• 제목/요약/키워드: Disperse

검색결과 648건 처리시간 0.021초

Relation between Chemical Structure of Yellow Disperse Dyes and Their Lightfastness

  • Kim, Sung-Dong;Park, Eun-Jin
    • Fibers and Polymers
    • /
    • 제2권3호
    • /
    • pp.159-163
    • /
    • 2001
  • Five yellow disperse dyes were synthesized and their dyeing, fastness and photodegradation behaviors were investigated. It was found that dyes derived from phenylindole and N-alkylaminobenzene showed dye uptake directly proportional to the dye concentration, but the build-up of dyes derived from carbazole and pyridone were not good. The wavelength at maximum absorption. molar extinction coefficient. and the tendency to the photodegradation were strongly dependent on the electron donating ability of the coupling component. The dye, whose coupling component was phenylindole, possessed the excellent dyeing properties and the high degree of lightfastness. UVA had an effect on the inhibition of the photodegradation especially for the easily photodegradabte dyes.

  • PDF

분산염료 분자구조에 따른 PET-PU blend의 염색성 (Dyeing properties of PET-PU according to molecular structure of disperse dye)

  • 박종호;이종렬;최연지;이주은;김성동
    • 한국염색가공학회:학술대회논문집
    • /
    • 한국염색가공학회 2008년도 제38차 학술발표대회
    • /
    • pp.80-82
    • /
    • 2008
  • The distributions of 3 disperse dyes with different molecular structures among polyurethane (PU) and polyester (PET) in dyeing PET-PU blend and which dye structure contaminated less PU portion were studied. The amounts of dyes left substrates after reduction clearing and washing were measured to prove which dye structure had an effect on improving washing fastness. Disperse dye with high molecular weight showed similar distribution onto PU and polyester by dying both substrates with similar rate and less contamination to polyurethane while other dyes distributed to PU faster than to PET had.

  • PDF

Dyeing Performance of Disperse Dyes Based on 2-aminothiazole for Cellulose Triacetate and Nylon Fibers

  • Maradiya, Hari-Raghav;Patel, Vithal-Soma
    • Fibers and Polymers
    • /
    • 제3권1호
    • /
    • pp.43-48
    • /
    • 2002
  • A series of monoazo disperse dyes based on 2-amino-4-phenylthiazole was prepared using various N,N-dialkvlaniline derivatives as the coupling component. The dyes were characterized by IR spectral studies, visible absorption spectroscopy and elemental analysis. The dyeing performance of these dyes was assessed on cellulose triacetate and nylon fibers. These dyes were found to give a wide range of colour shades varying from bright red to royal blue with very good depth, brightness and levelness on fibers. The dyed fibers showed good to very good light fastness and very good to excellent fastness to washing, perspiration, rubbing and sublimation. The dyebath exhaustion and fixation on the fibers were found to be very good.

가교제와 분산염료를 이용한 면/폴리에스테르 혼방직물의 염색 - 그에 따른 물성 변화 및 염색견뢰도 - (Dyeing of Cotton/Polyester Blends with Disperse Dyes and Crosslinking Agent - The Changes of Physical Properties and Colorfastness -)

  • 김은아;유효선
    • 한국의류학회지
    • /
    • 제26권10호
    • /
    • pp.1401-1411
    • /
    • 2002
  • To Save energy and cost one bath/one step dyeing and finishing on cotton/polyester blends is carried out with disperse dyes in the presence of crosslinking agent. Cotton 100 %, cotton/polyester 70/30, 50/50, 35/65, polyester 100 % fabrics were used. wrinkle recovery angle, tensile strength retention and tearing strength retention were determined in according to the dyebath composition, and also determined while the concentration of DMDHEU, molecular weight and concentration of PEG were varied. Colorfastness to abrasion, washing and light were tested. For cotton and cotton/polyester blends dyed in the presence of DMDHEU/PEG, wrinkle recovery was improved. Tensile strength retention and tearing strength retention were decreased, in compared with dyed fabrics without DMDHEU. Colorfastness to abrasion was good but colorfastness to washing and to light were poor for the fabrics dyed in the presence of DMDHEU/PEG.

Dyeing Properties of Polyurethane-impregnated PET Knit

  • Park, Jong-Ho;Kim, Sung-Dong
    • 한국염색가공학회지
    • /
    • 제20권5호
    • /
    • pp.35-40
    • /
    • 2008
  • Dyeing and washing fastness properties of polyurethane-impregnated polyester (PU-impregnated PET), and the distribution of two disperse dyes between PET and PU film were studied to investigate the effect of PU portion to exhaustion and washing fastness. Dyeing properties of PU-impregnated PET were quite different with those of PET: PU-impregnated PET absorbed disperse dye linearly from the early stage of dyeing to equilibrium, and it exhibited excellent build-up property up to 4 %owf dyeing. The absorbed dye on PU film at early dyeing stage migrated to more substantive PET at the temperature higher than $115^{\circ}C$. The amount of exhausted dye on PET portion was larger than on PU film and the distribution ratio was $2.08{\sim}2.34$. The grade of washing fastness of PU-impregnated PET was the same as or lower by $0.5{\sim}1$ grade than PU film whose washing fastness was lower by $0.5{\sim}1$ than PET.

Dyeing Study on DMF-Modified Polyesters for Morphology Characterization

  • Park, Myung-Ja
    • The International Journal of Costume Culture
    • /
    • 제5권2호
    • /
    • pp.53-65
    • /
    • 2002
  • Morphology of polyester fiber was physically modified by solvent treatment. PET fiber was treated with N,N-dimethylformamide (DMF) at 100, 120, $140^{circ}C$ for 10 minutes without tension. The structural changes in the morphology of DMF-induced modified PET fiber were FTIR and SEM analysis. Also dyeing behavior of DMF-treated polyester fibers with various disperse dyes was studied to detect changes of amorphous area in fine structure. DMF treatment resulted in increases in total void content, degree of crystallinity, trans isomer content, chain folding, segmental mobility and molecular packing, but it resulted in decreases in amorphous orientation, intermolecular forces and individual void size through longitudinal shrinkage, lateral welling and removal of oligomers. Void-size distribution could be estimated from the dye uptake with various sizes of disperse dyes. In contrast to the large increases in dye uptake with small dye molecules, there is no and little dye uptake with the bulkiest dye, which means that void size is bigger or smaller than the volume of each dye. Diffusion rates of dye molecules showed increases. This dyeing study revealed that the disperse dyeing is very effective method for characterizing the internal morphology of polyester fiber.

  • PDF

용제염색에 관한 기초적 연구 제2보 물, TCE 및 물/TCE 처리를 한 PET의 염색성 (A Foundamental Study on the Solvent Dyeing Part 2. Dyeing Properties of PET Treated with Water, TCE and water/TCE Emulsion)

  • 정두진
    • 한국의류학회지
    • /
    • 제3권2호
    • /
    • pp.37-41
    • /
    • 1979
  • In order to obtain tasic information for solvent dyeing, polyethylene terephthalate (PET) films was pretreated with water, tetrachloroethylene (TCE) and water/TCE emulsion for three hours at $140^{\circ}C$ for stabilizing the substrate. By film roll cyliderical method, Disperse Red 60, Disperse Yellow 42, and Disperse Blue 27 were diffused in the films and examined dyeing properties. The results are summarized as follows; 1) Diffusion coefficient increases in the order, waterTCE>water/TCE 2) A linear relationship between diffusion coefficient and shrinkage was Observed 3) The temperature dependence of the diffusion coefficient can't be expressed by WLF equation.

  • PDF

초임계 이산화탄소에 의한 아라미드(Nomex) 방적사의 분산염료에 대한 염색성에 관한 연구 (A Study on Dyeing Ability of Aramid(Nomex) Spun Yarn in Supercritical Carbon Dioxide using Disperse dyes)

  • 용관중;박영환;김한석;유기풍;김인회;남성우
    • 한국염색가공학회지
    • /
    • 제15권2호
    • /
    • pp.93-101
    • /
    • 2003
  • To acquire dyeing ability on aramid(Nomex) spun yarn in supercritical fluid dyeing, supercritical fluid dying(SFD) machine of 3L scale was designed. C. I. Disperse Red 60 and Red 360 were used in this work. It was possible to increase dyeing ability and to get level dyeing of fiber by attaching assistance devices(controlling device of supercritical fluid, nozzle, cover of carrier, etc.) to SFD machine. Physical properties(tensile strength, elongation, shrinkage) of Nomex spun yam treated by SFD were not changed. K/S values of dyed Nomex spun yam with Red 360 were higher than that with Red 60 and color fastness of dyed Nomex spun yam by SFD was similar to that by conventional dyeing method.

폴리에스테르/카티온화 면 혼방품의 분산염료/반응성염료에 의한 일욕염색계에 관한 연구 (Studies on the One Bath Exhaust Dyeing System of Polyester/Cationized Cotton Blends with Disperse Dye/Reactive Dye)

  • 성우경
    • 한국염색가공학회지
    • /
    • 제10권2호
    • /
    • pp.18-28
    • /
    • 1998
  • in order to overcome disadvantage of the conventional two bath dyeing method of polyester/cotton blends, it had prompted significant effort to the development of the one bath dyeing method which can accomplish sayings in time, energy and water usage. Also, when dyeing polyester/cotton blends by the one bath dyeing method, the high salt concentrations needed for the reactive dye can cause particles of disperse dye, used for the polyester component, to aggregate. A supplementary problem that can occasionally be happened is the change of hue that occurs on dyed polyester in an alkaline dyebath. To improve dyeing property of polyester/cotton blends, cotton component was pretreated with epichlolohydrine-trimethylamine hydrochloride in aqueous solution of sodium hydroxide to produce a cationized cotton that can be dyed under neutral conditions with reactive dye in a non-electrolytic or il little electrolytic dyebath. The one bath dyeing method of polyester/cationized cotton blends with disperse dye/reactive dye mixture resulted in a satisfactory dyeing property and color yield in comparison with ordinary two bath dyeing method.

  • PDF

비수계 염색용 마이크로캡슐의 제조 및 성질 (Preparation and Characterization of Microcapsule for non-aqueous dyeing)

  • 최창남;박원규;변수진;이기영
    • 한국염색가공학회지
    • /
    • 제15권5호
    • /
    • pp.327-332
    • /
    • 2003
  • In this study, the polyurethane microcapsules for non-aqueous dyeing containing iron oxide and disperse dyes were prepared by in-situ polymerization method using hexamethylene diisocyanate(HDI) with ethylene glycol(EG). And the size, shape, and particle size distribution of microcapsules prepared were investigated. The size and shape of microcapsule were observed by optical microscope and scanning elecron microscope. The particle size distribution was analyzed by particle size analyzer. The microcapsule size and its distribution were largely effected by the existance of surface active agent in the system. When a surfactant did not exist in the system, the size distribution of microcapsules prepared was much uneven. By adding a surfactant, this phenomenon was disappeared. And the size of microcapsule was also effeced by the hydrophobicity of core material(disperse dye). It was considered due to the difference of dispersity of core materials. And the size of microcapsule prepared was inversely proportional to the stirring speed.