Optical properties of Yb3+ doped Y3Al5O12 single crystals derived by the Czochralski method according to growth atmosphere and doping concentration (Czochralski 법으로 성장된 Yb3+ doped Y3Al5O12 단결정의 성장 분위기 및 도핑 농도에 따른 광학적 특성)

  • Shim, Jang Bo;Lee, Young Jin;Kang, Jin Ki;Lee, Young Kuk
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.25 no.2
    • /
    • pp.68-73
    • /
    • 2015
  • Single crystals of $Yb^{3+}$ doped $Y_3Al_5O_{12}$ up to 25 at.% were grown by the Czochralski method. Using the pulling rate of 0.8 mm/h and the rotation rate of 10 rpm, single crystals with diameters of up to 40 mm and lengths up to 160 mm were obtained. The growth atmosphere was either pure nitrogen or the mixture of nitrogen and oxygen. The crystal was bluish green when using pure nitrogen and the crystal was colorless when using the mixture of 99 % nitrogen and 1 % oxygen. The concentration of $Yb^{3+}$ ions decreased with increasing the length of the crystal and $Yb^{3+}$ concentration of core area was slightly higher than the other areas in the compositional analysis. The fluorescence lifetime decreased with increasing the doping concentration of $Yb^{3+}$ ions.

Crystal Growth and Luminescence Properties of KCl Doped with Eu2+ Ions (KCl:Eu 단결정 성장과 형광특성)

  • Je, Jae-Yong;Jang, Kyoung-Hyuk;Park, Chul-Woo
    • Journal of Sensor Science and Technology
    • /
    • v.20 no.1
    • /
    • pp.30-34
    • /
    • 2011
  • Single crystal of KCl doped with $Eu^{2+}$ ions was grown by the Czochralski method in the high pressure Ar gas(purity 99.999 %) atmosphere with chamber pressure from which the crystal with high quality was obtained. As grown $KCl:Eu^{2+}$ crystal was checked by X-ray diffraction. Luminescence properties of KCl:Eu are investigated by laser-excitation spectroscopy under 355 nm excitation at 14 and 295 K. The broad emission band due to the $Eu^{2+}$ 5d $\rightarrow$ 4f transition is peaked at 417 nm with full width at half maximum of about 20 and 30 nm.

GROWTH AND CHARACTERIZATION OF $La_3Ga_5SiO_{14}$ SINGLE CRYSTALS BY THE FLOATING ZONE METHOD

  • Yoon, Won-Ki;Auh, Keun-Ho
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 1999.06a
    • /
    • pp.253-269
    • /
    • 1999
  • The development of telecommunication and information technology requires to develop new piezoelectric materials with small size, low impedance, wide pass band width and high thermal stability of frequency. Langasite (La3Ga5SiO14) single crystal has been researched substitute of quartz and LiNbO3 for the applications of SAW filter, BAW filter and resonator. Its single crystal growth has been carried out by Czochralski Method. So, in order to get single crystal with higher quality, in this study, lnagasite (La3Ga5SiO14) single crystal was grown by using Floating Zone (FZ) method and characterized. For the growth of langasite single crystals, the langasite powder was synthesized at 135$0^{\circ}C$ for 5hrs and the feed rod was sintered at 135$0^{\circ}C$ for 5hrs. The growing rate was 1.5mm/h and the rotation speed was 15 rpm for an upper rotation and 13 rpm for a lower rotation. In order to prevent the evaporation of gallium oxide, Ar and O2 gas mixture was flowed. The growth direction was analyzed by Laue back-scattered analysis. The composition of grown crystal was analyzed suing XRD and WDS. The electrical properties of grown crystal at various frequencies and temperature were discussed.

  • PDF

LiLa1-xNdx(MoO4)2 Single Crystal Growth by the Czochralski Method (쵸크랄스키법에 의한 LiLa1-xNdx(MoO4)2 단결정 육성 연구)

  • Bae In-Kook;Chae Soo-Chun;Jang Young-Nam;Kim Sang-Bae
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.9
    • /
    • pp.677-683
    • /
    • 2004
  • Nd:LLM (Nd:LiLa(MoO$_4$)$_2$) single crystals for the laser host material were grown by the Czochralski method. The Nd:LLM grown single crystals cracked easily, and the reasons of cracks are generally related with phase transition, incongruent melting, chemical heterogeneity of composition, geometric thermal structures of imbalance and growth direction. We confirmed that phase transition is not observed by TG-DTA thermal analysis, and the XRD analysis revealed congruent melting in our products. It was confirmed that the volatilization of Li$_2$O composition is the important reason of chemical heterogeneity. The geometric thermal profile of the resistance furnace of our own design was controlled with a crucible height. Also, Nd:LLM crystal affected growth direction, and was the best quality in case of (101) growth direction. The distribution and effective distribution coefficient of Nd$^{3+}$ ion were accomplished by PIXE analysis.s.

The crystal growth and ferroelasticity of the crystal $KMgCl_3$ ($KMgCl_3$결정의 육성과 강탄성적 성질에 관한 연구)

  • 조용찬;정희태;박상언;박진습;황윤회;정세영
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.8 no.4
    • /
    • pp.544-549
    • /
    • 1998
  • The single crystal of $KMgCl_3$ was grown in Ar atmosphere by Czochralski method for the first time. For the stoichiometric composition, $K_2MgCl_4$ crystal was obtained, and the nonstoichiometric method was used for the $KMgCl_3$ crystal growth. The phase transition sequences of $KMgCl_3$ were investigated by the DTA, DSC and the ferroelastic properties by using the high temperature polarizing microscope and the thermomechanical system. The temperature dependences of the ferroelastic domains and the spontaneous strain obtained from the stress-strain hysteresis loops were analyzed.

  • PDF

Growth and Properties of Co-doped Ce,Mn:LiTaO3 Single Crystals

  • Gang, Bong-Hoon;Rhee, Bum-Ku;Lim, Ki-Soo;Bae, Sung-Ho;Joo, Gi-Tae
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.8
    • /
    • pp.711-714
    • /
    • 2002
  • The Ce, Mn: $LiTaO_3$ crystals were grown by Czochralski method in congruent ${\varphi}$3" $LiTaO_3$ single crystal growing conditions. Concentrations of Ce and Mn in melt were respectively 0.1 mole%. As-grown crystals were red, transparent and the grown crystals were tested with oxidation/reduction treatment for clor and other properties. Influence of Ce and Mn dopants on $LiTaO_3$ crystal properties was discussed. And the nonlinear optical properties of the Ce, Mn: $LiTaO_3$ crystal are being studied.

Effect of applied magnetic fields on Czochralski single crystal growth (Part II) (Czochralski 단결성 성장특성제어를 위한 자장형태에 관한 연구 (Part 2))

  • Chang Nyung Kim
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.4 no.1
    • /
    • pp.46-56
    • /
    • 1994
  • The characteristics of flows, temperatures, concentrations of the boron are numerically studied when uniform axial magnetic fields are applied in the Czechralski crucible. The to governing factors to the flow regimes are buoyancy, thermocapillarity, centrifugal forces, magnetic forces, diffusion coefficient and segregation coefficient of the boron. Since the concentration of the boron is so low that buoyancy effects are negligible, it cannot affect the flow and temperature fields. From the fact that the flow fields are rotationally symmetric, two velocity components in the meridional plane and the circumferential velocity are calculated together with the temperature in the steady state. Based on the known velocity and temperature distributions the unsteady concentration distributions of the boron are calculated. As the strength of the magnetic is increased, the flow velocities are decreased. Circumferential velocities are large near the crucible side-wall and in the region below the rotating crystal. Steep temperatures gradient near the edge of the rotating crystal causes the Marangoni convection. It has been found out that the convection characteristics affects the unsteady transport phenomena of the boron.

  • PDF

Core region and optical properties of Er3+ doped Y3Al5O12 single crystals (Er3+ doped Y3Al5O12 단결정의 core 영역 및 광학적 특성)

  • Shim, Jang Bo;Lee, Young Jin;Kang, Jin Ki;Lee, Young Kuk
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.25 no.3
    • /
    • pp.111-115
    • /
    • 2015
  • $Er^{3+}$ doped $Y_3Al_5O_{12}$ (Er:YAG) single crystals, in which the concentrations of $Er^{3+}$ ion were 5, 7.3, 8, and 10 at.%, were grown by the Czochralski method under nitrogen atmosphere. The <111> oriented Er:YAG single crystals with diameters of up to 50 mm were grown at a pulling rate of 1.0 mm/h and rotation rate of 10 rpm. The thick part of the core region was generated mainly when there was a diameter change during the crystal growth. The concentrations of $Er^{3+}$ ion in the crystals were the same as it was in the melt. $Er^{3+}$ concentration of core region was slightly higher than the other regions in the compositional analysis. The fluorescence lifetime was saturated according to the increase of $Er^{3+}$ doping concentrations.

Micro-defects in $LiNbO_3$ single crystals with congruent melting composition (조화용융성조성을 가진 $LiNbO_3$ 단결성의 미소결함)

  • 김현기;권달회;이선우;심광보;오근호
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.9 no.3
    • /
    • pp.267-272
    • /
    • 1999
  • Micro-defects in the undoped and MgO-doped $LiNbO_3$ single crystals, which were grown from a congruent melting composition (48.6 mol% $Li_2$O) by the CZ (Czochralski) method, were analyzed using microscopic techniques such as optical microscopy (OM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Effects of the dopant and g value (the fraction solidfied) on the domain structure and micro-defect were investigated to build a corelationship with a growth condition of crystal. It was observed that the micro-defect concentrated near the domain wall is caused by high stress. Especially, the micro-defect was observed to be biased toward a certain side of the domain wall.

  • PDF

Effect of Temperature Gradient on the Defects of Nd;YAG Single Crystal Grown by Czochralski Method (융액인상법에 의한 Nd;YAG 단결정 성장시 온도구배의 변화에 따른 결함거동)

  • 김한태;배소익;이상호;정수진
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.10
    • /
    • pp.1015-1020
    • /
    • 1997
  • In the Nd;YAG crystal growth by Czochralski method, the relationship between the core formation and the solid-liquid interface was observed by controlling the temperature gradient in the furnace. When the crystal was grown along<111> direction, defects and core area were reduced as the temperature gradient increased. The optimum temperature gradient was found to be higher than 4$0^{\circ}C$/cm. The Nd3+ concentration analysis by ICP-Mass showed that the segregation coefficient was about 20% higher in the core region than core-free region, where the segregation coefficients of core region and core-free region were 0.22 and 0.18, respectively.

  • PDF