Al-Zn 합금의 직접용융산화법을 이용한 ZnO 나노와이어의 제작 (Fabrication of ZnO Nanowires by Direct Melt Oxidation of Al-Zn Alloy)

  • 이근형;김일수;신병철;이원재
    • 한국전기전자재료학회논문지
    • /
    • 제21권11호
    • /
    • pp.995-999
    • /
    • 2008
  • ZnO nanowires with tetrapod shape were formed on the surface of the sample by direct melt oxidation of Al-Zn alloy at $1000^{\circ}C$ in air. X-ray diffraction (XRD) pattern revealed that the ZnO nanowires had wurtzite structure of hexagonal phase. Any other element except Zn and O was not detected in energy dispersive X-ray spectrum. The c- and a-axis lattice constants estimated from the XRD pattern were 0.520 and 0.325 nm, respectively. These are in well accordance with those of bulk ZnO single crystal, indicating high quality crystallinity. The green light emission at a wavelength of 510 nm was observed from the nanowires at room temperature, which was ascribed to high density of oxygen vacancies in nanowires.

Cu-C$u_2$O의 공정반응에 의한 구리와 알루미나의 직접접합 (The Direct Bonding of Copper to Alumina by $Cu-Cu_2$O Eutectic Reaction)

  • 유환성;이임열
    • 한국재료학회지
    • /
    • 제2권4호
    • /
    • pp.241-247
    • /
    • 1992
  • 본 연구에서는 $Cu-Cu_2$O의 공정반응에 의한 구리와 알루미나의 직접접합에 대하여 연구 하였다. $1.5{\times}10^{-1}$torr, $1015^{\circ}C$에서 산화시킨 후 $10_{-3}$torr, 107$5^{\circ}C$에서 접합시킨 시편의 접합력과 계면특성을 인장시험, SEM, EDS 및 XRD를 통하여 분석하였다. 3분 산화시켜 접합하면 우수한 접합강도를 보이며 산화시간이 이보다 짧거나 길면 결합력은 저하하였다. 과단은 알루미나 공정조직 계면에서 발생하였으며 파단후 $Al_2O_3$표면에는 Cu쪽에서 빠져나간 $Cu_2$O nodule의 존재하였는 바 접합력은 $Cu_2$O-A$l_2O_3$계면보다는 $Cu-Cu_2$O계면에 좌우됨을 보여주고 있다. 접합력은 접합시간에 따라 완만한 증가를 보였으며 CuA$l_2O_4$$CuAlO_2$의 반응생성물이 접합중 형성되었다.

  • PDF

APPLICATION OF UNCERTAINTY ANALYSIS TO MAAP4 ANALYSES FOR LEVEL 2 PRA PARAMETER IMPORTANCE DETERMINATION

  • Roberts, Kevin;Sanders, Robert
    • Nuclear Engineering and Technology
    • /
    • 제45권6호
    • /
    • pp.767-790
    • /
    • 2013
  • MAAP4 is a computer code that can simulate the response of a light water reactor power plant during severe accident sequences, including actions taken as part of accident management. The code quantitatively predicts the evolution of a severe accident starting from full power conditions given a set of system faults and initiating events through events such as core melt, reactor vessel failure, and containment failure. Furthermore, models are included in the code to represent the actions that could mitigate the accident by in-vessel cooling, external cooling of the reactor pressure vessel, or cooling the debris in containment. A key element tied to using a code like MAAP4 is an uncertainty analysis. The purpose of this paper is to present a MAAP4 based analysis to examine the sensitivity of a key parameter, in this case hydrogen production, to a set of model parameters that are related to a Level 2 PRA analysis. The Level 2 analysis examines those sequences that result in core melting and subsequent reactor pressure vessel failure and its impact on the containment. This paper identifies individual contributors and MAAP4 model parameters that statistically influence hydrogen production. Hydrogen generation was chosen because of its direct relationship to oxidation. With greater oxidation, more heat is added to the core region and relocation (core slump) should occur faster. This, in theory, would lead to shorter failure times and subsequent "hotter" debris pool on the containment floor.

MgO를 이용한 다공성 탄소 섬유 제조 및 이를 이용한 연료전지용 촉매 특성 (Preparation of Porous Carbon Fiber by Using MgO Powder and Its Characteristics of Catalysts for Fuel Cell)

  • 남기돈;김상경;임성엽;백동현;이병록;정두환
    • Korean Chemical Engineering Research
    • /
    • 제46권6호
    • /
    • pp.1142-1147
    • /
    • 2008
  • Nano-MgO와 메조페이스 피치로부터 복합 탄소섬유를 만들고 MgO를 제거함으로써 직접 메탄올 연료전지용 촉매 담지체로서의 다공성 탄소섬유를 제조하였다. 이 다공성 탄소섬유의 비표면적은 $8{\sim}58m^2/g$ 이고, 표면기공구조는 마이크로기공이 거의 없이 MgO 입자크기 유래의 메조기공(10~15 nm)으로 구성된 것이 특징이며, MgO 혼입량(1~10 wt%)에 따라 조절할 수 있었다. 본 다공성 탄소섬유를 담지체로 이용하여 함침법으로 60 wt% Pt-Ru 촉매를 담지하였으며, 제조된 Pt-Ru 촉매의 메탄올 산화 특성 및 단위전지 성능 측정 결과 상용촉매에 비하여 5~10% 이상 향상된 값을 나타내었다