• Title/Summary/Keyword: Concrete Surface Treatment

Search Result 120, Processing Time 0.028 seconds

An Experimental Study on Corrosion Behavior in Steel of Concrete Applied with Arc Metal Spray Method Surface Treatment Technology Using EIS (EIS를 이용한 아크 금속용사 표면처리기법이 적용된 강재의 콘크리트 내 부식 거동에 관한 실험적 연구)

  • Yoon, Chang-Bok;Park, Jang hyun;Lee, Han-Seung
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.3
    • /
    • pp.87-95
    • /
    • 2020
  • As an experimental study on the corrosion behavior of steel materials to which ATMS method using EIS was applied in concrete, immersion of Ca(OH)2 saturated aqueous solution and NaCl aqueous solution simulating the environment inside concrete The corrosion behavior was tested. The equivalent circuit was derived through the analysis of the Nyquist plot, and the interfacial resistance and the polarization resistance of the Ca(OH)2 aqueous solution were compared, and Al ATMS was the best interfacial resistance and Zn ATMS was the best polarization resistance. After burying ATMS steel material of cement mortar, the initial immersion impedance measurement value was the highest in the Zn ATMS test body in the impedance measurement by the immersion time by immersing it in the NaCl aqueous solution. Al ATMS test piece has the highest impedance and is highly reliable. This is because Al, which has a high ionization tendency, is continuously oxidized in a strong alkaline environment to form a film and protect the steel from permeation of chlorine ions.

Deterioration Diagnosis and Conservation Treatment of the Three-storied Stone Pagoda in the Cheongryongsa Temple, Anseong, Korea (안성 청룡사삼층석탑의 풍화훼손도 진단과 보존처리)

  • Lee, Sun-Myung;Lee, Myeong-Seong;Jo, Young-Hoon;Lee, Chan-Hee;Jeon, Seong-Won;Kim, Ju-Ok;Kim, Sun-Duk
    • Economic and Environmental Geology
    • /
    • v.40 no.5
    • /
    • pp.661-673
    • /
    • 2007
  • Rock materials of the three-storied stone pagoda in the Cheongryongsa temple in Korea are mainly composed of gneissose two-mica granite and fine-grained granite. This stone pagoda shows structural instability due to cracks and breaking-out of the stones. The surface properties of the stone is highly degraded by various inorganic pollutants and epilithic biospecies. Therefore, this study carried out comprehensive deterioration diagnosis by non-destructive methods, and some conservation treatments base on the diagnosis were carried out to reduce weathering progress. As the treatments, the biospecies and lichen that covering on the stone surfaces were removed by dry and wet cleaning, and degraded concrete applied to the pagoda for restoration in the past was removed and repaired with epoxy resin. Oxidized iron plates inserted between the rock properties were also substituted titanium stainless steels. After all processes are completed, we sprayed consolidant on the rock surface. Finally, the ground of the stone pagoda was rearranged using small rock aggregates, and the fence was established for control of artificial deterioration by visitors and environmental maintenance.

Deterioration and Conservation Treatment of the Three Storied Stone Pagoda in Seoak-ri, Gyeongju (경주 서악리 삼층석탑의 훼손상태 및 보존처리)

  • Lee, Myeong-Seong;Jeong, Min-Ho;Jung, Young-Dong;Lee, Chan-Hee
    • Journal of Conservation Science
    • /
    • v.18 s.18
    • /
    • pp.63-74
    • /
    • 2006
  • All rock materials of the three storied stone pagoda in Seoakri were composed of light gray alkali granite with medium grained and developed with small mialolitic cavities. This stone pagoda is preserving almost archetype except the head part because there was repair work already. But, foundation, basement and roof rocks are serious state by microbial invasion such as lichens. Because there are tree and grass that cause direct effect to stone pagoda surrounding. Therefore, conservation treatment executed the primary dry cleaning and secondary wet cleaning treatment. Stone surface is partly not removed well such as lichens which part removed using cleansing device that use high temperature steam. Some treated part concrete and epoxy resin remove and retreatment with mixing talc and alkali granite powder to epoxy resin. Did color matching at mixing process of epoxy resin and fillers to properties with set the feel of a material. Also, drainage ditched to minimize inflow of rainwater fall from slope that is on the east of stone pagoda, tree and grass in stone pagoda surrounding wished to do remove and control occurrence of lichens hereafter minimizing moisture conteats.

  • PDF

Evaluation of Adhesion Characteristics of Crack Sealants Used in Asphalt Concrete Pavement (아스팔트 콘크리트 포장용 균열실링재의 부착특성 평가)

  • Lee, Jae-Jun;Kim, Seung-Hoon;Baek, Jong-Eun;Lim, Jae-Kyu;Kim, Yong-Joo
    • International Journal of Highway Engineering
    • /
    • v.17 no.2
    • /
    • pp.55-62
    • /
    • 2015
  • Cracking is an inevitable fact of asphalt concrete pavements and plays a major role in pavement deterioration. Pavement cracking is one of the main factors determining the frequency and method of repair. Cracks can be treated with a number of preventative maintenance actions, including overlay surface treatments such as slurry sealing, crack sealing, or crack filling. Pavement cracks can show up as one or all of the following types: transverse, longitudinal, fatigue, block, reflective, edge, and slippage. Crack sealing is a frequently used pavement maintenance treatment because it significantly extends the pavement service life. However, crack sealant often fails prematurely due to a loss of adhesion. Because current test methods are mostly empirical and only provide a qualitative measure of the bond strength, they cannot accurately predict the adhesive failure of the sealant. This study introduces a laboratory test aimed at assessing the bonding of hot-poured crack sealant to the walls of pavement cracks. A pneumatic adhesion tensile testing instrument (PATTI) was adopted to measure the bonding strength of the hot-poured crack sealant as a function of the curing time and temperature. Based on a limited number of test results, the hot-poured crack sealants have very different bonding performances. Therefore, this test method can be proposed as part of a newly developed performance-based standard specification for hot-poured crack sealants for use in the future. PURPOSES : The purpose of this study was to evaluate both the adhesion and failure performance of a crack sealant as a function of its curing time and curing temperature. METHODS: A pneumatic adhesion tensile testing instrument (PATTI) was adopted to measure the adhesion performance of a crack sealant as a function of the curing time and curing temperature. RESULTS: With changes in the curing time, curing temperature, and sealant type, the bond strengths were found to be significantly different. Also, higher bond strengths were measured at lower temperatures. Different sealant types produced completely different bond strengths and failure behaviors. CONCLUSIONS: The bonding strength of an evaluated crack sealant was shown to differ depending on various factors. Two sealant types, which were composed of different raw materials, were shown to perform differently. The newly proposed test offers the possibility of evaluating and differentiating between different crack sealants. Based on alimited number of test results, this test method can be proposed as part of a newly developed performance-based standard specification for crack sealants or as part of a guideline for the selection of hot-poured crack sealant in the future.

Interfacial Pullout Characteristics of Recycled PET Fiber With Hydrophilic Chemical Treatments in Cement Based Composites (화학적 친수성 처리율에 따른 재생 PET 섬유와 시멘트 복합재료와의 계면 인발 특성)

  • Won, Jong-Pil;Park, Chan-Gi;Kim, Yoon-Jeong;Park, Kyung-Hoon
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.3
    • /
    • pp.333-339
    • /
    • 2007
  • The purpose of this study was to enhance bond performance between recycled PET (polyethylene telephthalat) fiber and cement composites through hydrophilic treatment using maleic anhydride grafted polypropylene(mPP). The mPP with various concentration of 0%, 5%, 10%, 15% and 20% to determine effect on bond behavior of recycled PET fiber were applied as experimental variables. Dog bone shaped specimens according to JCI SF-8 was applied to evaluate the bond strength and pullout energy. The results showed increased bond strength and pullout energy as concentration of mPP. Concentration of 15% mPP showed the most effective results while 20% showed reduced performance results. Because 15% mPP ensures perfect coating while 20% makes thick coating area that resulted in crack propagation and consequent separation of PET fiber and coated area during pullout load occurred. Enhancement mechanism of bond performance of recycled PET fiber and cement composites with each concentration of mPP could be conformed through investigation of microstructure of fiber surface.

Improvement of existing drainage system for leakage treatment in exiting underground structures (운영중인 지하구조물의 누수처리를 위한 유도배수공법의 개선)

  • Kim, Dong-Gyou;Yim, Min-Jin
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.19 no.4
    • /
    • pp.669-683
    • /
    • 2017
  • The objective of this study is to propose a modification of the previously proposed drainage system for catching the partial leakage of underground concrete structures. Two techniques were proposed for applying the drainage system only to the leaking parts. One was for conveying leaking groundwater to the collection point in the drainage system and the other was for conveying the collected groundwater to the primary drainage system of the underground concrete structure. Four waterproofing materials for conveying leaking groundwater to the catchment point of the drainage system, Durkflex made of porous rubber material, KE-45 silicone adhesive with super strong adhesion, Hotty-gel made of polymeric materials and general silicone adhesive were evaluated for waterproofing performance. Hotty-gel only showed perfect waterproof performance and the other three waterproof materials leaked. The modified drainage system with Hotty-gel and drainage pipe with fixed saddle to convey the leaking groundwater from the catchment point to the primary drainage system were tested on the concrete retaining wall. The waterproof performance and the drainage performance were evaluated by injecting 1,000 ml of water in the back of the modified drainage system at the 7-day, 14-day, 21-day, 28-day, 2-month and 3-month. There was no problem in waterproof performance and drainage performance of the modified drainage system during 3 months. In order to evaluate the construction period and construction cost of the modified drainage system, it was compared with the existing leaching repair method in surface cleaning stage, leakage treatment stage, and protective barrier stage. Total construction period and construction cost were compared in considering the contents of work, repair material, construction equipment, working time, and total number of workers. As a result of comparing and analyzing in each construction stage, it was concluded that the modified drainage system could save construction period and construction cost compared to the existing leaching repair method.

Effect of freezing and thawing on the drainage system for leakage treatment (유도배수공법에서 동결융해의 영향)

  • Kim, Dong-Gyou;Yim, Min-Jin
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.19 no.6
    • /
    • pp.1059-1075
    • /
    • 2017
  • The objective of this study was to evaluate the freezing and thawing resistance of the existing drainage system for leakage treatment of underground concrete structures operating in cold regions. The freezing and thawing test was conducted on 4 types of drainage system specimens to evaluate the freezing and thawing resistance of the drainage system. The freezing and thawing resistance was evaluated on 4 types of Hotty-gel, as a waterproofing material, connection methods and on two methods to fix the drainage board with Hotty-gel on the surface of cement concrete specimen. One cycle of the freeze-thaw testing was 48 hours (24 hours of freezing and 24 hours of thawing), and the temperatures of freezing and thawing were at $-18^{\circ}C$ and $10^{\circ}C$, respectively. Among the 4 types of Hotty-gel connection methods, leakage occurred after 28 cycles (8 weeks) of freeze-thawing only in the Hotty-gel connection method with the 'V' groove applied to the corner of the drainage board. No leakage occurred in the 3 types of Hotty-gel connection methods. In two fixing methods, leakage occurred in the method of fixing the drainage board on the cement concrete specimen using the washer, screw and plastic wall plug. Leakage occurred at one point after 10 cycles (3 weeks) of freezing and thawing. After 28 cycles (8 weeks) of freezing and thawing, leakage point increased to 5 points. As time passed, the leak point was not increased, but the amount of leakage was increased at each leak point. The Hotty-gel connection method with cross-sectional diagonal shape was evaluated to be the highest in the production efficiency considering the production time and manufacturing method of the Hotty-gel connection shape. In the construction efficiency considering the construction time and construction method, the fixing method of air nailer, fixed nail and washer was superior to that of the washer, screw and plastic wall plug.

Deterioration Diagnosis and Source Area of Rock Properties at the West Stone Pagoda, Gameunsaji Temple Site, Korea (감은사지 서탑의 풍화훼손도 진단 및 석재의 산지추정)

  • Lee Chan Hee;Lee Myeong Seong;Suh Mancheol;Choi Seok-Won;Kim Man Gap
    • Economic and Environmental Geology
    • /
    • v.37 no.5
    • /
    • pp.569-583
    • /
    • 2004
  • The rock properties of the West pagoda in the Gameunsaji temple site are composed mainly of dark grey porphyritic granodiorite with medium grained equigranular texture and developed with small numerous dioritic xenoliths. These xenoliths occurred with small holes due to different weathering processes. As a weathering results, the rock properties of this pagoda occur wholly softened to physical hardness because of a complex result of petrological, meteorological and biological causes. Southeastern part of the pagoda deteriorated seriously that the surface of rock blocks showed partially exfoliations, fractures, open cavities in course of granular decomposition of minerals, sea water spray and crystallization of salt from the eastern coast. The Joint between blocks has small or large fracture cross each other, contaminated and corrupted for inserting with concrete, cement mortar, rock fragments and iron plates, and partially accelerated coloration and fractures. There are serious contamination materials of algae, fungus, lichen and bryophytes on the margin and the surface on the roof stone of the pagoda, so it'll require conservation treatment biochemically for releasing vegetation inhabiting on the surface and the discontinuous plane of the blocks because of adding the weathering activity of stones and growing weeds naturally by soil processing on the fissure zone. Consisting rock for the conservation and restoration of the pagoda would be careful choice of new rock properties and epoxy to reinforce for the deterioration surfaces. For the attenuation of secondary contamination and surface humidity, the possible conservation treatments are needed.

Acid Drainage and Damage Reduction Strategy in Construction Site: An Introduction (건설현장 산성배수의 발생현황 및 피해저감대책)

  • Kim, Jae-Gon
    • Economic and Environmental Geology
    • /
    • v.40 no.5
    • /
    • pp.651-660
    • /
    • 2007
  • Acid drainage has been recognized as an environmental concern in abandoned mine sites for long time. Recently, the environmental and structural damage by acid drainage is a current issue in construction sites in Korea. Here, the author introduces the type of damages by acid drainage in construction sites and emphasizes the importance of geoscience discipline in solving the problem. Metasedimentary rock of Okcheon group, coal bed of Pyeongan group, Mesozoic volcanic rock. and Tertiary sedimentary and volcanic rocks are the major rock types with a high potential for acid drainage upon excavation in Korea. The acid drainage causes the acidification and heavy metal contamination of soil, surface water and groundwater, the reduction of slope stability, the corrosion of slope structure, the damage on plant growth, the damage on landscape and the deterioration of concrete and asphalt pavement. The countermeasure for acid drainage is the treatment of acid drainage and the prevention of acid drainage. The treatment of acid drainage can be classified into active and passive treatments depending on the degree of natural process in the treatment. Removal of oxidants, reduction of oxidant generation and encapsulation of sulfide are employed for the prevention of acid drainage generation.

Development of Optimum Grip System in Developing Design Tensile Strength of GFRP Rebars (GFRP 보강근의 설계 인장강도 발현을 위한 적정 그립시스템 개발)

  • You Young-Chan;Park Ji-Sun;You Young-Jun;Park Young-Hwan;Kim Keung-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.6 s.90
    • /
    • pp.947-953
    • /
    • 2005
  • Previous test results showed that the current ASTM(American Standard for Testing and Materials) grip adapter for GFRP(Glass Fiber Reinforced Polymer) rebar was not fully successful in developing the design tensile strength of GFRP rebars with reasonable accuracy. It is because the current ASTM grip adapter which is composed of a pair of rectangular metal blocks of which inner faces are grooved along the longitudinal direction does not take into account the various geometric characteristics of GFRP rebar such as surface treatment, shape of bar cross section as well as physical characteristics such as poisson effect, elastic modulus in the transverse direction and so on. The objective of this paper is to provide how to proportion the optimum diameter of inner groove in ASTM grip adapter to develop design tensile strength of GFRP rebar. The proportioning of inner groove in ASTM grip adapter is based on the force equilibrium of GFRP rebar between tensile capacity and minimum frictional resistance required along the grip adapter. The frictional resistance of grip adapter is calculated based on the compressive strain compatibility in radial direction induced by the difference between diameter of GFRP rebar and inner groove In ASTM grip. All testing procedures were made according to the CSA S806-02 recommendations. From the preliminary test results on round-type GFRP rebars, it was found that maximum tensile loads acquired under the same testing conditions is highly affected by the diameter of inner groove in ASTM grip adapter. The grip adapter with specific dimension proportioned by proposed method recorded the highest tensile strength among them.