Effects of core characters and veneering technique on biaxial flexural strength in porcelain fused to metal and porcelain veneered zirconia

  • Oh, Ju-Won;Song, Kwang-Yeob;Ahn, Seung-Geun;Park, Ju-Mi;Lee, Min-Ho;Seo, Jae-Min
    • The Journal of Advanced Prosthodontics
    • /
    • 제7권5호
    • /
    • pp.349-357
    • /
    • 2015
  • PURPOSE. The purpose of this study was to assess the impact of the core materials, thickness and fabrication methods of veneering porcelain on prosthesis fracture in the porcelain fused to metal and the porcelain veneered zirconia. MATERIALS AND METHODS. Forty nickel-chrome alloy cores and 40 zirconia cores were made. Half of each core group was 0.5 mm-in thickness and the other half was 1.0 mm-in thickness. Thus, there were four groups with 20 cores/group. Each group was divided into two subgroups with two different veneering methods (conventional powder/liquid layering technique and the heat-pressing technique). Tensile strength was measured using the biaxial flexural strength test based on the ISO standard 6872:2008 and Weibull analysis was conducted. Factors influencing fracture strength were analyzed through three-way ANOVA (${\alpha}{\leq}.05$) and the influence of core thickness and veneering method in each core materials was assessed using two-way ANOVA (${\alpha}{\leq}.05$). RESULTS. The biaxial flexural strength test showed that the fabrication method of veneering porcelain has the largest impact on the fracture strength followed by the core thickness and the core material. In the metal groups, both the core thickness and the fabrication method of the veneering porcelain significantly influenced on the fracture strength, while only the fabrication method affected the fracture strength in the zirconia groups. CONCLUSION. The fabrication method is more influential to the strength of a prosthesis compared to the core character determined by material and thickness of the core.

지르코니아 코어의 종류와 도재 두께에 따른 색상의 변화 (The study on the shade color change that depends on the kind of zirconia core and the porcelain thickness)

  • 염미옥;이종혁;신수연;신승철;조자원
    • 대한치과기공학회지
    • /
    • 제32권4호
    • /
    • pp.341-350
    • /
    • 2010
  • Purpose: This study focused on achieving desired shades by combining zirconia core with different thickness porcelain in order to make dental prostheses effectively. Methods: White and colored $LAVA^{TM}$ All Ceramic (3M-ESPE, Seefeld, Germany), and Zirkonzahn (Bruneck, Italy) Trans and prettau were used to have Zirconia. LAVATM Ceram (3M-ESPE, Germany) and ICE (Zirkonzahn, Italy) powder were used to have the porcelain. We made quadrilateral specimen of thickness 0.3mm, 0.5mm, 0.7mm and diameter 10 to use zirconia ceramics system of 2 kinds that color tone reappearance way is different and produced total 120 specimens to 4 experimental groups. We used Spectrophotometer to analyze color tone. Data's value getting by dispersal colorimetry period found L*, a*, b* value using Excel program. We used one-way ANOVA to use SPSS WIN 12.0 program. Results: All L*, a*, b* indexes of zirconia core and porcelain veneer in LAVA group and Zirkonzahn group were different. When you combine the white zirconia core of LAVA group with a porcelain veneer, the thickness of the porcelain must be more than 0.5mm to meet the standard target. When all the colored zirconia cores of LAVA group were combined with porcelain veneers, there was no significant difference from the standard target. When the zirconia cores of Zirkonzahn group are combined with porcelain veneers, the thinner thicknesses were closer to the standard tab than thicker thicknesses; however, there was a significant difference in all combinations, with Delta E* value indicating more than 3. Conclusion: When it comes to colored zirconia, which is the most popular, the thicknesses of both a core and a dentin veneer must be more than 0.3mm to get an appropriate shade. There is more possibility to get desirable shades when the thicknesses of a white core are thinner; however, they would be vulnerable to the environment and lose their color. When combine a zirconia core with a dentin veneer, using Zirkonzahn group needs more considerations in order to meet the standard target.

도재 소성 과정에서의 고온이 지르코니아 코어의 변연적합도에 미치는 영향 (Influence of High Temperature of the Porcelain Firing Process on the Marginal Fit of Zirconia Core)

  • 김재홍;김기백
    • 치위생과학회지
    • /
    • 제13권2호
    • /
    • pp.135-141
    • /
    • 2013
  • 본 연구는 치과에서 사용되는 심미 보철물 중에 하나인 지르코니아 기반의 전부도재관 제작 시 지르코니아 코어 위에 상부 도재를 축성하고 소성하는 과정에서 발생되는 고온이 완성된 전부도재관의 변연적합도에 미치는 영향을 분석함으로써 임상적 허용이 가능한지 알아볼 뿐 아니라, 치과보철치료를 위한 치과의사, 치과위생사, 치과기공사의 보철물 선택 시 임상적 참고자료로 제공할 목적으로 수행되었다. 심미에 가장 많은 영향을 미치는 상악 중절치를 지대치로 선정하여 동일한 모형 10개 제작 후 각각의 지대치에 적합한 지르코니아 코어를 제작하였다. 제작된 코어의 변연적합도 측정 후 코어 위에 상부 도재를 축성하여 전부도재관을 완성한 뒤 2차 측정을 실시하였으며, 측정 후 비교 분석 된 결과는 다음과 같다. 변연적합도는 지르코니아 코어 제작한 후 전부도재관으로 제작되는 과정에 따라 더 커졌으며, 통계적으로도 유의한 차이를 보였다(p<0.001). 그러나 전부도재관에서 총 80회 측정된 변연적합도의 값에서 임상적 허용 수치인 $120{\mu}m$을 넘지 않는 결과를 보였으며, 이와 같은 결과를 토대로 지르코니아 코어 위에 상부 도재 소성 시 변연적합도가 커지긴하나 임상적으로 허용이 가능하다는 결론을 도출하였다.

Influence of surface modification techniques on shear bond strength between different zirconia cores and veneering ceramics

  • Mosharraf, Ramin;Rismanchian, Mansour;Savabi, Omid;Ashtiani, Alireza Hashemi
    • The Journal of Advanced Prosthodontics
    • /
    • 제3권4호
    • /
    • pp.221-228
    • /
    • 2011
  • PURPOSE. Veneering porcelain might be delaminated from underlying zirconia-based ceramics. The aim of this study was the evaluation of the effect of different surface treatments and type of zirconia (white or colored) on shear bond strength (SBS) of zirconia core and its veneering porcelain. MATERIALS AND METHODS. Eighty zirconia disks (40 white and 40 colored; 10 mm in diameter and 4 mm thick) were treated with three different mechanical surface conditioning methods (Sandblasting with $110{\mu}m$ $Al_2O_3$ particle, grinding, sandblasting and liner application). One group had received no treatment. These disks were veneered with 3 mm thick and 5 mm diameter Cercon Ceram Kiss porcelain and SBS test was conducted (cross-head speed = 1 mm/min). Two and one way ANOVA, Tukey's HSD Past hoc, and T- test were selected to analyzed the data (${\alpha}=0.05$). RESULTS. In this study, the factor of different types of zirconia ceramics (P=.462) had no significant effect on SBS, but the factors of different surface modification techniques (P=.005) and interaction effect (P=.018) had a significant effect on SBS. Within colored zirconia group, there were no significant differences in mean SBS among the four surface treatment subgroups (P=0.183). Within white zirconia group, "Ground group" exhibited a significantly lower SBS value than "as milled" or control (P=0.001) and liner (P=.05) groups. CONCLUSION. Type of zirconia did not have any effect on bond strength between zirconia core and veneer ceramic. Surface treatment had different effects on the SBS of the different zirconia types and grinding dramatically decreased the SBS of white zirconia- porcelain.

열가압성형도재 코어의 가시광선 투과율에 관한 연구 (A study on the visible wave of transmittance pressable ceramic core)

  • 정인호;이상덕;남상용
    • 대한치과기공학회지
    • /
    • 제34권1호
    • /
    • pp.1-9
    • /
    • 2012
  • Purpose: The purpose of this study was to investigate the transmittance differences of pressable ceramic core due to thickness within the visible light spectrum. Methods: 36 specimens were divided into 2 groups (0.6mm, 0.8mm) which have each 3 specimens. The size of specimens was 10mm high and 10mm wide. The transmittance of specimens are measured by spectrophotometer Model Cary 500 that can measure infrared-ray, visible wave and ultraviolet-ray. Results: The results shows that there was no significant difference between specimen's thickness(0.6mm, 0.8mm) and transmittance. Conclusion: The individual's color perception is personal and there are numerous factors that influence on it. In general, human eye can perceive the color of thing only within visible light spectrum but in this experiment through spectrophotometer there was no big difference between specimen's thickness(0.6mm, 0.8mm) and transmittance. To sum up, The most important factors were a layed porcelain structure and its thickness rather than core thickness in the porcelain crown. Also, When making all ceramic core with dead pulp (nervous treatment tooth) when used as a restorative esthetic think is more efficient to improve.

지르코니아 코어의 두께에 따른 분광광도계 투과율에 관한 연구 (A study on the transmittance due to thickness of zirconium core)

  • 정인호;박명자;김주원
    • 대한치과기공학회지
    • /
    • 제33권2호
    • /
    • pp.129-136
    • /
    • 2011
  • Purpose: The purpose of this study was to investigate the transmittance differences of zirconium core due to thickness within the visible light spectrum. Methods: 36 specimens were divided into 3 groups (0.6mm, 0.8mm, 1.0mm) which have each 12 specimens. The size of specimens was 10mm high and 10mm wide. The transmittance of specimens are measured by spectrophotometer Model Cary 500 that can measure infrared-ray, visible wave and ultraviolet-ray. Results: The results shows that there was no significant difference between specimen's thickness and transmittance. Conclusion: The individual's color perception is personal and there are numerous factors that influence on it. In general, human eye can perceive the color of thing only within visible light spectrum but in this experiment through spectrophotometer there was no big difference between specimen's thickness and transmittance. To sum up, The most important factors were a layed porcelain structure and its thickness rather than core thickness in the porcelain crown.

Spectrophotometer를 이용한 지르코니아 코어의 두께 및 도재축성법에 따른 색조의 변화에 대한 연구 (The study on the color change according to zirconia core thickness, and build-up technique using spectrophotometer)

  • 허성윤;김재홍;손호정
    • 대한치과기공학회지
    • /
    • 제33권4호
    • /
    • pp.313-321
    • /
    • 2011
  • Purpose: The purpose of this study was to compare color parameters of different fabrication method of Lava ceram powder, Lava DVS blocks, IPS e.max ceram and IPS e.max zirpress. Methods: The three available shades(A1, A2, A3.5) of Lava & Kavo zirconia blocks were examined. For each of three colors, three different thickness were tested, 5 times of measurement frequency. The measurements were made using a spectrophotometer equipped with an integrating sphere using the CIE $L^*$, $a^*$, $b^*$ colorimetric system. Results: Lava build-up group and Lava DVS group showed clinically perceived color difference, on the other hand IPS e.max build-up group and IPS e.max zirpress group did not show clinically perceived color difference to shade allowed on core. When the thickness of porcelain veneer increased from Lava and IPS e.max groups, color differences(${\Delta}E$) were decreased. Conclusion: All-ceramic system has color characteristics that clinicians have to consider when selecting materials. Also, manufacturers of different porcelain systems must make every effort to achieve color reproducibility.

Comparative fracture strength analysis of Lava and Digident CAD/CAM zirconia ceramic crowns

  • Kwon, Taek-Ka;Pak, Hyun-Soon;Yang, Jae-Ho;Han, Jung-Suk;Lee, Jai-Bong;Kim, Sung-Hun;Yeo, In-Sung
    • The Journal of Advanced Prosthodontics
    • /
    • 제5권2호
    • /
    • pp.92-97
    • /
    • 2013
  • PURPOSE. All-ceramic crowns are subject to fracture during function. To minimize this common clinical complication, zirconium oxide has been used as the framework for all-ceramic crowns. The aim of this study was to compare the fracture strengths of two computer-aided design/computer-aided manufacturing (CAD/CAM) zirconia crown systems: Lava and Digident. MATERIALS AND METHODS. Twenty Lava CAD/CAM zirconia crowns and twenty Digident CAD/CAM zirconia crowns were fabricated. A metal die was also duplicated from the original prepared tooth for fracture testing. A universal testing machine was used to determine the fracture strength of the crowns. RESULTS. The mean fracture strengths were as follows: $54.9{\pm}15.6$ N for the Lava CAD/CAM zirconia crowns and $87.0{\pm}16.0$ N for the Digident CAD/CAM zirconia crowns. The difference between the mean fracture strengths of the Lava and Digident crowns was statistically significant (P<.001). Lava CAD/CAM zirconia crowns showed a complete fracture of both the veneering porcelain and the core whereas the Digident CAD/CAM zirconia crowns showed fracture only of the veneering porcelain. CONCLUSION. The fracture strengths of CAD/CAM zirconia crowns differ depending on the compatibility of the core material and the veneering porcelain.

유한요소법을 이용한 심미치관보철의 설계에 따른 치아와 보철물의 응력분산에 관한 연구 (A Finite Element Analysis of Stress Distribution in the Tooth and Crown According to Design of Esthetic Crown)

  • 이명곤;정인성;김지환
    • 대한치과기공학회지
    • /
    • 제21권1호
    • /
    • pp.115-121
    • /
    • 1999
  • This investing was carried out to evaluate the alteration of stress distribution on teeth and esthetic crowns. Analyzing the stress distribution by the two-dimensional finite element methods, a model of lower 1st molar according to the porcelain fused metal crown an the porcelain fused glass ceramic core crown and the all glass ceramic crown. 1. The pattern of stress distribution showed no apparent differences. 2. The greatest von Mises values were concentrated around the central fossa of all esthetic crowns. The greatest Maximum principle value were concentrated around the interface between the base of esthetic crown and the abutment tooth. It was found that the apatite glass ceramic could be applicable for use in dental crown prosthesis.

  • PDF

지르코니아 코어 두께에 따른 전부도재관의 상부도재 축성방법이 보철물 색조에 미치는 영향 (The Effect of Veneering Techniques on the Color Parameters of Y-TZP Based All Ceramic Restoration of Varying Ceramic Core Thickness)

  • 허성윤;손호정;김혜영;김재홍
    • 치위생과학회지
    • /
    • 제12권2호
    • /
    • pp.123-129
    • /
    • 2012
  • 이 연구에서는 지르코니아 코어의 두께를 달리 제작하여 동일한 색조의 상부도재를 축성함에 있어 제작방법을 다르게 하여 두 상반된 시편을 각각 분광측색장치를 이용하여 CIE $L^*,a^*,b^*$ 색체계로 산출하여 객관적으로 색차를 비교, 분석하여 다음과 같은 결론을 얻었다. 1. 지르코니아 코어의 두께가 두꺼워 지고 상부도재의 두께가 얇아지면서 $L^*$ 값의 수치는 높아지며 $a^*,b^*$ 값은 낮아지는 경향을 띠었다. 상부도재 축성방법을 다르게 제작한 시편에서도 같은 결과를 보였다. 동일한 색조 시편에서 HP군은 PST군에 비해 $L^*$ 값의 수치는 낮게 측색되어 어두운 경향을 보였으며 $a^*,b^*$ 값도 낮은 수치를 보여 황색의 경향을 띠었다. 2. HP군, PST군 모두 동일한 색조에서 지르코니아 코어 두께와 상부도재 제작방법 간에 교호작용은 없었다(P=.083). 지르코니아 코어의 두께에 따라서는 통계적으로 유의한 차이는 존재하였으며(P=.001), 두께가 0.3 mm의 시편 A1, A2 색조에서 색차 값($E^*$)은 3.7 이상으로 나타났고, 그 이외 시편에서는 3.7 이하로 분석되어 임상가능 허용치로 나타났다. 이상의 결과로 볼 때 지르코니아를 이용한 전부 도재관 제작 시 같은 색조의 재료 일지라도 제작방식과 상부도재의 재료에 따라 색차 값이 존재하므로 이를 감안하여 보철물 제작에 사용해야 할 것으로 사료되며, 특히 코어의 두께가 얇은 보철물에서는 임상 허용치 이상의 색차 값을 보이므로 코어의 두께를 좀 더 추가하여 설계한 보철물이 바람직하다고 생각된다.