• Title/Summary/Keyword: Dental resin cement

Search Result 232, Processing Time 0.024 seconds

A STUDY ON THE DENTAL HEALTH STATUS OF A COLLEGE GIRL STUDENTS (S여대생(女大生)의 구강보건 실태조사)

  • Kim, Jung-Sik
    • Restorative Dentistry and Endodontics
    • /
    • v.6 no.1
    • /
    • pp.123-132
    • /
    • 1980
  • The author conducted a dental survey of a college girl students and compared with that of E college students 10 years ago which based on the same criteria. The items of this survey included the prevalence of dental caries, DMFT and the kinds of restored material. All college students 1,414 were examined in May 1978, with the recommended criteria and method of W.H.O.. Among them, the data of 1,393 were analyzed for this study. The following results were obtained: 1. The average number of present teeth were 28.97${\pm}$1.64. 2. The prevalence of dental caries was 84.92% and D.M.F. index was 15.51. Average D.M.F. teeth were 4.49${\pm}$3.69. 3. The average number of decayed (D) teeth were 2.09${\pm}$2.16. 4.30% of the present decayed teeth was secondary decay, and 2.44% of the decayed teeth was indicated for extraction. 4. The average number of missing(M) teeth were 0.32${\pm}$0.79. It included 8.56% of root fragements. 5. Average number of filled(F) teeth were 2.09${\pm}$3.17. F-ratio of this group was 46.45%. The analysis revealed 50.88% of amalgam alloy, 31.41% of gold inlays, and 1.20%, the least among the filling materials, silicate cement or composite resin. 6. While the prosthodontic treatment, such as crown and bridge has reduced than that of 10 years ago, the fillings and inlays as the conservative means has increased.

  • PDF

Changes in occlusion of indirect restorations according to universal adhesives (범용 상아질 접착제에 따른 간접 수복물의 교합 변화)

  • Byun, Ji-Eun
    • Journal of Korean Academy of Dental Administration
    • /
    • v.9 no.1
    • /
    • pp.7-13
    • /
    • 2021
  • The present randomized controlled trial aimed to evaluate changes in occlusion of indirect restorations before and after attachment using resin cement according to universal adhesives. This study included patients who underwent indirect restoration treatment at the Yonsei University Dental Hospital between April and October 2016. Universal adhesives requiring light curing and those not requiring light curing were used in this study. Changes in occlusion before and after adhesion of the indirect restoration were evaluated using articulating paper and shimstock as well as through the discomfort felt by the patients. To analyze the differences between the universal adhesive, Fisher's exact tests were performed using SPSS ver. 22.0 software. Of the 39 cases of indirect restoration, 29 were included in the study. A change in occlusion after adhesion of the indirect restoration was observed in only one case of universal adhesive that required light curing. The patient felt that the occlusion increased after the attachment of the restoration, and it was observed that the occlusion point was different from that before attachment. However, the results of the analysis were not statistically significant. Based on the findings, the universal adhesives did not affect the occlusion before and after indirect adhesion restoration using RelyX Ultimate.

INFLUENCE OF TOOTH SURFACE ROUGHNESS AND TYPE OF CEMENT ON RETENTION OF COMPLETE CAST CROWNS (치아표면 거칠기와 시멘트 종류가 전부주조관의 유지력에 미치는 영향)

  • Kim, Kil-Su;Song, Chang-Yong;Ahn, Seung-Geun;Park, Charn-Woon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.4
    • /
    • pp.465-473
    • /
    • 1999
  • Bond strength of luting cements to dentin is a critical consideration for success of complete cast crowns. This study was performed to evaluate the relationship between surface characteristics of teeth prepared for complete cast crowns and retention of cemented restorations. Eighty artificial crowns were cast for standardized complete crown tooth preparations accomplished with the use of a special device on recently extracted human teeth. Coarse diamond(#102R, Shofu) and superfine finishing diamond(#SF102R, Shofu) burs of similar shape were used. Crowns in each group were randomly subdivided into few subgroups of 10 for luting cements selected for this study: zinc phosphate cement (FLECK' S), polycarboxylate cement (Poly-F), rein-forced glass ionomer cement (Fuji PLUS). and adhesive resin cement (Panavia 21). Retention was evaluated by measuring the tensile load required to dislodge the artificial crown from tooth preparations with an Instron testing machine, and analysed by one-way ANOVA and Student's t-test. The obtained results were as follows ; 1. When tooth preparation was done with coarse diamond bur, retentive force was diminished in order of Panavia 21 Fuji PLUS, FLECK'S, and Poly-F. Retentive forces showed the significant difference between Fuji PLUS group and FLECK'S group(p<0.001). 2. When tooth preparation was done with superfine diamond bur, retentive force was diminished in order of Fuji PLUS, Panavia 21, FLECK'S, and Poly-F. Retentive forces showed the significant difference between Panavia 21 group and FLECK'S group(p<0.001). 3. Retentive force in coarse tooth surfaces was significantly higher than that in superfine tooth surface with all luting cements(p<0.001), and cement residues were almost retained with-in the cast crown in all groups.

  • PDF

Characterization of the Stress in the Luting Cement layer Influenced by Material Properties of Full Veneer Crown (전부피개관의 물성과 시멘트의 물성이 시멘트 내부의 응력에 미치는 영향)

  • Lee, Jun-Young;Lee, Kyu-bok;Lee, Chung-Hee;Jo, Kwang-Hun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.25 no.1
    • /
    • pp.1-12
    • /
    • 2009
  • The objective of this study was to test the effects of crown material, cement type, the direction in which stress is applied and distribution of luting cement that might lead to cement microfracture using 2D Finite Element Method. Twenty three finite element models with a chamfer margin configuration were generated for a mandibular first molar. Crown models exhibited four crown materials: type 3 gold alloy, Ni-Cr alloy, ceramic and composite resin, and two luting cements: zinc phosphate and glass ionomer cements with a thicknesses of $70{\mu}m$. Modeled crowns were loaded axially or obliquely at unit load of 1 N. Areas and levels of stress concentrations within the cement were determined. Stress in the cement layer at the margins of crowns were higher than those in the area away from the margin. Stress under oblique loads were much higher than under axial load. The stiffer crown material produced higher stress and similarly, higher stress were found in cements with the greater Young's modulus.

The Effect of Surface Treatment on the Shear Bond Strength of Resin Cement to Zirconia Ceramics (표면처리가 지르코니아와 레진 시멘트의 전단결합강도에 미치는 효과)

  • Jung, Seung-Hyun;Kim, Kye-Soon;Lee, Jae-In;Lee, Jin-Han;Kim, Yu-Lee;Cho, Hye-Won
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.25 no.2
    • /
    • pp.83-94
    • /
    • 2009
  • The aim of this study was to investigate the shear bond strength between zirconia ceramic and resin cement according to various surface treatments. The surface of each zirconia ceramic was subjected to one of the following treatments and then bonded Rely X Unicem or Rely X ARC resin cement; (1) Rocatec system and $50{\mu}m$ surface polishing, (2) No treatment and $50{\mu}m$ surface polishing, (3) Rocatec system and $1{\mu}m$ surface polishing, (4) No treatment and $1{\mu}m$ surface polishing. Each of eight bonding group was tested in shear bond strengths by universal testing machine(Z020, Zwick, Ulm, Germany) with crosshead speed of 1mm/min. The results were as follows; 1. Rocatec treatment groups showed greater bonding strengths than No Rocatec groups. There was significant difference of among groups(P<0.001) 2. For Rocatec groups, $50{\mu}m$ surface roughness groups showed greater bonding strengths than $1{\mu}m$ surface roughness groups.(P<0.001) But for No Rocatec groups, There was no significant difference of among groups(P>0.05) 3. Rely X Unicem groups showed greater bonding strengths than Rely X ARC groups. There was significant difference of among groups(P<0.01) Within the conditions of this study, Rocatec treatment was an effective way of increasing zirconia bonds to a resin cement, even in the case of self-adhesive resin cement.

Shear bond strength of the three different kinds of resin cement on CAD/CAM ceramic inlay (CAD/CAM 세라믹 인레이에 대한 3종의 레진 시멘트의 전단결합강도에 관한 연구)

  • Baek, Chul-Woo;Park, Cheol-Woo;Park, Jun-Sub;Ryu, Jae-Jun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.51 no.1
    • /
    • pp.20-26
    • /
    • 2013
  • Purpose: The purpose of this study was to evaluate the bond strengths between the latest CAD/CAM ceramic inlay and various resin cements which are used primarily for esthetic restoration. Materials and methods: Cylindrical ceramic blocks(Height: 5 mm, diameter: 3 mm) were fabricated by using Cerec3 and bonded on the dentin of the ninety extracted caries-free molars using three different kinds of resin cement(Unicem$^{(R)}$, Biscem$^{(R)}$, and Variolink II$^{(R)}$) according to the manufacturer's instructions. Ninety specimens were divided into 3 groups according to three different kinds of resin cement. Half of each group were conducted thermocycling under the conditions of the $5-55^{\circ}C$, 5,000 cycle but the other half of them weren't. All specimens were kept in normal saline $37^{\circ}C$, for 24 hours before measuring the bond strength. The shear bond strength was measured by Universal testing machine with a cross head speed of 0.5 mm/min. The results were analyzed statistically by t-test and one-way ANOVA. Results: Unicem$^{(R)}$ group showed the highest shear bond strength despite a slight decline by thermocycling. The shear bond strength of Unicem$^{(R)}$ group and ValiolinkII$^{(R)}$ group were significantly influenced by thermocycling, whereas Biscem$^{(R)}$ group was not influenced (P<.05). There were no significant differences in the bond strength between the three groups without thermocycling, but there was significant differences between Unicem$^{(R)}$ group and Valiolink II$^{(R)}$ group with thermocycling(P<.05). Conclusion: It has been shown to be clinically effective when the self-adhesive resin cements Unicem$^{(R)}$ and Biscem$^{(R)}$ were used instead of the etch-and-rinse resin cement Valiolink II$^{(R)}$ during the bonding of CAD/CAM ceramic inlay restorations with teeth.

EFFECTS OF RESIN CEMENTS, CERAMIC SURFACE TREATMENTS AND THERMOCYCLING ON SHEAR BOND STRENGTH OF IPS EMPRESS CERAMIC (레진시멘트, 표면처리 및 열순환에 따른 IPS Empress의 전단결합강도)

  • Han, Jeong-Min;You, Young-Dae;Lee, Yong-Keun;Im, Mi-Kyung;Lee, Su-Jong
    • Restorative Dentistry and Endodontics
    • /
    • v.24 no.3
    • /
    • pp.473-481
    • /
    • 1999
  • This study evaluated the shear bond properties of IPS Empress glass ceramic to enamel and dentin surfaces with three ceramic surface treatments, and three resin cements. The influence of thermocycling was also investigated. The purpose of this study was to investigate the influences of resin cements, ceramic surface treatments, and thermocycling on shear bond properties. Ninety freshly extracted, noncarious human molars were selected for this study. The surface treatments of ceramic were etching <5.0% hydrofluoric acid, application of silane coupling agents(Tokuso Ceramic Primer, Clearfil porcelain bond, Monobond-S), and the combination of the two methods. Empress cylinders were bonded to enamel and dentin surfaces with three kinds of resin cements(Bistite resin cement, Panavia 21, Variolink). The specimens were aged in $37^{\circ}C$ distilled water for 24 hours. Half of the specimens were then thermocycled 500times between $5^{\circ}C$ and $55^{\circ}C$ with a dwell time of 15 seconds. Each specimen was debonded in shear mode and measured shear bond properties by using the universal testing machine(Zwick 020, Germany). The data were analyzed by SPSS/PC+(one-way ANOVA, Scheffe' s test and t-test). The results were as follows : 1. Without thermocyling, there was significant difference of shear bond strength to enamel surface between Bistite Resin Cement and Panavia 21 in case of etched and silane-treatment(p<0.05). 2. Without thermocyling, the shear bond strength of a group treated with silane and etching was significantly higher than that of a group treated with silane or etching with the application of Panavia 21 and Variolink(p<0.05). 3. A group treated with etching with the application of Variolink only showed a decrease of shear bond strength after thermocycling(p<0.05).

  • PDF

A study on the dental technology and fabrication cost analysis of implant prosthesis for National Health Insurance (건강보험 급여화 관련 임플란트보철물의 기공원가 분석 연구)

  • Cho, Mi-Hyang;Lee, Gwang-Young;Lee, Hee-kyung;Nam, Shin-Eun;Ryu, Jae-Kyung;Kwon, Hyok-Mun;Kim, Kyung-Rok;Cho, Hong-Kyu
    • Journal of Technologic Dentistry
    • /
    • v.42 no.2
    • /
    • pp.149-162
    • /
    • 2020
  • Purpose: The purpose of this study was to conduct a cost accounting of implant prosthesis according to the fabrication activities. Methods: In this study, the cost price of implant prosthesis fabrication activities was calculated by the bottom-up costing approach for material and labor cost and the top-down costing approach for expenses and other. Results: The total cost price was estimated to 220,000 ~ 310,000 won per one implant prosthesis. By product, the screw type was estimated to 220,000 ~ 230,000 won, and when the stent and tray were included, it was 260,000 ~ 270,000 won, which increased about 40,000 won. And, the cement type with more material and labor time was estimated to 250,000 ~ 260,000 won, and when the stent and tray were included, it was about 300,000 won. Conclusion: In terms of the fabrication cost ratio by items, it was shown that material cost and labor cost accounted for about 40% and 30% of the total cost structure for resin case, respectively, which was the opposite for porcelain. It was shown that expenses and general administrative expenses accounted for about 15%, and profits were about 11% ~ 14% in both cases.

The effect of tooth bleaching agent contained 35% hydrogen peroxide on the color, microhardness and surface roughness of tooth-colored restorative materials (35% 과산화수소를 함유한 치아미백제가 심미수복재의 색, 미세경도 및 표면 거칠기에 미치는 영향)

  • Shim, Youn-Soo
    • Journal of Korean society of Dental Hygiene
    • /
    • v.12 no.3
    • /
    • pp.533-541
    • /
    • 2012
  • Objectives : The purpose of this study was to evaluate the effects of tooth bleaching agent contained 35% hydrogen peroxide on the color, microhardness and surface roughness of tooth-colored restorative materials. Methods : Four types of tooth-colored restorative materials, including a composite resin(Filtek Z350 ; Z350), a flowable composite resin(Filtek P60 : P60), a compomer(Dyract$^{(R)}$ AP ; DY), and a glass-ionomer cement(KetacTM Molar Easymix ; KM) were used in the study. The specimens($8mm{\times}5mm$) were made by using a customized acrylic mold. Each material was divided into two groups equally(n=40) : experimental group(35% HP) and control group(distilled water). 35% HP group was treated 30 mim/5 days for 15 days. Each 30 minute treatment session consisted of two 15 minute cycles of gel application with 20 second light exposure. The authors measured the color, microhardness, and roughness of the specimens before and after bleaching. The data were analyzed with ANOVA and T-test. Results : 35% HP group showed an apparent color change(${\Delta}E^*$) than control group. In particular, DY and KM showed a noticeable color change and statistically significant differences(p<0.05). 35% HP group showed a reduction in microhardness. Z350 and P60 does not have a statistically significant difference(p>0.05), DY and KM showed a statistically significant difference(p<0.05). Percentage microhardness loss(PML) of control group was 0.6 to 5.5% in the group, 35% HP group was 6.6 to 34.6%. Roughness was increased in 35% HP group after bleaching. Especially DY and KM were significantly increased(p<0.05). Conclusions : Bleaching agents may affect the surface of existing restorations; therefore, they should not be used indiscriminately when tooth-colored restorations are present.

Attachment of Human Gingival Fibroblast to Various Subgingival Restorations;A Comparative Study in Vitro (다양한 치은 연하 수복물에 대한 치은 섬유아 세포 부착 연구)

  • Lee, Eun-Suk;Song, In-Taeck;Lim, Jeong-Su;Kim, Hyung-Seop
    • Journal of Periodontal and Implant Science
    • /
    • v.29 no.3
    • /
    • pp.621-636
    • /
    • 1999
  • When mucoperiosteal flaps are positioned and sutured to desirable position, the wound contains several interface between tissues which differ fundamentally in composition & biological reaction. Thus the C-T surface of the flap will, on one hand, oppose another vascularized surface, and on the other, the avascular dental material for example, when root resoptions, fractured root, endodontic perforation, deep root carious lesions were filled with amalgam, glass ionomer, resin etc. Recently, a number of case report described the successful treatment of a subgingival root lesion with restorative material & free gingival graft, open flap surgery, but more objective research was needed . Most of study on restorative materials were concerned for cytotoxicity not for actual healing event on that materials and its influencing factors such as biocompatibility, surface wettability, surface topography . The aim of this in vitro study was to evaluate the effect of amalgam, resin modified glass ionomer, composite resin per se, and their surface roughness on the growth of human gingival fibroblast. The cells were obtained and placed on culture flask and incubated for 3 days with the prepared test materials. Then count the attached cell number with hemocytometer,(n=12) and 2 samples were examined with SEM about attachment cell morphology . Another 4 samples were evaluated on their surface roughness with Talysurf and average surface roughness value(Ra) were obtained. Statistical difference in attached cell number, roughness value were analyzed using ANOVA. The number of attached cell was as follows, for root dentin specimen 16.7${\pm}$4.41, resin modified glass ionomer 14.0${\pm}$4.15, resin 8.13${\pm}$3.63, amalgam 0.72${\pm}$3.33(${\times}10^3$). Between root dentin and resin-modified glass ionomer, no significant difference was observed, but resin, amalgam showed a significant less cell numbers than for root dentin, resin modified glass ionomer cement. SEM examination expressed many cell surface attachment apparatus in root dentin and resin modified glass ionomer specimens. For resin specimen, cell attachment was observed but exposed less appratus. The average surface roughness value are following results. Dentin specimen 0.6972${\pm}$ 0.104, resin modified glass ionomer 0.0822${\pm}$0.009, resin 0.0875${\pm}$0.005, amalgam 4.2145${\pm}$0.985(${\mu}m$). Between root dentin, resin-modified glass ionomer, and resin, no significant difference was observed, but amalgam showed a significant more rough surface than other groups. When evlauated the interrelationship between cell attachment and surface roughness, therefore, there was weak reverse correlation.(pearson correlation : - 0.593) These results suggest that resin modified glass ionomer have the favorable healing potential when used for subgingival restoration. And for relationship between cell attachment and surface characteristics, further investigations were needed.