The Influence of Inorganic Pigments on the Compressive Strength and Absorption of Cement Mortars (무기안료가 시멘트모르타르의 압축강도와 흡수율에 미치는 영향)

  • Shon, Hyuk;Lee, Jae-Yong;Go, Seong-Seok
    • Journal of the Korean Society of Safety
    • /
    • v.19 no.2
    • /
    • pp.104-111
    • /
    • 2004
  • The aim of this study was to investigate the influence of inorganic pigments on the physical properties of cement mortar. For this purpose, the compressive strength and absorption test were carried out on cement mortar imxed with inorganic pigments by changing the proportion of cement mortar, water-cement ratio, and ratio of pigment. The result of this study can be summarized as follows: the compressive strength of colored mortar rapidely increased in red and yellow mortar, as the mix ratio of pigment increased. In case of green and black mortar, however, the compressive strength decresed as the mix ratio incresed. In case of red and yellow mortar, the absorption of colored mortar increased as the mixing ratio increased, if the mean particle diameter of the pigment is small. In case of green and black mortar, the absorption ratio decreased as the mix ratio increased. After investigating the overall physical properties of colored mortar, it was confirmed that the proper mix ratio of pigment securing the properties of colored mortar was below 6% of the weight of the cement to be used.

Wake galloping phenomena between two parallel/unparallel cylinders

  • Kim, Sunjoong;Kim, Ho-Kyung
    • Wind and Structures
    • /
    • v.18 no.5
    • /
    • pp.511-528
    • /
    • 2014
  • The characteristics of wake galloping phenomenon for two parallel/unparallel circular cylinders were investigated via wind tunnel tests. The two cylinders were initially deployed in parallel and wake galloping phenomena were observed by varying the center-to-center distance. The effect of an unparallel arrangement of two cylinders was next investigated by fixing the spacing ratio of one side of the cylinders at 5.0D and the other side at 3.0D, in which D represents the diameter of the cylinder. For the unparallel disposition, the 5.0D side showed a small, limited vibration while the 3.0D side produced much larger amplitude of vibration, resulting in a rolling motion. However, the overall amplitude appeared to decrease in unparallel disposition when compared with the amplitude of the 3.0D - 3.0D parallel case. This represents the mitigation effect of wake galloping due to the unparallel disposition between two cylinders. Flow visualization tests with particle image velocimetry were conducted to identify flow fields between two cylinders. The test results demonstrate the existence of a complex interaction of the downstream cylinder with the shear layer generated by the upstream cylinder. When the spacing ratio was large enough, the shear layer was not observed and the downstream cylinder showed only limited random vibration.

Research on Thymopentin Loaded Oral N-Trimethyl Chitosan Nanoparticles

  • Yuan, Xiao-Jia;Zhang, Zhi-Rong;Song, Qing-Guo;He, Qin
    • Archives of Pharmacal Research
    • /
    • v.29 no.9
    • /
    • pp.795-799
    • /
    • 2006
  • Peptides, although high efficacy and specificity in their physiological function, usually have low therapeutical activities due to their poor bioavailability when administrated orally. Nanoparticles have been regarded as a useful vector for targeted drug delivery system because they can protect drug from being degraded quickly and pass the gastrointestinal barriers. Here we described a novel oral N-trimethyl chitosan nanoparticles formulation containing thymopentin (Tp5-TMC-NP). N-trimethyl chitosan (TMC) was synthesized and then used to prepare Tp5-TMC-NP by ionotropic gelation. A three-factor, five-level CCD (Central Composite Design) design was used in the optimization procedure, with HPLC as the analyzing method. The resulting Tp5-TMC-NP had a regular spherical surface and a narrow particle size range with a mean diameter of 110.6 nm. The average entrapment efficiency was 78.8%. The lyophilized Tp5-TMC-NP formulation was stable in $4^{\circ}C\;or\;-20^{\circ}C$ after storage of 3 months without obvious changes in morphology, particle size, pH and entrapment ratio. The results of the flow cytometer determination showed that the ratio of $CD4^+/CD8^+$ of Wistar female rat given Tp5-TMC-NP (ig) was 2.59 time that of the group given Tp5 (ig).

Effects of stenotic severity on the flow structure in a circular channel under a pulsatile flow

  • Kim, Kyung-Won;Cheema, Taqi-Ahmad;Park, Cheol-Woo
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.38 no.2
    • /
    • pp.140-146
    • /
    • 2014
  • Stenosis is the drastic reduction in the cross-sectional area of blood vessel caused by accumulations of cholesterol. It affects the blood flow property and structure from the fluid dynamic point of view. To understand the flow phenomenon more clearly, a particle image velocimetry method is used and the fluid dynamic characteristics in a circular channel containing stenosis structure is investigated experimentally in this study. Different stenotic-structured models made of acrylic material are subjected to a pulsatile flow generated by an in-house designed pulsatile pump. The inner diameter of the tube inlet is 20 mm and the length of reduced area for stenosis ranges between 35mm and 40mm. It is circulated continuously through a circular channel by the pump system. Pressure is measured at four different sections during systolic and diastolic phase changes. The phase-averaged velocity field distribution shows a recirculation regime after the stenotic structure. The effects of the stenotic obstructions are found to be more severe when the aspect ratio is varied.

PIV Measurements of Flow and Turbulence Characteristics of Round Jet in Crossflow (횡단류 제트의 유동 및 난류특성치에 대한 PIV 측정)

  • Kim, Kyung-Chun;Kim, Sang-Ki;Yoon, Sang-Youl
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.24 no.3
    • /
    • pp.382-389
    • /
    • 2000
  • The instantaneous and ensemble averaged flow characteristics of a round jet issuing normally into a crossflow was studied using a flow visualization technique and Particle Image Velocimetry measurements. Experiments were performed at a jet-to-crossflow velocity ratio, 3.3, and two Reynolds numbers, 1050 and 2100, based on crossflow velocity and jet diameter. Instantaneous laser tomographic images of the vertical center plane of the crossflow jet showed that there exist very different natures in the flow structures of the near field jet even though the velocity ratio is the same. It was found that the shear layer becomes much thicker when the Reynolds number is 2100 due to the strong entrainment of the inviscid fluid by turbulent interaction between the jet and crossflow. The mean and second order statistics were calculated by ensemble averaging over 1000 realizations of instantaneous velocity fields. The detail characteristics of mean flow field, stream wise and vertical r.m.s. velocity fluctuations, and Reynolds shear stress distributions were presented. The new PlV results were compared with those from previous experimental and LES studies.

Dry Fine Grinding of Rice Husk Ash using a Stirred Ball Mill (교반 볼밀을 이용한 왕겨재의 건식 미세분쇄에 관한 연구)

  • 박승제;최연규;김명호;이종호
    • Journal of Biosystems Engineering
    • /
    • v.25 no.1
    • /
    • pp.39-46
    • /
    • 2000
  • This work was conducted to study the operating characteristics of a grinding system designed to obtain fine rice husk ash powder. To find better utilizing of rice husk, a valuable by-product from rice production, once the rice husk was incinerated and the thermal energy was recovered from the furnace, the ash was fed and pulverized in the grinding system resulting a fine powder to be used as a supplementary adding material to the portland cement manufacturing . The rice husk ash grinding system consisted of a high speed centrifugal fan for the preliminary coarse milling and a dry-type stirred ball mill for the subsequent fine grinding . Total grinding time 9 5, 15, 30, 45 min), impeller speed (250, 500, 750 rpm) , and mixed ratio (4.8, 7.9, 14.9) were three operating factors examined for the performance of a stirred ball mill used for the fine grinding of ash. With the stirred ball mill used in this study, the minimum attianable mean diameter of rice husk ash powder appeared to be 2 ${\mu}{\textrm}{m}$. During the find grinding, the difference in specific surface area of powder showed an increase and the grinding energy efficiency decreased with the increase in total grinding time, impeller speed ,and mixed ratio. For the operating conditions employed , the resulting mean diameter of fine ash powder, specific energy input, and grinding energy efficiency were in the range of 1.79 --16.04${\mu}{\textrm}{m}$, 0.072-5.226kWh/kg, an d1.11-12.15$m^2$/Wh, respectively. Grinding time of 30 min , impeller speed of 750 rpm, and mixed ratio of 4.8 were chosen as the best operating conditions of the stirred ball mill for fine grinding . At these conditions, mean particle diameter of the fine ash, grinding energy efficiency, grinding throughtput, and specific energy input were 2.73${\mu}{\textrm}{m}$, 3.95$m^2$/Wh, 0.25kg/h, and 1.22kWh/kg, respectively.

  • PDF

The Characteristics of Swirl Spray Combustion in Gas Turbine Combustor (가스터빈 연소기내의 선회분무연소 특성)

  • Hong, Jeong-Gu;Kim, Hyeok-Ju
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.20 no.8
    • /
    • pp.2721-2730
    • /
    • 1996
  • The present study conducted experimental study of spray combustion to investigate the effect of the inlet conditions of fuel and air on the flame structure, the flame stability and the characteristics of emission in the can-type model of a gas turbine combustor. In the experiment, the diameter of fuel droplet was measured using Malvern particle size analyser and temperatures in the combustion chamber were measured with R-type shielded thermocouple. In addition, flame structure was taken picture with camera and analysed. Gas analyser was also used to analyse the concentration of each components of exhausting gas. The experimental results showed that the flame condition was optimal with swirl number, 0.63 and equivalence ratio, 0.5 for controlling the flame stability, the combustion temperature and the NOx concentration. The present study concluded that both the flame structure and the emission formation were strongly affected by the swirl intensity, which selection was found as an important parameter for either stabilizing flame or lowering the quantity of NOx.

A study on spray characteristics of the triplet impinging stream type injector for liquid rocket (액체 로켓용 충돌형 Triplet 인젝터의 미립화 특성에 관한 연구)

  • Park, Sung-Young;Kim, Seon-Jin;Park, Seung-Woon;Kim, Yoo
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.20 no.3
    • /
    • pp.1005-1014
    • /
    • 1996
  • An experimental investigation has been carried out to examine the influence of injector design variables and operating conditions on the resultant drop size for triplet impinging streams injectors. The variables studied in this investigation are pressure drop, impinging angle, orifice length to diameter ratio, and impinging point distance. Droplet-size data are obtained using water as the propellant simulant by Malvern Particle Analyzer System. Drop size decreases with increasing impinging angle and pressure drop while other injector parameters remain constant at the same point. But it is found that there is no noticeable droplet-size change which results from change in orifice length to diameter ratio or impinging point distance within the investigated range.

Preparation and Characterizations of C60/Polystyrene Composite Particle Containing Pristine C60 Clusters

  • Kim, Jung-Woon;Kim, Kun-Ji;Park, Soo-Yeon;Jeong, Kwang-Un;Lee, Myong-Hoon
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.9
    • /
    • pp.2966-2970
    • /
    • 2012
  • Fullerene/polystyrene ($C_{60}$/PS) nano particle was prepared by using emulsion polymerization. Styrene and fullerene were emulsified in aqueous media in the presence of poly(N-vinyl pyridine) as an emulsion stabilizer, and polymerization was initiated by water soluble radical initiator, potassium persulfate. The obtained nano particles have an average diameter in the range of 400-500 nm. The fullerene contents in the nano particle can be controlled up to 15 wt % by varying the feed ratio, which was confirmed by themogravimetric analysis (TGA) and elemental analysis (EA). The structure and morphologies of the $C_{60}$/PS nano particles were examined by various analytical techniques such as dynamic light scattering (DLS), scanning electron microscope (SEM), transmission electron microscope (TEM), electron diffraction (ED) pattern, X-ray powder diffraction (XRD), and UV spectroscopy. Unlike conventional $C_{60}$/PS particles initiated by organic free radical initiators, in which the fullerene is copolymerized forming a covalent bond with styrene monomer, the prepared $C_{60}$/PS nano particles contain pristine fullerene as secondary particles homogeneously distributed in the polystyrene matrix.

Uranium Particle Identification with SEM-EDX for Isotopic Analysis by Secondary Ion Mass Spectrometry

  • Esaka, Fumitaka;Magara, Masaaki
    • Mass Spectrometry Letters
    • /
    • v.7 no.2
    • /
    • pp.41-44
    • /
    • 2016
  • Secondary ion mass spectrometry (SIMS) is a promising tool to measure isotope ratios of individual uranium particles in environmental samples for nuclear safeguards. However, the analysis requires prior identification of a small number of uranium particles that coexist with a large number of other particles without uranium. In the present study, this identification was performed by scanning electron microscopy - energy dispersive X-ray analysis with automated particle search mode. The analytical results for an environmental sample taken at a nuclear facility indicated that the observation of backscattered electron images with × 1000 magnification was appropriate to efficiently identify uranium particles. Lower magnification (less than × 500) made it difficult to detect smaller particles of approximately 1 μm diameter. After identification, each particle was manipulated and transferred for subsequent isotope ratio analysis by SIMS. Consequently, the isotope ratios of individual uranium particles were successfully determined without any molecular ion interference. It was demonstrated that the proposed technique provides a powerful tool to measure individual particles not only for nuclear safeguards but also for environmental sciences.