• Title/Summary/Keyword: DC potential difference method

Search Result 11, Processing Time 0.025 seconds

A Study on Detecting Flaws Using DC Potential Drop Method (직류전위차법을 이용한 결함검출에 관한 연구)

  • Bae, Bong-Guk;Seok, Chang-Seong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.4 s.175
    • /
    • pp.874-880
    • /
    • 2000
  • In this paper, a DC potential drop measurement system was used to find the position of the flaw on a simple thin plate. Four-point probe test was evaluated and used for this study. In the four-point probe test, the more distance between current pins provides the more measurable scope, the less voltage difference, and the more voltage difference rate. In the other hand, the more distance between voltage pins provides the less voltage difference and the less voltage difference rate. An optimized four-point probe was applied to measure the relation between voltage and the relative position of flaw to the probe. The Maxwell 21) simulator was used to analyze the electromagnetic field, and it showed that the analytical result was similar to the experimental result within 11.4% maximum error.

Corrosion Fatigue Characteristics of A106-GrB Steel Weldments in NaC1 solution (A106 GrB강 용접부의 염수중 부식피로특성)

  • 김철한
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.6 no.3
    • /
    • pp.65-72
    • /
    • 1997
  • The horizontal corrosion fatigue tester has been developed for investigating environmental strength. Using this tester, we investigated about corrosion fatigue caracteristics for A106-Gr B steel weldments in 3.5% synthetic seawater and room temperature. Considered parameter is only frequency of 1, 3 and 5Hz.. and Corrosion fatigue crack length was measured by DC potential difference method. From the results, we could find that the horizontal corrosion fatigue tester could be well applied to estimation of fatigue strength. and, In case of 5Hz., corrosion fatigue crack growth pate of A106-Gr B steel weldment was transgranular, and of 1 and 3Hz. showed that transgranular and interfranular was mixed. Also, Material constants of corrosion fatigue crack growth estimated in each frequency were C=9.33$\times$$10^{-9}$ and m=2.93 in 1Hz., C=9.77$\times$$10^{-10}$ and m=3.47 in 3Hz., C=1.02$\times$$10^{-10}$ and m=4.05 in 5Hz

  • PDF

Development of A Floating Solar Thermoelectric Generator Using A Dome Shaped Fresnel Lens for Ocean Application

  • Seong-Hoon Kim;Jeung-Sang Go
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.26 no.6_1
    • /
    • pp.1001-1010
    • /
    • 2023
  • To solve the problem that photovoltaic panels can not harvest electrical energy at a cloudy day and night, a floating solar thermoelectric generator (FSTEG, hereafter) is studied. The FSTEG is consisted of a dome shaped Fresnel lens to condense solar energy, a thermoelectric module connected with a heat sink to keep temperature difference, a floating system simulating a wavy ocean and an electrical circuit for energy storage. The dome shaped Fresnel lens was designed to have 29 prisms and its optical performance was evaluated outdoors under natural sunlight. Four thermoelectric modules were electrically connected and its performance was evaluated. The generated energy w as stored in a Li-ion battery by using a DC-DC step-up converter. For the application of ocean environment, the FSTEG was covered by the dome shaped Fresnel lens and sealed to float in a water-filled reservoir. The harvested energy shows a potential and a method that the FSTEG is suitable for the energy generation in the ocean environment.

Fatigue Life Evaluation of Spot Weldment Using DCPDM (직류전위차법을 이용한 점용접부의 피로수명 평가)

  • 유효선;이송인;권일현;안병국
    • Journal of Welding and Joining
    • /
    • v.19 no.1
    • /
    • pp.58-64
    • /
    • 2001
  • The initiation and propagation lives of fatigue crack were studied for spot weldments composed of cold rolled steel plates(SPC$\times$SPC) and galvanized steel plates(GA$\times$GA) using DC potential drop method(DCPDM). Through the various test results, it was known that the fatigue crack initiation and propagation behaviors in all specimens could be definitely detected by DCPDM. The fatigue crack initiation life( $N_{i}$) detected by DCPDM in SPC$\times$SPC and GA$\times$GA spot weldments increased as the welding current and the nugget diameter( $N_{d}$) increased. The fatigue crack propagation life($\Delta$ $N_{f-i}$) declined as the difference of $N_{i}$ and the fatigue fracture life( $N_{f}$) also increased according to the decrease of fatigue load, $\Delta$P and the increase of nugget diameter. In the same spot weldments, the increase of nugget diameter came to increase fatigue crack propagation life owing to a decrease of stress concentration in front of nugget, especially the increasing extent for GA$\times$GA spot weldment was very high. In the welding current 6kA, $N_{f}$ for GA$\times$GA spot weldment decreased more than that of SPC$\times$SPC specimen due to zinc layer coated in steel plate and undersized nugget diameter. On the other hand, in 8kA and 10kA, the GA$\times$GA spot weldment showed higher $N_{f}$ in spite of lower $N_{i}$, than that of SPC$\times$SPC specimen except 3,000N fatigue load.ue load. load.d.

  • PDF

Corrosion Fatigue Characteristics of A106-GrB Steel Weldments in NaCl solution (A106 GrB강 용접부의 염수중 부식피로 특성)

  • 김철환
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 1997.04a
    • /
    • pp.143-149
    • /
    • 1997
  • the horizontal corrosion fatigue tester has been developed for investigating environmental strength. Using this tester, we investigated about corrosion fatigue caracteristic for A106 GrB steel weldments in 3.5% synthetic seawater and room temperature. Considered parameter is only frequency of 1,3 and 5Hz. and Corrosion fatigue crack length was measured by DC potential difference method. From the results, we could find that the horizontal corrosion fatiued tester could be well applied to estimation of fatigue strength. and In case of 5Hz, corrosion fatigue crack growth path of A106 GrB steel weldment was transgranular, and of 1 and 3Hz showed that transgranular and intergranular was mixed. Also, Corrosion fatigue crack growth caracteristic values estimated in each frequency were C=9.33 x 10-9 and m=2.93 in 1Hz, C=9.77x10-10 and m=3.47 in 3Hz, C=1.02x10-10 and m=4.05 in 1Hz

  • PDF

Improvement of the performance of EOC Amp in AOC method using microprocessor (마이크로프로세서를 이용한 AOC 방식에서 EOG 앰프 성능 개선)

  • 고석남;이상세;정호춘;임승관;이영석;진달복;박병림
    • Proceedings of the IEEK Conference
    • /
    • 2000.06e
    • /
    • pp.218-221
    • /
    • 2000
  • The electronystagmography(ENG) means to measure and record CRP(Corneal-Retinal Potential) whenever the eyeball is moved by using a skin electrode stuck to the hi-temporal and the difference of CRP. Both the horizontal and vertical movement are known according to the position of the stuck skin electrode. In this paper, the variable time-constances to record the eyeball signal of the conventional EOG(Electro-Oculograph) Amplifier is chosen. The shorter the time-constance is, the worse the distortion of a signal is. But the unbalanced impedance of the electrode stuck on the hi-temporal is reduced. Also, the longer the time-constance is, the less the distortion of it signal is. But it is sensitive to the change of base line according to the unbalanced impedance. In order to solve these problems, an DC-Amplifier, the distortion of the eyeball signal is globally used. By solving unbalanced impedance problem of EOG amplifier, the distortion ratio of EOG amplifier is improved.

  • PDF

A Study on the Corrosion Susceptibility and Corrosion Fatigue Characteristics on the Material of Turbine Blade (Turbine Blade재료의 부식민감성과 부식피로특성에 관한 연구)

  • Jo, Seon-Yeong;Kim, Cheol-Han;Ryu, Seung-U;Kim, Hyo-Jin;Bae, Dong-Ho
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.3 s.174
    • /
    • pp.603-612
    • /
    • 2000
  • Corrosion characteristics on the 12Cr alloy steel of turbine blade was electro-chemically investigated in 3.5wt% NaCI and 12.7wt% Na2S04 solution, respectively. Electro-chemical polarization test, Huey test and Oxalic acid etching test were previously conducted to estimate corrosion susceptibility of the material. And, using the horizontal corrosion fatigue tester, corrosion fatigue characteristics of 12Cr alloy steel in distilled water, 3.5wt% NaCI solution, and 12.7wt%(1M) Na2S04 solution were also fracture-mechanically estimated and compared their results. Parameter considered was room temperature, 60'C and 90'C. Corrosion fatigue crack length was measured by DC potential difference method.Obtained results are as follows,1) 12Cr alloy steel showed high corrosion rate in 3.5wt% NaCI solution and Na2S04 solution at high tempratue.2) Intergranular corrosion sensitivity of 12 Cr alloy was smaller than austenitic stainless steel.3) Corrosion fatigue crack growth rate in 3.5wt% NaCI and 12.7wt%(IM) Na2S04 solution is entirely higher than in the distilled water, and also increased with the temperature increase.

New Strategy for Eliminating Zero-sequence Circulating Current between Parallel Operating Three-level NPC Voltage Source Inverters

  • Li, Kai;Dong, Zhenhua;Wang, Xiaodong;Peng, Chao;Deng, Fujin;Guerrero, Josep;Vasquez, Juan
    • Journal of Power Electronics
    • /
    • v.18 no.1
    • /
    • pp.70-80
    • /
    • 2018
  • A novel strategy based on a zero common mode voltage pulse-width modulation (ZCMV-PWM) technique and zero-sequence circulating current (ZSCC) feedback control is proposed in this study to eliminate ZSCCs between three-level neutral point clamped (NPC) voltage source inverters, with common AC and DC buses, that are operating in parallel. First, an equivalent model of ZSCC in a three-phase three-level NPC inverter paralleled system is developed. Second, on the basis of the analysis of the excitation source of ZSCCs, i.e., the difference in common mode voltages (CMVs) between paralleled inverters, the ZCMV-PWM method is presented to reduce CMVs, and a simple electric circuit is adopted to control ZSCCs and neutral point potential. Finally, simulation and experiment are conducted to illustrate effectiveness of the proposed strategy. Results show that ZSCCs between paralleled inverters can be eliminated effectively under steady and dynamic states. Moreover, the proposed strategy exhibits the advantage of not requiring carrier synchronization. It can be utilized in inverters with different types of filter.

Reverse engineering technique on the evaluation of impression accuracy in angulated implants (경사진 임플란트에서 임플란트 인상의 정확도 평가를 위한 역공학 기법)

  • Jung, Hong-Taek;Lee, Ki-Sun;Song, So-Yeon;Park, Jin-Hong;Lee, Jeong-Yol
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.59 no.3
    • /
    • pp.261-270
    • /
    • 2021
  • Purpose. The aim of this study was (1) to compare the reverse engineering technique with other existing measurement methods and (2) to analyze the effect of implant angulations and impression coping types on implant impression accuracy with reverse engineering technique. Materials and methods. Three different master models were fabricated and the distance between the two implant center points in parallel master model was measured with different three methods; digital caliper measurement (Group DC), optical measuring (Group OM), and reverse engineering technique (Group RE). The 90 experimental models were fabricated with three types of impression copings for the three different implant angulation and the angular and distance error rate were calculated. One-way ANOVA was used for comparison among the evaluation methods (P < .05). The error rates of experimental groups were analyzed by two-way ANOVA (P < .05). Results. While there was significant difference between Group DC and RE (P < .05), Group OM had no significant difference compared with other groups (P > .05). The standard deviations in reverse engineering were much lower than those of digital caliper and optical measurement. Hybrid groups had no significant difference from the pick-up groups in distance error rates (P > .05). Conclusion. The reverse engineering technique demonstrated its potential as an evaluation technique of 3D accuracy of impression techniques.

Electrochemical Evaluation of Corrosion Property of Welded Zone of Seawater Pipe by DC Shielded Metal Arc Welding with Types of Electrodes (선박 해수배관에서 용접봉의 종류에 따라 직류 아크 용접한 용접부위의 부식특성에 관한 전기화학적 평가)

  • Lee, Sung-Yul;Lee, Kyu-Hwan;Won, Chang-Uk;Na, Shane;Yoon, Young-Gon;Lee, Myeong-Hoon;Kim, Yun-Hae;Moon, Kyung-Man;Kim, Jin-Gyeong
    • Journal of Ocean Engineering and Technology
    • /
    • v.27 no.3
    • /
    • pp.79-84
    • /
    • 2013
  • The seawater pipes in the engine rooms of ships are surrounded by severely corrosive environments caused by fast flowing seawater containing chloride ions, high conductivity, etc. Therefore, it has been reported that seawater leakage often occurs at a seawater pipe because of local corrosion. In addition, the leakage area is usually welded using shielded metal arc welding with various electrodes. In this study, when seawater pipes were welded with four types of electrodes(E4311, E4301, E4313, and E4316), the difference between the corrosion resistance values in their welding zones was investigated using an electrochemical method. Although the corrosion potential of a weld metal zone welded with the E4316 electrode showed the lowest value compared to the other electrodes, its corrosion resistance exhibited the best value compared to the other electrodes. In addition, a heat affected zone welded with the E4316 electrode also appeared to have the best corrosion resistance among the electrodes. Furthermore, the corrosion resistance of the weld metal zone and heat affected zone exhibited relatively better properties than that of the base metal zone in all of the cases welded with the four types of electrodes. Furthermore, the hardness values of all the weld metal zones were higher than the base metal zone.