• 제목/요약/키워드: Dissolution-precipitation

검색결과 173건 처리시간 0.026초

수용액 합성법의 2단계 성장온도 변화를 통한 ZnO 결정의 선택적 용해 현상 (Selective Dissolution of ZnO Crystal by a Two-step Thermal Aging in Aqueous Solution)

  • 김정석;채기웅
    • 한국세라믹학회지
    • /
    • 제48권4호
    • /
    • pp.263-268
    • /
    • 2011
  • ZnO hexagonal rods grown in aqueous solution can be changed into a tubular shape by two-step aging in the course of the growing process. In the first step, hexagonal ZnO rods is grown by aging at $90^{\circ}C$ under a highly supersaturated aqueous solution giving rise to a fast precipitation rate. Meanwhile, during the second step aging at $60^{\circ}C$ in the same aqueous solution, the hexagonal polar face (001) having higher surface energy than (010) side planes dissolves to minimize surface energy. Hence the flat (001) face changes to a craterlike face and the hexagonal rod length of ZnO decreases at an initial-stage of this step aging. The formation of the (101) wedge-type faces is ascribed to the resultant of competitive reactions between the dissolution of polar face minimizing the surface energy which is a dominant reaction at the initial stage and the precipitation reaction dissipating supersaturation. At a later stage of the second-step the reaction rates of these two processes in the aqueous solution become similar and the overall reaction is terminated.

세륨연마재 폐슬러리 건조분말로부터 희토류와 알루미늄의 분리 (Separation of Rare Earth and Aluminium from the Dried Powder of Waste Cerium Polishing Slurry)

  • 윤호성;김철주;김성돈;이진영;조성욱;김준수
    • 자원리싸이클링
    • /
    • 제12권5호
    • /
    • pp.10-15
    • /
    • 2003
  • 본 연구에서는 세륨연마재 폐슬러리 건조분말로부터 세륨을 포함한 희토류성분과 알루미늄을 분리하고자 하였다. 출발원료인 세륨연마재 폐슬러리 건조분말의 희토류 중에는 산화세륨이 전체 희토류 성분의 약 40% 정도 함유되어 있는데, 산화세륨은 희토류원소들 중에서 가장 안정된 형태로 이에 대한 분해가 용이하지 않다. 그러므로 황산화반응을 이용하여 산화세륨을 분해하므로써 희토류의 분리ㆍ회수율을 향상시키고자 하였으며, 침출용액으로부터 희토류와 알루미늄을 분리하기 위하여, 희토류 원소들은 황산매질에서 황산나트륨과 반응하여 황산나트륨희토류(ReㆍNa($SO_4$)$_2$)를 형성하면서 침전되는 특성을 이용하였으며 쉽게 희토류와 알루미늄을 분리할 수 있었다.

Na2CO3-H2O2 탄산염 용액의 안정성 평가 (Evaluation of Na2CO3-H2O2 Carbonate Solution Stability)

  • 이일희;임재관;정동용;양한범;김광욱
    • 방사성폐기물학회지
    • /
    • 제9권3호
    • /
    • pp.131-139
    • /
    • 2011
  • 연구는 $Na_2CO_3-H_2O_2$ 탄산염 용액의 숙성시간에 따른 안정성을 U의 산화 용해액, Cs/Re의 선택적 침전 여과액 및 U의 산성화 침전 여과액으로 구분하여 검토하였다. 숙성시간에 따른 산화 용해액 내 조성 변화는 거의 없었으며, Cs/Re의 선택적 침전에도 아무 영향이 없이 산화 용해액으로부터 순차적으로 Re과 Cs의 침전제거가 가능하였다. 그러나 U의 산성화 침전에서는 산화 용해액이나 Cs/Re의 선택적 침전 여과액을 장시간 동안 숙성시킬 경우 U이 uranyl peroxocarbonato complex에서 uranyltricarbonate로 일부 전환되어 U의 침전회수를 감소시켰다. 그러므로 99% 이상의 U을 회수하기 위해서는 산화 용해액 및 Cs/Re의 선택적 침전 여과액의 숙성시간을 각각 7일 이내에서 처리하는 것이 효과적이다. 그리고 SF 의 산화/용해${\rightarrow}$Cs과 Re(/Tc)의 선택적 침전${\rightarrow}$ U의 산성화 침전 등을 순차적으로 수행하여, 산화/용해에서는 대부분의 U과 FP 중 일부가 함께 용해 되었으며, 함께 용해된 FP 중 Re과 Cs은 각각 TPPCl 및 NaTPB로 99% 이상을 침전제거할 수 있었다. 그리고 산성화 (pH 4) 침전에서는 U을 거의 100% 침전회수 하여 $Na_2CO_3-H_2O_2$ 탄산염 용액에서 침전법으로 SF로부터 U 만의 회수 타당성을 확인하였다.

Equilibrium calculations for HyBRID decontamination of magnetite: Effect of raw amount of CuSO4 on Cu2O formation

  • Lee, Byung-Chul;Kim, Seon-Byeong;Moon, Jei-Kwon
    • Nuclear Engineering and Technology
    • /
    • 제52권11호
    • /
    • pp.2543-2551
    • /
    • 2020
  • Calculations of chemical equilibrium for multicomponent aqueous systems of the HyBRID dissolution of magnetite were performed by using the HSC Chemistry. They were done by using a Pitzer-based aqueous solution model with the recipe of raw materials in experiments conducted at KAERI. The change in the amounts of species and ions and the pH values of the solution at equilibrium was observed as functions of temperature and raw amount of CuSO4. Precipitation of Cu2O occurred at a large amount of CuSO4 added to the solution, while no precipitation of Cu(OH)2 was found at any amounts of CuSO4. The E-pH diagrams for Cu were constructed at various Cu concentrations to provide the effect of the Cu concentration on the pH values at boundaries where the coexistence of Cu+ ion and Cu2O solid occurred. To prevent Cu+ ions from being precipitated to Cu2O, the raw amount of CuSO4 should be adjusted so that the pH value of the solution from the equilibrium calculation is less than that from the E-pH diagram. We provided guidelines for the raw amount of CuSO4 and the pH value of the solution, which prevent the formation of Cu2O precipitates in the HyBRID dissolution experiments for magnetite.

비페닐디메칠디카르복실레이트 연질캅셀제의 설계 및 제제학적 평가 (Design and Pharmaceutical Evaluation of Biphenyl Dimethyl Dicarboxylate Elastic Capsules)

  • 전인구;곽혜선;문지현
    • Biomolecules & Therapeutics
    • /
    • 제4권4호
    • /
    • pp.419-427
    • /
    • 1996
  • To solubilize practically insoluble biphenyl dimethyl dicarboxylate (DDB), which has been used for the treatment of chronic hepatitis as tablets or hard capsules, the solubilities of DDB in various hydrophilic, oily and hydrocarbon vehicles, and aqueous surfactant solutions were measured by high performance liquid chromatography. It was found that, among the vehicles studied, polyethylene glycol (PEG) 300 revealed the best solvency, and the solubility reached 17.6 mg/ml at 37$^{\circ}C$. The addition of glycyrrhizic acid ammonium salt (GAA) to DDB-PEG 300 solution (5-20 mg/g) inhibited the formation of precipitates, and at the concentration of 10 mg/g, any precipitaction was not observed even after 2 years at 4$^{\circ}C$. Furthermore, GAA markedly enhanced the permeation of DDB through the rabbit duodenal mucosa in a concentration dependent manner. The addition of copolyvidone (ca. 1.0%) to DDB-GAA-PEG 300 system (1 : 0.5 97.5 w/w) was most effective in preventing the considerable precipitation of DDB-PEG 300 solution (7.5 mg/750 mg) when mixed with water of 300-900 ml at 37$^{\circ}C$. GAA showed a synergistic effect in the prevention of precipitate formation. This finding suggests that this DDB formulation may form less precipitation when DDB soft capsules disintegrate and diffuse into the gastrointestinal fluid, resulting in improving the bioavailability Dissolution rate of DDB (7.5 mg) from sort elastic capsules of DDB-GAA-PEG 300 system was rapid. The supersaturation state was maintained for 2 hr at the concentration of 7.35$\pm$3.3 mg in 900 ml of water without precipitation. The total amount of DDB dissolved from this new formulation was 5.3 and 6.1 times higher, when compared to marketed DDB tablets (25 mg) and capsules (7.5 mg), respectively.

  • PDF

Physicochemical Characterization and Dissolution Properties of CS-891 with Different Crystallinity

  • Lee, Woo-Young;Park, Byoung-Woo;Park, Yong-Sun
    • Journal of Pharmaceutical Investigation
    • /
    • 제35권4호
    • /
    • pp.279-285
    • /
    • 2005
  • Ground CS-891 (N-[1-(4-methoxyphenyl)-1-methylethyl]-3-oxo-4-aza-5a-androst-1-ene-$17{\beta}$-carboxamide) of poorly water soluble drug was obtained using a Heiko Seisakusho model TI-100 vibration mill, and samples with different crystallinity were prepared at mixture ratios of 10:0, 7:3, 5:5, 3:7 and 0:10 (intact;ground CS-891). Physicochemical characterizations were obtained using qualitative and quantitative X-ray diffractometry, different scanning calorimetry (DSC), scanning electron microscopy (SEM), Quantasorb surface area analyzer, and controlled atmosphere microbalance. With increase of amorphous CS-891 in mixture ratios, the intensities of X-ray diffraction peaks of crystalline CS-891 were decreased, whereas surface area, water absorption, and exothermic peaks in DSC were increased. The apparent solubility of ground CS-891 was $4.4\;{\mu}g/ml$ and the solubility of intact CS-891 was $3.1\;{\mu}g/ml$ at $37{\pm}1^{\circ}C$. The apparent precipitation rates of CS-891 in a supersaturated solution during the solubility test were increased with an increase of amorphous CS-891, and a crystalline form of CS-891 transformed from amorphous CS-891 after the solubility test was found by X-ray diffraction analysis, DSC and SEM. The dissolution profiles of CS-891 with different crystallinity at $37{\pm}1^{\circ}C$ by the USP paddle method were investigated, and the apparent dissolution rate constant of ground CS-891 was about 5.9-fold higher than that of intact CS-891. A linear relationships between the crystallinity of CS-891 and the apparent dissolution rate constant (r>0.96) were obtained.

Continuous Preconcentration of Sn2+/Sn4+ by the On-line Sulfide Precipitation-Dissolution

  • Yeon, Pyung-Heum;Yoon, Young-Suk;Oh, Se-Woung;Nam, Sang-Ho;Par, Yong-Nam
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권8호
    • /
    • pp.1156-1160
    • /
    • 2004
  • The technique of an on-line preconcentration by the direct sulfide precipitation has been developed. Sn was homogeneously precipitated by sulfide, which was generated in situ from the hydrolysis of thioaceteamide. Precipitate was collected on a filter in the line and dissolved out instantaneously by KOH to be sent to an ICP. The enrichment factor was 4 with the sampling speed of 15/hr for 1.0 mL of sample. It was increased to more than 40 times when the sampling volume was increased to 10 mL with the sampling speed of 5/hr. $Sn^{2+}/Sn^{4+}$ could be separately determined with the on-line precipitation technique. The method was applied to the analysis of NIST SRM 1566 Oyster sample and yielded good agreement with the certified value.

수열합성법을 이용한 TiO2 나노 입자의 합성 (Synthesis of Nano-sized TiO2 Powder using a Hydrothermal Process)

  • 김강혁;이우진;김동규;이성근;이상화;김인수
    • 대한금속재료학회지
    • /
    • 제48권6호
    • /
    • pp.543-550
    • /
    • 2010
  • This paper investigated the synthesis conditions of nano-sized $TiO_2$ powder in a hydrothermal process at a temperature range of $100{\sim}180^{\circ}C$ considering the precipitation agent, precipitation pH, reaction temperature and time. Titanium hydroxide formed by $NH_4OH$ exhibited a lower crystallization temperature than that by NaOH and formed less aggregated $TiO_2$ particles. As the precipitation pH increased above 8, the shape of the particles changed from spherical to needle form, which appeared to be caused by dissolution and re-precipitation of the titanium hydroxide in an alkali environment.

Biocementation via soybean-urease induced carbonate precipitation using carbide slag powder derived soluble calcium

  • Qi, Yongshuai;Gao, Yufeng;Meng, Hao;He, Jia;Liu, Yang
    • Geomechanics and Engineering
    • /
    • 제29권1호
    • /
    • pp.79-90
    • /
    • 2022
  • Soybean-urease induced carbonate precipitation (EICP), as an alternative to microbially induced carbonate precipitation (MICP), was employed for soil improvement. Meanwhile, soluble calcium produced from industrial waste carbide slag powder (CSP) via the acid dissolution method was used for the EICP process. The ratio of CSP to the acetic acid solution was optimized to obtain a desirable calcium concentration with an appropriate pH. The calcium solution was then used for the sand columns test, and the engineering properties of the EICP-treated sand, including unconfined compressive strength, permeability, and calcium carbonate content, were evaluated. Results showed that the properties of the biocemented sand using the CSP derived calcium solution were comparable to those using the reagent grade CaCl2. Scanning electron microscopy (SEM) and X-ray diffraction (XRD) analyses revealed that spherical vaterite crystals were mainly formed when the CSP-derived calcium solution was used. In contrast, spherical calcite crystals were primarily formed as the reagent grade CaCl2 was used. This study highlighted that it was effective and sustainable to use soluble calcium produced from CSP for the EICP process.

산 침출 시 실리카 광물의 용해 및 제거 (Dissolution and Removal of Silicates in Acid Leaching Process)

  • 박경호;남철우;김현호
    • 자원리싸이클링
    • /
    • 제24권1호
    • /
    • pp.3-11
    • /
    • 2015
  • 산 침출에 있어서 생성되는 가용성 실리카는 고액분리 시 여과를 어렵게 하고 목적금속의 순도를 저하시키는 등 습식제련공정에 있어서 큰 문제점으로 대두되고 있다. 따라서 본 고에서는 실리케이트 광물과 산과의 반응성, 가용성 실리카의 특성, 제거방법에 대하여 검토하였다. 가용성 실리카는 알카리 전처리에 의한 제거, 결정상태의 $SiO_2$로 변환, 응집 등의 방법을 통한 여과성 향상 등의 방법으로 처리할 수 있다.