Kim, Sug-Won;Lee, Ui-Jong;Woo, Kee-Do;Kim, Dong-Keun
Journal of Korea Foundry Society
/
v.21
no.1
/
pp.7-14
/
2001
The research on new DRA(discontinuous reinforced alloy) and CRA(continous reinforced alloy) composites has been carried out to improve the properties of ceramic fiber and particle reinforced metal matrix composites(MMCs). Effects of alloying elements and aging conditions on the microstructures and aging behavior of Al-Si-Cu-Mg-(Ni)-SiCp composite have been examined. The specimens used in this study were manufactured by duplex process. The first squeeze casting is the process to make precomposite and the second squeeze casting is the process to make final composite. The hardening behavior was accelerated with decreasing the size of SiCp particle in the composites. It is considered that the dislocation density increased with increasing SiCp size, due to the different thermal deformation between Al matrix and SiCp during quenching after the solution treatment. Peak aging time to obtain the maximum hardness in 3 ${\mu}m$ SiCp reinforced Al composite was reduced than that in large size(5, 10 ${\mu}m$) of SiCp because of difference in dislocation density. Aging hardening responce(${\Delta}H$ = $H_{Max}.-H_{S.T}$) of composites was greater than that of unreinforced Al alloy because of higher density of second phases in matrix.
The fabrication of Fe alloy-40 wt.%TiC composite materials using spark plasma sintering process after ball-milling was studied. Raw powders to fabricate Fe alloy-TiC composite were Fe alloy, $TiH_{2}$ and activated carbon. Fe alloy powder was Distaloy AE (4%Ni-1%Cu-0.5%Mo-0.01%C-bal.%Fe) made by Hoeganes company with better toughness and lower melting point. These powders were ball-milled in horizontal attrition ball mill at a ball-to-powder weight ratio of 30 : 1. After that, these mixture powders were sintered by using spark plasma sintering apparatus for 5 min at $1200-1275^{\circ}C$ in vacuum atmosphere under $10^{-3}$ torr. DistaloyAE-40 wt.%TiC composite was directly synthesized by dehydrogenation and carburization reaction during sintering process. The phase transformation of as-milled powders and sintered materials was confirmed using X-ray diffraction (XRD) and transmission electron microscope (TEM). The density and harness materials was measured in order to confirm the densification behavior. In case of DistaloyAE-40 wt.%TiC composite retained for 5 min at $1275^{\circ}C$, it has the relative density of about 96% through the influence of rapid densification and fine TiC particle reinforced Fe-based composites materials.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2007.06a
/
pp.18-18
/
2007
지난 수년 동안 Sn-3.0Ag-0.5Cu 합금은 전자산업의 표준 무연솔더 조성으로 전자제품의 제작에 사용되어져 왔으며, 그 신뢰성도 충분히 검증되어 대표적인 무연 솔더 조성으로의 입지를 굳혀왔다. 그러나 전자제품의 mobile화에 따른 내충격 신뢰성에 대한 요구와 최근의 급격한 Ag 가격의 상승은 Ag 함량의 축소에 의한 원가절감을 요청하게 되었으며, 이에 따라 소량의 Ag를 함유하는 솔더 조성 개발에 대한 연구가 산업 현장을 중심으로 절실히 요청되고 있다. Sn-Ag-Cu의 3원계 함긍에서 Ag는 합금의 융점을 낮추고, 강도와 같은 합금의 기계적 특성을 증가시키는 한편, 모재에 대한 합금의 젖음성을 향상시키는데 필수적인 원소로 인식되고 있다. 따라서 Sn-Ag-Cu의 3원계 함금에서 Ag의 함량을 감소시키게 되면, 합금액 액상선 온도와 고상선 온도가 벌어져 pasty range(또는 mush zone)가 증가하게 되고, wettability도 감소하게 되어 솔더 합금으로서의 요구 특성을 많이 상실하게 된다. 또한 Ag 함량을 감소시키게 되면 합금의 elongation이 향상되면서 내 impact 수명이 향상되는 효과를 볼 수 있으나, 합금의 creep 특성 및 기계적인 강도는 감소하면서 열싸이클링 수명은 감소하는 경향을 나타내게 된다. 따라서 솔더 합금의 내 impact 수명과 열싸이클링 수명을 동시에 만족시키지 위해서는 Ag 함량을 최적화하기 위한 고려가 필요하며, 합금원소에 대한 연구가 요청된다고 하겠다. 한편 Ag의 함량을 3wt.% 이상으로 첨가할 경우에도 비교적 느린 응고 속도에서는 조대한 판상의 $Ag_3Sn$ 상을 형성하는 경향이 있어 외관 물량을 야기 시킬 가능성이 매우 커지는 현상도 보고되고 있다. 따라서 Ag의 첨가량을 최적화 하면서 솔더 재료로서의 특성을 계속적으로 유지하기 위해서는 제 4 원소의 함유가 필수적이라고 할 수 있다. 본 연구에서는 Sn-Ag-Cu계에 첨부하는 제 4원소로서 In을 선택하였다. 비록 In은 Ag보다 고가이기 때문에 산업적인 적용을 위한 솔더 합금 원소로는 거의 각광받지 못했으나, 본 연구의 결과로는 In은 매우 소량 첨가할 경우에도 Sn-Ag-Cu계 합금, 특히 소량의 Ag를 함유하는 Sn-Ag-Cu계 합금의 wettabilty와 기계적 특성 향상에 매우 효과적임을 알 수 있었다. 결론적으로 본 연구를 통해 구현된 Sn-Ag-Cu-In계 최적 솔더 조성의 경우 Sn-3.0Ag-0.5Cu의 표준 조성에 비하여 약 18%의 원자재 가격 절감을 도모할 수 있을 것으로 예상되는 한편. Sn-3.0Ag-0.5Cu에 유사하거나 우수한 wettability 특성을 나타내었고. Sn-1.0Ag-0.5Cu 또는 Sn-l.2Ag-0.5Cu-0.05Ni 조성보다는 월등히 우수한 wettability 특성을 나타내었다. 더구나 Sn-Ag-Cu-In계 최적 솔더 조성은 합금의 강도 저하는 최소화 시키면서 합금의 elongation은 극적으로 향상시켜 합금의 toughness 값이 매우 우수한 특성을 가짐을 알 수 있었다. 이렇게 우수한 toughness 값은 솔더 조인트의 대표적 신뢰성 요구 특성인 열싸이클링 수명과 내 impact 수명을 동시에 향상시킬 수 있을 것으로 예상된다. 요컨대 본 연구를 통해 구현된 Sn-Ag-Cu-In계 솔더 조성은 최적 솔더 조성에서 요구되는 4가지 인자, 즉, 저렴한 원재료 가격, 우수한 wettability 특성, 합금 자체의 높은 toughness, 안정하고 낮은 성장 속도의 계면 반응층 생성을 모두 만족시키는 특징을 가짐으로서 기존 무연솔더 조성의 새로운 대안으로 자리 잡을 것으로 기대된다.
Proceedings of the Korean Magnestics Society Conference
/
1991.05a
/
pp.73-74
/
1991
The films with ferromagnetic fine particles dispersed in nonmagnetic matrix, such as $Fe-Al_2O_3$ and Fe-Cu have been studied for use of magnetic recording medium, optically device and sensor. Their magnetic properties depend strongly on structural parameter such as size and volume fraction of ferromagnetic particles. Fe-Cr-Ni alloy sputtered films also have microstructure with ferromagnetic -- b.c.c phase and nonmagnetic f.c.c phase grains. Magnetic properties of these films depend strongly on such a unique structure. These are depend on the ratio in volume of ferromagnetic particles to nonmagnetic ones $V_F/V_N$, the saturation magnetization Ms increased with increase of $V_F/V_N$. The coercivity Hc of the as-deposited films took maximum value of about 200 Oe at adequate $V_F/V_N$ and then Ms and Squareness S were 500 emu/cc and 0.5, respectively.(omitted)
본 실험은 고출력 반도체 레이저의 p-side-down 마운팅용 솔더로서 AuSn 합금 솔더(80wt%:20wt%)의 적합성에 대해 연구하였다. $1{\mu}m$이하의 균일도로 폴리싱 된 Cu heat sink의 표면에 두께 $1{\mu}m$의 Ni로 코팅을 한다음, AuSn 다층박막은 e-beam 증착기로 AuSn 합금 솔더는 열증착기로 각각 증착하였다. 열처리는 산화 방지를 위해 $N_2$ 분위기에서 행하였으며, 동일한 압력으로 마운팅을 하였다. 표면의 거칠기와 형상은 AFM(Atomic Force Microscope)과 SEM(Scanning Electron Microscopy)으로 그리고 Au와 Sn의 성분비는 AES(Auger Electron Spectroscopy) 로 비교하였다. 또한 CW(연속발진)을 통한 L-I(Light-Current)측정을 통해 본딩상태를 비교하였다.
Proceedings of the Korean Society for Technology of Plasticity Conference
/
2004.05a
/
pp.265-268
/
2004
In this present study, mechanical properties of the Zr-Ti-Cu-Ni-Be bulk metallic glass are characterized by compression test over a wide range of temperatures and strain rates. Three different types of deformation behavior have been identified as a result, viz., Newtonian viscous flow, non-Newtonian flow and brittle fracture without plastic deformation. A transition state theory is applicable fur the flow stress - strain rate curve that contains the transition from Newtonian to non-Newtonian flow. Based on the relationship between viscosity and strain rate within undercooled liquid state, we can easily obtain the experimental deformation map and suggest the boundaries among different deformation behavior of this alloy.
Proceedings of the Korean Society for Technology of Plasticity Conference
/
2004.10a
/
pp.199-202
/
2004
In this present study, an attempt was made to determine the deformation mode of the Zr-Ti-Cu-Ni-Be bulk metallic glass by compression test over a wide range of temperatures and strain rates. From the results, empirical deformation map could be constructed including the boundaries of different deformation modes. Considering power dissipation map and instability map developed on the basis of the Dynamic Materials Model (DMM), the processing map for extrusion could also be constructed. In addition, the macroscopic formability of this BMG alloy has also been examined through the extrusion in laboratory scale within undercooled liquid state. From the results of macroscopic extrusion formability, both deformation map and processing map present good criteria to determine optimal forming conditions.
Bocchini, G. F.;Ienco, M. G.;Pinasco, M. R.;Stagno, E.;Baggioli, A.;Gerosa, R.;Rivolta, B.
Proceedings of the Korean Powder Metallurgy Institute Conference
/
2006.09a
/
pp.405-406
/
2006
Raw materials from different sources, produced by a given process and having equal chemical composition, are supposed to be equivalent. The differences in sintering behavior have been investigated on P/M steels obtained from four diffusion-bonded powders (Fe + Ni + Cu + Mo) on atomized iron base, at the same alloy contents. Two levels of carbon and two sintering conditions have been investigated. Dimensional changes, C content, hardness, microhardness pattern, universal hardness, fractal analysis, pore features, microstructure features, and rupture strength have been compared to characterize different raw materials. The results show that the claimed equivalence is not confirmed by experimental data.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2005.07a
/
pp.274-275
/
2005
The tensile strain dependency of critical current in YBCO coated conductors was examined at 77K and in the self magnetic field. A commercially available YBCO sample with Cu stabilizer layer was supplied. There existed a peak in the relation between the Ie and tensile strain, and the reversible variation of $I_c$ with applied tensile strain was found. In the neutral axis Ni alloy RABiTS-$Y_2O_3$/YSZ/$CeO_2$ buffered YBCO tape, the $I_c$ recovered reversibly until the applied strain reached to about 0.5%, representing that a significant residual compressive strain induced during cooling to 77 K influenced the axial strain tolerance of YBCO conductors. To investigate the strain and stress influence on the $I_c$, the stress-strain characteristics of YBCO conductors measured at 77 K were discussed.
Eckert, Jurgen;Bartusch, Birgit;Schurack, Frank;He, Guo;Schultz, Ludwig
Journal of Powder Materials
/
v.9
no.6
/
pp.394-408
/
2002
Nanostructured high strength metastable Al-, Mg- and Ti-based alloys containing different amorphous, quasicrystalline and nanocrystalline phases are synthesized by non-equilibrium processing techniques. Such alloys can be prepared by quenching from the melt or by powder metallurgy techniques. This paper focuses on one hand on mechanically alloyed and ball milled powders containing different volume fractions of amorphous or nano-(quasi)crystalline phases, consolidated bulk specimens and, on the other hand. on cast specimens containing different constituent phases with different length-scale. As one example. $Mg_{55}Y_{15}Cu_{30}$- based metallic glass matrix composites are produced by mechanical alloying of elemental powder mixtures containing up to 30 vol.% $Y_2O_3$ particles. The comparison with the particle-free metallic glass reveals that the nanosized second phase oxide particles do not significantly affect the glass-forming ability upon mechanical alloying despite some limited particle dissolution. A supercooled liquid region with an extension of about 50 K can be maintained in the presence of the oxides. The distinct viscosity decrease in the supercooled liquid regime allows to consolidate the powders into bulk samples by uniaxial hot pressing. The $Y_2O_3$ additions increase the mechanical strength of the composites compared to the $Mg_{55}Y_{15}Cu_{30}$ metallic glass. The second example deals with Al-Mn-Ce and Al-Cu-Fe composites with quasicrystalline particles as reinforcements, which are prepared by quenching from the melt and by powder metallurgy. $Al_{98-x}Mn_xCe_2$ (x =5,6,7) melt-spun ribbons containing a major quasicrystalline phase coexisting with an Al-matrix on a nanometer scale are pulverized by ball milling. The powders are consolidated by hot extrusion. Grain growth during consolidation causes the formation of a micrometer-scale microstructure. Mechanical alloying of $Al_{63}Cu_{25}Fe_{12}$ leads to single-phase quasicrystalline powders. which are blended with different volume fractions of pure Al-powder and hot extruded forming $Al_{100-x}$$(Al_{0.63}Cu_{0.25}Fe_{0.12})_x$ (x = 40,50,60,80) micrometer-scale composites. Compression test data reveal a high yield strength of ${\sigma}_y{\geq}$700 MPa and a ductility of ${\varepsilon}_{pl}{\geq}$5% for than the Al-Mn-Ce bulk samples. The strength level of the Al-Cu-Fe alloys is ${\sigma}_y{\leq}$550 MPa significantly lower. By the addition of different amounts of aluminum, the mechanical properties can be tuned to a wide range. Finally, a bulk metallic glass-forming Ti-Cu-Ni-Sn alloy with in situ formed composite microstructure prepared by both centrifugal and injection casting presents more than 6% plastic strain under compressive stress at room temperature. The in situ formed composite contains dendritic hcp Ti solid solution precipitates and a few $Ti_3Sn,\;{\beta}$-(Cu, Sn) grains dispersed in a glassy matrix. The composite micro- structure can avoid the development of the highly localized shear bands typical for the room temperature defor-mation of monolithic glasses. Instead, widely developed shear bands with evident protuberance are observed. resulting in significant yielding and homogeneous plastic deformation over the entire sample.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.