• Title/Summary/Keyword: EH36-TMCP steel

Search Result 6, Processing Time 0.024 seconds

Microstructures and Impact Properties of 500mm Single Pass Electrogas Weldment for EH36 TMCP steels (EH36 TMCP강의 50mm 1 패스 일렉트로가스 용접부의 조직 및 충격특성)

  • 이해우;고대은
    • Journal of Welding and Joining
    • /
    • v.17 no.3
    • /
    • pp.96-101
    • /
    • 1999
  • Microstructures and mechanical properties of weldments were studied for EH36 TMCP higher-strength hull steel with electrogas welding jprocess. In case of a newly designed EH36 TMCP steel for large heat input welding process, the Microstructures of HAZ shows more narrow width of grain coarsed region than that of conventional EH36 TMCP weldments, the amount of acicular ferrite, which is beneficial to impact toughness, increased while the amount of grain-boundary ferrite decreased. Charpy V-notched impact tests show that a newly designed EH36 TMCP steel weldment satisfies all the requirement of specifications, especially at the fusion line +2mm where the conventional EH36 TMCP steel fails to exceed the requirement.

  • PDF

Characteristics of plate forming by flame heating for TMCP steel (TMCP 강재의 곡가공 특성)

  • Yun, Jung-Geun;Sin, Sang-Beom;Kim, Ha-Geun;Kim, Gyeong-Gyu
    • Proceedings of the KWS Conference
    • /
    • 2005.11a
    • /
    • pp.6-8
    • /
    • 2005
  • The purpose of this study is to evaluate characteristics of plate forming by flame heating for E and EH36 TMCP steel. The characteristics of interest were heat-formability of TMCP steel and mechanical properties of heated area. For a given dimension, heat-formability of TMCP steel was inferior to that of a conventional steel because TMCP steel required more heating passes and time. Angular distortion and transverse shrinkage of TMCP steel decreased with an increase in line heating speed for given heating conditions. The mechanical properties of TMCP steel after plate forming by flame heating were high enough to satisfy the requirements.

  • PDF

Analysis of Mechanical Behavior and Fracture Toughness $K_{IC}$ on EGW Welded Joints for High Strength EH36-TMCP Ultra Thick Plate (고강도 극후판 EH36-TMCP강 EGW용접부의 역학적 거동 및 파괴인성 $K_{IC}$에 관한 해석)

  • Bang, Hee-Seon;Bang, Han-Sur;Joo, Sung-Min
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.22 no.6
    • /
    • pp.565-572
    • /
    • 2009
  • This work intends to establish the reliability and fracture toughness $K_{IC}$ criterion of welded joints by EGW for high strength EH36-TMCP ultra thick plate. For this, firstly thermo elasto-plastic analysis has been carried out on two pass X-groove butt joint model to clarify the thermal and mechanical behaviour(residual stress, plastic strain, magnitude of stress and their distribution and production mechanism). Moreover, to establish fracture criterion, analysis of fracture toughness $K_{IC}$ has been performed under the notch machined and residual stress with the load condition on EGW welded joints. A quantitative fracture criterion for EGW welded joints is suggested by using $K_{IC}$.

Effect of Groove Conditions on the Mechanical Properties of Welds Produced by the Combined Welding Process of Flux Cored Arc and Electro Gas in EH36 TMCP Steel Plate for Hull Structures (선체구조용 EH36 TMCP 후판의 FCAW 및 EGW 조합 용접부 기계적 성질에 미치는 개선조건의 영향)

  • Kim, Kihyuk;Kim, Kiwon;Sim, Hoseop;Bae, Kangho;Hong, Hyunuk;Park, Byunggyu
    • Journal of Welding and Joining
    • /
    • v.33 no.5
    • /
    • pp.35-40
    • /
    • 2015
  • Characterization of microstructures and mechanical properties of 83mm thickness EH36-TM welds produced by the combined flux cored arc (FCA) and electro gas (EG) welding processes has been studied with the two different groove conditions, single-V (SV) and double-V (DV) bevels. The welding consumables used for FCA and EG welding processes were ASME/AWS A5.29 (E81T1-K2) and A5.26 (EG72T), respectively. Experimental results showed that all the mechanical properties of welds such as tensile property, CVN toughness and Vickers hardness met IACS requirements. The tensile strength of EG welded plates were reduced by approximately 4% (DV: 3.8%, SV: 4.2%) compared to the base metal. The hardness value of SV-beveled weld metal was slightly lower than that of DV-beveled one. There were no significant differences as per welding groove conditions except for the weld metal. In addition, at the fusion line, the toughness of SV condition was 20J lower and the weld metal was 40J lower than DV condition, respectively. On the basis of microstructural analysis, grain boundary ferrite (GBF) structures for SV condition were 2 times higher volume fraction than for DV condition and their packet sizes were coarsened to almost double. It was thus suggested that the GBF volume fractions and packet sizes in the weld metal of EH36-TM steel plates are the most important factors affecting the mechanical properties of the combined FCA and EG welded joint. Nevertheless, all the results of welds with both DV and SV conditions were found to be excellent.

Analysis of Welding Residual Stress Redistributions on Notched Multi-pass FCA Butt Weldment (노치가공에 의한 다층 FCA 용접부의 잔류응력 재분포 특성)

  • Bang, Hee-Seon;Bang, Han-Sur;Oh, Ik-Hyun;Kim, Jun-Hyung
    • Journal of Welding and Joining
    • /
    • v.28 no.1
    • /
    • pp.86-91
    • /
    • 2010
  • In the present study, two-dimensional plane deformation thermo elasto-plastic analysis has been carried out, in order to investigate the thermal and mechanical behaviour (residual stress, plastic strain, magnitude of stress and their distribution and production mechanism) on multi-pass FCA butt weldment of high strength EH36-TMCP ultra thick plate. Moreover, this study can be considered as a basis for analysing the fracture toughness, KIC, and its effect on welding residual stress redistribution with notch on multi-pass FCA butt weldment, in future. The results of welding residual stress obtained from thermo elasto-plastic analysis has been compared and verified with the results measured by XRD.

A Study of Fatigue Crack Growth Behaviour for Ferrite-Bainite Dual Phase Steel (Ferrite-Bainite dual phase 강의 피로균열진전 특성 평가)

  • Kim, Deok-Geun;Cho, Dong-Pil;Oh, Dong-Jin;Kim, Myung-Hyun
    • Journal of Welding and Joining
    • /
    • v.34 no.1
    • /
    • pp.41-46
    • /
    • 2016
  • With the recent increase in size of ships and offshore structures, there are more demand for thicker plates. As the thickness increases, it is known that fatigue life of the structures decrease. To improve the fatigue life, post weld treatments techniques, such as toe grinding, TIG dressing and hammer peening, are typically employed. However, these techniques require additional construction time and production cost. Therefore, it is of crucial interest steels with longer fatigue crack growth life compared to conventional steels. This study investigates fatigue crack growth rate (FCGR) behaviours of conventional EH36 steel and Ferrite-Bainite dual phase EH36 steel (F-B steel). F-B steel is known to have improved fatigue performance associated with the existence of two different phases. Ferrite-Bainite dual phase microstructures are obtained by special thermo mechanical control process (TMCP). FCGR behaviours are investigated by a series of constant stress-controlled FCGR tests. Considering all test conditions (ambient, low temperature, high stress ratio), it is shown that FCGR of F-B steel is slower than that of conventional EH36 steel. From the tensile tests and impact tests, F-B steel exhibits higher values of strength and impact energy leading to slower FCGR.