• Title/Summary/Keyword: Copper Bonding

Search Result 166, Processing Time 0.02 seconds

Unidirectionally Solidified Cu Rod Fabrication Using Continuous Casting Apparatus with Cooled Mold (냉각주형식 연속주조장치에 의한 일방향응고 Cu 선재의 제조)

  • Cho, Hoon;Cho, In-Sung
    • Journal of Korea Foundry Society
    • /
    • v.29 no.5
    • /
    • pp.198-203
    • /
    • 2009
  • In order to manufacture copper ultra fine wire used for bonding wire in integrated circuit package, continuous casting process, which can produce high purity copper rod with small cross section, and wiredrawing process have to be optimized to prevent wire brakeage during entire manufacturing process of fine wire. The optimum condition for producing copper rod with mirror surface has to established by investigation of the effects of several parameters such as withdrawal speed, superheat and rod diameter on grain morphology of the cast rod and on its drawing characteristics to fine wire. The purpose of this study is to propose the optimized process parameters in continuous casting process in order to produce cast rod without internal defects, and to predict microstructure orientation suitable for wire drawing process.

Effects of Friction Pressure on Bonding Strength and a Characteristic of Fracture in Friction Welding of Cu to Cu-W Sintered Alloy (동-텅스텐 소결합금(Cu-W)과 동(Cu)의 마찰용접에서 마찰압력이 접합강도와 파단특성에 미치는 영향)

  • 강성보;민택기
    • Journal of Welding and Joining
    • /
    • v.15 no.4
    • /
    • pp.90-98
    • /
    • 1997
  • A copper-tungsten sintered alloy(Cu-W) has been friction welded to a tough pitch copper in order to investigate the effect of friction pressure on bonding strength and a charicteristic of fracture. The tensile strength of the friction welded joint was increased up to 90% of the Cu base metal under the condition of friction time 1.2 sec, friction pressure 4.5kgf/$\textrm{mm}^2$ and upset pressure 10kgf/$\textrm{mm}^2$. From the results of fracture surface analysis, the increase of friction pressure could remarkably decrease the force and the time to be normally acted on weld interface. The W particles which were included in the plastic zone of Cu side could induce fracture adjacent to the weld interface because their existance in Cu induces a decrease in available section area and an increase in notch effect. Therefore, the tensile strength was decreased at high friction pressure (6kgf/$\textrm{mm}^2$) because the destruction of W was increased by an increase in mechanical force and crack was formed at weld interface.

  • PDF

Numerical Prediction of Solder Fatigue Life in a High Power IGBT Module Using Ribbon Bonding

  • Suh, Il-Woong;Jung, Hoon-Sun;Lee, Young-Ho;Choa, Sung-Hoon
    • Journal of Power Electronics
    • /
    • v.16 no.5
    • /
    • pp.1843-1850
    • /
    • 2016
  • This study focused on predicting the fatigue life of an insulated gate bipolar transistor (IGBT) power module for electric locomotives. The effects of different wiring technologies, including aluminum wires, copper wires, aluminum ribbons, and copper ribbons, on solder fatigue life were investigated to meet the high power requirement of the IGBT module. The module's temperature distribution and solder fatigue behavior were investigated through coupled electro-thermo-mechanical analysis based on the finite element method. The ribbons attained a chip junction temperature that was 30℃ lower than that attained with conventional round wires. The ribbons also exhibited a lower plastic strain in comparison with the wires. However, the difference in plastic strain and junction temperature among the different ribbon materials was relatively small. The ribbons also exhibited different crack propagation behaviors relative to the wires. For the wires, the cracks initiated at the outmost edge of the solder, whereas for the ribbons, the cracks grew in the solder layer beneath the ribbons. Comparison of fatigue failure areas indicated that ribbon bonding technology could substantially enhance the fatigue life of IGBT modules and be a potential candidate for high power modules.

The Direct Bonding of Copper to Alumina by $Cu-Cu_2$O Eutectic Reaction (Cu-C$u_2$O의 공정반응에 의한 구리와 알루미나의 직접접합)

  • Yu, Hwan-Seong;Lee, Im-Yeol
    • Korean Journal of Materials Research
    • /
    • v.2 no.4
    • /
    • pp.241-247
    • /
    • 1992
  • The direct bonding of Cu to $Al_2O_3$, employing the $Cu-Cu_2$O eutectic skin melt, is investigated. The bonding force and interface structure of samples prepared by oxidation at $1015^{\circ}C$ in $1.5{\times}10^{-1}$torr followed by bonding at 107$5^{\circ}C$ under $10_{-3}$ torr vacuum have been studied using peeling test, SEM, EDS and XRD. It has been found that the optimal strength is obtained for 3 minutes of oxidation while the adhesion force is decreased with oxidation shorter or longer than 3 minutes. The rupture occured at alumina-eutectic interface. Fractured surface of $Al_2O_3$covered with $Cu_2$O nodules pulled out of the Cu indicates that bonding strength is governed by $Cu-Cu_2$O interface and not by $Cu_2$O-A$l_2O_3$interface. The bonding force is slightly increased with bonding time and the reaction phases of CuA$l_2O_4$and $CuAlO_2$are formed at interface during the bonding.

  • PDF

Experimental Study on the Interface Bonding Characteristics of a Pin-bushing Bearing (핀부시 베어링 소재의 계면접합특성에 관한 실험적 연구)

  • Kim, Chung-Kyun;Kim, Do-Hyun
    • Tribology and Lubricants
    • /
    • v.24 no.6
    • /
    • pp.315-319
    • /
    • 2008
  • This paper presents the interface bonding characteristics between a phosphor bronze and a steel plate for pin-bush bearings. The pin-bush bearing is an important component in which is used to reduce a friction loss and a wear against the piston pin. The pin-bush bearing is manufactured by hot-pressing a phosphor bronze and a back metal of a steel plate. This paper investigated the bonding interface characteristics in which is manufactured by melting a copper based bronze and a steel plate. The hardness from the inner surface of a bronze to the outer one of steel has been measured using a Vickers hardness tester. The experimental results show that the hardness of a bronze is superior to that of the conventional bronze and the transient hardness of pin-bush bearings is gradually increasing to the hardness of the steel back metal. This means that the bonding interface zone of pin-bush bearings may be fabricated by defusing a bronze to the steel plate due to a density difference between two materials.

Finite Element Simulation of Interface Bonding in Kinetic Sprayed Coatings (유한요소 시뮬레이션을 통한 저온 분사 코팅의 계면 접합에 대한 연구)

  • Bae, Gyu-Yeol;Kang, Ki-Cheol;Yoon, Sang-Hoon;Lee, Chang-Hee
    • Journal of Welding and Joining
    • /
    • v.26 no.6
    • /
    • pp.74-80
    • /
    • 2008
  • A finite element modeling approach has been described for the simulation and analysis of the micron-scaled solid particle impact behavior in kinetic spraying process, using an explicit code (ABAQUS 6.7-2). High-strain-rate plastic deformation and interface bonding features of the copper, nickel, aluminum, and titanium were investigated via FEM in conjunction with the Johnson-Cook plasticity model. Different aspects of adiabatic shear instabilities of the materials were characterized as a concept of thermal boost-up zone (TBZ), and also discussed based upon energy balance concept with respect to relative recovery energy (RRE) for the purpose of optimizing the bonding process.

Effects of cooling rate on Microstructure and Bond Strength in WC-Co/Cu/SM45C steel joint (WC-Co/Cu/SM45C강접합에 미세조직 및 접합강도에 미치는 냉각속도의 영향)

  • 정승부;양훈모
    • Journal of Welding and Joining
    • /
    • v.17 no.2
    • /
    • pp.104-111
    • /
    • 1999
  • The interfacial microstructure and bond strength were examined for WC-Co/Cu/SM45C steel join using a nickel-plated copper in vacuum at 1323K for 0.6ks∼3.6ks. After bonding, microstructure in bonding interface was observed by OM(Optical Microscopy), SEM(Scanning Electron Microscopy) and EPMA(Eelectron Probe Micro Analyzer). The oil cooling was carried out at 353K, the cooling rate in air and furnace was 22K/s and 4.4K/s. respectively. It was found that dendritic widths increased with the content of cobalt and bonding times at 1323K. As a whole, bond strength values at the same bonding condition decreased in this order: WC-13wt.%Co/SM45Csteel. WC-8wt.%Co/SM45Csteel and WC-4wt.%Co/SM45Csteel. The bond strength of WC-13wt.%Co/S45C steel joint in oil cooling was 273MPa. This value was greatly higher than those of 125MPa in furnace cooling and 93MPa in air cooling at 1323K for 0.6ks. The bond strength values were found to be closely associated with the content of cobalt in WC-Co and cooling rate.

  • PDF