Carbon-Nanofiber Reinforced Cu Composites Prepared by Powder Metallurgy

  • Weidmueller, H.;Weissgaerber, T.;Hutsch, T.;Huenert, R.;Schmitt, T.;Mauthner, K.;Schulz-Harder, S.
    • 한국분말재료학회지
    • /
    • 제13권5호
    • /
    • pp.321-326
    • /
    • 2006
  • Electronic packaging involves interconnecting, powering, protecting, and cooling of semiconductor circuits fur the use in a variety of microelectronic applications. For microelectronic circuits, the main type of failure is thermal fatigue, owing to the different thermal expansion coefficients of semiconductor chips and packaging materials. Therefore, the search for matched coefficients of thermal expansion (CTE) of packaging materials in combination with a high thermal conductivity is the main task for developments of heat sink materials electronics, and good mechanical properties are also required. The aim of this work is to develop copper matrix composites reinforced with carbon nanofibers. The advantages of carbon nanofibers, especially the good thermal conductivity, are utlized to obtain a composite material having a thermal conductivity higher than 400 W/mK. The main challenge is to obtain a homogeneous dispersion of carbon nanofibers in copper. In this paper, a technology for obtaining a homogeneous mixture of copper and nanofibers will be presented and the microstructure and properties of consolidated samples will be discussed. In order to improve the bonding strength between copper and nanofibers, different alloying elements were added. The microstructure and the properties will be presented and the influence of interface modification will be discussed.

Nanocomposite Magnetic Materials

  • Ludwig Schultz;Alberto Bollero;Axel Handstein;Dietrich Hinz;Karl-Hartmut Muller;Golden Kumar;Juergen Eckert;Oliver Gutfleisch;Anke Kirehner Aru Yan
    • 한국분말재료학회지
    • /
    • 제9권6호
    • /
    • pp.381-393
    • /
    • 2002
  • Recent developments in nanocrystalline and nanocomposite rare earth-transition metal magnets are reviewed and emphasis is placed on research work at IFW Dresden. Principal synthesis methods include high energy ball milling, melt spinning, mold casting and hydrogen assisted methods such as reactive milling and hydrogenation-disproportionation-desorption-recombination. These techniques are applied to NdFeB-, PrFeB- and SmCo-type systems with the aim to produce high remanence magnets with high coercivity. Concepts of maximizing the energy density in nanostructured magnets by either inducing a texture via anisotropic HDDR or hot deformation or enhancing the remanence via magnetic exchange coupling are evaluated. With respect to high temperature applications melt spun $Sm(Co_{0.74}Fe_{0.1}Cu_{0.12}Zr_{0.04})_{7.5}$ ribbons were prepared, which showed coercivities of up to 0.53 T at 50$0^{\circ}C$. Partially amorphous $Nd_{60}Fe_xCo_{30-x}Al_{10}(0{\leq}x{\leq}30)$ alloys were prepared by copper mold casting. The effect of transition metal content on the glass-forming ability and the magnetic properties was investigated. The $Nd_{60}Co_{30}Al_{10}$ alloy exhibits an amorphous structure shown by the corresponding diffraction pattern. A small substitution of Co by 2.5 at.% Fe results In the formation of Fe-rich crystallites embedded in the Nd-rich amorphous matrix. The Fe-rich crystallites show hard magnetic behaviour at room temperature with a coercivity value of about 0.4 T, relatively low saturation magnetization and a Curie temperature of 500 K.

치과용 합금 주조 시의 소환온도와 주조 후 냉각방법이 미세조직과 부식거동에 미치는 영향 (The Effect of Burn-out Temperature and Cooling Rate on the Microstructure and Corrosion Behavior of Dental Casting Gold Alloy)

  • 이상혁;함덕선;김학관;장주웅;김명호
    • 대한치과기공학회지
    • /
    • 제22권1호
    • /
    • pp.69-78
    • /
    • 2000
  • The microstructure and corrosion behavior of commercially dental casting gold alloys were investigated to clarify the effect of burn-out temperature and cooling rate. In the case of water quenching after casting, only the αphase, which is typical dendritic microstructure of golda alloy, was detected. However, the precipitates along the grain boundary were detected only at the slow cooling rate and they increased inversely proportional to the burn-out temperature. This might be due to the time difference which solute atom could diffuse. EPMA and SEM results also demonstrated that the precipitate should be lamellar structure consisted of Ag rich phase(${\alpha}_1$) and Cu rich phase (${\alpha}_2$). In terms of corrosion, the galvanic coupling was formed due to the difference of composition between precipitates and matrix at the slow cooling rate. In the case of water quenching, the critical current density($i_p$) which indicate the degree of corrosion was lowest at $650^{\circ}C$ and below the burnout temperature, $i_p$ increased with it because of the effect of grain boundary segregation. But above the temperature, $i_p$ increased with it. This may be due to the strain field effect by residual thermal stress.

  • PDF

Source Identification and Quantification of Coarse and Fine Particles by TTFA and PMF

  • Hwang, In-Jo;Bong, Choon-Keun;Lee, Tae-Jung;Kim, Dong-Sool
    • Journal of Korean Society for Atmospheric Environment
    • /
    • 제18권E4호
    • /
    • pp.203-213
    • /
    • 2002
  • Receptor modeling is one of statistical methods to achieve reasonable air pollution strategies. In order to maintain and manage ambient air quality, it is necessary to identify sources and to apportion its sources for ambient particulate matters. The main purpose of the study was to survey seasonal trends of inorganic elements in the coarse and fine particles. Second, this study has attempted emission sources qualitatively by a receptor method, the PMF mo-del. After that. both PMF (positive matrix factorization) model and TTFA (target transformation factor analysis) model were applied to compare and to estimate mass contribution of coarse and fine particle sources at the receptor. A total of 138 sets of samples was collected from 1989 to 1996 by a low volume cascade impactor with 9 size fraction stages at Kyung Hee University in Korea. Sixteen chemical species (Si, Ca, Fe, K, Pb, Na, Zn, Mg, Ba, Ni, V, Mn, Cr, Br, Cu. Co) were characterized by XRF. The study result showed that the weighted arithmetic mean of coarse and fine particles were 51.3 and 54.4 $\mu\textrm{g}$/㎥, respectively. Contribution of both particle fractions were esti-mated using TTFA and PMF models. The number of estimated sources was seven according to TTFA model and 8 according to PMF model. Comparison of TTFA and PMF revealed that both methodologies exhibited similar trends in their contribution pattern. However, large differences between contributions were observed in some sour-ces. The results of this study may help to suggest control strategies in local countries where known source profiles do not exist.

STD 11 강의 오스테나이트화 온도에 따른 제 특성의 정량 분석 (Quantitative Analysis of Metallographic Characteristics with Austenitizing Temperature in STD 11 Steel)

  • 김조은;주용후;장우양
    • 열처리공학회지
    • /
    • 제30권5호
    • /
    • pp.215-221
    • /
    • 2017
  • The effect of austenitizing temperature on the degree of carbides re-solutionizing, mean graine size, hardness and the volume fraction of retaind austenite ($V_{\gamma}$) etc., has been studied by means of metallography, X-ray diffractometry and hardness measurement in STD 11 tool steel. As austenitizing temperature increases, the amount of alloying elements which is re-dissolved into matrix increases, resulting in increase of $V_{\gamma}$, due to the chemical stabilization of austenite. The Vickers hardness value decreases with increasing austenitizing temperature, which is attributed to grain size as well the volume fractions of $V_{\gamma}$ and carbides. Theoretical diffraction intensity of (200) ${\alpha}^{\prime}$, (211) ${\alpha}^{\prime}$ (200) ${\gamma}$ and (220) ${\gamma}$ peaks obtained by $CuK_{\alpha}$ chracteristics X-ray (${\lambda}=0.15429nm$) was calculated, and quantitative analysis of $V_{\gamma}$ could be carried out by X-ray diffraction method. The resultant value is well coincided with the value obtained by image analysis method. When the quenched specimen is tempered above $200{\sim}400^{\circ}C$ for 30 min, the transition carbides i.e., MC and $M_2C$ in the size of about 20 nm begin to precipitate at $300^{\circ}C$.

나노점토가 연질 폴리우레탄/점토 다공성 나노복합체의 기계적 특성에 미치는 영향 (Effect of Nanoclay on Mechanical Properties of Porous Flexible Polyurethane/Clay Nanocomposites)

  • 옥경민;김규헌;김경록;김동현;김춘환;박홍채;윤석영
    • 한국재료학회지
    • /
    • 제23권7호
    • /
    • pp.366-372
    • /
    • 2013
  • Flexible polyurethane/clay porous nanocomposite foams were synthesized using natural and organically modified montmorillonite clays such as bentonite, closite 10A and closite 30B. The content of nanoclays was varied from 1 to 5 wt% of polyol. Dispersion of clay in Polyurethane(PU) matrix was investigated by X-ray diffraction(Cu-$K{\alpha}$ rays of wavelength $1.54{\AA}$) using an X-ray diffractometer. Also, we determined that the thermal resistance of PU foam increased with added clay, compared to that of pure PU foam. The cell size and the fraction of open cells of the precursor foam were controlled by the addition of clay to the polyurethane foam. Modified clays were found to be more efficient cell openers than the unmodified clay. In addition, the tensile strength and elongation of the polyurethane/clay porous nanocomposites were examined. Increasing clay content increased the mechanical properties of the composites, such as tensile strength, and elongation at break. However, increasing the content over 5 wt% deteriorated the properties of the composites. We found that the nanofillers(bentonite, closite 10A and closite 30B) improved the thermal stability of the nanocomposite foam. The nanocomposite foam containing 3 wt% of closite 30B exhibited the best tensile strength and thermal stability.

Use of hybrid materials in the trace determination of As(V) from aqueous solutions: An electrochemical study

  • Tiwari, Diwakar;Jamsheera, A.;Zirlianngura, Zirlianngura;Lee, Seung Mok
    • Environmental Engineering Research
    • /
    • 제22권2호
    • /
    • pp.186-192
    • /
    • 2017
  • The carbon paste electrode (CPE) was modified with the pristine bentonite and hybrid material (HDTMA-modified bentonite). The modified-CPEs are then employed as working electrode in an electrochemical detection of As(V) from aqueous solutions using the cyclic voltammetric measurements. Cyclic voltammograms revealed that As(V) showed reversible behavior onto the working electrode. The hybrid material-modified carbon paste electrode showed significantly enhanced electrochemical signal which was then utilized in the low level detection of As(V). Moreover, the studies were conducted at neutral pH conditions. The electrochemical studies were conducted with scan rates (20 to 200 mV/s) to deduce the mechanism of redox processes involved at the electrode surface. The anodic current was linearly increased, increasing the concentration of As(V) from 5.0 to $35.0{\mu}g/g$ using the hybrid material-modified electrode. This provided fairly a good calibration line for As(V) detection. The presence of varied concentrations of As(III) in the determination of total arsenic was studied. The influence of several cations and anions viz., Cu(II), Mn(II), Zn(II), Pb(II), Cd(II), Fe(III), $Cl^-$, $NO_3{^-}$, $PO_4{^{3-}}$, EDTA and glycine in the detection of As(V) from aqueous solution was also studied. Further, in an attempt to simulate the real matrix analysis, the tap water sample was spiked with As(V) and subjected for As(V) detection using the modified-CPE.

석재가공용 다이아몬드 톱의 제조 및 특성 (The fabrication and characterization of hard rock cutting diamond saw)

  • 이현우;전우용;이오연;설경원
    • 한국분말재료학회지
    • /
    • 제11권5호
    • /
    • pp.412-420
    • /
    • 2004
  • The purpose of the present study is to determine an optimum composition using cheaper powders keeping with high performance of hard rock cutting diamond saw blade. With 50Fe-20(Cu . Sn)-30Co specimen, a part of Co was replaced by Ni(5%, 10%, and 15%, respectively). These specimens were hot pressed and sintered for predetermined time at various temperature. Sintering is performed by two different methods of temperature controlled method and specimen dimension controlled method. In order to determine the property of the sintered diamond saw blade, 3 point bending tester, X-ray diffractometer, and SEM were used. As the Co in the bond alloy was replaced by Ni, the hardness of the specimen increased. Thus the 50Fe-20(CuㆍSn)-15Co-15Ni specimen showed the maximum hardness of 104(HRB). The results of 3 point bending test showed that flexure strength decreased along with increase in Ni content. This is attributed to the formation of intermetallic compound(Ni$_{x}$Sn) determined by X-ray diffraction. The fracture surface after 3 point bending test showed that diamond was fractured in the specimen containing 0%, 5%, and 10%Ni, and the fracture occurred at the interface between diamond and matrix in the specimen containing 15%Ni. The cutting ability test showed that the abrasive property was not changed in the specimen containing 0%, 5%, and 10%Ni. The optimum composition determined in this study is 50Fe-20(CuㆍSn)-20Co-10Ni.

유동상 화힉증착에 의한 리튬이차전지 전극용 탄소재료의 표면개질 (Surface Modification of Synthetic Graphite as an Electrode by Fluidized-bed Chemical Vapor Deposition for Lithium Secondary Batteries)

  • 류덕현;이중기;박달근;윤경석;조병원;설용건
    • 전기화학회지
    • /
    • 제3권3호
    • /
    • pp.173-177
    • /
    • 2000
  • 리튬 이차 전지의 성능은 부극으로 쓰이는 탄소재료의 표면의 미세 구조에 크게 의존한다. 본 연구에서는 이러한 표면 구조의 개질을 위해 유동상 화학증착법을 도입하여 금속 및 금속 산화물을 탄소재료 표면에 코팅하여 그 성능을 전기 화학적으로 평가하였다. 주석산화물을 코팅한 탄소 전극은 원래의 탄소 전극에 비해 용량의 상승을 나타내었으나 사이클이 진행됨에 따라 주석산화물이 코팅된 전지의 용량은 심각한 부피 변화에 의해 저하되어 사이클 수명이 감소되었다. 그러나, 부피 변화를 완화시켜주는 비활성 매트릭스 역할을 하는 구리를 주석 산화물 위에 코팅함으로 인해 부피 변화에 의한 용량 저하를 감소시킬 수 있었다.

On-line monitoring system 개발에 관한 음극 액상 글로우 방전의 기초 연구 (Fundamental study of electrolyte cathode atomic discharge for development of on-line monitoring system)

  • 김경미;우영아;조원보;김효진
    • 분석과학
    • /
    • 제15권6호
    • /
    • pp.496-501
    • /
    • 2002
  • Electrolyte cathode atomic discharge (ELCAD)는 용액 중에 포함된 미량 중금속을 연속 자동적으로 측정하기 위한 새로운 광학 측정기로서 플라스마에 의한 중금속들의 방출 강도를 측정하는 원자방출 분광법의 하나이다. 특히 이 방법은 검액을 전처리하지 않고 직접 분석할 수 있기 때문에 온라인 (on-line) 현장분석이 가능하다. ELCAD에서는 분위기 가스로 공기를 이용하고, 양극부분에 백금 전극을 사용하며, 음극에서는 연속적으로 전해질 시료를 주입하면서 플라스마를 형성하면서 미량의 중금속을 분석할 수 있다. 액상 글로우 방전의 기초 특성 연구로는 철의 원자 방출선 세기를 구한 다음 Einstein-Boltzmann식을 사용하여 플라스마 온도를 구한 다음 구리, 납, 철 및 니켈의 미량 분석 및 간섭 현상에 대해서 연구하였고, 검출 한계를 구하였다.