The acrylic resin was first introduced as denture base materials in 1937 and it is commonly used for denture base fabrication nowadays. Three different curing cycles (Conventional curing cycle, short curing cycle and long curing cycle) and three commercially available heat-activated acrylic resins (Vertex RS, Lucitone 199 and ProBase Hot) were investigated to find the curing cycle and material that showed the minimum shrinkage of the resin during polymerization process. A brass master mold was fabricated and duplicated by additional silicone impression material. Stone molds were made by pouring of type III dental stone (SILKY-ROCK YELLOW, Whip-Mix, Louisville, Kentucky). It was embedded in the flask. Strain gauge and thermocouple were embedded in the specimen. Strain gauge and thermocouple were connected to signal conditioning amplifier and data was recorded by pre-programmed software. The parameters ESmax (Maximum expansion strain), Sb (Strain measured just before deflasking procedure), Sa (Strain measured just after deflasking procedure) and Sf (Strain measured at the end of the experiment) were measured. ${\Delta}$S was calculated from Sb and Sa (${\Delta}$S=Sb-Sa). In the experiment concerned about materials, the parameters 90-ESmax (Maximum expansion strain measured during early 90 minutes of curing procedure), 180-ESmax (Maximum expansion strain measured from 90 minutes to 180 minutes), Sb, Sa, ${\Delta}$S and Sf were measured and the following conclusions were made. 1. The ESmax value of conventional curing cycle showed the largest value and the 180-ESmax value of Lucitone 199 showed the smallest value. 90-ESmax values showed no significant difference (p<0.05). 2. ${\Delta}$S values of conventional curing cycle showed the positive values. ${\Delta}$S values of short curing cycle and long curing cycle showed the negative values. All three materials cured by conventional curing cycle showed the positive values. 3. The Sf values of long curing cycle and ProBase Hot (cured by conventional curing cycle) showed the smallest values.
본 논문은 프리캐스트 콘크리트 구조물의 조기강도를 촉진시키기 위한 양생공법 중에서 증기양생에 대한 연구내용으로서, 콘크리트 원주형 공시체와 목업체의 실험을 통하여 초기재령에서 요구되는 강도가 발현될 수 있는 증기양생주기와 최고온도를 정량화하여 최적 증기양생온도주기를 고찰하였다. 또한 고온의 증기양생으로 인하여 발생된 콘크리트의 높은 온도와 거푸집 제거시에 발생되는 균열의 발생원인과 대책에 대하여 기술하였으며, 궁극적으로는 PC 부재를 생산하는 과정에서의 조기강도발현과 품질확보를 동시에 만족하면서 경제성 있는 제작방법을 제시하였다.
This study was conducted to made a grid alloy (Pb-Ca-Sn-Al) which has a temporary composition ratio in order to improve the efficiency of lead acid batteries. The positive activity material made a 3BS(tri-basic lead sulfate; $3PbO{\cdot}PbSO_4{\cdot}H_2O$) by a low temperature curing and it evaluates the plate efficiency through the life cycle testing. The initial current capacity of low temperature curing plate was excellent but the life cycle was not good (S1). As for the S2 plate, however, the initial current capacity and the life cycle were superior.
Positive plate was composed of lead hydroxide via reaction between lead oxide and $H_2O$ and lead sulfate was formed of the reaction of lead hydroxide with sulfuric acid. And its density is $3.8g/cm^3$, $4.0g/cm^3$, $4.2g/cm^3$ and $4.4g/cm^3$ by controlling volume of refined water. Curing of positive plate is done for low ($45^{\circ}C$, 40hr, over 95% of relative humidity) & high ($80^{\circ}C$, 40hr, over 95% of relative humidity) temperature, which created 3BS & 4BS active materials. Experimental result of DOD with 100% life cycle test shows that it was not related to the density of active materials but to the low & high temperature aging of active materials. The test makes us to understand that the crystallization which is made by curing of active materials is a more of a main factor than density of active materials under the deep cycle using circumstances. The active materials which were from the high temperature curing are better for deep cycle performance.
In this work, the cure cycle of co-cured metal/composite structure was investigated to decrease fabricating thermal residual stresses between the metal and the composite material. DSC (Differential scanning calorimetry) experiment and static lap shear test of co-cured aluminum/composite double lap joint as well as the curvature experiment of co-cured steel/composite strip were performed to investigate the effect of curing cycle on the thermal residual stress of co-cured hybrid structures. From the experiments, it was found that post curing method after abrupt cooling of co-cured aluminum/composite hybrid structure at certain point of degree of cure during curing process could eliminate fabricating the thermal residual stresses.
This study investigates the paste mixing of positive active materials which, affect the life cycle of batteries in Pb-Ca-Sn grids, and generation of 4BS in a curing process and considers the effects of these things on the initial charge characteristics and life cycle. In the results of the experiments applied in this study, it was possible to reduce the curing time in which the fine 4BS was formed by the mixing of the positive active materials of lead acid battery applied at high temperature compared to that of the existing coarse 4BS and that represented some improvements in the life cycle performance.
Soil-cement mixtures involve problems in it's durability in grain size distribution and mineral composition of the used soils as well as in cement content, compaction energy, molding water content, and curing. As an attempt to solve the problems associated with durability of weathered granite soil with cement treated was investigated by conducting tests such as unconfined compression test, it's moisture, immers, wet-dry and freeze-thaw curing, mesurement of loss of weight with wet-dry and freeze-thaw by KS F criteria and CBR test with moisture curing on the five soil samples different in weathering and mineral composition. The experimental results are summarized as follows; The unconfined compressive strength was higher in moisture curing rather than in the immers and wet-dry, while it was lowest in freeze-thaw. Decreasing ratio of unconfined compressive strength in soil-cement mixtures were lowest in optimum moisture content or in the dry side rather than optimum moisture content with freeze-thaw. The highly significant ceofficient was obtained between the cement content and loss of weight with freeze-thaw and wet-dry. It was possible to obtain the durability of soil-cement mixtures, as the materials of base for roads, containing above 4 % of cement content, above 3Okg/cm$_2$ of unconfined compressive trength with seven days moisture curing or 12 cycle of freeze-thaw after it, above 100% of relative unconfined compressive strength, 80% of index of resistance, below 14% of loss of weight with 12 cycle of wet-dry and above 1. 80g/cm$_2$ of dry density.
The strength level for removal of lining concrete in tunnel is increased from 2.94MPa to 4.9MPa in 2004. This result in the increase of concrete curing time, and construction time would be delayed. In this study, in order to improve the efficiency of construction cycle and satisfy the strength criterion, a curing method is adopted, which is considering the hydration heat in the lining concrete member. As a result, it is shown that the concrete curing time for form removal is about 20hrs without the adjustment of concrete mix design. And construction cycle time is not changed compared to that before the change of strength criterion.
The influence of red lead($Pb_3O_4$) to curing and formation reaction properties when it was added in positive material of lead acid battery for vehicle use has been investigated. At the results, it was confirmed that the addition of red lead led 4BS crystal size to be smaller and increased the rates of 4BS formation and Pb consumption. Consequently the curing time was shortened to half compared with that of red lead-free one. In addition to this, the lead acid battery prepared by adding red lead showed 14% higher efficiency at the life cycle test than that without red lead.
The present study performed low-pressure steam curing with mortar specimens in order to examine the temperature profile and strength development of steam curing in high-strength specimens of 100MPa. In addition, as a basic research to utilize PC products, we examined the effects of curing temperature and time in steam curing cycle on strength development resulting from the hydration of cement within the range of high strength by changing four factors affecting the quality of PC displacement time, peak curing temperature, peak temperature duration, and ascending and descending gradient of temperature - in various patterns, and analyzed the optimal strength development characteristic based on the relation between temperature profile and strength development. With regard to the high-temperature curing characteristic of PC, we performed an experiment on the strength characteristic according to the temperature profile of high-strength mortar, and from the results of the experiment according to curing characteristic, displacement time, peak curing temperature, peak temperature duration, and ascending and descending gradient of temperature, we drew conclusions as follows.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.