자동차 이차전지 제조를 위한 알루미늄과 무산소동의 레이저 용접특성 (Laser Welding Characteristics of Aluminum and Copper Sheets for Lithium-ion Batteries)

  • 강민정;박태순;김철희;김정한
    • Journal of Welding and Joining
    • /
    • 제31권6호
    • /
    • pp.58-64
    • /
    • 2013
  • Several joining methods involving resistance welding, laser welding, ultrasonic welding and mechanical joining are currently applied in manufacturing lithium-ion batteries. Cu and Al alloys are used for tab and bus bar materials, and laser welding characteristics for these alloys were investigated with similar and dissimilar material combinations in this study. The base materials used were Al 1050 and oxygen-free Cu 1020P alloys, and a disk laser was used with a continuous wave mode. In bead-on-plate welding of both alloys, the joint strength was higher than the strength of O tempered base material. In overlap welding, the effect of welding parameters on the tensile shear strength and bead shape was evaluated. Tensile shear strength of overlap welded joint was affected by interfacial bead width and weld defect formation. The tensile-shear specimen was fractured at the heat affected zone by selecting proper laser welding parameters.

EXPERIMENTAL STUDY ON LASER AND HOT AIR REFLOW SOLDERING OF

  • Tian, Yanhong;Wang, Chunqing
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.469-474
    • /
    • 2002
  • Laser and hot air reflow soldering of PBGA solder ball was investigated. Experimental results showed that surface quality and shear strength of solder bumps reflowed by laser was superior than the solder bumps reflowed by hot air, and the microstructure inside the solder bumps reflowed by laser was much finer. Analysis on interfacial reaction showed that eutectic solder reacted with Au/Ni/Cu pad shortly after the solder was melted. Interface of solder bump reflowed by laser consists of a continuous AuSn$_4$ layer and remnant Au element. Needle-like AuSn$_4$ grew sidewise from interface, and then spread out to the entire interface region. A thin layer of Ni$_3$Sn$_4$ intermetallic compound was found at the interface of solder bump reflowed by hot air, AuSn$_4$ particles distributed inside the whole solder bump randomly. It is the combination effect of the continuous AuSn$_4$ layer and finer eutectic microstructure inside the solder bump reflowed by laser that resulted in higher shear strength.

  • PDF

격자형 용접 주행로봇의 개발 ( 제1보 : 주행제어 및 용접선 추적제어 ) (Development of Mobile Robot for Welding of Lattice Type - Mobile Speed Control and Seam Tracking Control -)

  • 감병오;전양배;강치정;주갑영;김상봉
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2000년도 특별강연 및 추계학술발표대회 개요집
    • /
    • pp.34-36
    • /
    • 2000
  • It is difficult to realize automation of welding of lattice type in shipbuilding and assembly processing of shipbuilding and steel structures. Usually, the welding parts of lattice type are welded manually. So there are limitations in continuous and stable quality controls and in increase in productivity because the welding quality depends on worker's skill. That is, automation in welding is necessary. This paper shows shows the development results of a moblie robot for welding of lattice type. Specially. algorithms for its mobile speed and seam tracking controls are introduced.

  • PDF

연속파형 Nd:YAG레이저를 이용한 S45C 강판의 레이저 용접 모니터링에 관한 연구 (A Study on the Monitoring of Laser Welding for S45C Steel Sheets Using Nd:YAG Laser with Continuous Waves)

  • 김도형;신호준;유영태
    • 한국생산제조학회지
    • /
    • 제21권5호
    • /
    • pp.814-823
    • /
    • 2012
  • Fluctuation of light intensity from the keyhole becomes more significant in full penetration welding than partial penetration welding, since the plasma produced in the keyhole can escape from the rear side of the keyhole. The plasma optical radiation emitted during Nd:YAG laser welding of S45C steel samples has been detected with a Photodiode and analyzed under different process conditions. As the results, the BOP was performed for welding, behavior of plasma, spatter or plume was monitored to determine the reference signal. Then, random combination was made for comparison with the reference signal, which aimed at verifying reliability of the welding monitoring system that this study intended to develop.

웨이브렛 변환을 이용한 전자빔 용접 진단 (Electron Beam Welding Diagnosis Using Wavelet Transform)

  • 윤충섭
    • Journal of Welding and Joining
    • /
    • 제21권6호
    • /
    • pp.33-39
    • /
    • 2003
  • Wavelet transform analysis results show a spectrum energy distribution of CWT along scale factors distinguish the partial, full and over penetration in a electron beam welding by analyzing the curve of spectrum energy at small scale, middle and large scale range, respectively. Two types of signals collected by Ion collector and x-ray sensors and analyzed. The acquired signals from sensors are very complicated since these signals are very closely related the dynamics of keyhole which interact the very high density energy with materials during welding. The results show the wavelet transform is more effective to diagnosis than Fourier Transform, further for the general welding defects which are not a periodic based, but a transient, non-stationary and time-varying phenomena.

2024 알루미늄의 마찰용접에 관한 연구 (A study on friction welding of 2024 aluminium)

  • 송오성;강춘식
    • Journal of Welding and Joining
    • /
    • 제8권3호
    • /
    • pp.24-30
    • /
    • 1990
  • 2024 Aluminium was welded by domestic manufactured continuous type friction welder. The problems and optimum condition were studied in 2024 Al-2024 Al cases. Mechanical tests and microstructure analysis were studeid. Interfacial temperature of welding was predicted by FDM. The obtained results are as follows: 1) In case of Al-Al, the optimum condition range was wide. 2) At the boundary zone, fine recrystallized zone was not harmful to the mechanical property and no growth of precipitation was observed. 3) In case of Al-Al, temperature gradient can be predictedby FDM and heat input can be taken as weld parameter.

  • PDF

저탄소강의 고출력 $CO_2$ 레이저 빔 용접 (High power $CO_2$ laser beam welding for low carbon steels)

  • 김재도
    • Journal of Welding and Joining
    • /
    • 제7권4호
    • /
    • pp.12-21
    • /
    • 1989
  • Laser beam welding parameters have experimentally investigated, using a continuous wave 3kW $CO_2$ laser with the various travel speeds, beam mode and laser beam power in low carbon steels. An optimum position of focus and the effect of shielding gas on penetration depth with varying the flow range of 0.5 to 5.1m/min have been combined to investigate the effect of laser power and travel speed on penetration depth and bead width. It is found that the optimum position of focus in 3kW class laser is 0.5 to 1.5mm below the surface of the material. The flow rate of shielding gas affects the penetration depth and He is more effective than Ar. The penetration depth in laser welds of low carbon steels is between two and four times of the bead width. Laser beam welding of butt joints in 2mm thick carbon steel has been carried out to establish a weldability lobe. The lobe indicating acceptable welding conditions is introduced.

  • PDF

Nd:YAG 레이저를 이용한 자동차 배터리용 SS41 다층박판 이종두께 T형상 용접 특성 (T-joint Welding Characteristics of Multi-thin Plate Dissimilar Thickness of SS41 of Automobile Battery by using Nd:YAG Laser)

  • 양윤석;황찬연;유영태
    • 한국정밀공학회지
    • /
    • 제29권10호
    • /
    • pp.1078-1088
    • /
    • 2012
  • In this paper, we present research experimental results about the different thickness T-joint welding of the high power continuous wave(CW) Nd:YAG laser for the secondary battery of a vehicle. Although the conventional method used for the secondary battery is a argon TIG welding, we utilize a laser welding to improve Tungsten Inert Gas(TIG) welding's weakness. The laser, which has a couple of advantage such as aspect ratio, low Heat Affected Zone(HAZ), good welding quality and fast productivity utilized in this work is a CW Nd:YAG laser. In order to observe laser welding sections, we used a optical microscope. Through the analysis of the metallographic, hardness, aspect ratio, and heat input, we obtained the desired data in condition of 1800 W laser beam power and 1.8 m/min and 2.0 m/min laser beam travel speeds. In order to compare electric resistances of the argon TIG welding and laser welding, we made an actual battery and the electric resistance of the laser welding is reduced by 40~45% comparing with the argon TIG welding.

오스테나이트계 304 스테인리스강의 Nd:YAG 레이저 맞대기 용접특성 (Butt Welding Characteristics of Austenitic 304 Stainless Steel Using a Continuous Wave Nd:YAG Laser Beam)

  • 유영태;오용석;신호준;임기건
    • 대한기계학회논문집A
    • /
    • 제28권2호
    • /
    • pp.165-173
    • /
    • 2004
  • Laser beam welding is increasingly being used in welding of structural steels. The laser welding process is one of the most advanced manufacturing technologies owing to its high speed and deep penetration. The thermal cycles associated with laser welding are generally much faster than those involved in conventional arc welding processes, leading to a rather small weld zone. Experiments are performed for 304 stainless steel plates changing several process parameters such as laser power, welding speed, shielding gas flow rate, presence of surface pollution, with fixed or variable gap and misalignment between the similar and dissimilar plates, etc. The following conclusions can be drawn that laser power and welding speed have a pronounced effect on size and shape of the fusion zone. Increase in welding speed resulted in an increase in weld depth/ aspect ratio and hence a decrease in the fusion zone size. The penetration depth increased with the increase in laser power.