GLASS FIBER REINFORCED STRIP CROWN IN PRIMARY TEETH (강화형 strip crown의 사용)

  • Kim, Dae-Eop
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.32 no.1
    • /
    • pp.132-135
    • /
    • 2005
  • The purpose of this study was to propose the modified strip crown technique for esthetic restoration of primary anterior teeth using glass fibers. Celluloid crown form(3M, USA), Z100(P shade, 3M, USA). Aeliteflo(Bisco Inc., USA), and Clearfil SE Bond(Kuraray Medical Inc., Japan) were used for this technique. Mesh type of glass fiber(TESCERA Fiber Mesh, Bisco Inc, USA) was used for reinforcing material. After trimming the celluloid crown form, resin adhesive and flowable resin were applied on the pre-shaped glass fiber mesh. That mesh was placed on the lingual surface of inside of celluloid crown form and followed by light activation. Composite resin was filled into the celluloid crown form and put it on a prepared tooth and then light activated and finished the margin. The new modified strip crown technique can provide esthetics and increased durability for restoration of primary anterior teeth.

  • PDF

A Case of Root Canal Treatment and Crown Therapy on Fractured Canine Teeth of Lion (골절된 사자 견치의 근관치료 및 Crown 장착 1례)

  • 이기환;신남식;권수완;김양범;이은창;정성목;이충호;김완희;권오경
    • Journal of Veterinary Clinics
    • /
    • v.17 no.1
    • /
    • pp.298-298
    • /
    • 2000
  • Seven years old male lion in Everland Zoo has three fractured canine tooth. To avoid the risk of a possible fracture with pulp exposure after restroration of largest abration defects, endodontic therapy was performed. The pulp chamber was filled with calcium hydroxide, zinc oxide cement and gutta percha. We also installed the Crown prosthesis was installed in fractured canine tooth to protect the tooth and to improve the cosmetics and function of the tooth. The lion could eat in one day and there were no any signs of dental problem. It is the obvious prophylactic procedure for wild animal is the inclusion of an oral examination at every opportunity to handle the animal. It is considered that crown prosthesis after endodontic therapy was useful for maintaining normal physiological function and for provention of additional fracture or complication.

  • PDF

Influence of porcelain veneering on the marginal fit of Digident and Lava CAD/CAM zirconia ceramic crowns

  • Pak, Hyun-Soon;Han, Jung-Suk;Lee, Jai-Bong;Kim, Sung-Hun;Yang, Jae-Ho
    • The Journal of Advanced Prosthodontics
    • /
    • v.2 no.2
    • /
    • pp.33-38
    • /
    • 2010
  • PURPOSE. Marginal fit is a very important factor considering the restoration's long-term success. However, adding porcelain to copings can cause distortion and lead to an inadequate fit which exposes more luting material to the oral environment and causes secondary caries. The purpose of this study was to compare the marginal fit of 2 different all-ceramic crown systems before and after porcelain veneering. This study was also intended to verify the marginal fit of crowns originated from green machining of partially sintered blocks of zirconia (Lava CAD/CAM system) and that of crowns obtained through machining of fully sintered blocks of zirconia (Digident CAD/CAM system). MATERIALS AND METHODS. 20 crowns were made per each system and the marginal fit was evaluated through a light microscope with image processing (Accura 2000) at 50 points that were randomly selected. Each crown was measured twice: the first measurement was done after obtaining a 0.5 mm coping and the second measurement was done after porcelain veneering. The means and standard deviations were calculated and statistical inferences among the 2 groups were made using independent t-test and within the same group through paired t-test. RESULTS. The means and standard deviations of the marginal fit were $61.52{\pm}2.88{\mu}m$ for the Digident CAD/CAM zirconia ceramic crowns before porcelain veneering and $83.15{\pm}3.51{\mu}m$ after porcelain veneering. Lava CAD/CAM zirconia ceramic crowns showed means and standard deviations of $62.22{\pm}1.78{\mu}m$ before porcelain veneering and $82.03{\pm}1.85{\mu}m$ after porcelain veneering. Both groups showed significant differences when analyzing the marginal gaps before and after porcelain veneering within each group. However, no significant differences were found when comparing the marginal gaps of each group before porcelain veneering and after porcelain veneering as well. CONCLUSION. The 2 all-ceramic crown systems showed marginal gaps that were within a reported clinically acceptable range of marginal discrepancy.

Potential of monolithic zirconia crown using Ko's coloring (심미 수복 치료의 관점에서 바라본 Ko's Coloring을 이용한 Monolithic zirconia crown의 가능성)

  • Ko, Kyung-Hun
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.25 no.2
    • /
    • pp.109-126
    • /
    • 2016
  • According of the development and spread of CAD/CAM, a number of prostheses we have done had been replaced. Dental technicians have a difficulty reproducing natural color when producing these zirconia crowns. Difficulty reproducing natural color when producing these zirconia crowns. In my case, in the beginning of experimenting with zirconia, I had a hard time dealing with zirconia and I have tried solve these problems. Therefore, I would like to share Ko's coloring technique made of my effort with you.

How Can We Improve Crown-Implant Ratio in Reconstructed Mandible with Fibular Free Flap?: A New Surgical Technique Using 3D RP Model and Reconstruction Titanium Plates

  • Kim, Dong-Young;Ahn, Kang-Min
    • Journal of International Society for Simulation Surgery
    • /
    • v.4 no.1
    • /
    • pp.13-16
    • /
    • 2017
  • Fibular free flap reconstruction is the flap of the choice in long-span mandibular bone reconstruction. The most common disadvantage of the fibular flap is short bone height to install dental implant. Double barrel fibular flap has been tried, however, bulky flap in the oral cavity hinder its use. Titanium reconstruction plate has been used simultaneously with the free fibular flap to stabilize occlusion and to fix the fibular flap. In this study, titanium reconstruction plate was fixed in the lower border of the mandible and the fibular free flap was fixed in the superior border of the titanium plate to improve implant-crown ratio. This new technique improved the longevity of the dental prosthodontics with dental implants.

Actinomyces: a deceptive infection of oral cavity

  • Thukral, Rishi;Shrivastav, Kirti;Mathur, Vidhi;Barodiya, Animesh;Shrivastav, Saurabh
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.43 no.4
    • /
    • pp.282-285
    • /
    • 2017
  • Actinomycosis is an infrequent chronic infection regarded as the most misdiagnosed disease by experienced clinicians. The Office of Rare Diseases at the National Institute of Health has also listed this disease as a "rare disease." This article presents a case report of actinomycosis of the alveolus with unusual clinical features but a successful resolution. It also states the importance of biopsy of deceptive inflammatory lesions that do not respond or recur after conventional treatment modalities.

A MORPHOMETRIC STUDY OF THE MAXILLARY PRIMARY FIRST MOLARS USING THREE-DIMENSIONAL SCANNER (3차원 스캐너를 이용한 상악 제1유구치 치관의 크기와 형태에 관한 연구)

  • Lee, Jong-Beom;Kim, Chong-Chul;Hahn, Se-Hyun;Lee, Sang-Hoon
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.33 no.4
    • /
    • pp.643-652
    • /
    • 2006
  • The purpose of this study was to elucidate the size and morphologic characteristics of maxillary primary first molars in Korean children using three-dimensional laser scanner and compare three-dimensional image with preformed stainless steel crown. Scanned three-dimensional images of dental cast taken from 132 children(male 62, female 70) by three-dimensional laser scanner(Breuckmann opto-Top HE100, INUS, Korea) were used. Mesiodistal diameter, buccolingual diameter, occlusogingival height and crown shape of each image were calculated by Rapidform 2004 program(INUS, Korea). The values were statistically compared by independent samples t-test with 95% of significant level. The results were as follows : 1. No significant difference in crown size was found between left and right maxillay primary first molar(p>0.05). 2, Significant difference in mesiodistal diameter, buccolingual diameter, buccal occlusogingival height was found between male and female (p<0.05), and crown size of male was bigger than that of female. 3. Average image of maxillay primary first molar was shaped three-dimensionally and measured. In comparison with 3M stainless steel crown, this image was similar with No.4 or No.5 SS crown in male, No.4 in female. In comparison with ILSUNG SS crown, this image was similar with No.5 in male, No.4 in female. 4 Mesiolingual line angle area, distolingual line angle area and buccogingival ridge were more obvious in average image than 3M stainless steel crown. ILSUNG SS crown was more square and had longer mesiodistal diameter than average 3D image.

  • PDF

Assessment of Internal Fitness on Resin Crown Fabricated by Digital Light Processing 3D Printer

  • Kang, Wol;Kim, Min-Su;Kim, Won-Gi
    • Journal of dental hygiene science
    • /
    • v.19 no.4
    • /
    • pp.238-244
    • /
    • 2019
  • Background: Recently, three-dimensional (3D) printing has been hailed as a disruptive technology in dentistry. Among 3D printers, a digital light processing (DLP) 3D printer has certain advantages, such as high precision and relatively low cost. Therefore, the latest trend in resin crown manufacturing is the use of DLP 3D printers. However, studies on the internal fitness of such resin crowns are insufficient. The recently introduced 3D evaluation method makes it possible to visually evaluate the error of the desired area. The purpose of this study is to evaluate the internal fitness of resin crowns fabricated a by DLP 3D printer using the 3D evaluation method. Methods: The working model was chosen as the maxillary molar implant model. A total of 20 resin crowns were manufactured by dividing these into two groups. One group was manufactured by subtractive manufacturing system (PMMA), while the other group was manufactured by additive manufacturing system, which uses a DLP 3D printer. Resin crowns data were measured using a 3D evaluation program. Internal fitness was calculated by root mean square (RMS). The RMS was calculated using the Geomagic Verify software, and the mean and standard deviation (SD) were measured. For statistical analysis, IBM SPSS Statistics for Windows ver. 22.0 (IBM Corp., USA) was used. Then, independent t-test was performed between the two groups. Results: The mean±SD of the RMS were 41.51±1.51 and 43.09±2.32 for PMMA and DLP, respectively. There was no statistically significant difference between PMMA and DLP. Conclusion: Evaluation of internal fitness of the resin crown made using a DLP 3D printer and subtractive manufacturing system showed no statistically significant differences, and clinically acceptable results were obtained.

The effect of different cooling rates and coping thicknesses on the failure load of zirconia-ceramic crowns after fatigue loading

  • Tang, Yu Lung;Kim, Jee-Hwan;Shim, June-Sung;Kim, Sunjai
    • The Journal of Advanced Prosthodontics
    • /
    • v.9 no.3
    • /
    • pp.152-158
    • /
    • 2017
  • PURPOSE. The purpose of this study was to evaluate the influence of different coping thicknesses and veneer ceramic cooling rates on the failure load of zirconia-ceramic crowns. MATERIALS AND METHODS. Zirconia copings of two different thicknesses (0.5 mm or 1.5 mm; n=20 each) were fabricated from scanning 40 identical abutment models using a dental computer-aided design and computer-aided manufacturing system. Zirconia-ceramic crowns were completed by veneering feldspathic ceramics under different cooling rates (conventional or slow, n=20 each), resulting in 4 different groups (CONV05, SLOW05, CONV15, SLOW15; n=10 per group). Each crown was cemented on the abutment. 300,000 cycles of a 50-N load and thermocycling were applied on the crown, and then, a monotonic load was applied on each crown until failure. The mean failure loads were evaluated with two-way analysis of variance (P=.05). RESULTS. No cohesive or adhesive failure was observed after fatigue loading with thermocycling. Among the 4 groups, SLOW15 group (slow cooling and 1.5 mm chipping thickness) resulted in a significantly greater mean failure load than the other groups (P<.001). Coping fractures were only observed in SLOW15 group. CONCLUSION. The failure load of zirconia-ceramic crowns was significantly influenced by cooling rate as well as coping thickness. Under conventional cooling conditions, the mean failure load was not influenced by the coping thickness; however, under slow cooling conditions, the mean failure load was significantly influenced by the coping thickness.

The Effect of Abutment Inclined Angle on the Marginal Fit of Zirconia All-ceramic Crown (지대주 경사각이 지르코니아 전부도재관의 변연적합도에 미치는 영향)

  • Lee, Seo-Yeon;Chung, In-Sung;Jeon, Byung-Wook
    • Journal of Technologic Dentistry
    • /
    • v.38 no.3
    • /
    • pp.111-117
    • /
    • 2016
  • Purpose: The present study was performed to investigate the effect of abutment inclined angle on the marginal fit of zirconia all-ceramic crown. Methods: The Ti abutments with 3 different inclined angle($2^{\circ}$, $4^{\circ}$ and $6^{\circ}$) were fabricated. The zirconia copings were fabricated for each abutment by using dental CAD/CAM system. The manufactured zirconia copings were duplicated through silicone replica technique, and a replicated specimen was sectioned in the center of bucco-lingual and mesio-distal axial to measure the marginal fit by using a stereo microscope. The results were analyzed using a one-way ANOVA with SPSS 22.0 for Windows(${\alpha}=0.05$). Results: On the bucco-lingual axial, marginal fit was the RL3($41.5{\pm}3.4{\mu}m$), RL2($44.3{\pm}4.3{\mu}m$) and RL1($47.5{\pm}5.7{\mu}m$), respectively. On the mesio-distal axial, marginal fit was the RL3($41.1{\pm}3.7{\mu}m$), RL2($45.7{\pm}5.3{\mu}m$) and RL1($46.2{\pm}4.5{\mu}m$), respectively. One-way ANOVA showed statistically significant difference between groups for marginal fit(p<0.05). Conclusion: For marginal fit of the abutments inclined angle, RL3 specimen was superior. The abutment inclined angle had influence on marginal fit of the zirconia copings. The marginal fit of each group were within clinically acceptable range.