• Title/Summary/Keyword: Coarse particle

Search Result 413, Processing Time 0.025 seconds

Concentration Characteristics and Health Effect Assessment of Atmospheric Particulate Matters During Asian Dust Storm Episodes (황사 에피소드 발생시 대기먼지의 농도 특성과 인체 영향)

  • Kang, Gong-Unn
    • Journal of Environmental Health Sciences
    • /
    • v.35 no.1
    • /
    • pp.21-35
    • /
    • 2009
  • The Asian dust storms which originated in the deserts of Mongolia and China transported particles to Korea and led to a high concentration of atmospheric particulate matters (PM) of more than $1000{\mu}g/m^3$ throughout the country in the spring, of 2007. Public concern, in Korea, about the possible adverse effects of these dust events has increased, as these dust storms can contain various air pollutants emitted from heavily industrialized eastern China. The objectives of this study were to understand the concentration characteristics of PM as a function of particle size between the Asian dust storm episodes and non-Asian dust period and to consider the mass size distribution of PM in the Asian dust storms and their water soluble ion species on the potential, possible effects on deposition levels in the three regions (nasopharyngeal, tracheobronchial, and alveolar) of the human respiratory system. The size distribution of PM mass concentration during the Asian dust storms showed a peak in the coarse particle region due to the long-range transport of soil particles from the deserts of Mongolia and China, which was identified by HYSPLIT-4 model for backward trajectory analysis of air arriving in the sampling site of Iksan. During the non-Asian dust period, there were two different types in PM size distribution: bimodal distribution when low concentrations of $PM_{2.5}$ were observed, while unimodal distribution having a peak in fine particle region when high concentrations of $PM_{2.5}$ were showed. This unimodal distribution with high concentrations of fine particulate and secondary air pollutants such as ${SO_4}^{2-}$, ${NO_3}^-$, ${NH_4}^+$ was found to be due to the long-range transport of air pollutants from industrialized eastern China. During the Asian dust storms, the mean concentrations of PM that can be deposited in the nasopharyngeal, tracheobronchial, and alveolar region were $128.8{\mu}g/m^3$, $216.5{\mu}g/m^3$, and $89.6{\mu}g/m^3$, respectively. During the non-Asian dust period, the mean concentrations of PM that can be deposited in the nasopharyngeal, tracheobronchial, and alveolar region were $8.4{\mu}g/m^3$, $9.5{\mu}g/m^3$ and $38.5{\mu}g/m^3$, respectively.

A Study on the Beneficiation of Illite by Selective Grinding and Air Classification (선택분쇄 및 공기분급에 의한 일라이트의 정제기술 연구)

  • Kim Sang-Bae;Cho Sung-Baek;Kim Wan-Tae;Yoon Sung-Dae
    • Journal of the Mineralogical Society of Korea
    • /
    • v.18 no.1
    • /
    • pp.19-31
    • /
    • 2005
  • A study on the beneficiation of illite occurring in Youngdong province is performed with applying selective grinding and air classification techniques. Quartz and illite are occurred as major components, and sulfide minerals such as pyrite, chalcopyrite are associated as minor components. The result of sieving test shows that contents of Al₂O₃, K₂O and ignition loss are increased, whereas SiO₂ is decreased with particle size decrease. Fe₂O₃ content is almost same in all the particle size range but slightly lower at coarse particles. The yield of fine particles is increased with increasing rotor speed in both grinding stage and air classification stage. When the selective grinding and air classification are carried out at optimal condition, yield of the concentrate is 76.16 wt.%. The chemical compositions of the concentrate are SiO₂70.13%, Al₂O₃ 19.40%, Fe₂O₃ 1.62%, K₂O 5.20%, and ignition loss 2.77%. The beneficiation process developed in the current study is very effective method which purification and particle size control can be achieved simultaneously.

Characteristics of Heat Absorption by Gas in a Directly-irradiated Fluidized Bed Particle Receiver (태양열 유동층 흡열기의 기체 열흡수 특성)

  • Park, Sae Han;Kim, Sung Won
    • Korean Chemical Engineering Research
    • /
    • v.59 no.2
    • /
    • pp.239-246
    • /
    • 2021
  • Characteristics of hydrodynamics and heat absorption by gas in a directly-irradiated fluidized bed particle receiver (50 mm-ID X 150 mm high) of SiC particles have been determined. Solid holdups of SiC particles show almost constant values with increasing gas velocity. Fine SiC particles (SiC II; dp=52 ㎛, ρs=2992 kg/㎥) showed low values of relative standard deviation of pressure drop across bed but high solids holdups in the freeboard region compared to coarse SiC particles (SiC I; dp=123 ㎛, ρs=3015 kg/㎥). The SiC II exhibited higher values of temperature difference normalized by irradiance due to the effect of additional solar heat absorption and heat transfer to the gas by the particles entrained in the freeboard region in addition to the efficient thermal diffusion of the solar heat received at bed surface. Heat absorption rate and efficiency increased with increasing the gas velocity and fluidization number. The SiC II showed maximum heat absorption rate of 17.8 W and thermal efficiency of 14.8%, which are about 33% higher than those of SiC I within the experimental gas velocity range.

Experimental Study on the Development of EMP Shielded Concrete Using Industrial By-products (산업부산물을 사용한 EMP차폐 콘크리트 개발에 관한 실험적 연구)

  • Min, Tae-Beom;Kim, Hyeong-Cheol;Choi, Hyun-Kuk;Roh, Jeong-Heon;Kim, Kuk-Joo;Park, Young-Jun
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.6
    • /
    • pp.477-484
    • /
    • 2019
  • The purpose of this study is to present basic data for developing concrete with EMP shielding as the structure materials when constructing an EMP shielded building structure. In order to use metal-based recycled aggregates with excellent conductivity and easy procurement for EMP shielding concrete, an evaluation of the stability evaluation and EMP shielding performance was performed. Through the stability evaluation, it was found that the coarse aggregate stability criterion was satisfied, but the oxidized slag did not satisfy the fine aggregate stability criterion, the oxidized slag is not satisfied. In addition, as a result of fresh concrete, the workability is increased and the air volume is decreased. The compressive strength is increased due to the high density and coarse granularity of the recycled aggregates, which increased the cement paste and adhesion, thereby increasing the compressive strength. The results of an EMP shielding test show that aggregates with high shielding performance are electronic arc furnace(EAF) Oxidizing Slag and Cooper Slag. The shielding performance is expected to increase if the average particle size of aggregate is small or uniformly distributed.

Factors Affecting Lipid Oxidation In Full-fat Soy Flour (전지 대부분의 유지산화에 미치는 인자)

  • Kim, Chul-Jai;Lee, C.C.;Johnson, L.A.
    • Korean Journal of Food Science and Technology
    • /
    • v.23 no.6
    • /
    • pp.732-738
    • /
    • 1991
  • Corsoy 79 soybeans were ground into 8-(coarse) and 24-mesh (fine) full-fat soy flours. From the particle size analysis, the 8-mesh full-fat soy flours were found to have larger values for geometric mean diameter and geometric standard deviation. However, the distribution moduli of coarse and fine soy flours were similar and indicated soybeans were nearly 'brittle'. Development of hydrolytic and oxidative rancidities of coarsely and finely ground full-fat soy flours were followed from grinding to 24 hrs later. No increases in peroxide value and conjugated dienes in the oil and hexanal content in the headspace of the flour were observed when the moisture was 10.7% or less. At 14.9% moisture and above, lipid oxidation increased with increased moisture content and storage time. Free fatty acid contents increased slightly at all moisture contents. However, hydrolysis did not exceed 0.06% over the moisture range of 4 to 18%, which is of little practical significance. Fine grinding increased oxidative and hydrolytic rancidities, especially at 14.9% moisture and above. these findings indicate that raw soybeans can be ground to full-fat soy flours and stored up to 24 hrs without undergoing significant lipid and flavor deterioration if the moisture content is 11% or less.

  • PDF

Concentration Characteristics of Atmospheric PM2.5, PM10 and TSP during the Asian Dust Storm in Iksan Area (익산지역에서 황사발생시 PM2.5, PM10 TSP의 농도 특성)

  • Kang, Gong-Unn;Kim, Nam-Song;Kim, Kyung-Suk;Kim, Mi-Kyung;Lee, Hyun-Ju
    • Journal of Environmental Health Sciences
    • /
    • v.33 no.5
    • /
    • pp.408-421
    • /
    • 2007
  • The concentration characteristics of atmospheric particle matters (PM) including $PM_{2.5},\;PM_{10}$, and TSP were evaluated through the measurement data of PM_{2.5}$ (fine particulate), PM_{10-2.5}$ (coarse particulate), and PM_{over-10}$ collected using a MCI (multi-nozzle cascade impactor) sampler of a three-stage filter pack in spring of 2006 in Iksan area. During the sampling period of 10-15 March and 24 days from 8 April to 2 May, 32 samples for PM of each size fractions were collected, and then measured for PM mass concentrations and water-soluble inorganic ion species. Average concentrations of $PM_{2.5},\;PM_{10}$, TSP were $57.9{\pm}44.1mg/m^3$, $96.6{\pm}89.1mg/m^3$, and $114.8{\pm}99.7mg/m^3$, respectively. Water-soluble inorganic ion fractions to PM mass were found to be 36.5%, 18.0%, and 11.1% for $PM_{2.5}$, $PM_{10-2.5}$ and $PM_{over-10}$, respectively. By showing the high concentrations of PM samples during Asian dust events, those three fractions of PM were distinguished between the samples of Asian dust event and the samples of no event. However, the increase of PM concentrations observed during Asian dust events showed a different pattern for some Asian dust events. The differences of those three fractions in the size distribution may depend on differences on place of occurrence of Asian dust storm and course of transport from China continent to Iksan area in Korea. However, the extent of PM mass contribution during Asian dust events was generally dominated by the coarse particles rather than the fine fraction of PM. The variations of water-soluble inorganic ion species concentration in those three PM fractions between the samples of Asian dust event and the samples of no event were also discussed in this study.

Development of the Testing Method for Impurity Content in Recycled Aggregate for Concrete Structure (구조체 콘크리트용 순화골재의 이물질 함유량 시험방법 개발)

  • Lee, Do-Heun;Jun, Myoung-Hoon;Jaung, Jae-Dong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.1 no.1
    • /
    • pp.72-80
    • /
    • 2005
  • A recycled aggregate contains impurities that affect negative effects on physical properties of concrete. Therefore, a test method for examining impurities content in recycled aggregate is necessary before use of recycled aggregate. In this study, the test method by visual examination for separating impurities in recycled fine and coarse aggregates was developed. The results of the test are as follow: 1. The current KS F 2576 was necessary for comprehensive revision including types of tested recycled aggregate, definition of terminology, quantity of sample, and test method. 2. Visual examination is appropriate for larger than impurity panicle size of 1.2mm, and the larger panicle size the shorter time was required. 3. For the impurity content test by visual examination, the easiness and accuracy of the test can be obtained from the condition of sample weight of 30 grams with particle size of 2.5mm to 5mm for recycled fine aggregate and the condition of sample weight of 1 kilogram with panicle size of larger than 5mm for recycled coarse aggregate.

  • PDF

The study on the Crushability of Weathered Cranite Soils (화강암질 풍화토의 파쇄성에 관한 연구)

  • 도덕현;강우묵
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.21 no.2
    • /
    • pp.81-103
    • /
    • 1979
  • The weathered granite soil involves problems in its stability in soil structures depending upon the reduction of soil strength due to the water absorption, crushability, and content of colored mineral and feldspar. As an attemt to solve the problems associated with soil stability, the crushability of weathered granite soil was investigated by conducting tests such as compaction test, CBR test, unconfined compression test, direct shear test, triaxial compression test, and permeability test on the five soil samples different in weathering and mineral compositions. The experimental results are summarized as follows: The ratio of increasing dry density in the weathered granite soil was high as the compaction energy was low, while it was low as the compaction energy was increased. The unconfined compressive strength. and CBR value were highest in the dry side rather than in the soil with the optimum moisture content, when the soil was compacted by adjusting water content. However, the unconfined compressive strength of smples, which were compacted and oven dried, were highest in the wet side rather than in soil with the optimum moisture content. As the soil becomes coarse grain, the ratio of specific surface area increased due to increased crushability, and the increasing ratio of the specific surface area decreased as the compaction energy was increased. The highest ratio of grain crushability was attained in the wet side rather than in the soil with the optimum moisture content. Such tendency was transforming to the dry side as the compaction energy was increased. The effect of water on the grain crushability of soil was high in the coarse grained soil. The specific surface area of WK soil sample, when compacted under the condition of air dried and under the optimum moisture content, was constant regardless of the compaction energy. When the weathered granite soil and river sand with the same grain size were compacted with low compaction energy, the weathered granite soil with crushability had higher dry density than river sand. However, when the compaction energy reached to certain point over limitation, the river sand had higher dry density than the weathered granite soil. The coefficient of permeability was lowest in the wet side rather than in the optimum moisture content, when the soil was compacted by adjusting soil water content. The reduction of permeability of soil due to the compaction was more apparent in the weathered granite soil than in the river sand. The highly significant correlation coefficient was obtained between the amount of particle breakage and dry density of the compacted soil.

  • PDF

Experimental Study on the Effect of Degree of Saturation on the Electrical Conductivity of Soils (포화도에 따른 흙의 전기전도도 변화에 대한 실험적 연구)

  • Ko, Hyojung;Choo, Hyunwook
    • Journal of the Korean Geotechnical Society
    • /
    • v.39 no.8
    • /
    • pp.29-39
    • /
    • 2023
  • The degree of saturation determines the connectivity of void space and the particle surface. Thus, it greatly affects the electrical conductivity of soils. This study aimed to analyze the electrical conductivities of coarse grains with a high relevance of pore water conduction and fine grains with a high relevance of surface conduction based on the degree of saturation. It also aimed to express the electrical conductivity of unsaturated soils as a combination of surface and pore water conductions using the modified Archie's equation. Samples were prepared in a plastic cell equipped with four electrodes, and the electrical conductivity was measured based on the porosity at various degrees of saturation (40%~100%). The results demonstrate that Archie's equation can be used to express the electrical conductivity of coarse grains, with a saturation exponent of ~1.93 regardless of the pore water conductivity. However, the saturation exponent of fine grains varied considerably with pore water concentration. This variation can be attributed to the relative magnitude of surface conduction with respect to the electrical conductivity of soils at different pore water concentrations. Thus, the degree of saturation has varying effects on pore water conduction and surface conduction. Therefore, different saturation exponents must be used for pore water conduction and surface conduction to predict the electrical conductivity of unsaturated soils using the modified Archie's equation.

Analysis of Fundamental Properties of Concrete Using Mix of Coarse Aggregate With Formation Causes (성인이 다른 굵은 골재를 혼합사용한 콘크리트의 기초적 특성 분석)

  • Noh, Sang-Kyun;Kim, Young-Hee;Kim, Jeong-Bin;Han, Cheon-Goo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.1
    • /
    • pp.15-21
    • /
    • 2015
  • Recently, attempts of replacing some of natural aggregate with mix of low quality aggregate are carried out for stable supply of aggregate. However, low quality aggregate such as recycled aggregate produced during the disposal process of construction wastes and by-product aggregate produced by industrial activities has problem of failing to comply to KS Standards. Therefore, we have compared fundamental properties of concrete by using granite crushed aggregate, recycled aggregate, blast furnace and electric arc furnace slag aggregate for effective utilization of lacking aggregate resources. As the result, slump in case of mixed use of aggregate was increased 0~10% compared to single use. Therefore, it is judged to be economically advantageous as it can expect effects in unit quantity or reduction of SP agent. Compressive strength in case of mixed use of aggregate was increased 0~10% compared to single use as it filled internal crevice of concrete with continuous particle size distribution. Accordingly, if we utilize by satisfying standard particle scope through mix of aggregate with different cause of formation in proper ratio, it was possible to confirm utility of mixed aggregate with demonstration of effects of increases of fluidity and compressive strength of concrete.