In the recent years, a rigid pavement composed of a flat concrete slab has ken constructed due to the desirable structural strength of concrete, durability and economy. However, despite of precise design and construction of concrete highway pavement, some sections of the 88 Olympic express highway, Jung-bu express highway, and Kyung-bu express highway, which have shown premature cracking, faulting, and pumping before the end of their intended service life, have already been viewed with great concerns by highway officials and engineers. Since environmental variations and traffic loads might be considered as major factors to cause pavement failure problems, the thermal load due to temperature variations between top and bottom surface of the concrete slab was highlighted to verify analytical behavior of concrete slab using the finite element method.
This study evaluated characteristics and performance of recycled concrete as a pavement which was constructed on a low volume road. The recycled concrete was prepared by replacing a half of coarse aggregate with recycled aggregate. Natural sand from a source was used as fine aggregate together with admixtures such as plasticizer and fly ash (0.8% and 5% by wt. of cement, respectively). The length, thickness and width of the pavement were 100mm, 20cm and 3m, respectively. From construction experience, it was found that workability and finishability of the recycled concrete mixture were relatively poor, but strengths were satisfactory. Flexural strength, compressive strength and elastic modulus at 28 days were approximately 45Kg/$\textrm{cm}^2$, 250Kg/$\textrm{cm}^2$, and 240,000 Kg/$\textrm{cm}^2$, respectively. The pavement could be constructed by hand without much difficulty. The surface was finished smoothy by wet fabric and only minor cracks were found on the surface.
OBJECTIVES : This study is to develop the optimum mixing proportions for cement concrete pavement with using recycled aggregates. METHODS : The mixture varied recycled coarse aggregates content from 50 % to 100 % to replace the natural coarse aggregates by weight. Tests for fundamental properties as a cement concrete pavement were conducted before and after hardening of the concrete. RESULTS : It was found that the variation in the amount of the recycled aggregate affected the compressive and flexural strength development, as well as the chloride ion penetration resistance. As the amount of the recycled aggregate content increased the compressive and flexural strength and the resistance to chloride ion penetration decreased. However, the resistance to freeze-thaw reaction was affected significantly. In addition, the gradation of the aggregate became worse and hence so did the coarseness factor as the recycled aggregate amount increased. CONCLUSIONS : The fundamental properties of the concrete with recycled aggregate does not seem to be appropriate when the recycled aggregate quality is not guaranteed up to a some level and its replacement ratio is over 50%. The optimized gradation of the aggregates should also be sought when the recycled aggregate is used for the cement concrete pavement materials.
This study was performed to evaluate the void ratio, compressive and flexural strength, and permeability coefficient used powdered waste glass, $CaCO_3$, recycled coarse aggregate and unsaturated polyester resin to find optimum mix design of permeable polymer concrete for pavement. The void ratio and permeability coefficient of permeable concrete for pavement was decreased with increasing the powdered waste glass, respectively. The compressive strength and flexural strength was increased with increasing the powdered waste glass, respectively. In addition, this study found out that required amount of binder was decreased with increasing the powdered waste glass. This fact is expected to have economical effects during the use of powdered waste glass in the manufacture of permeable polymer concrete for pavement. Therefore, powdered waste glass and recycled coarse aggregate can be used for permeable polymer pavement.
Stormwater pollution is a major problem in urban areas. Pollutants like heavy metals and harmful chemicals in the runoff can endanger soil and ground water, when they are not sufficiently removed doting infiltration. Strength and infiltration capacity of porous concrete are the major problems that must be considered if permeable pavement system are demanded to be used in a drive way application. In this study, a series of compacted porous concrete mixtures and the system of pavement ate tested for the physical characteristics like compressive strength, flexural strength, unit weight, porosity, water permeability, and the purification capacity of contaminated water. The test results obtained indicate that the strength and infiltration capacity of porous concrete are strongly related to its matrix proportion and compaction energy and providing adequate filter layers underneath pavement surface course is one of the most important design considerations of permeable pavement system for pollution retention purpose.
PURPOSES : So far, aged cement concrete pavement on express highways has been rehabilitated mainly with asphalt concrete inlay. However, potholes were the major problem, and they shortened the life of the inlay mainly owing to the poor drainage of water once it infiltrated the interface of the concrete and asphalt. The purpose of this study is to compare the performance and economic efficiency of asphalt overlay and inlay. METHODS : Overlay and inlay were compared through accelerated pavement testing, and a life-cycle cost analysis was conducted in this study using the CA4PRS program. RESULTS and CONCLUSIONS : It was found from accelerated pavement testing that the overlay exhibited reflective crack resistance that was more than twice as effective as that of inlay. The total cost (construction cost + user cost) within the analysis period (20 years) of the overlay was 37% lower than that of the inlay.
본 연구의 주 목적은 교면포장 공법 중에서 인천대교에 사용된 구스 아스팔트와 귤현 대교에 사용된 SMA의 적용 사례를 통하여 발전된 교면포장 공법을 제시하는데 있다. 두 공법의 시공사례를 비교 분석한 결과, 구스 아스팔트는 고온에서의 유동저항성이 작아 소성변형에 취약하며, 이에 반하여 SMA포장은 유지관리에 용이하고 소성변형 등에 유리하다는 것을 알 수 있었다. 이러한 결과는 강상판 교면포장 공법이 발달된 선진국에서는 보편화되어서, 그에 따른 국내에서의 해결방안을 제시하였다. 그러나, 국내의 경우 다양한 시공 실적이 미흡한 실정이어서 향후 적절한 시공관리와 체계적인 연구를 통하여 보다 발전된 교면 포장공법이 제시되어져야 할 것으로 사료된다.
International Journal of Concrete Structures and Materials
/
제19권1E호
/
pp.17-23
/
2007
In rainy weather, permeable concrete pavement has advantages such as good drainage, increased skid resistance, reduced splash and spray behind vehicles for improving the safety of driving vehicles as well as reduction of the traffic noise. It also contributes to improvement of traffic environment. In this study, the fundamental properties of permeable concrete in accordance with maximum size of aggregate, sand percentage and unit cement content were investigated for practical use of permeable concrete pavement. Although the permeability standard for typical permeable asphalt-concrete pavement is $1{\times}10^{-2}cm/sec$, the researchers determined that the coefficient of permeability of the permeable concrete should be set higher at $1{\times}10^{-1}cm/sec$. Then, the researchers measured the coefficient of permeability, strength, void ratio, and continuous void ratio of the permeable concrete while varying maximum size of the aggregate, sand percentage, unit cement content for detailed analysis. It was found that the void ratio, continuous void ratio, and flexural strength were about 15%, 12%, and 5.0MPa, respectively, when the permeability of the concrete was set at $1{\times}10^{-1}cm/sec$. Given that the maximum size of aggregate was $10{\sim}13mm$, we reached the conclusion that the best mix design for permeable concrete was $0{\sim}20%$ of sand percentage and $380kg/m^3$ of unit cement content.
Recently, Korea Highway Corporation has attemped to improve the highway safety in accordance with minimizing user's imconveniences. Currently, the Anti Skidding Pavement(ASP) has been introduced as a safety countermeasure on the safety frailty sections. In this study, a series of field evaluations on pavement skid resistance have been conducted on the skid frailty sections to analyze the effects and problems of the Anti Skidding Pavement (ASP), and to understand the behavior of pavement skid resistance due to pavement type, section characteristics, vehicles' speed and traffec volume. Test results show the Anti Skidding Pavement (ASP) has the effects to induce vehicles' speed reduction. However, there are no effects to increase skid resistance. According to these results, it is demanded to improve the applying method of current Anti Skidding Pavement (ASP) to devise an effective safety countermeasure for pavement skid, and to increase pavement skid resistance.
Hydronic heated road pavement (HHP) systems have well studied and documented by many researchers. However, most of the systems run on asphalt, only a few are tested with concrete, and there rarely is a comparison between those two common road materials in their heating and cooling performance. The aim of this study is to investigate the thermal performance of the HHP, such as heat dissipation performance in winter season while focusing on the surface temperature of the concrete and asphalt pavement. For preliminary study a small-scale experimental system was designed and installed to evaluate the heat transfer characteristics of the HHP in the test field. The system consists of concrete and asphalt slabs made of 1 m in width, 1 m in length, and 0.25 m in height. In two slabs, circulating water piping was embedded at a depth of 0.12 m at intervals of 0.16 m. Heating performance in winter season was tested with different inlet temperatures of 25℃, 30℃, 35℃ and 40℃ during the entire measurement period. The results indicated that concrete's heating performance is better than that of asphalt, showing higher surface temperatures for the whole experiment cases. However, the surface temperature of both concrete and asphalt pavement slabs remained above 0℃ for all experimental conditions. The heat dissipation performance of concrete and asphalt pavements was analyzed, and the heat dissipation of concrete pavement was greater than that of asphalt. In addition, the higher the set temperature of the circulating water, the higher the heat dissipation. On the other hand, the concrete pavement clearly showed a decrease in heat dissipation as the circulating water set temperature decreased, but the decrease was relatively small for the asphalt pavement. Based on this experiment, it is considered that a circulating water temperature of 20℃ or less is sufficient to prevent road ice. However, this needs to be verified by further experiments or computational fluid dynamic (CFD) analysis.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.