A confocal microscopic study of dentinal infiltrations in one-bottle adhesive systems bonded to Class V cavities

  • Kim, Hyung-Su;Park, Sung-Ho
    • 대한치과보존학회:학술대회논문집
    • /
    • 대한치과보존학회 2001년도 추계학술대회(제116회) 및 13회 Workshop 제3회 한ㆍ일 치과보존학회 공동학술대회 초록집
    • /
    • pp.576.2-576
    • /
    • 2001
  • The purpose of this study was to evaluate the effect of dentinal sclerosis and tubular orientation on Class V restoration bonded with three dentin bonding agents using confocal laser scanning microscope(CLSM). Class V cavities were prepared from freshly extracted caries-free human teeth. thirty of these cavities were divided into two groups based upon the status of class V cavities: Group 1, cervical abrasive lesions without preparation; Group 2, artificially-prepared wedge-shaped cavities.(omitted)

  • PDF

The effects of dentin bonding agent formulas on their polymerization quality, and together with tooth tissues on their microleakage and shear bond strength: an explorative 3-step experiment

  • Erfan, Mohmmad;Jafarzadeh-Kashi, Tahereh Sadat;Ghadiri, Malihe;Rakhshan, Vahid
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권5호
    • /
    • pp.333-345
    • /
    • 2014
  • PURPOSE. Bonding agents (BA) are the crucial weak link of composite restorations. Since the commercial materials' compositions are not disclosed, studies to formulize the optimum ratios of different components are of value. The aim of this study was to find a proper formula of BAs. MATERIALS AND METHODS. This explorative experimental in vitro study was composed of 4 different sets of extensive experiments. A commercial BA and 7 experimental formulas were compared in terms of degree of conversion (5 experimental formulas), shear bond strength, mode of failure, and microleakage (3 experimental formulas). Statistical analyses were performed (${\alpha}$=.05). The DC of selected formula was tested one year later. RESULTS. The two-way ANOVA indicated a significant difference between the shear bond strength (SBS) of two tissues (dentin vs. enamel, P=.0001) in a way that dentinal bonds were weaker. However, there was no difference between the four materials (P=.283). The adhesive mode of failure was predominant in all groups. No differences between the microleakage of the four materials at occlusal (P=.788) or gingival (P=.508) sites were detected (Kruskal-Wallis). The Mann-Whitney U test showed a significant difference between the microleakage of all materials (3 experimental formulas and a commercial material) together at the occlusal site versus the gingival site (P=.041). CONCLUSION. A formula with 62% bisphenol A-glycidyl methacrylate (Bis-GMA), 37% hydroxy ethyl methacrylate (HEMA), 0.3% camphorquinone (CQ), and 0.7% dimethyl-para-toluidine (DMPT) seems a proper formula for mass production. The microleakage and SBS might be respectively higher and lower on dentin compared to enamel.

공초점레이저주사현미경을 이용한 심미수복재와 상아질의 접착계면에 관한 연구 (A CONFOCAL LASER SCANNING MICROSCOPIC STUDY ON THE INTERFACE BETWEEN TOOTH COLORED RESTORATIVE MATERIALS AND DENTIN)

  • 박병철;조영곤;문주훈
    • Restorative Dentistry and Endodontics
    • /
    • 제25권3호
    • /
    • pp.313-320
    • /
    • 2000
  • The purpose of this study was to evaluate on the interfacial morphology between dentin and restorative materials. In this in vitro study, the cavity wall restorated with 3 different kinds of tooth colored restorative materials [resin-modified Glass Ionomer cement (Fuji II LC), composite resin (Z-100), compomer (Dyract)]. The thirty extracted human molar teeth without caries and/or restorations are used. The experimental teeth were randomly divided into three groups of ten teeth each. In each group, Wedge shaped cavities (width: 3mm, length: 2mm, depth: 1.5mm) were prepared at the cementoenamel junction on buccal and lingual surfaces. The adhesive of composite resin were mixed with rhodamine B. Primer of composite resin, Prime & Bond 2.1 of Dyract and liquid of Fuji II LC were mixed with fluorescein. In group 1, the cavity wall was treatment with dentin conditioner, and then restorated with Fuji II LC. In group 2, the cavity wall was treatment with Prime & Bond 2.1 and then restorated with Dyract. In group 3, the cavity wall was etching with 10% maleic acid, applied with primer and bonding agent and then restorated with Z-100. The interface between dentin and restorative materials was observed by fluoresence imaging with a confocal laser scanning microscope. The results were as follows : 1. In Glass ionomer group, adaptation of resin modified Glass-ionomer restoration against cavity wall is tight, but the crack formed inside of restoration were observed. 2. In Dyract group, the penetration of resin tag is shorter and the width of hybrid layer is narrower than composite resin group. 3. In Z-100 group, primer penetrated deeply through dentinal tubule. Also bonding agent was penetrated along the primer, but the penetration length is shorter than primer part, and in 3-D image, the resin tag is conical shape and lateral branch is observed.

  • PDF

Inhibition of matrix metalloproteinases: a troubleshooting for dentin adhesion

  • de Moraes, Izadora Quintela Souza;do Nascimento, Ticiano Gomes;da Silva, Antonio Thomas;de Lira, Lilian Maria Santos Silva;Parolia, Abhishek;de Moraes Porto, Isabel Cristina Celerino
    • Restorative Dentistry and Endodontics
    • /
    • 제45권3호
    • /
    • pp.31.1-31.20
    • /
    • 2020
  • Matrix metalloproteinases (MMPs) are enzymes that can degrade collagen in hybrid layer and reduce the longevity of adhesive restorations. As scientific understanding of the MMPs has advanced, useful strategies focusing on preventing these enzymes' actions by MMP inhibitors have quickly developed in many medical fields. However, in restorative dentistry, it is still not well established. This paper is an overview of the strategies to inhibit MMPs that can achieve a long-lasting material-tooth adhesion. Literature search was performed comprehensively using the electronic databases: PubMed, ScienceDirect and Scopus including articles from May 2007 to December 2019 and the main search terms were "matrix metalloproteinases", "collagen", and "dentin" and "hybrid layer". MMPs typical structure consists of several distinct domains. MMP inhibitors can be divided into 2 main groups: synthetic (synthetic-peptides, non-peptide molecules and compounds, tetracyclines, metallic ions, and others) and natural bioactive inhibitors mainly flavonoids. Selective inhibitors of MMPs promise to be the future for specific targeting of preventing dentin proteolysis. The knowledge about MMPs functionality should be considered to synthesize drugs capable to efficiently and selectively block MMPs chemical routes targeting their inactivation in order to overcome the current limitations of the therapeutic use of MMPs inhibitors, i.e., easy clinical application and long-lasting effect.

Benzalkonium Chloride가 NTG-GMA/BPDM계 및 DSDM계 상아질접착제의 접착성능에 미치는 영향 (EFFECT OF BENZALKONIUM CHLORIDE ON DENTIN BONDING WITH NTG-GMA/BPDM AND DSDM SYSTEM)

  • 신일;박진훈
    • Restorative Dentistry and Endodontics
    • /
    • 제20권2호
    • /
    • pp.699-720
    • /
    • 1995
  • 본 연구는 양이온 계면활성효과를 가져 소독제로 사용되고 있는 benzalkonium chloride 수용액을 상아질 표면에 대한 습윤용 처리제로 적용시킬 경우 상아질접착제의 접착성능에 미치는 영향을 관찰하기 위해 시행되었다. 소의 하악전치 80개를 8개군으로 분류하여 순면의 상아질을 노출시켜서 산처리한 후 물로 습윤 상태를 유지시킨 대조군과 0.1%, 0.5% 및 1% 농도의 benzalkonium chloride 수용액으로 습윤시킨 실험군으로 나누어 NTG-GMA/BPDM계 상아질접착제인 All-bond 2와 DSDM 계 상아질접착제인 Aelitebond를 각각 접착시킨 후 접착시험을 시행하였다. 상아질 표면을 10% 인산수용액으로 처리한 후 습윤과정을 거친 시편을 각 접착시스템의 primer와 bonding resin을 도포하고 Aelitefil 복합레진으로 접 착시 킨후 항온조에서 24시간 방치한 뒤 인장접착강도를 측정하고, 상아질표면 및 파단면의 양상을 주사전자 현미경으로 관찰하였으며 FT-IR을 사용하여 전처리 전후의 상아질 표면을 분석하여 다음의 결과를 얻었다. 1. NTG-GMA/BPDM 계 상아질접착제 (All-bond 2)로 접착시킨 경우 물로 습윤시킨 대조군에 비해 0.1 % benzalkonium chloride 수용액으로 습윤시킨 군에서 유의하게 높은 인장접착강도를 보였으나(p<0.05), 0.5% 및 1.0 % benzalkonium chloride 수용액으로 습윤시킨 군에서는 유의한 차이가 나타나지 않았다. 2. DSDM계 상아질접착제 (Aelitebond) 로 접착시킨 경우 물로 습윤시킨 대조군과 0.1 %, 0.5% 및 1.0 % benzalkonium chloride 수용액으로 습융시킨 군 간의 인장접착강도의 유의한 차이는 없었다(p>0.05). 3. Benzalkonium chloride 수용액의 적용과 관계 없이 전체적으로 NTG-GMA/ BPDM계 상아질접착제로 접착시킨 경우가 DSDM계 상아질접착제로 접착시킨 경우보다 인장접착강도가 높았으며, 파단양상의 관찰결과에서도 NTG-GMA /BPDM계 상아질접착제를 사용한 경우는 응집성 및 혼합성 파단양상이, DSDM 계 상아질접착제를 사용한 경우는 부착성 파단양상이 우세하였다. 4. 주사전자 현미경적 관찰상에서 benzalkonium chloride 수용액 적용 유무에 따른 각 상아질 표면의 primer 도포양상의 뚜렷한 차이는 관찰되지 않았으나, 상아질 표면에 대한 benzalkonium chloride 수용액 적용 전후의 FT-IR 분석결과 에서는 0.1 % benzalkonium chloride 수용액으로 습윤 처리 시킨 군이 대조군에 비해 NTG-GMA/ BPDM 및 DSDM primer의 도포효과를 다소 향상시킨 소견이었다.

  • PDF

광중합형과 자가중합형 글라스 아이오노머 시멘트의 변연 접합성에 관한 연구 (A STUDY ON THE ADAPTATION OF LIGHT-CURED AND SELF-CURED GLASS-IONOMER CEMENTS TO TOOTH STRUCTURE)

  • 박일윤;조영곤;허승면
    • Restorative Dentistry and Endodontics
    • /
    • 제19권1호
    • /
    • pp.148-158
    • /
    • 1994
  • The purpose of this study was to compare the adaptation to tooth structure of light - cured glass ionomer cement with that of self -cured glass ionomer cement. In this study, class V cavities were prepared on the buccal surfaces of 10 extracted human premolar teeth, and teeth were randomly assigned 2 groups of 5 teeth each. The cavities of self-curing glass ionomer cement group were restored with the Fuji n. and the cavities of lightcuring glass ionomer cement group were restored with the Fuji II LC. The surfaces of glass ionomer cements were applied with All-Bond 2 adhesive, and cured with visible light. The restored teeth were stored in 100% relative humidity at $37^{\circ}C$ for 24 hours. And then. the roots of the teeth were removed with the tapered fissure bur and the remaining crowns were sectioned occlusogingivally through the center of glass ionomer restorations. Adaptation at tooth-restoration interface was assessed occlusally. axially, and gingivally by scanning electron microscope. The results were as follows : 1. On the occlusal margin, the group of self - curing glass ionomer cement showed closer adaptation to both enamel and dentin than the group of light-curing glass ionomer cement showing 5/lm gap between cement and tooth structure. 2. On the axial wall. the group of light-curing glass ionomer cement showing 5-$7{\mu}m$ gap between cement and dentin showed closer adaptation to dentin than the group of self -curing glass ionomer cement showing 10-$15{\mu}m$ gap between cement and dentin. 3. On the gingival margin, the group of light-curing glass ionomer cement showing 2-$5{\mu}m$ gap between cement and dentin(X 1200) showed closer adaptation to dentin than the group of self-curing glass ionomer cement showing 20pm gap between cement and dentin(X 600). 4. The group of self -curing glass ionomer cement showed closer adaptation on the occlusal margin than on the gingival margin, and the group of light-curing glass ionomer cement showed similar adaptation on both occlusal and gingival margins.

  • PDF

접착레진의 추가도포가 자가부식형 접착제의 상아질에 대한 미세인장접착강도에 미치는 영향 (Effect of additional coating of bonding resin on the microtensile bond strength of self-etching adhesives to dentin)

  • 정문경;조병훈;손호현;엄정문;한영철;정세준
    • Restorative Dentistry and Endodontics
    • /
    • 제31권2호
    • /
    • pp.103-112
    • /
    • 2006
  • 본 실험에서는 자가부식형 접착제와 콤포짓트 레진 사이의 산도의 차이를 완화시킬 수 있는 접착레진을 자가부식형 접착제 위에 추가적으로 도포할 경우, 상아질에 대한 접착력을 개선할 수 있는지를 연구하였다. 자가부식형 접착제로는 실험실에서 직접 제작한 실험용 자가부식형 접착제 (pH: 1.96)와 Adper Prompt (3M ESPE, VSA, pH: 1.0)를 사용하였으며, 중성의 접착레진으로 All-Bond 2의 D/E bonding resin (Bisco Inc., USA, pH: 6.9)을 사용하였다. 두 대조군에서는 두 가지 자가부식형 접착제를 각각 두번씩 도포하였으며, 두 실험군에서는 각 자가부식형 접착제를 한번 도포한 후 그 위에 D/E bonding resin을 추가 도포하였다. Z-250 하이브리드 복합레진을 쌓아올려 모레시계 형태의 시편을 제작하여 미세인장강도를 측정하고 t-test를 이용하여 비교하였다. 파절 양상은 입체현미경과 주사전자현미경을 이용하여 관찰하였다. D/E bonding resin을 추가 도포한 미세 인장접착강도는 유의하게 증가되었고, 접착층과 복합레진 또는 접착층과 상아질 사이의 파절을 보인 시편의 수는 감소하고, 접착층 내의 파절을 보인 시편의 수는 증가되었다. 따라서 자가부식형 접착제와 복합레진의 산도의 차이를 완화할 수 있는 중성의 접착레진을 추가 도포할 경우 미세인장접착강도를 증가시킬 수 있음을 확인하였다.

수 종의 복합레진 접착 시스템에서의 미세 누출의 비교 (COMPARISON OF MICROLEAKAGE WITH THREE DIFFERENT ADHESIVE SYSTEMS)

  • 석충기;남동우;남순현;김영진;김현정
    • 대한소아치과학회지
    • /
    • 제31권4호
    • /
    • pp.636-644
    • /
    • 2004
  • 최근 자가 부식형 접착 시스템이 개발되어 법랑질 및 상아질에 모두 적용할 수 있고, 임상적 술식을 단순화 시켰다. 이 접착 시스템은 적용하기 용이하고 임상적으로도 법랑질 및 상아질에 높은 결합강도를 보인다고 보고되고 있다. 이 연구는 in vitro 상에서 복합레진 5급 와동의 법랑질 및 상아질 경계에서 전부식 처리를 동반한 one-bottle 접착시스템과 자가 부식형 접착 시스템을 사용하였을 때 미세 누출을 비교하기 위해 시행하였다. 교정적 목적으로 발치된 30개의 소구치를 무작위적으로 3개 군으로 나누었다; 1 군 (Single $Bond^{(R)}$ + Filtek $Z250^{(R)}$), 2 군 (Clearfil SE $Bond^{(R)}$ + Filtek $Z250^{(R)}$), 3 군 (Adper Prompt $L-Pop^{(R)}$ + Filtek $Z250^{(R)}$). 표준화된 5급 와동을 각 소구치 협면, 설면에서 백악-법랑경계에 평행하게 형성하였으며, 와동의 치은측 1/2은 백악법랑경계보다 1mm 치근단으로 연장하였다. 접착 시스템을 제조자의 지시대로 적용한 다음 복합레진을 충전하고 제조자의 지시대로 광중합하였다. 시편을 $37^{\circ}C$ 증류수에 5일 간 보관 후 $5^{\circ}C{\pm}2^{\circ}C$$55^{\circ}C{\pm}2^{\circ}$에서 1000회 열순환한 다음, 2% methylene blue 용액에 12시간 침잠시켰다. $Isomet^{TM}$ (Buehler Co., Lake Bluff, IL, USA)을 사용하여 치아를 충전물 중앙에서 종절단한 후 입체 현미 경하에서 25배의 배율로 색소 침투도를 평가하였다. 결과는 t-test 와 one-way ANOVA를 이용하여 통계처리 하였다. 결과는 다음과 같았다. ${\cdot}$ 실험에 사용 된 접착 시스템 중에 미세 누출을 완벽하게 방지하는 접착 시스템은 없었다. ${\cdot}$ 상아질 경계에서의 미세 누출이 법랑질 경계에서보다 통계학적으로 유의하게 더 많았다(p<0.0001). ${\cdot}$ 법랑질 경계에서 자가 부식형 접착 시스템은 전부식 처리를 동반한 one-bottle접착 시스템과 통계학적으로 유의한 차이를 보이지 않았다. ${\cdot}$ 상아질 경계에서, 자가 부식형 접착 시스템은 전부식 처리를 동반한 one-bottle 접착 시스템과 통계학적으로 유의한 차이를 보이지 않았다.

  • PDF

Influence of 10-MDP concentration on the adhesion and physical properties of self-adhesive resin cements

  • Shibuya, Kazuhiko;Ohara, Naoko;Ono, Serina;Matsuzaki, Kumiko;Yoshiyama, Masahiro
    • Restorative Dentistry and Endodontics
    • /
    • 제44권4호
    • /
    • pp.45.1-45.10
    • /
    • 2019
  • Objectives: Self-adhesive resin cements contain functional monomers that enable them to adhere to the tooth structure without a separate adhesive or etchant. One of the most stable functional monomers used for chemical bonding to calcium in hydroxyapatite is 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP). The aim of this study was to evaluate the influence of the10-MDP concentration on the bond strength and physical properties of self-adhesive resin cements. Materials and Methods: We used experimental resin cements containing 3 different concentrations of 10-MDP: 3.3 wt% (RC1), 6.6 wt% (RC2), or 9.9 wt% (RC3). The micro-tensile bond strength of each resin cement to dentin and a hybrid resin block (Estenia C&B, Kuraray Noritake Dental) was measured, and the fractured surface morphology was analyzed. Further, the flexural strength of the resin cements was measured using the three-point bending test. The water sorption and solubility of the cements following 30 days of immersion in water were measured. Results: The bond strength of RC2 was significantly higher than that of RC1. There was no significant difference between the bond strength of RC2 and that of RC3. The water sorption of RC3 was higher than that of any other cement. There were no significant differences in the three-point bending strength or water solubility among all three types of cements. Conclusions: Within the limitations of this study, it is suggested that 6.6 wt% 10-MDP showed superior properties than 3.3 wt% or 9.9 wt% 10-MDP in self-adhesive resin cement.

수중 보관이 접착용 레진의 물리적 성질에 미치는 영향 (The Influence of Water Storage on Mechanical Properties of Adhesive Resin)

  • 김원찬;이광원;이정;유미경;김정희
    • 구강회복응용과학지
    • /
    • 제22권2호
    • /
    • pp.193-202
    • /
    • 2006
  • Objective To evaluate the influence of water storage on the mechanical properties of dental adhesives over 1 and 3 months. Materials and Methods Adhesive resin sheets were prepared by pouring either All-bond 2(AB), Clearfil SE Bond(SE) into a mold measuring $15{\times}15{\times}0.9mm$. After solvent in primer evaporation, the adhesives were light-cured and removed from the mold and divided in two pieces, trimmed to hourglass shape that were used to determine the micro-tensile strength(MTS). Another hourglass shaped metal mold measuring $2.0{\times}1.5mm$ in cross-section area was made to determine the Young's modulus(E). Adhesive specimens for Young's modulus(E) were prepared in the same method. Specimens were stored at $37^{\circ}C$ in distilled water and tested after 1 and 3 months. The data were analyzed by one-way ANOVA and Tukey's test. Results Water storage significantly decreased the micro-tensile strength(MTS) of AB and SE specimens after 1 and 3 months(P<0.05). The Young's modulus(E) were also decreased after water storage for 1 and 3 months, but statistically not significant in each group of AB and SE group respectively. Conclusions Long-term exposure of adhesive resin to water can cause reduction of mechanical properties. It may compromise resin/dentin bonds and affect longevity of restorations.