• 제목/요약/키워드: Controlled low-strength

검색결과 249건 처리시간 0.028초

Study of thin film transition liquid crystal display (TFT-LCD) optical waste glass applied in early-high-strength controlled low strength materials

  • Wang, Her-Yung;Chen, Jyun-Sheng
    • Computers and Concrete
    • /
    • 제5권5호
    • /
    • pp.491-501
    • /
    • 2008
  • The present study verifies compressive strength, ultrasonic pulse velocity, electrical resistance,permeable ratio, and shrinkage from waste glass controlled low strength materials (WGCLSM) and early-high-strength WGCSLM specimens, by replacing the sand with waste glass percentages of 0%, 10%,20%, and 30%. This study reveals that increasing amounts of waste LCD glass incorporated into concrete increases WGCLSM fluidity and reduces the setting time, resulting in good working properties. By increasing the glass to sand replacement ratio, the compressive strength decreases to achieve low-strength effects. Furthermore, the electrical resistance also rises as a result of increasing the glass to sand replacement ratio. Early-high-strength WGCSLM aged 28 days has twice the electrical resistance compared to general WGCSLM. Early-high-strength WGCSLM aged 7 days has a higher ultrasonic pulse velocity similar to WGCSLM aged 28 days. The variation of length with age of different compositions is all within the tolerance range of 0.025%. This study demonstrates that the proper composition ratio of waste LCD glass to sand in early-high-strength WGCSLM can be determined by using different amounts of glass-sand. A mechanism for LCD optical waste glass usage can be established to achieve industrial waste minimization, resource recycling, and economic security.

Bottom ash를 함유한 저강도 고유동 재료의 내구성능 (Durability Characteristics of Controlled Low-Strength Materials using Bottom Ash)

  • 원종필;이용수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.1203-1206
    • /
    • 2001
  • The main intent of this research is to determine the feasibility of utilizing bottom ash as CLSM(Controlled Low-strength Materials). The durability tests including permeability, repeated wetting and drying, freezing and thawing for bottom ash CLSM were conducted. Laboratory test results indicated that CLSM using bottom ash has acceptable durability performance.

  • PDF

석탄회를 활용한 CLSM의 최적배합비 산정에 관한 연구 (A Study on the Optimum Mixing Ratio of CLSM Clculated Utilizing Coal Ash)

  • 강혜주;이후석;황병일;강석표
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2017년도 추계 학술논문 발표대회
    • /
    • pp.159-160
    • /
    • 2017
  • Recently, researches on controlled low strength materials using coal ashes have been actively conducted in Korea. Controlled Low Strength Material by using a large amount of Coal Ashes, which is a by-product of the industry, will solve the environmental problems caused by coal ash as well as economic formulation. In this paper, the compressive strength and flow of the CLSM binder were investigated in order to select the optimum mixing ratio.

  • PDF

석탄회를 사용한 저강도 고유동화재의 경화 특성 분석 (Curing Characteristics of Controlled Low Strength Material Made with Coal Ashes)

  • 김주형;조삼덕;공진영;정혁상;천병식
    • 한국지반환경공학회 논문집
    • /
    • 제11권11호
    • /
    • pp.77-85
    • /
    • 2010
  • 석탄회를 주재료로 하는 저강도 고유동화재의 특성을 분석하기 위해 일축압축강도시험을 수행하였으며, 경화 시간을 분석하였다. 동일한 배합비 상태에서 함수비가 낮을수록 일축압축강도 증가율이 큰 것으로 나타났으며, 초기 3일 동안에는 이와 같은 현상이 뚜렷하게 나타나고 있음을 확인하였다. 또한, 가장 경제적인 시멘트 첨가비로 소형 모형지반을 조성하여 동적콘관입시험을 통해 배합비에 따른 저강도 고유동화재의 특성을 분석한 결과, 목표 일축압축강도인 500kPa(콘관입률 20mm/blow) 도달시간은 약 10일 정도 소요되는 것으로 나타났으며, 10일이 경과한 후에는 배합비와 상관없이 경화속도가 급격하게 감소하는 것으로 나타났다.

저강도 고유동 충전재의 성능에 미치는 광미 전처리의 영향 (Effect of Pretreatment of Mine Tailings on the Performance of Controlled Low Strength Materials)

  • 밀리언 타페세;김형기
    • 자원리싸이클링
    • /
    • 제26권3호
    • /
    • pp.32-38
    • /
    • 2017
  • 광산 부산물인 광미를 건설용으로 대량활용하기 위해서는 내부의 중금속을 제거하기 위한 전처리가 필요하다. 본 연구에서는 전처리 된 광미를 필러(Filler)로 혼입한 저강도 고유동 충전재(Controlled low strength material, CLSM)의 성능에 대해 실험적으로 평가하였다. 전처리가 충전재의 저 성능에 미치는 영향을 평가하기 위해서 전처리 되지 않은 광미 이외에도 고주파 가열 처리, 고주파 가열 후 자력선별 처리한 광미를 실험에 사용하였다. 시멘트의 혼입량은 광미 질량의 10%, 20%, 30%로 설정하였다. 배합설계한 모든 충전재는 미국 콘크리트학회의ACI Committee 229에서 제시한 유동성 200 mm 이상 및 강도 0.3-8.3 MPa의 기준을 만족하는 동시에 최종 침하량은 1% 이하임을 확인하였다.

고로슬래그미분말 및 하수슬러지를 혼입한 시멘트계 저강도 재료의 기초적 물성 (Fundamental Properties of Controlled Low Strength Materials Mixed Blast Furnace Slag and Sewage Sludge)

  • 김동훈;박신;임남기
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.53-54
    • /
    • 2015
  • As the result of uniaxial compression strength test on the CLMS mixing BFS and SS with BFS 4000, it required to determine the desired strength through increasing unit quantity of cement in mixing process because of dramatic strength deterioration of strength according to increasing replacing rate. In this study's result, regardless of differences in fine aggregates used, in order to get uniaxial compression strength in the scope exceeding criteria of minimum strength for applying to the field, the most reasonable combination was to mix replacing BFS with fineness of 6000 in 30%. For the CLMS mixing BFS and SS, in order to improve flow ability by securing quantity of minimum unit and to repress bleeding rate with securing uniaxial compress strength considering the field applicability, regardless of differences in fine aggregates used, to mix BFS over 6000 in 30% was most effective.

  • PDF

석탄회를 활용한 CLSM의 동결융해에 의한 강도 특성 (The Strength Characteristics By Freezing and Thawing of Controlled Low Strength Material Using Coal Ash)

  • 현호규;김선태;정혁상;천병식
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2010년도 추계 학술발표회 2차
    • /
    • pp.32-37
    • /
    • 2010
  • Recently, the land area for many people has been limited because of industrialization and modernization in Korea. The large-scale constructions like the reclamation development projects have been progressed to resolve this problem mentioned above. Therefore, as many of the usefulconstruction materials as possible are needed to perform the large-scale construction projects. Many studies for the utilization of pond ash which has a similar characteristic of sand have been conducted and there has been often occurred many structural problems on roadbed in winter. Therefore, the characteristics of the freezing and thawing for Controlled Low-Strength Material (CLSM) using pond ash were analyzed and evaluated by unconfined compressive strength test in this study. As a result of this study, it was confirmed that new CLSM using pond ash with cement (8.2% by weight)was able to stand for the freezing and thawing behavior.

  • PDF

석탄회를 활용한 저강도고유동화재의 일축압축강도 및 플로우 특성 (Characteristics of Uncofined Compressive Strength and Flow in Controlled Low Strength Materials Made with Coal Ash)

  • 공진영;강형남;천병식
    • 한국지반공학회논문집
    • /
    • 제26권1호
    • /
    • pp.75-83
    • /
    • 2010
  • 저강도고유동화재는 다짐이 필요 없고 유동성이 큰 물질로 일반적으로 시멘트, 비회, 잔골재, 물, 혼화제 등을 혼합하여 만들어진다. 기존의 CLSM은 잔골재로 모래를 사용하고 있으나 때문에 모래가 점점 구하기 어려워지는 현재 우리나라 실정에서는 그대로 사용하기 곤란하다. 본 연구에서는 모래대신 매립회를 이용하여 매립회, 비회, 시멘트, 물의 혼합물로 만들어진 CLSM의 강도특성을 조사하여 사용가능성을 제시하고자 한다. 일축압축강도실험결과 기준 일축압축강도(0.5MPa~1.0MPa)를 만족하는 배합비는 매립회와 비회의 혼합비 0:100~70:30, 시멘트비 3.0~5.0%, 함수비 31~34%로 나타났다. 플로우시험 결과 매립회와 비회를 혼합하여 사용하는 모든 경우(매립회와 비회의 비 30:70~70:30)에서 기준 플로우값(0.2m)를 만족하였다.

급결성 유동화처리토의 특성에 관한 실험적 연구 (A experimented study on Rapid-Setting Flowable Material)

  • 이상일;조대호;한상재;김수삼
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2006년도 춘계 학술발표회 논문집
    • /
    • pp.1295-1302
    • /
    • 2006
  • Controlled low-strength material(CLSM) which is easily excavated and also known as flowable material, is commonly used as a backfill in utility trenches and other applications. In this study, a rapid-setting flowable material a kind of CLSM made with a field soil were evaluated by an experimental study. The properties ordinarily desired from the mix are: (a) flow under gravity; (b) hardening for early workability(after 4 hours)and cover; and (c) ultimate strength low enough to allow ready excavation. Fluidity of fresh material is evaluated using a simple spread test. Hardening is measured by a mortar penetrometer, and these values are correlated with unconfined compressive strength. It is desirable to keep the ultimate strength to less than $5.6kg/cm^2$ somewhat less target strength is selected for the 28-day value.

  • PDF