• Title/Summary/Keyword: Differential Shrinkage

Search Result 79, Processing Time 0.024 seconds

Synthesis and characterization of Mg-Si thermoelectric compound subjected to mechanical alloying (기계적 합금화에 의한 Mg-Si계 열전화합물의 합성 및 평가)

  • Lee, Chung-Hyo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.3
    • /
    • pp.121-127
    • /
    • 2007
  • We have applied mechanical alloying (MA) to get $Mg_2Si$ thermoelectric material with nano-sized grains. An optimal milling and heat treatment conditions to obtain the single phase of $Mg_2Si$ compound with fine microstructure were investigated by X-ray diffraction and differential scanning calorimetry (DSC) measurement. The $Mg_{66.7}Si_{33.3}$ MA samples ball-milled for $20{\sim}180\;hrs$ exhibit two broad exothermic heat releases around $220^{\circ}C$ and $570^{\circ}C$. On the other hand, MA sample ball-milled far 260 hrs exhibits only a sharp exothermic peak at $230^{\circ}C$ Single phase Mg2Si powder can be obtained by MA of $Mg_{66.7}Si_{33.3}$ mixture for 60 hours and subsequently heated up to $620^{\circ}C$. Sintering of the MA powders was performed in a spark plasma sintering (SPS) machine using graphite dies at $800{\sim}900^{\circ}C$ under 50 MPa. The shrinkage of sintering sample during SPS was significant at about $200^{\circ}C$. All compact bodies have a high relative density above 94% with metallic glare on the surface.

The Characteristics of Vacuum Drying Disks of Domestic Softwoods (I) (국산 침엽수재 원판(圓板)의 진공건조(眞空乾燥) 특성 (I))

  • Lee, Nam-Ho;Lee, June-Ho;Kim, Jong-Mann;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.24 no.2
    • /
    • pp.46-54
    • /
    • 1996
  • This study was carried out to investigate the vacuum drying characteristics of 50mm- and 75mm- thick tree disks of some domestic softwoods for substituting the conventional hardwoods as the materials for wood crafts. Though the elapsed drying times from green to in-use moisture content(MC) were largely shortened by vacuum drying, the tree disks treated by EWS couldn't be dried to in-use MC, and so sapwood stains also were occurred severely. We suggest EWS treatment is undesirable for the species with very high sapwood portion or vacuum drying with hot water circulation heating system. Heart checks were slight, but sapwood checks, which have never been trouble in drying process of tree disks, were severe. For the reasonable explanation it is suggested MC differences between sapwood and heartwood were large and most of tree disks had already no barks before drying test. Ginkgo was vacuum-dried with very slight drying defects such as heart checks, sapwood checks. V-cracks and sapwood stains. In Korean red pine and pitch pine V-cracks were severely occurred. And it was found the special feature that most of these defected tree disks contained several V-cracks within one tree disk. It can be considered as the causes that the region of sapwood was defected by the several checks at the early drying stage because of the steep MC gradient along the radial direction, and then at the later drying stage the drying stresses due to differential shrinkage were concentrated on these brittle spots.

  • PDF

Investigation on Behaviors of Concrete Interfaces Repaired Using Anchors (앵커로 보수한 콘크리트 계면 거동의 고찰)

  • Song Hyung-Soo;Lee Chin-Yong;Yoon Dong-Yong;Min Chang-Shik;Choi Dong-Uk
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.6 s.90
    • /
    • pp.885-892
    • /
    • 2005
  • Recently, the damaged concrete structures are often strengthened or repaired using the polymer concrete or the polymer cement mortar. In the repaired concrete structures at early ages, internal stresses could be developed due to the differential drying shrinkage of the repair material. Due to the difference of the thermal coefficients of the repair material and existing concrete, additional stresses also could be developed as the structures are subjected to the ambient temperature changes. Theses environmentally-induced stresses can sometimes be large enough to cause damage to the structures, such as debonding of the interface between the two materials. In this study, a rational procedure was developed where anchors can be designed and installed to prevent damages in such structures by thermally-induced stresses. Finally, through the experimental study and numerical study, the effects of the repair method using anchors with debonding was investigated and discussed the results.

Homogeneous Shape Forming of Alumina by Pressure-Vacuum Hybrid Slip Casting (가압-진공 하이브리드 주입성형에 의한 알루미나의 균질 성형)

  • Cho, Kyeong-Sik;Song, In-Beom;Kim, Jae
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.6
    • /
    • pp.592-600
    • /
    • 2012
  • Conventional methods for preparing ceramic bodies, such as cold isostatic pressing, gypsum-mold slip casting, and filter pressing are not completely suitable for fabricating large and thick ceramic plates owing to disadvantages of these processes, such as the high cost of the equipment, the formation of density gradients, and differential shrinkage during drying. These problems can be avoided by employing a pressure-vacuum hybrid slip casting approach that considers not only by the compression of the aqueous slip in the casting room (pressure slip casting) but also the vacuum sucking of the dispersion medium (water) around the mold (vacuum slip casting). We prepared the alumina formed bodies by means of pressure-vacuum hybrid slip casting with stepwise pressure loading up to 0.5 MPa using a slip consisting of 40 vol% solid, 0.6 wt% APC, 1 wt% PEG, and 1 wt% PVA. After drying the green body at $30^{\circ}C$ and 80% RH, the green density of the alumina bodies was about 56% RD. The sintered density of an alumina plate created by means of sintering at $1650^{\circ}C$ for 4 h exceeded 99.8%.This method enabled us to fabricate a $110{\times}110{\times}20$ mm alumina plate without cracks and with a homogeneous density, thus demonstrating the possibility of extending the method to the fabrication of other ceramic products.

The Behavior Characteristics of Segmental Crib Retaining Wall by Model Test (모형실험에 의한 조립식 격자 옹벽의 거동 특성)

  • 김상수;신방웅;김용언;이재영;변동건
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 1999.10a
    • /
    • pp.449-456
    • /
    • 1999
  • The concrete wall is the most useful of retaining structure which can obtain the engineering stability, but has problems that is not friendly with nature environment in a fine view, such as poor rear drainage, and shrinkage crack by temperature difference, etc. Because of this problems, the research for a segmental crib retaining wall has been performed. A segmental crib retaining wall is quickly and easily erected because is possible to be erected as the individual members, and is not sensitive to differential settlement and earthquakes. Also, it shows effective drainage and has a friendly advantage with nature environment because of being able to be planted with vines and shrubs in retaining walls The design of crib retaining walls has traditionally been based on classical soil mechanics theories. These theories, originally derived by Rankine(1857) and Coulomb(1776), assume that the wall acts as a rigid body. This assumption results in failure being predicted by either monolithic overturning or base sliding mechanisms. However, the wall consists of individual members which have been created a three dimensional grid. This grid confines an fill mass which becomes part of the wall. The filled wall resists the earth pressure with the same mechanism of classical gravity walls. Because of the flexibility of the individual segment, it allows relative movement between the individual members within the wall. The three dimensional flexible grid leads to stress redistribution when the wall is subjected to external or fill loads. Due to the flexibility and the stress redistribution, the failure of segmental crib wall consists of not only overturing and base sliding but the local deformation and the failure between the segmental members. It has been researched in the field that due to this flexibility and load redistribution, serviceability failure of segmental crib walls is unlikely to be due to overturning or base sliding. Therefore, in this study, the relative displacement appearance of retaining wall due to variation of inclination is measured to examine this behavior characteristics. Also, the behavior characteristics of retaining walls by surcharge load, and location of acting point of retaining wall rear, and the displacement characteristics and deflections are estimated about the existence and nonexistence of Rear Stretcher performing an role in transmitting earth pressure of Header and Stretcher organizing retaining walls. This research focuses on the characteristics due to the behavior of retaining walls. This research focuses on the characteristics due to the behavior of retaining walls.

  • PDF

Characterization and consolidation of thermoelectric CrSi2 compound prepared by mechanical alloying (MA법으로 제조된 CrSi2 열전화합물의 평가 및 치밀화)

  • Lee, Chung-Hyo;Kim, Young
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.3
    • /
    • pp.135-141
    • /
    • 2013
  • Mechanical alloying was carried out to produce $CrSi_2$ thermoelectric compound using a mixture of elemental $Cr_{33}Si_{67}$ powders. An optimal milling and heat treatment conditions to obtain the single phase of $CrSi_2$ compound with fine microstructure were investigated by X-ray diffraction and differential scanning calorimetry measurement. $CrSi_2$ intermetallic compound with a grain size of 70 nm could be obtained by MA of $Cr_{33}Si_{67}$ powders for 70 hours and subsequently annealed at $650^{\circ}C$. Consolidation of the MA powders was performed in a spark plasma sintering (SPS) machine using graphite dies at $600{\sim}1000^{\circ}C$ under 60 MPa. The shrinkage of MA samples during SPS consolidation process increased gradually with increasing temperature up to $1000^{\circ}C$ and relatively significant at about $600^{\circ}C$. We tend to believe that these behaviors are deeply related to form a $CrSi_2$ compound during heating process, as can be realized from the DSC measurement. Electrical conductivity and Seebeck coefficient of sintered bodies were measured up to $900^{\circ}C$. Seebeck coefficient and power factor of $Cr_{33}Si_{67}$ compact prepared by MA and SPS at $1000^{\circ}C$ showed the maximum value of $125{\mu}V/K$ at $400^{\circ}C$ and $4.3{\times}10^{-4}W/mK^2$ at $350^{\circ}C$, respectively.

Studies on the Physical Properties of Major Tree Barks Grown in Korea -Genus Pinus, Populus and Quercus- (한국산(韓國産) 주요(主要) 수종(樹種) 수피(樹皮)의 이학적(理學的) 성질(性質)에 관(關)한 연구(硏究) -소나무속(屬), 사시나무속(屬), 참나무속(屬)을 중심(中心)으로-)

  • Lee, Hwa Hyoung
    • Journal of Korean Society of Forest Science
    • /
    • v.33 no.1
    • /
    • pp.33-58
    • /
    • 1977
  • A bark comprises about 10 to 20 percents of a typical log by volume, and is generally considered as an unwanted residue rather than a potentially valuable resourses. As the world has been confronted with decreasing forest resources, natural resources pressure dictate that a bark should be a raw material instead of a waste. The utilization of the largely wasted bark of genus Pinus, Quercus, and Populus grown in Korea can be enhanced by learning its physical and mechanical properties. However, the study of tree bark grown in Korea have never been undertaken. In the present paper, an investigative study is carried out on the bark of three genus, eleven species representing not only the major bark trees but major species currently grown in Korea. For each species 20 trees were selected, at Suweon and Kwang-neung areas, on the same basis of the diameter class at the proper harvesting age. One $200cm^2$ segment of bark was obtained from each tree at brest height. Physical properties of bark studied are: bark density, moisture content of green bark (inner-, outer-, and total-bark), fiber saturation point, hysteresis loop, shrinkage, water absorption, specific heat, heat of wetting, thermal conductivity, thermal diffusivity, heat of combustion, and differential thermal analysis. The mechanical properties are studied on bending and compression strength (radial, longitudinal, and tangential). The results may be summarized as follows: 1. The oven-dry specific gravities differ between wood and bark, further more even for a given bark sample, the difference is obersved between inner and outer bark. 2. The oven-dry specific gravity of bark is higher than that of wood. This fact is attributed to the anatomical structure whose characters are manifested by higher content of sieve fiber and sclereids. 3. Except Pinus koraiensis, the oven-dry specific gravity of inner bark is higher than that of outer bark, which results from higher shrinkage of inner bark. 4. The moisture content of bark increases with direct proportion to the composition ratio of sieve components and decreases with higher percent of sclerenchyma and periderm tissues. 5. The possibility of determining fiber saturation point is suggested by the measuring the heat of wetting. With the proposed method, the fiber saturation point of Pinus densiflora lies between 26 and 28%, that of Quercus accutissima ranges from 24 to 28%. These results need be further examined by other methods. 6. Contrary to the behavior of wood, the bark shrinkage is the highest in radial direction and the lowest in longitudinal direction. Quercus serrata and Q. variabilis do not fall in this category. 7. Bark shows the same specific heat as wood, but the heat of wetting of bark is higher than that of wood. In heat conductivity, bark is lower than wood. From the measures of oven-dry specific gravity (${\rho}d$) and moisture fraction specific gravity (${\rho}m$) is devised the following regression equation upon which heat conductivity can be calculated. The calculated heat conductivity of bark is between $0.8{\times}10^{-4}$ and $1.6{\times}10^{-4}cal/cm-sec-deg$. $$K=4.631+11.408{\rho}d+7.628{\rho}m$$ 8. The bark heat diffusivity varies from $8.03{\times}10^{-4}$ to $4.46{\times}10^{-4}cm^2/sec$. From differential thermal analysis, wood shows a higher thermogram than bark under ignition point, but the tendency is reversed above ignition point. 9. The modulus of rupture for static bending strength of bark is proportional to the density of bark which in turn gives the following regression equation. M=243.78X-12.02 The compressive strength of bark is the highest in radial direction, contrary to the behavior of wood, and the compressive strength of longitudinal direction follows the tangential one in decreasing order.

  • PDF

Preservation of Strawberries and Cucumbers Packaged by Low density polyethylene film impregnated with antimicmbial agent, Scutellariae baicalensis extract (황금추출물을 함유한 항균성 포장필름을 이용한 딸기와 오이의 저장효과)

  • 정순경;조성환
    • Food Science and Preservation
    • /
    • v.9 no.3
    • /
    • pp.271-276
    • /
    • 2002
  • To develop a wrapping film, which suppresses the microbial decay through the storage and prolongs the selflife of fruits and vegetables, the antimicrobial packaging films were prepared and applied to the preservation of strtwberries and cucumbers. Low density polyethylene(LDPE) film of 50㎛ thickness was faricated with 1% of Scutellariae baicalensis extract. The LDPE film impregnated with Scutellariae baicalensis extract showed antimicrobial activity on the disk test against Bacillus cereus, Escherchia coli and Fusarium sp.. The antimicrobial film changed the color and light transmittance, but did not affect heat shrinkage, mechanical tensile strength and wattability. Strawberries and cucumbers were separately wrapped with packaging films in the state of closely-adhered packaging as well as modified atmosphere packaging(MAP). The wrapped strawberries and cucumbers were stored for 21 days at 5$\^{C}$ and for 40 days at l0$\^{C}$, respectively. For the packaged strawberries and cucumbers at 5$\^{C}$ and 10$\^{C}$, the LDPE film impregnated with Scutellariae baicalensis extract showed the reduced growth of total aerobic bacteria, molds and yeasts and did not give any negative effect on other quality attributes during storage in comparison with conttrol film without any additive.

Model of Drying Stress Distribution in Disks End-wrapped in Korean Paper and Effects of End-wrappings on Prevention of Drying Defects for Vacuum Drying of Disks (한지(韓紙) 엔드래핑처리 원판(圓板)의 감압건조응력(減壓乾燥應力) 분포모형(分布模型) 및 엔드래핑스의 건조결함(乾燥缺陷) 예방효과(豫防效果))

  • Lee, Nam-Ho;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.19 no.1
    • /
    • pp.31-63
    • /
    • 1991
  • It was proved that in conventional kiln drying of disks piling position in the kiln exerted a great influence on drying rates, and the larger the variation of disk diameter, the more undulating drying rates of disks. While in vacuum drying disks there was no influence on drying rates. By the end-wrapping treatments and the radial direction of disks tangential surface stresses in the core of disks were slightly compressive in three species. In control disks the drying stresses distributed into one step-style that compressive stresses in the pith side of 6cm from pith were larger than those in the bark side, while in the disks end-wrapped with Korean paper the drying stresses distributed uniformly, because flow rates of free water in disks had no difference between heart-and sap-wood by obstruction of evaporating water from surface of disks by end-wrapping with Korean paper. And end-wrapping with Korean paper considerably restrained those. Tangential differential shrinkage stresses developed the maximum tensile stress near the bark and with approaching the pith the stresses gradually reduced and changed into compressive stresses in near the pith. At the end of vacuum drying the maximum tangential tensile stresses of disks end-wrapped with Korean paper were smaller than those of control disks, and critical moisture contents causing the V-shaped crack of disks end-wrapped with Korean paper were lower than those of control disks because of the set by obstruction of evaporating water of end-wrapping with Korean paper. In the experiment of vacuum drying stress distribution the disks end-wrapped with Korean paper or aluminum foil in three species were free from V-shaped cracks and control disks were defected very slightly by V-shaped cracks. And also disks end-wrapped with Korean paper were free from heart checks in Alnus japonica and Juglans sinensis, and heart checks were occurred very slightly in others. Especially, not to speak of disks end-wrapped with Korean paper, vacuum drying of disks end-wrapped with aluminum foil prevented effectively drying defects, moreover drying times could be shortened, that is. Ginkgo biloba, Alnus japonica, and Juglans sinensis disks could be dried from green to in-use moisture content in 110 hours, 272 hours, and 407 hours, respectively.