
  • The corrosion behaviors of laser-welded super duplex stainless steel tubes with post-weld heat treatment(PWHT) conditions(950, 1000, 1050, 1100 ℃ for 5 and 30 min) were evaluated by electrochemical potentiodynamic polarization and critical pitting temperature measurements. This study showed that the critical metallurgical factors affecting the degradation of corrosion resistance of a steel tube in as-welded condition were the unbalanced phase fraction(ferrite:austenite = 94:4), Cr2N precipitation, and phase transformation from the austenite phase to ɛ-martensite(via stress-induced phase transformation). The improvement in the corrosion resistance of the welded specimen depends greatly on the PWHT conditions. The specimens after PWHT conducted below 1000 ℃ showed inferior corrosion resistance, caused by precipitation of the sigma phase enriched with Cr and Mo. At 1100 ℃ for a longer duration in PWHT, the ferrite phase grows, and its fraction increases, leading to an unbalanced phase fraction in the microstructure. As a result, pitting can be initiated primarily at the interface between the ferrite/austenite phase, particularly in base metal.