THREE DIMENSIONAL ATOM PROBE STUDY OF NI-BASE ALLOY/LOW ALLOY STEEL DISSIMILAR METAL WELD INTERFACES

  • Choi, Kyoung-Joon;Shin, Sang-Hun;Kim, Jong-Jin;Jung, Ju-Ang;Kim, Ji-Hyun
    • Nuclear Engineering and Technology
    • /
    • v.44 no.6
    • /
    • pp.673-682
    • /
    • 2012
  • Three dimensional atom probe tomography (3D APT) is applied to characterize the dissimilar metal joint which was welded between the Ni-based alloy, Alloy 690 and the low alloy steel, A533 Gr. B, with Alloy 152 filler metal. While there is some difficulty in preparing the specimen for the analysis, the 3D APT has a truly quantitative analytical capability to characterize nanometer scale particles in metallic materials, thus its application to the microstructural analysis in multi-component metallic materials provides critical information on the mechanism of nanoscale microstructural evolution. In this study, the procedure for 3D APT specimen preparation was established, and those for dissimilar metal weld interface were prepared near the fusion boundary by a focused ion beam. The result of the analysis in this study showed the precipitation of chromium carbides near the fusion boundary between A533 Gr. B and Alloy 152.

Characteristics of dissimilar laser welding of high Mn steel (고Mn강의 이종 레이저용접 특성)

  • Jeong, Bo-Yeong;Han, Tae-Gyo;Lee, Jong-Bong
    • Proceedings of the KWS Conference
    • /
    • 2007.11a
    • /
    • pp.190-192
    • /
    • 2007
  • High Mn steel has been developed for automotive applications since the steel has an excellent combination of strength and ductility. However, from the viewpoint of welding, high Mn steel has a few problems related to its chemical composition. In this study, development of dissimilar laser welding technology has been investigated for expanding application of high Mn steel. The results have shown that dissimilar weld joint between high Mn steel and carbon steel has poor erichsen property using STS309L filler wire or not.

  • PDF

Characterization of Mechanical Properties in the Heat Affected Zones of Alloy 82/182 Dissimilar Metal Weld Joint (Alloy 82/182 이종금속 용접부 열영향부의 기계적물성치 특성 파악)

  • Kim, Jin-Weon;Kim, Jong-Sung;Lee, Kyung-Soo
    • Proceedings of the KSME Conference
    • /
    • 2008.11a
    • /
    • pp.73-78
    • /
    • 2008
  • The paper presents the characteristics of mechanical properties within the heat affected zone (HAZ) of dissimilar metal weld between SA508 Gr.1a and F316 stainless steel (SS) with Alloy 82/182 filler metal. Tensile tests were performed using small-size specimens taken from the HAZ regions close to both fusion lines of weld, and the micro-structures were examined using optical microscope (OM) and transmission microscope (TEM). The results showed that significant gradients of the yield stress (YS), ultimate tensile stress (UTS), and elongations were observed within the HAZ of SA508 Gr.1a. This was attributed to the different microstructures within the HAZ. In the HAZ of F316 SS, however, the welding effect dominated the YS and elongation rather than UTS, and TEM micrographs conformed the strengthening in the HAZ of F316 SS was associated with a dislocation-induced strain hardening.

  • PDF

Characteristics of Dissimilar CO2 Laser Welding for High Mn Steel and Low Carbon Steel (고Mn강과 저탄소강의 CO2 레이저 이종용접 특성)

  • Jeong, Bo-Young;Han, Tae-Kyo
    • Journal of Welding and Joining
    • /
    • v.28 no.3
    • /
    • pp.36-41
    • /
    • 2010
  • High Mn steel has been developed for automotive applications since the steel has an excellent combination of strength and ductility. However, from the viewpoint of welding, high Mn steel has a few problems related to its chemical composition. This paper describes characteristics of dissimilar $CO_2$ laser welding for expanding application of high Mn steel. From this work it was cleared that dissimilar laser welded joint between high Mn steel and carbon steel had poor formability due to the formation of martensite within weld metal. In order to improve ductility of welded joint, the method of controlling the dilution ratio of high Mn steel was suggested.

Mechanics Evaluations of Stress Corrosion Cracking for Dissimilar Welds in Nuclear Piping System (원자력 배관 이종금속 용접부 웅력부식균열의 역학적 평가)

  • Park, Jun-Su;Na, Bok-Gyun;Kim, In-Yong
    • Proceedings of the KWS Conference
    • /
    • 2005.11a
    • /
    • pp.38-40
    • /
    • 2005
  • Fracture mechanics evaluation of stress corrosion cracking (SCC) in the dissimilar metal weld (DMW) for the nuclear piping system is performed; simulating the transition joint of the ferritic nozzle to austenitic safe-end fabricated with the Inconel Alloy A82/182 buttering and welds. Residual stresses in the DMW are computed by the finite element (FE) analyses Then, to investigate the SCC in the weld root under the combined residual and system operation stresses, the fracture mechanics parameters for a semi-elliptical surface crack are evaluated using the finite element alternating method (FEAM). As a result, it is found that the effect of weld residual stresses on the crack-driving forces is dominant, as high as three times or more than the operation stresses.

  • PDF

Crack growth analysis and remaining life prediction of dissimilar metal pipe weld joint with circumferential crack under cyclic loading

  • Murthy, A. Ramachandra;Gandhi, P.;Vishnuvardhan, S.;Sudharshan, G.
    • Nuclear Engineering and Technology
    • /
    • v.52 no.12
    • /
    • pp.2949-2957
    • /
    • 2020
  • Fatigue crack growth model has been developed for dissimilar metal weld joints of a piping component under cyclic loading, where in the crack is located at the center of the weld in the circumferential direction. The fracture parameter, Stress Intensity Factor (SIF) has been computed by using principle of superposition as KH + KM. KH is evaluated by assuming that, the complete specimen is made of the material containing the notch location. In second stage, the stress field ahead of the crack tip, accounting for the strength mismatch, the applied load and geometry has been characterized to evaluate SIF (KM). For each incremental crack depth, stress field ahead of the crack tip has been quantified by using J-integral (elastic), mismatch ratio, plastic interaction factor and stress parallel to the crack surface. The associated constants for evaluation of KM have been computed by using the quantified stress field with respect to the distance from the crack tip. Net SIF (KH + KM) computed, has been used for the crack growth analysis and remaining life prediction by Paris crack growth model. To validate the model, SIF and remaining life has been predicted for a pipe made up of (i) SA312 Type 304LN austenitic stainless steel and SA508 Gr. 3 Cl. 1. Low alloy carbon steel (ii) welded SA312 Type 304LN austenitic stainless-steel pipe. From the studies, it is observed that the model could predict the remaining life of DMWJ piping components with a maximum difference of 15% compared to experimental observations.

Laser Welding of Seal Tube for Instrumented Irradiation Fuel Test (계장핵연료 조사시험용 실튜브 레이저용접기술)

  • Kim Soo-Sung;Lee Chul-Yong;Kim Woong-Ki;Park Geun-Il;Koh Jinh-Yun;Seo Jun-Seok
    • Journal of Welding and Joining
    • /
    • v.23 no.6
    • /
    • pp.43-48
    • /
    • 2005
  • This work was carried out to obtain sound welds and to select a most suitable binary metal joint among three different dissimilar binary metal combinations such as Zr-4/Ta, Mo/Ta and Ti/Ta(seal tube/sensor sheath) joints fur the instrumented nuclear fuel irradiation test. To do this, Taguchi experimental method was employed to optimize the experimental data. In addition, metallography, micro-focus x-ray radiography and hardness test were conducted to examine the welds. From the weld bead appearance, penetration depth and bead width as well as weld defects standpoint, Zr-4/Ta joint is suggested for the circumferential joining between a seal tube and a sensor sheath. The optimized welding parameters based on Zr-4/Ta joint are suggested as well.

Microstructure of Electron Beam Welded Cu / STS 304 Dissimilar Materials (전자빔 용접된 Cu / STS 304강의 미세조직에 관한 연구)

  • Park, Kyoung-Tae;Kim, In-Ho;Baek, Jun-Ho;Chun, Byung-Sun
    • Journal of Welding and Joining
    • /
    • v.28 no.2
    • /
    • pp.47-53
    • /
    • 2010
  • According to the research report for the recent a few years, the dissimilar welding of Cu and STS 304 alloy have been presented that a weldability is very poor. This article present a study on Lap joint by Electron beam welding dissimilar materials. The weld metals was constituted between pure copper and STS 304 steel. The experiment was performed with 125mA welding current, 520mA focusing current. The Vacuum condition of chamber is 5${\times}$10-5torr and welding speed is 300mm/min. Showing the bead shape of weld metal, the thickness of the stainless 304 using as the protect materials is 3mm and the thickness of a copper is 15mm. The analysis about the microstructure were carried out in which it was observed with SEM. The results showed that complex heterogeneous fusion zone microstructure characterized both by rapid cooling and mixing of the molten metal, however the liquation crack was formated in the fusion line.

Studies on weldment performance of Ti/Al dissimilar sheet metal joints using laser beam welding

  • Kalaiselvan, K.;Elango, A.;Nagarajan, N.M.;Mathiazhagan, N.;Vignesh, Kannan
    • Coupled systems mechanics
    • /
    • v.7 no.5
    • /
    • pp.627-634
    • /
    • 2018
  • Laser beam welding is more advantageous compared to conventional methods. Titanium/Aluminium dissimilar alloy thin sheet metals are difficult to weld due to large difference in melting point. The performance of the weldment depends upon interlayer formation and distribution of intermetallics. During welding, aluminium gets lost at the temperature below the melting point of titanium. Therefore, it is needed to improve a new metal joining techniques between these two alloys. The present work is carried for welding TI6AL4V and AA2024 alloy by using Nd:YAG Pulsed laser welding unit. The performance of the butt welded interlayer structures are discussed in detail using hardness test and SEM. Test results reveal that interlayer fracture is caused near aluminium side due to low strength at the weld joint.

Friction Welding of Dissimilar Press Punch Materials and Its Evaluation by AE (신소재 금형펀치의 이종재 마찰용접 개발과 AE품질평가를 위한 연구)

  • 오세규;박일동;이원석
    • Journal of Welding and Joining
    • /
    • v.15 no.2
    • /
    • pp.43-53
    • /
    • 1997
  • The complete joining method for dissimilar press punch materials and its real-time evaluation method is not available at present. Brazing method has been used for joining them, but it is known that the welded joint by the brazing has the lower bonding efficiency and reliability than the diffusion welding. The friction welding with a diffusion mechanism in bonding was applied in this study. This work was carried out to determine the proper friction welding conditions and to analyze mechanical properties of friction welded joints of sintered carbide tool materials (SKNM50 for the blade part of press punch) to alloy steel (SCM440 for the shank part of press punch) using aluminum (A6061 for the interlayer material) as an insert material between the sintered carbide tool materials and the alloy steel. In addition, acoustic emission test was carried out during friction welding to evaluate the weld quality.

  • PDF