• 제목/요약/키워드: Dual phase steels

검색결과 65건 처리시간 0.022초

Q&P와 AM강의 잔류오스테나이트 분율과 안정도에 따른 인장특성 거동 (Effects of Stability and Volume Fraction of Retained Austenite on the Tensile Properties for Q&P and AM Steels)

  • 변상호;오창석;남대근;김영석;강남현;조경목
    • 한국재료학회지
    • /
    • 제19권6호
    • /
    • pp.305-312
    • /
    • 2009
  • The effects of Quenching and Partitioning (Q&P) and Annealed Martensite (AM) heat treatment on the microstructure and tensile properties were investigated for 0.24C-0.5Si-1.5Mn-1Al steels. The Q&P steels were annealed at a single phase ($\gamma$) or a dual phase (${\gamma}+{\alpha}$), followed by quenching to a temperature between $M_s$ and $M_f$. Then, enriching carbon was conducted to stabilize the austenite through the partitioning, followed by water quenching. The AM steels were intercritically annealed at a dual phase (${\gamma}+{\alpha}$) temperature and austempered at $M_s$ and $M_s{\pm}50^{\circ}C$, followed by cooling in oil quenching. The dual phase Q&P steels showed lower tensile strength and yieldyield strength than those of the single phase Q&P steels, and tThe elongation for the dual phase Q&P steel was partitioning 100s higher than that of that for the single phase Q&P steels as the partitioning time was less than 100s up to partitioning 100s. For AM steels, the tensile/yield strength decreased and the total elongation increased as the austempering temperature increased. The stability of the retained austenite controlled the elongation for Q&P steels and the volume fraction of the retained austenite controlled the elongation for AM steels.

EFFECTS OF HEAT TREATMENTS ON MICROSTRUCTURES AND MECHANICAL PROPERTIES OF DUAL PHASE ODS STEELS FOR HIGH TEMPERATURE STRENGTH

  • Noh, Sanghoon;Choi, Byoung-Kwon;Han, Chang-Hee;Kang, Suk Hoon;Jang, Jinsung;Jeong, Yong-Hwan;Kim, Tae Kyu
    • Nuclear Engineering and Technology
    • /
    • 제45권6호
    • /
    • pp.821-826
    • /
    • 2013
  • In the present study, the effects of various heat treatments on the microstructure and mechanical properties of dual phase ODS steels were investigated to enhance the high strength at elevated temperature. Dual phase ODS steels have been designed by the control of ferrite and austenite formers, i.e., Cr, W and Ni, C in Fe-based alloys. The ODS steels were fabricated by mechanical alloying and a hot isostatic pressing process. Heat treatments, including hot rolling-tempering and normalizing-tempering with air- and furnace-cooling, were carefully carried out. It was revealed that the grain size and oxide distributions of the ODS steels can be changed by heat treatment, which significantly affected the strengths at elevated temperature. Therefore, the high temperature strength of dual phase ODS steel can be enhanced by a proper heat treatment process with a good combination of ferrite grains, nano-oxide particles, and grain boundary sliding.

신선 가공된 이상 조직강의 냉간 성형성에 대한 연구 (Study on the Cold Formability of Drawn Dual-Phase Steels)

  • 박경수;최상우;이덕락;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 추계학술대회논문집
    • /
    • pp.269-273
    • /
    • 2003
  • There is a growing interest to replace the commercial steels with non-heat treated steels, which does not involve the spheroidization and quenching-tempering treatment. However, Non-heat treated steels should satisfy high strength and good formability without performing heat treatment. Therefore, it is important to investigate optimum materials showing a good combination of strength and formability after the drawing process. In this study, Dual-Phase Steels were studied as candidate materials for non-heat treated steels, which have different martensite morphologies and volume fractions obtained through heat-treatment of intercritical quenching (IcQ), intermediate quenching (ImQ) and step quenching (SQ). The mechanical properties of DP steels were measured by tension and compression tests. Also, the cold formability of three DP steels which have similar tensile strength value was investigated by estimating the deformation resistance and the forming limit. The deformation resistance which is important factor in determining die life was estimated by calculating the deformation energy. And the forming limit was estimated by measuring the critical strain revealing crack initiation at the notch tip of the specimens.

  • PDF

신선 가공된 이상 조직강의 냉간 성형성에 대한 연구 (A Study on the Cold Formability of Drawn Dual-Phase Steels)

  • 박경수;최상우;이덕락;이종수
    • 소성∙가공
    • /
    • 제13권1호
    • /
    • pp.84-89
    • /
    • 2004
  • There is a growing interest to replace the commercial steels with non-heat treated steels, which does not involve the spheroidization and quenching-tempering treatment. However, Non-heat treated steels should satisfy high strength and good formability without performing heat treatment. Therefore, it is important to investigate optimum materials showing a good combination of strength and formability after the drawing process. In this study, Dual-Phase Steels were studied as candidate materials for non-heat treated steels, which have different martensite morphologies and volume fractions obtained through heat-treatment of intercritical quenching (IcQ), intermediate quenching (ImQ) and step quenching (SQ). The mechanical properties of DP steels were measured by tension and compression tests. Also, the cold formability of three DP steels which have similar tensile strength value was investigated by estimating the deformation resistance and the forming limit. The deformation resistance which is important factor in determining die life was estimated by calculating the deformation energy. And the forming limit was estimated by measuring the critical strain revealing crack initiation at the notch tip of the specimens.

페라이트-마르텐사이트 複合組織鋼의 衝擊破壞擧動 (Study on the impact fracture behavior with the ferrite-martensite dual phase steels)

  • 송삼홍;오택렬
    • 대한기계학회논문집
    • /
    • 제12권1호
    • /
    • pp.19-27
    • /
    • 1988
  • 본 연구에서는 화학성분, 마르텐사이트 체적율, 연결도, 모상위경 및 제2상의 형태를 되도록 일정하게 하고, 제1상과 제2상의 경도비만을 변화시켰을 때의 충격降伏荷重 및 충격최대하중의 거동, 충격속도가 하중작용시간에 미치는 영향, 흡수에너지 및 延性-胞性거동 등을 고찰하였다.

複合組織鋼의 衝擊破壞擧動에 영향 을 주는 마르텐사이트 體積率의 效果 (Effects of the Martensive Volume Fraction on the Behavior of Impact Fracture of Dual Phase Steels)

  • 송삼홍;오택열;장두수
    • 대한기계학회논문집
    • /
    • 제7권4호
    • /
    • pp.372-378
    • /
    • 1983
  • Use of dual phase steel are growing for its high strength and light weight in automobiles. The effect of the martensite volume fraction with various impact velocities on the strength, ductility and absorbed energy of dual phase (ferrite-martensite) steels were investigated in low carbon 1.5% Mn steels which were soaked at 700.deg. C, 730.deg. C, 780.deg. C, and brine quenched. Both the yield load and the maximum impact load increased when the martensite volume fraction increased, the loading time and the absorbed energy of the specimen decreased when the martensite volume fraction increased.

複合組織鋼의 衝擊破壞特性에 미치는 노치形狀 및 硬度比의 영향 (Effect of notch shape and hardness ratio on characteristics of impact fracture in dual phase steels)

  • 김정규;유승원;김일현
    • 오토저널
    • /
    • 제10권2호
    • /
    • pp.46-53
    • /
    • 1988
  • Effect of Notch Shape and Hardness Ratio on Characteristics of Impact Fracture in Dual Phase Steels. In this study, it is investigated the effect of notch shape and hardness ratio on the characteristics of impact fracture in dual phase steels. The impact test was carried out at the temperature range from -40.deg. C to room temperature with Instrumented Charpy Impact Tester. The main results obtained are as follows; 1, The maximum impact bending strength (.sigma.$_{max}$) increases with the tensile strength. Also, the impact energy depends on .sigma.$_{max}$. 2, In room temperature, the impact energy depends on crack-initiation energy (E$_{i}$) in case of the high hardness ratio (R=3.4), whereas depends on crack-propagation energy (E$_{p}$) in case of the low hardness ratio (R=1.8) and the dependence of crack-initiation energy of the impact characteristics decreases with increasing test temperature. These phenomena are result from the difficulty of cleavage facet formation.ion.ion.

  • PDF

저탄소 2상조직강의 열처리공정 조건에 따른 기계적특성 변화

  • 김훈동;박진성;문만빈
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2010년도 춘계학술발표대회
    • /
    • pp.40.1-40.1
    • /
    • 2010
  • Recently high strength steel sheets with high formability for automotive parts have been being developed to meet the demands for passenger safety and weight reduction of car body. Among these high strength steels, dual-phase steels are regarded as one of the attractive steels due to their excellent mechanical properties including high strength and ductility. However, to be successfully applied to automotive parts they should be corrosion resistant enough to satisfy the required quality of car maker. This also requires their feasibility for galvannealed production including hot dip galvanizability. In this study has been placed on understanding the effects of heat-treatment(austenizing and isothermal treatment) on the microstructures and mechanical properties of a 0.06C-0.03Si-2.0Mn high strength steel for cold forming. The microstructure and phase distribution were examined with eth aids of SEM, EBSD, TEM etc.. Through the study the production of 590MPa grade DP GA steels with good formability and galvaniability were shown to be possible.

  • PDF

복합조직강의 응력-변형 거동에 관한 이론치와 실험치 (The Theoretical and Experimental Value on the Stress-Strain Behavior of Dual Phase Steels)

  • 오택열;김석환;유용석
    • 한국표면공학회지
    • /
    • 제26권2호
    • /
    • pp.63-70
    • /
    • 1993
  • The mechanical properties of ferrite-martensited dual phases steels are affected by the microstructural factors, such as martensited volume fractions, ferrite grain size, strength ratio, connectivity, etc. Two phase alloys are technologically important. However, there is a lack of understanding as to stress-strain behavior of dual phase alloy in terms of stress-strain behavior of each component phases. The lack of the understanding stems from the complex deformation behavior of two phase alloys. The aim of this study is to rationalize stress-strain behavior of dual phase alloy in terms of the stress-strain behavior of component phase by systematically considering all the factors listed above. It was found that for a given martensite volume fraction, the calculated stress-strain curve was higher for a finer particles size than for a coarse particle sized within the range of the strains considered, and this behavior was seen for all the different volume fraction alloys considered. The calculated stress-strain curves were compared with corresponding experimental curves, and in general, good agreement was found. The maximum difference in flow stress between the calculated and the experimental results occurs at the nearly beginning of the plastic deformation.

  • PDF

미세조직이 고려된 이상 조직강의 유한 요소 해석 (Micro-mechanical FE Analysis of Dual-phase Steels)

  • 하진진;이진우;김지훈;;이명규
    • 소성∙가공
    • /
    • 제24권3호
    • /
    • pp.194-198
    • /
    • 2015
  • Microstructure based FE simulations were conducted to investigate the micro-mechanical properties of ferrite-martensite dual-phase steels. The FE model was built based on real microstructure images which were characterized by optical microscopy through the thickness direction. Serial sectioned 2D images were converted into semi-2D representative volume elements (RVEs) model. Each RVE model was subjected to a non-proportional loading condition and the mechanical response was analyzed on both the macroscopic and microscopic levels. Macroscopically, stress-strain curves were described under tension-compression and tension-orthogonal tension conditions and the Bauschinger effect was well captured for both loading paths. In addition, micromechanical properties were investigated in the view of stress-strain partitioning and strain localization during monotonic tension.