A STUDY ON THE BOND STRENGH OF 4-META ACRYLIC RESIN DENTURE BASE TO COBALT-CHROMIUM ALLOYS (4-META의치상레진과 Cobalt-Chromium계 합금의 접착강도에 관한 연구)

  • Sung, Moo Gyung;Kim, Kwang Nam;Chang, Ik Tae
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.28 no.2
    • /
    • pp.29-51
    • /
    • 1990
  • This study was designed to compre the tensile bond strength of 4-META containging denture base resin to Co-Cr alloys after various surface treatments. Especially the surface treatment of sandblasting the mental with aluminum oxide and treating in oxidizing solution composed of 3% aqueous sulfuric acid with 1% potassium manganate were compared. Effect of surface roughness on bonding was measured after sandblasting with 50um, 300um aluminun oxide and polishing with emery pater. Also the effects of wax and wax solvent on bonding were observed. According to the type of polymerization process, heat-cured Meta-Dent resin and autopolymerizing Meta-Fast resin were used. For some specimnens, the tensile bond strength were measured agter three pre-conditions : 1day after bonding, immersed in water at $75^{\circ}C{\pm}3^{\circ}C$ for 4weeks, under normal ambient condition for 4weeks. The following results were obtained from this study : 1. The bond strengths of resins containing 4-META were significantly higher than those of conventional denture base resins(p<0.05). 2. Autopolymerizing Meta-Fast resin had higher bond strength than heat-cured Meta-Dent, resin(p<0.05). 3. The bond strengths of Biosil and Nobilium to 4-META containging resins were not significally different(p>0.05). 4. Stable adhesion can be achieved when mechanically roughen the metal surface by snadblasting with $50{\mu}m$ aluminum oxide than treating in an oxidizing soluing with potassium manganate(p<0.05). 5. Once the metal surface is contaminated with wax, the bond srtength decreased greatly in spite of wax wash with boiling water. But the bond strength recovered significantly with the use of wax solvent 6. Meta-Dent resin had higher bond strength when roughen the metal surface with $50{\mu}m$ aluminum oxide than with $300{\mu}m$ aluminum oxide(p<0.05). In case of Meta-Fast, resin, the use of $300{\mu}m$aluminum oxide was a little advantageous of bonding, but was statistically insignificant(p>0.05).

  • PDF

Nonthermal plasma on the shear bond strength of relining resin to thermoplastic denture base resin (열가소성 의치상 레진과 첨상용 레진의 접착 강도에 저온플라즈마가 미치는 효과)

  • Manaloto-Ceballos, Liezl;Labriaga, Wilmart;Song, So-Yeon;Park, Jin-Hong;Lee, Jeong-Yol;Shin, Sang-Wan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.56 no.3
    • /
    • pp.199-205
    • /
    • 2018
  • Purpose: This study evaluated the effect of nonthermal plasma treatment on the bond strength of autopolymerizing relining resin to the injection molded thermoplastic denture base resins (TDBRs) with different surface treatments. Materials and methods: Acrylic Resin (Acrytone), Polyester (Estheshot-Bright), Polyamide (Valplast) and Polypropylene (Weldenz) were subjected to various surface treatments: No treatment, Nonthermal plasma, Sandblasting, Sandblasting and nonthermal plasma. Specimens were bonded using an autopolymerizing relining resin. Shear bond strength was tested using universal testing machine with crosshead speed of 1 mm/min. Statistical analysis by two-way analysis of variance with Tukey's test post hoc was used. Results: Acrytone showed significantly higher shear bond strength value among other TDBR group while Weldenz had the lowest. The sandblasting and nonthermal plasma condition had significantly higher shear bond strength value in all of the resin groups (P < .05). Conclusion: The use of nonthermal plasma treatment showed limited effect on the shear bond strength between TDBRs and relining resin, and combination of nonthermal plasma and sandblasting improved the shear bond strength between TDBR and reline material.

A Study on the Tensile Strength between Light-cured Relining Resin and Metal Denture Base (광중합형 이장재와 금속의치상 간의 결합력에 관한 연구)

  • Park, In-Chae;Lee, Joon-Kyu;Chung, Chae-Heon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.16 no.3
    • /
    • pp.211-220
    • /
    • 2000
  • The use of autopolymerizing-cured resin and light-cured resin for direct relining of complete and partial dentures has been popular. This investigation compared the adhesion of autopolymerizing-cured reline resin(Tokuso Rebase, Mild Rebaron) or light-cured reline resin(Mild Rebaron LC, Lighton-U) to metal base or resin base. Cylindrical samples were made from metal($Biosil^{(R)}$) or heat-cured resin(QC-20) and were prepared to produce a flat bonding surface. Cylindrical metal samples were roughened by scratch or by scratch and sandblast and were treated with primer(MR Bond) after scratch and sandblast. And then, liners were prossesed to the cylindrical metal or resin samples according to the manufacturer's recommendations so as to bond metal base or resin base. The specimens were tested in pure tension by using an Instron Univesal testing machine for the four direct reline resins. The results were as follows ; 1. In comparison with tensile bond strength of material relined on resin base or metal base, the case of resin base produced significantly higher tensile bond strength than the case of metal base. 2. Metal surface pretreatment or primer improved the tensile bond strength between the reline resin and the metal($Biosil^{(R)}$) base. 3. The tensile bond strength of Mild Rebaron LC relined on resin base or metal base were similar to those of the other reline resins.

  • PDF

A Study on the Tensile Strength between Light-cured Relining Resin and Metal Denture Base (광중합형 이장재와 금속의치상 간의 결합력에 관한 연구)

  • Park, In-Chae;Lee, Joon-Kyu;Chung, Chae-Heon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.16 no.2
    • /
    • pp.161-170
    • /
    • 2000
  • The use of autopolymerizing-cured resin and light-cured resin for direct relining of complete and partial dentures has been popular. This investigation compared the adhesion of autopolymerizing-cured reline resin(Tokuso Rebase, Mild Rebaron) or light-cured reline resin(Mild Rebaron LC, Lighton-U) to metal base or resin base. Cylindrical samples were made from metal($Biosil^{(R)}$) or heat-cured resin(QC-20) and were prepared to produce a flat bonding surface. Cylindrical metal samples were roughened by scratch or by scratch and sandblast and were treated with primer(MR Bond) after scratch and sandblast. And then, liners were prossesed to the cylindrical metal or resin samples according to the manufacturer's recomendations so as to bond metal base or resin base. The specimens were tested in pure tension by using an Instron Univasal testing machine for the four direct reline resins. The results were as follows ; 1. In comparison with tensile bond strength of material relined on resin base or metal base, the case of resin base produced significantly higher tensile bond strengths than the case of metal base. 2. Metal surface pretreatment or primer improved the tensile bond strength between the reline resin and the metal($Biosil^{(R)}$) base. 3. The tensile bond strengths of Mild Rebaron LC relined on resin base or metal base were similar to those of the other reline resins.

  • PDF

Evaluation of polymethyl methacrylate resin mechanical properties with incorporated halloysite nanotubes

  • Abdallah, Reham M.
    • The Journal of Advanced Prosthodontics
    • /
    • v.8 no.3
    • /
    • pp.167-171
    • /
    • 2016
  • PURPOSE. This study inspects the effect of incorporating halloysite nanotubes (HNTs) into polymethyl methacrylate (PMMA) resin on its flexural strength, hardness, and Young's modulus. MATERIALS AND METHODS. Four groups of acrylic resin powder were prepared. One group without HNTs was used as a control group and the other three groups contained 0.3, 0.6 and 0.9 wt% HNTs. For each one, flexural strength, Young's modulus and hardness values were measured. One-way ANOVA and Tukey's test were used for comparison (P<.05). RESULTS. At lower concentration (0.3 wt%) of HNT, there was a significant increase of hardness values but no significant increase in both flexural strength and Young's modulus values of PMMA resin. In contrast, at higher concentration (0.6 and 0.9 wt%), there was a significant decrease in hardness values but no significant decrease in flexural strength and Young's modulus values compared to those of the control group. CONCLUSION. Addition of lower concentration of halloysite nanotubes to denture base materials could improve some of their mechanical properties. Improving the mechanical properties of acrylic resin base material could increase the patient satisfaction.

Esthetic removable partial denture with implants and resin clasp: Case report (임플란트와 레진 클래스프를 이용한 심미 가철성 국소의치 증례)

  • Kim, Su-Min;Jeon, Young-Chan;Jeong, Chang-Mo;Yun, Mi-Jung;Huh, Jung-Bo
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.53 no.1
    • /
    • pp.58-65
    • /
    • 2015
  • For the rehabilitation of fully edentulous patients, implant-supported removable partial dentures can be considered as one of the treatment options with complete dentures or implant-supported overdentures. If removable partial dentures are used in combination with a small number of implants placed in strategically important positions, it can offer additional stability, retention and support through implants and reduce a burden of surgical procedures compared with fixed implant-supported prostheses with extensive implant placement. Moreover, the economical benefit can be expected as well. The purpose of this case report is to present a treatment in which an implant-supported removable partial denture was fabricated considering residual alveolar bone status and demands after teeth loss in a patient who had been using a distal extension removable partial denture for a long period of time. In anterior area, fixed prostheses were fabricated with implant placement and in posterior area, short implants provide only support for the removable partial denture. In addition, denture base and clasp were made of thermoplastic acrylic resin. Finally, functionally and aesthetically satisfying treatment results can be achieved.

Three-dimensional analysis of artificial teeth position according to three type complete mandibular denture before and after polymerization (세 가지 방식으로 제작한 하악 총의치의 중합 전후에 따른 인공치아 위치 3차원 분석)

  • Park, Jin-Young;Kim, Dong-Yeon;Kim, Won-Soo;Lee, Gwang-Young;Jeong, Il-Do;Bae, So-Yeon;Kim, Ji-Hwan;Kim, Woong-Chul
    • Journal of Technologic Dentistry
    • /
    • v.40 no.4
    • /
    • pp.217-224
    • /
    • 2018
  • Purpose: The aim of this study was to evaluate accuracy of three type complete mandibular denture of before and after polymerization. Methods: Mandibular edentulous model was selected as the master model. 15 study models were made by Type IV stone. Wax complete mandibular dentures were produced by the denture base and artificial teeth. Before and after curing, STL files were obtained using a blue scanner. By superimposing the digitized complete mandibular denture data(after curing) with the CAD-reference(before curing) three-dimensionally, visual fit-discrepancies were drawn by calculating the root mean square (RMS) and visualized on a color-difference map. Each calculated RMS-value was statistically analyzed by 1-way analysis of variance(ANOVA) (${\alpha}=.05$). Results: Mean(SD) RMS-values was OM group $88.98(6.10){\mu}m$, BM group $82.35(13.46){\mu}m$, BDM group $77.83(9.46){\mu}m$. The results of the 1-way ANOVA showed no statistically significant differences in the RMS values of the Three groups for the material (P > .241). Conclusion : Deformation of artificial teeth position was observed in all groups after resin polymerization. But the values, all group were within the clinically acceptable range. The values of BDM group showed the least deformation than the other two groups.

Implant-assisted removable partial denture using Milled-Bar and Attachment in partially edentulous maxilla: A case report (상악 부분 무치악 환자에서 Milled-bar와 어태치먼트를 이용한 임플란트 부분 피개의치 수복 증례 보고)

  • Jeong, Yun-Su;Jeong, Chang-Mo;Yun, Mi-Jung;Lee, So-Hyoun;Huh, Jung-Bo
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.60 no.4
    • /
    • pp.412-419
    • /
    • 2022
  • For treatment of partially edentulous patients, a treatment using implant is widely used. Treatment method using implant are implant fixed prostheses and removable partial dentures, and for patients with severe bone resorption, removable implant overdenture with the effects of aesthetic and reducing cost can be used as treatment options. Specially, prosthesis with milled-bar and attachment has the effect of being splinted between implant fixtures, higher retention and stability than conventional removable partial denture. And it has the effect of improvement of aesthetic through lip support by denture base. In this case, the patient with severe alveolar bone resorption and partial edentulous maxilla and mandible was treated by implant-assisted removable partial denture using Milled-bar and ADD-TOC attachment. The esthetic was improved by removing the clasp because of effects of additional retention by using the attachment, and reducing palatal coverage of implant-assisted removable partial denture. The clinical results were satisfactory on the aspect of aesthetic and masticatory function.

A STDUY ON THE SURFACE MORPHOLOGY AND BOND STRENGTH OF DENTURE BASE RESIN TO COBALT-CHROMIUM ALLOY AFTER VARYING MODES OF SURFACE TREATMENT (COBALT-CHROMIUM 합금의 표면처리방법에 따른 레진 의치상의 접착강도 및 표면상태에 대한 연구)

  • Vang, Mong-Sook;Park, Young-Jon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.35 no.1
    • /
    • pp.78-94
    • /
    • 1997
  • The purpose of this experiment was to determine the effects of various treatments on denture base resin to metal bond for cobalt-chromium alloy. The metal surface was treated as follows. Group 1 : Sandblasted with $50{\mu}m$ aluminum oxide. Group 2 : Sandblasted with $250{\mu}m$ aluminum oxide. Group 3 : Sandblasted with $250{\mu}m$ aluminum oxide and followed by silicoating. Group 4 : Electrochemically etched. Group 5 : treated with oxidizing solution. Group 6 : Beaded with $200{\mu}m$ retention structure and followed by silicoating. All specimens were applied with 4-META resin and were thermocycled 1000 times at temperature of $5^{\circ}C$ to $55^{\circ}C$. The effects of various surface treatments on the bond strength between 4-META resin and metal interface were measured by using the universal testing machine. All specimens were observed with SEM. The results were as follows 1. The bond strength of 4-META resin were significantly higher to Co-Cr alloy. 2. The bond strength decreased in the following orders : group 6, group 3, groups 1 and 2, group 4, group 5 and there was no statistically significant difference in bond strength among groups 1 and 2.(p>0.05) 3. The bond strength of cobalt-chromium alloy to 4-META resin were not significantly different.(p>0.05) 4. The treated surface of groups 1, 2 and 3 has more fine undercut than that of groups 4 and 5 with SEM. 5. Stable adhesion can be achieved when mechanically roughened metal surface by sandblasting than treating in an electrochemical etching and an oxidizing solution with potassium manganate.

  • PDF

THE EFFECT OF CLASP DESIGN ON ABUTMENT TOOTH MOVEMENT FOR DISTAL EXTENSION REMOVABLE PARTIAL DENTURE (유리단 국소의치의 Clasp설계가 지대치 운동에 미치는 영향)

  • Yim, Soon-Ho;Chang, Ik-Tai
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.25 no.1
    • /
    • pp.17-40
    • /
    • 1987
  • The purpose of this study was to clarify the effect of clasp design on abutment tooth adjacent to a distal extension base under the influence by the location of functional loading. The RPI clasp, the Akers clasp and the combination clasp were selected for evaluation. Tests were performed at 10Kg, 20Kg, 30Kg loads on the buccal, central, lingual, mesial and distal positions of loading platform of each mandibular distal extension partial denture. The laser reflexion method was used for three dimensional measurement of abutment movement, which is possible to measure precisely without contact. The movement in the mesiodistal(X), buccolingual(Y), and occlusoapical(Z) directions and the rotational movement(R) were measured, and in addition, the total movement (SV) as expressed by the three dimensional summation vector independent of direction was calculated. The data were analyzed using Student t-test, p<.05. The following results were obtained from this study; 1. Clasp design did not generally affect the direction of abutment tooth movement except the movement in an undesirable occlusal direction in case of the Akers clasp and the combination clasp. 2. The greater the load on the prosthesis, the greater was the abutment tooth movement, and the direction of abutment tooth movement was affected by positional loading. 3. Each prosthesis was dislodged from the test base under the small amount of load in the distal load position, and the buccal loading showed the greatest abutment tooth movement under the maximum load. 4. RPI clasp was evaluated as the most favorable design.

  • PDF