Sintering and Microwave Dielectric Properties of $ZnWO_4$ ($ZnWO_4$ 소결특성 및 고주파 유전특성)

  • Lee, Kyoung-Ho;Kim, Yong-Chul
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.386-389
    • /
    • 2001
  • In this study, development of a new LTCC material using non-glassy system was attempted with repsect to reducing the fabrication process steps and cost down. Lowering the sintering temperature can be achieved by liquid phase sintering. However, presence of liquid phases usually decrease dielectric properties, especially the quality factor. Therefore, the starting material must have quality factor as high as possible in microwave frequency range. And also, the material should have a low dielectric constant for enhancing the signal propagation speed. Regarding these factors, dielectric constants of various materials were estimated by the Clausius-Mosotti equation. Among them, $ZnWO_4$ was turned out the suitable LTCC material. $ZnWO_4$ can be sintered up to 98% of full density at $1050^{\circ}C$ for 3 hours. It's measured dielectric constant, quality factor, and temperature coefficient of resonant frequency were 15.5, 74380GHz, and $-70ppm/^{\circ}C$, respectively. In order to modify the dielectric properties and densification temperature, $B_{2}O_{3}$ and $V_{2}O_{5}$ were added to $ZnWO_4$. 40 mol% $B_{2}O_{3}$ addition reduced the dielectric constant from 15.5 to 12. And the temperature coefficient of resonant frequency was improved from -70 to $-7.6ppm/^{\circ}C$. However, sintering temperature did not change due to either lack of liquid phase or high viscosity of liquid phase. Incorporation of small amount of $V_{2}O_{5}$ in $ZnWO_{4}-B_{2}O_{3}$ system enhanced liquid phase sintering. 0.1 wt% $V_{2}O_{5}$ addition to the $0.6ZnWO_{4}-0.4B_{2}O_{3}$ system, reduced the sintering temperature down to $950^{\circ}C$. Dielectric constant, quality factor, and temperature coefficient of resonant frequency were 9.5, 16737GHz, and $-21.6ppm/^{\circ}C$, respectively.

  • PDF

Sintering and Microwave Dielectric Properties of $ZnWO_4$ ($ZnWO_4$ 소결특성 및 고주파 유전특성)

  • 이경호;김용철
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.386-389
    • /
    • 2001
  • In this study, development of a new LTCC material using non-glassy system was attempted with respect to reducing the fabrication process steps and cost down. Lowering the sintering temperature can be achieved by liquid phase sintering. However, presence of liquid phases usually decrease dielectric properties, especially the quality factor. Therefore, the starting material must have quality factor as high as possible in microwave frequency range. And also, the material should have a low dielectric constant for enhancing the signal propagation speed. Regarding these factors, dielectric constants of various materials were estimated by the Clausius-Mosotti equation. Among them, ZnWO$_4$ was turned out the suitable LTCC material. ZnWO$_4$ can be sintered up to 98% of full density at 105$0^{\circ}C$ for 3 hours. It's measured dielectric constant, quality factor, and temperature coefficient of resonant frequency were 15.5, 74380GHz, and -70ppm/$^{\circ}C$, respectively In order to modify the dielectric properties and densification temperature, B$_2$O$_3$ and V$_2$O$_{5}$ were added to ZnWO$_4$. 40 mol% B$_2$O$_3$ addition reduced the dielectric constant from 15.5 to 12. And the temperature coefficient of resonant frequency was improved from -70 to -7.6ppm/$^{\circ}C$. However, sintering temperature did not change due to either lack of liquid phase or high viscosity of liquid phase. Incorporation of small amount of V$_2$O$_{5}$ in ZnWO$_4$-B$_2$O$_3$ system enhanced liquid phase sintering. 0.lwt% V$_2$O$_{5}$ addition to the 0.6ZnWO$_4$-0.4B$_2$O$_3$ system, reduced the sintering temperature down to 95$0^{\circ}C$ Dielectric constant, quality factor, and temperature coefficient of resonant frequency were 9.5, 16737GHz, and -21.6ppm/$^{\circ}C$ respectively.ively.

  • PDF

Effect of CdO addition on the microwave dielectric properties of BiNbO$_4$ceramics using mobile communication (이동통신용 BiNbO$_4$세라믹스의 CdO 첨가량에 따른 고주파 유전 특성)

  • 윤중락;이헌용
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1997.11a
    • /
    • pp.405-408
    • /
    • 1997
  • The microwave dielectric properties of CuO and CdO addition of BiNbO$_4$ceramics were investigated. As the content of CdO increased, sintered density and quality factor is decreased. With increase in sintering temperature, the dielectric constant and quality factor is increased. In case of specimen sintered at 96$0^{\circ}C$ with 0.03 wt% CuO and CdO, the microwave dielectric properties obtained were dielectric constant of 41.2, quality factor (Q$\times$f) of 6, 500, temperature coefficient of resonant frequency of ppm/$^{\circ}C$.

  • PDF

Dielectric sensor for cure monitoring of composite materials (복합재료 경화도 측정을 위한 유전 센서)

  • 김학성;권재욱;김진국;이대길;최진경;김일영
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2001.05a
    • /
    • pp.219-223
    • /
    • 2001
  • The on-line cure monitoring during the cure process of composite materials is important for better quality and productivity. The dielectric sensor for cure monitoring consists of base film and electrodes. Because the characteristic of dielectric sensor for the on-line cure monitoring is dependent on the base material, width and number of electrode, etc, the dielectric sensor should be standardized. And the selection of base film material of sensor is very important. In order to prevent the measuring errors generated from the increase of environmental temperature, the base film material should have stable dielectric constant with respect to environmental temperature. In this study, the newly developed dielectric sensor for cure monitoring was designed and the dissipation factor which is function of degree of cure was measured using the sensor. The relationship between the dissipation factor and degree of cure with respect to environmental temperature was investigated.

  • PDF

Development of the Dielectric sensor for the Cure monitoring of the high temperature Composites (고온 복합재료의 경화 모니터링을 위한 유전센서의 개발)

  • 김일영;최진경;최진호;이대길
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2000.11a
    • /
    • pp.22-28
    • /
    • 2000
  • The fiber reinforced composite materials is widely used in aircraft, space structures and robot arms because of high specific strength and high specific modulus. The on-line cure monitoring during the cure process of the composite materials has become an important research area for the better quality and productivity. In this paper, the dielectric circuit of the wheatstone bridge type for measuring the dissipation factor was designed and manufactured. Also, the dielectric sensor for the cure monitoring of the high temperature composites was developed. The residual thermal stresses of the dielectric sensor were analyzed by the finite element method and its dielectric characteristics under high temperature were evaluated. The on-line cure monitoring of the BMI resin was performed using the wheatstone bridge type circuit and developed high-temperature dielectric sensor.

  • PDF

Dielectric and Piezoelectric Properties of Pb(Zr1/2Ti1/2)O3-Pb(Cu1/3Nb2/3)O3-Pb(Mn1/3Nb2/3)O3 System (Pb(Zr1/2Ti1/2O3-Pb(Cu1/3Nb2/3)O3-Pb(Mn1/3Nb2/3)O3계의 유전 및 압전 특성)

  • Lee, Hyeung-Gyu;Kang, Hyung-Won;Choi, Ji-Hyun
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.10 s.281
    • /
    • pp.698-702
    • /
    • 2005
  • Dielectric and Piezoelectric properties of complex perovskite 0.92Pb($Zr_{1/2}Ti_{1/2})O_{3}-(0.08-x)Pb(Cu_{1/3}Nb_{2/3})O_{3}-xPb(Mn_{1/3}Nb_{2/3})O_{3}(0{\leq}x{\leq}0.080$) (PZT-PCN-PMN) system were investigated as a function of PMN content. With the increase of PMN content of the sintered specimens, tetragonal phase was coexisted with rhombohedral phase, the dielectric constant was decreased, mechanical quality factor ($Q_{m}$) was inceased, and optimal sintering temperature was increased up to 1050$^{\circ}C$. For the composition of x = 0.064 sintered at 1050$^{\circ}C$ for 2 h, 1939 of maximum mechanical quality factor ($Q_{m}$), 57$\%$ of electromechanical coupling factor ($k_{p}$), and 1100$^{\circ}C$ of dielectric constant, 0.37$\% $ of dielectric loss (tan $\delta$) were obtained.

Effects of PSN Substitution on the Microstructural and Piezoelectric Characteristics of PNN-PZT Ceramics (PSN 치환이 PNN-PZT 세라믹스의 미세구조 및 압전 특성에 미치는 영향)

  • 윤광희;민석규;류주현;박창엽;정희승
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.5
    • /
    • pp.356-361
    • /
    • 2001
  • The structureal, dielectric and piezoelectric properties of Pb[(Sb$\_$1/2/Nb$\_$1/2/)$\_$x/-(Ni$\_$1/3/Nb$\_$2/3/)$\_$0.15-x/-(Zr$\_$y/Ti$\_$1-y/)$\_$0.85/]O$_3$(x=0∼0.05, y=0.47∼0.52) ceramics were investigated with the substitution of Pb(Sb$\_$1/2/Nb$\_$1/2/)O$_3$(abbreviated PSN) and the Zr/Ti ratio. At Zr/Ti ratio of 50/50, tetragonality was decreased and grain size abruptly decreased with the increase of PSN substitution. Curie temperature was decreased and dielectric constant increased with the substitution of PSN. The coercive field increased and remnant polarization decreased with the substitution of PSN. Electromechanical coupling factor(k$\_$p/) showed the highest value of 0.622 at 1mol% PSN, but mechanical quality factor(Q$\_$m/) showed the minimum value at that composition. Dielectric constant and electromechanical coupling factor with the Zr/Ti ratio showed maximum values at Zr/Ti ratio of 50/50 and mechanical quality factor showed minimum values near the Zr/Ti ratio of 50/50.

  • PDF

Strain Analysis for Quality Factor oft he Layered Mg0.93Ca0.07TiO3-(Ca0.3Li0.14Sm0.42)TiO3 Ceramics at Microwave Frequencies

  • Cho, Joon-Yeob;Yoon, Ki-Hyun;Kim, Eung-Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.3
    • /
    • pp.222-225
    • /
    • 2002
  • Microwave dielectric properties of the layered and functionally graded materials (FGMs) of $Mg_{0.93}Ca_{0.07}TiO_3$ (MCT) and $(Ca_{0.3}Li_{0.14}Sm_{0.42})TiO_3$(CLST) were investigated as a function of the volume ratio of two components. Dielectric constant was decreased with an increase of the volume ratio of MCT which had a lower dielectric constant thant CLST. For the layered FGMs specimens, the difference of thermal expansion coefficients between two components induced thermal strain to dielectric layers, which was confirmed by the plot of ${\Delta}$k (X-ray diffraction peak width0 versus k (scattering vector) using the double-peak Lorentzian function, f(x). Quality factor of the specimens was affected by the thermal strain of dielectric layer, especially MCT layer. For the specimen with the volume ratio of MCT/CLST = 2, the qulaity factor of the specimen showed a minimum value due to the maximum thermal strain fo MCT layer.

Piezoelectric and Dielectric Properties of NaNbO3-LiNbO3 Ceramics according to the BaTiO3 Substitution (BaTiO3 치환에 따른 NaNbO3-LiNbO3 세라믹스의 압전 및 유전특성)

  • Lee, Sang-Ho;Yoo, Ju-Hyun;Mah, Suk-Burm;Kim, Seang-Goo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.3
    • /
    • pp.205-209
    • /
    • 2009
  • In this study, in order to develop the composition ceramics for lead-free ultrasonic motor, (1-x-0.09)$NaNbO_{3-x}BaTiO_3-0,09LiNbO_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $BaTiO_3$ substitution. All the specimens showed orthorhombic phase structure without secondary phase, $BaTiO_3$ substitution enhanced density, dielectric constant(${\epsilon}_r$) and electromechanical coupling factor($k_p$), However, mechanical quality factor was deteriorated. Curie temperature of specimens was observed as about $380^{\circ}C$. At the $BaTiO_3$ substitution of 4 mol%, density, electromechanical coupling factor($k_p$), dielectric constant(${\epsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum value of $4.493g/cm^3$, 0.236, 175, 70 pC/N, respectively.

Piezoelectric and Dielectric Characteristics of PAN-PZT Ceramics with BaCO3Addition (BaCO3첨가량에 따른 PAN-PZI계 세라믹스의 압전 및 유전특성)

  • 박타리;이동균;최지원;강종윤;김현재;윤석진;고태국
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.4
    • /
    • pp.356-360
    • /
    • 2002
  • The piezoelectric properties of $0.05Pb(Al_{0.5}Nb_{0.5})O_3-0.95Pb(Zr_{0.52}Ti_{0.48})O_3+0.7wt%Nb_2O_5+o.5wt%MnO_2$ ceramics with the additive of BaCO$_3$were investigated. As the addition of BaCO$_3$increased from 0 to 0.4 wt%, the dielectric constant ($\epsilon^T _{33}$), piezoelectric constant ($d_33$), electromechanical coupling factor ($k_p$), and mechanical quality factor ($Q_m$) increased, while the dielectric loss ($tan\delta$) decreased. The highest piezoelectric and dielectric properties were observed at $1200^{\circ}C$ of the sintered temperature with 0.4 wt% of $BaCO_3$, and the properties of $d_33$, $k_p$, and $Q_m$ were 339 pC/N, 60% and 1754, respectively.