Mechanical Properties of a Cu55Zr30Ti10Pd5 Bulk Amorphous Alloy (Cu55Zr30Ti10Pd5 비정질 합금의 기계적 거동)

  • Choi Won Wook;Gato H.;Kim Hyoung Seop;Hong Sun Ig;Inoue A.
    • Korean Journal of Materials Research
    • /
    • v.15 no.4
    • /
    • pp.281-284
    • /
    • 2005
  • Room and high temperature deformation behaviors of Cu-Zr-Ti-Pd bulk metallic glasses produced by copper mold casting were investigated. The addition of Pd was shown to enhance the glass forming ability and thermal stability of Cu-Zr-Ti base bulk metallic glass. The compressive strength of $Cu_{55}Zr_{30}Ti_{10}Pd_5$ bulk metallic glass was 2230 MPa with 1.8 plastic strain. The stress overshoot and yield drop phenomenon were observed below $487^{\circ}C$ and a drastic decrease in the flow stress was observed at $487^{\circ}C$. The stress overshoot is thought to be associated with stress-induced structural relaxation.

Cu-based Bulk Amorphous Alloys in the Cu-Zr-Ti-Ni-Pd System (Cu-Zr-Ti-Ni-Pd계 비정질 벌크합금의 형성과 성질)

  • Kim, Sung-Gyoo;Bae, Cha-Hurn
    • Journal of Korea Foundry Society
    • /
    • v.22 no.6
    • /
    • pp.304-308
    • /
    • 2002
  • The new Cu-Zr-Ti-Ni-Pd amorphous alloy system has been introduced and manufactured using melt-spinning and Cu-mold die casting methods. Amorphous formability, the supercooled liquid region before crystallization and mechanical properties of the alloys were examined. The reduced glass transition temperature(Trg = Tg/Tm) and the supercooled liquid region(${\Delta}$Tx = Tx-Tg) of $Cu_{49}Zr_{30}Ti_{10}Ni_5Pb_6$ alloy were 0.620 and 57 K respectively. $Cu_{49}Zr_{30}Ti_{10}Ni_5Pb_6$ amorphous alloy was produced in the rod shape with 2mm diameter using the Cu-mold die casting. The hardness value of the amorphous bulk alloy was 432 DPN.

Fabrication of Bulk Metallic Glass Alloys by Warm Processing of Amorphous Powders (비정질 분말의 열간 성형법에 의한 벌크 비정질합금의 제조)

  • 이민하;김도향
    • Journal of Powder Materials
    • /
    • v.11 no.3
    • /
    • pp.193-201
    • /
    • 2004
  • 1960년 Au-Si계 합금에서 처음으로 비정질상이 급속 응고법에 의해 보고된 이래/sup 1)/ 지난 40년 간 많은 합금계에서 비정질상이 보고되어졌다. 대표적으로 Fe-, Ni-, Co기 합금 등 많은 합금계에서 비정질상이 보고되었으나, 비정질상의 형성을 위해서는 약 105 K/s이상의 높은 냉각속도를 필요로 하였다. 1980년대 수백 K/s의 낮은 냉각속도 하에서도 비정질상이 형성될 수 있는 다원계 합금(multi-component alloy)이 Mg-Ln-(Ni, Cu, Zn), Ln-Al-TM 합금에서 보고되어 졌으나 많은 관심을 받지 못하다가 1993년 Zr-Ti-Ni-Cu-Be 합금에서 수 ㎝ 크기의 비정질합금 제조가 보고되면서 전 세계적으로 많은 관심을 받게 되었다. Zr-Ti-Ni-Cu-Be계 벌크 비정질 합금이 보고된 후 Zr-(Nb,Pd)-Al-TM, Pd-Cu-Ni-P, Fe-Co-Zr-Mo-W-B, Ti-Zr-Ni-Cu-Sn등 여러 합금계에서 벌크 비정질 합금이 보고되었다. (중략)

UHV Materials (초고진공계재료)

  • 박동수
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 1998.02a
    • /
    • pp.24-24
    • /
    • 1998
  • 반도체장비를 포함하는 초고진공장비의 園훌化가 급속히 그리고 절실히 요구되고 있는 것이 현실정이다. 當面해서 실현할 국산진공장비의 대상은 廣範圍하다. 즉, 각종 진공 pump ( (rotary, dry, diffusion, cryo, ion, turbo melecular pump), 진공 chamber, 진공 line, gate valve 를 위 시 한 진공 V머ve, flange, gasket, fl않d야lU, mainpulater 퉁 진공 部品이 다. 진공계 의 핵심 은 適切하고 優良한 진공재료의 선태파 사용이다. 진공장비는 사용자가 원하는 진공도를 원하 는 시간 동안 륨空度를 유지해 주어야 한다. 진공재료 선태의 기준사항은:(1) 기체의 透過성 (2) 薰했훌 (3) 혔體放出특성 - -outgassing과 degassing- (4) 機械的 량훌度 (5) 온도 의존성 (6) 化學톡성 (7) 加I성 및 鎔接 성 (8) 課電특성 (9) 磁氣특성 (10) 高速함子 및 放射線 특성 (11) 經濟성 및 調達생 둥이 다. 우량한 초고진공계재료는 풍부하게 개발되어 왔고, 또 新材料들이 개발되고 있다. 여기에서는 주로 초고진공 내지는 극고진공계의 構造材料, 機能材料, 部品材料 일반파 몇가지 신재료의 특 성에 관해서 記述한다. M Mild SteeHSAE, 1112, 1010, 1020, 1022, etc)., S Stainless SteeHAlSI, 304, 304L, 310, 316, 321, 347): 구조재료, chamber, fl하1ges A Aluminum과 Alloys (1060, 1100, 2014, 4032, 6(뻐1): 구조재료, chamber, flanges, gaskets A AI, Al 떠loy는 SS에 代替하는 역 할올 시 작하고 있다. C Copper, Copper Alloys(C11$\alpha$)0, C26800, C61400, Cl7200): 내장인자, gasket, cryopanel, tubing T Titanium, Ziriconium, Haf띠um 및 Alloys: 특히 Ti은 10n pump 용 getter material 이 외 에 U UHV,XHV용 chamber계로서 관심올 끌고 있다. N Nickel, Nickel Alloys (200, 204, 211, monel, nichrome): 부식 방지 , 전자장치 , 자기 장치 귀 금속(Ag, Au, Pt, Pd, Rh, Ir, Os, Ru): 보조부품, gasket, filament, coating, thermocouple, 접 합부위 T TiC, SiC, zrC, HfC, TaC 둥의 탄화물과, BN, TiN, AlN 동의 질화물, 붕화물이 둥장하고 었 다. 유리: Soda Lime, Borosilicate, Potash Soda Lead: View Port, Chamber envelope C Ceramics: AlZ03, BeO, MgO, zrOz, SiOz, MgOzSiOz, 3Alz032SiOz, Z$textsc{k}$hSiOz S상N4: e electrical, thermal insulators, crucibles, boats, single crystals, sepctr려 windows 저자는 최근 저자들이 발견한 Zr-Ti-Cu-Ni-Be amorphous alloys coated cham뾰r가 radiation p proof로 이용될 수 있는 사실을 점검하고 었다 .. Z.Y. Hua 들은 Cs3Sb를 새로운 photocathode 재료로 보고하고 있다.

  • PDF

Small-Scale Wind Energy Harvester Using PZT Based Piezoelectric Ceramic Fiber Composite Array (PZT계 압전 세라믹 파이버 어레이 복합체를 이용한 미소 풍력 에너지 하베스터)

  • Lee, Min-Seon;Na, Yong-Hyeon;Park, Jin-Woo;Jeong, Young-Hun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.32 no.5
    • /
    • pp.418-425
    • /
    • 2019
  • A piezoelectric ceramic fiber composite (PCFC) was successfully fabricated using $0.69Pb(Zr_{0.47}Ti_{0.53})O_3-0.31[Pb(Zn_{0.4}Ni_{0.6})_{1/3}Nb_{2/3}]O_3$ (PZT-PZNN) for use in small-scale wind energy harvesters. The PCFC was formed using an epoxy matrix material and an array of Ag/Pd-coated PZT-PZNN piezo-ceramic fibers sandwiched by Cu interdigitated electrode patterned polyethylene terephthalate film. The energy harvesting performance was evaluated in a custom-made wind tunnel while varying the wind speed and resistive load with two types of flutter wind energy harvesters. One had a five-PCFC array vertically clamped with a supporting acrylic rod while the other used the same structure but with a five-PCFC cantilever array. Stainless steel (thickness: $50{\mu}m$) was attached onto one side of the PCFC to form the PZT-PZNN cantilever. The output power, in general, increased with an increase in the wind speed from 2 m/s to 10 m/s for both energy harvesters. The highest output power of $15.1{\mu}W$ at $14k{\Omega}$ was obtained at a wind speed of 10 m/s for the flutter wind energy harvester with the PZT-PZNN cantilever array. The results presented here reveal the strong potential for wind energy harvester applications to supply sustainable power to various IoT micro-devices.

Thermal Stability of $\textrm{Fe}_{80-x}\textrm{P}_{10}\textrm{C}_{6}\textrm{B}_{4}\textrm{M}_{x}$(M=Transition Metal) Amorphous Alloys ($\textrm{Fe}_{80-x}\textrm{P}_{10}\textrm{C}_{6}\textrm{B}_{4}\textrm{M}_{x}$(M=Transition Metal) 비정질합금의 열적안정성)

  • Guk, Jin-Seon;Jeon, U-Yong;Jin, Yeong-Cheol;Kim, Sang-Hyeop
    • Korean Journal of Materials Research
    • /
    • v.7 no.3
    • /
    • pp.218-223
    • /
    • 1997
  • At the aim of finding a Fehased amorphous alloy with a wide supercooled liquid region (${\Delta}T_{x}=T_{x}-T_{g}$) before crystallization, the changes in glass transition temperatudfI$T_{g}$ and crystallization temperature ($T_{x}$) by the dissolution of additional M elements were examined for the $Fe_{80}P_{10}C_{6}B_{4}$(x~6at%. M= transition metals) amorphous alloys. The ${\Delta}T_{x}$ value is 27K for the Fe,,,P,,,C,,R, alloy and increases to 40K for the addition of M=4at%Hf, 4at%Ta or 4at%Mo. The increase in ${\Delta}T_{x}$ is due to the increase of $T_{x}$ exceeding the degree in the increase in $T_{g}$. The $T_{g}$ and $T_{x}$ increase with decreasing electron concentration (e/a) from about 7 38 to 7.05. The decrease of e/a also implies the increase in the attractive bonding state between the M elements and other constitutent elements. It is therefore said that $T_{g}$ and $T_{x}$ increase kith increasing attractive bonding force.

  • PDF