• 제목/요약/키워드: Coarse aggregate content

검색결과 140건 처리시간 0.029초

재생굵은골재를 사용한 초유동 콘크리트의 유동성 (Fluidity of Super Flow Concrete Using Recycled Coarse Aggregate)

  • 성찬용;박일순
    • 한국농공학회논문집
    • /
    • 제47권2호
    • /
    • pp.55-61
    • /
    • 2005
  • This study was performed to evaluate fluidity of super flow concrete using recycled coarse aggregate. The unit weight was $2,246{\sim}2,344\;kg/m^3$, the unit weights of these concrete were decreased with increasing the content of fly ash and recycled coarse aggregate. The slump flow was $58{\sim}63\;cm$, the Box type passing was $3.4{\sim}6.8\;cm$, respectively. The L type compacting was excellent in the fly ash content $10\%\;and\;20\%$, but, it was showed in good in the fly ash content $30\%$. The super flow concretes using recycled coarse aggregate were improved by substitution in the range of less than the fly ash content $20\%$ and recycled coarse aggregate content $75\%$. This recycled coarse aggregate can be used for super flow concrete.

재생굵은골재를 사용한 초유동 콘크리트의 강도 및 비파괴 특성 (Strengths and Non-destruction Properties of Super Flow Concrete Using Recycled Coarse Aggregate)

  • 성찬용
    • 한국농공학회논문집
    • /
    • 제47권1호
    • /
    • pp.25-32
    • /
    • 2005
  • This study was performed to evaluate strengths and non-destruction properties of super flow concrete using recycled coarse aggregate. At the curing age of 28 days, the compressive strength was 22.7-37.5 MPa, the splitting tensile strength was $2.65\~3.73$ MPa, the flexural strength was $5.78\~6.86$ MPa, the ultrasonic pulse velocity was $3,103\~3,480$ mis, the dynamic modulus of elasticity was $3.401{\times}104\~4.521{\times}104$MPa, respectively. The strengths, ultrasonic pulse velocity and dynamic modulus of elasticity of super flow concrete were decreased with increasing the content of recycled coarse aggregate. The super flow concretes using recycled coarse aggregate were improved by substitution in the range of less than the fly ash content 30010 and recycled coarse aggregate content $75\%$.

굵은 골재 입형 개선이 고성능콘크리트의 충전특성에 미치는 영향 (Influence of the Improveal Grain Shape of Coarse Aggregates on Compactability of High Performance Concrete)

  • 이승한;김희중;정용욱
    • 콘크리트학회논문집
    • /
    • 제12권4호
    • /
    • pp.103-111
    • /
    • 2000
  • The influence of the improvement of grain shape of the coarse aggregate to the unit powder content of concrete and the fine aggregate ratio for the increase of the flowability and segregation resistance of high performance concrete was examined. According to the experimental results, flowability and compacting of concrete presents best states in the S/a which has the smallest 패야 ratio. The coarse aggregate after improvement of grain shape, that has changed from the 0.68 of spherical rate of disk shape to 0.73, led fine aggregate ratio to be down 6% (i.e from 47% to 41%). The improvement of grain shape of the coarse aggregate also led the lowest unit powder content to be down 60kg/㎥ (ie from 530kg/㎥ to 470kg/㎥). And approximate 10% of unit water content has been reduced as unit powder content was down. However, the compressive strength after the improvement of grain shape of the coarse aggregate decreased to 5% due to decrease of adhesiveness of the aggregate and cement paste.

재생굵은골재를 사용한 고강도 콘크리트의 동결융해 특성 (Freezing and Thawing Properties of High Strength Concrete Using Recycled Coarse Aggregate)

  • 성찬용;임상혁
    • 한국농공학회논문집
    • /
    • 제46권2호
    • /
    • pp.59-66
    • /
    • 2004
  • This study was performed to evaluate the freezing and thawing properties of the high strength concrete using recycled coarse aggregate. The recycled coarse aggregate replaced natural crushed aggregate by 0%, 25%, 50%, 75% and 100%. The compressive strength of the concrete using recycled coarse aggregate showed more than 300 kgf/$cm^2$ at the curing age 28 days. The mass loss ratio by freezing and thawing was less than 1% at all mix type. The relative dynamic modulus of elasticity was decreased with increasing the freezing and thawing cycles. Also, the durability factor by the freezing and thawing was decreased with increasing the content of recycled coarse aggregate. But, the recycled concrete except 100% recycled coarse aggregate showed 60 or more durability factor in the freezing and thawing 300 cycles. Accordingly, these recycled coarse aggregate can be used for high strength concrete.

폴리프로필렌 섬유보강 환경친화형 포장재료의 개발 (Development of Polypropylene Fiber Reinforced Environmental Friendly Pavement Material for Farm Road)

  • 성찬용;김영익
    • 한국농공학회논문집
    • /
    • 제46권1호
    • /
    • pp.35-40
    • /
    • 2004
  • This study is performed to examine the physical and mechanical properties of eco-concrete using soil, natural coarse aggregate, excellent soil compound and polypropylene fiber. The test result shows that mass loss ratio is decreased with increasing the content of coarse aggregate and excellent soil compound. The compressive and flexural strengths are increased with increasing the content of coarse aggregate, excellent soil compound and polypropylene fiber. The coefficient of permeability is decreased with increasing the content of coarse aggregate and excellent soil compound, but it is increased in 0.2% polypropylene fiber content. The lowest coefficient of permeability is showed in $5.066\times 10^{-9}$cm/s. These eco-concrete can be used for farm road.

고유동콘크리트의 충전특성에 미치는 골재 입형의 영향 (The Influence of the Aggregate Grain Shape on Compactability of High Flowing Concrete)

  • 이승한;정용욱;이원기
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.21.2-274
    • /
    • 1999
  • This study aims to examine the influence of the unit powder content of concrete and the fine aggregate ration of high flowing concrete after the improvement of grain shape of the coarse aggregate. According to the experimental results, flowbility and compating of concrete presents the best states in the S/a which has the smallest void ratio. The coarse aggregate after improvement of grain shape has been changed from 0.68 circular ratio of disc shape to 0.73 circular shape. It lead to be down 6% of fine aggregate ratio (from 47% to 41%), which is satisfactory to compacting. Also, the improvement of grain shape of the coarse aggregate lead the lowest unit powder content to be down 60kg/㎥ from (530kg/㎥ to 470kg/㎥). And about 11% unit water content can be reduced as unit powder conent is down.

  • PDF

Use of waste glass as coarse aggregate in concrete: mechanical properties

  • Yan, Lan-lan;Liang, Jiong-Feng
    • Advances in concrete construction
    • /
    • 제8권1호
    • /
    • pp.1-7
    • /
    • 2019
  • The possibility of using recycled coarse glass aggregates as a substitute for natural crushed stone are relatively limited. In order to promote it for engineering application, this paper reports the effect of coarse glass aggregate on mechanical behavior of concrete. The coarse aggregates are substituted for coarse glass aggregate (CGA) as 0%,20%,40%,60%,80% and 100%.The results show that increasing the coarse glass aggregate content cause decrease in compressive strength, the elastic modulus, the splitting tensile strength, the flexural strength. An equation is presented to generate the relationship between cube compressive strength and prism compressive strength, the relationship between cube compressive strength and elastic modulus, the relationship between cube compressive strength and splitting tensile strength, the relationship between cube compressive strength and flexural strength of coarse glass concrete.

잔골재 조립율 및 굵은골재 입형이 콘크리트의 특성에 미치는 영향 (The Effect on the Properties of Concrete by Fine Aggregate Fineness Modulus and Grain Shape of Coarse Aggregate)

  • 정용욱;윤용호;이승한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.102-105
    • /
    • 2003
  • The purpose of this study is to examine the influence of the flowability and the compressive strength of concrete after the improving of grain shape of the coarse aggregate and fine aggregate fineness modulus. According to the experimental results, the coarse aggregate after improvement of grain shape it lead to be down by 6% fine aggregate ratio, from 47% to 41%. The 0.5% increase of fine aggregate fineness modulus lead to 3% increase of concrete slump, and 1% reduction of concrete air content. While compressive strength on fine aggregate fineness modulus, it was increased until fineness modulus 3.0, but after it reached by 3.5 it was decreased. The compressive strength of the coarse aggregate after improving the grain shape was decreased by 6% due to loss of the adhesion of cement paste.

  • PDF

복합이론에 의한 순환골재 콘크리트의 탄성계수 평가에 관한 기초적 연구 (A Basic Study for evaluation on the Elastic Modulus of Recycled Aggregate Concrete by using Composite Model)

  • 김현욱;김지윤;김완기;박원준
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 추계 학술논문 발표대회
    • /
    • pp.73-74
    • /
    • 2012
  • The elastic modulus of recycled aggregate concrete (RAC) can be evaluated by using composite models with experiment. In this study, Hashin's composite model was adapted to evaluate elastic modulus considering physical properties of recycled coarse aggregate (RCA) that mortar is attached. Elastic modulus testes for cement paste, mortar and recycled coarse aggregate concrete were carried out considering W/C and recycled coarse aggregate content rate. As a result, the elastic modulus of RAC was evaluated comparing with both experiment results and the existing estimation formula. Those can be used for further studies as a preliminary data.

  • PDF

폴리프로필렌 섬유보강 에코콘크리트의 동결융해 특성 (Freezing and Thawing Properties of Polypropylene Fiber Reinforced Eco-concrete)

  • 성찬용
    • 한국농공학회논문집
    • /
    • 제48권2호
    • /
    • pp.59-66
    • /
    • 2006
  • This study is performed to evaluate freezing and thawing properties of polypropylene fiber reinforced eco-concrete using soil, natural coarse aggregate, soil compound and polypropylene fiber. The mass loss ratio is decreased with increasing the content of natural coarse aggregate and soil compound, but it is increased with increasing the content of polypropylene fiber. The ultrasonic pulse velocity, dynamic modulus of elasticity and durability factor are increased with increasing the content of natural coarse aggregate and soil compound, but it is decreased with increasing the content of polypropylene fiber. The mass loss ratio, ultrasonic pulse velocity, dynamic modulus of elasticity and durability factor are $1.49{\sim}3.32%,\;1,870{\sim}2,465\;m/s,\;77X10^2{\sim}225X10^2\;MPa\;and\;84.6{\sim}92.8$ after freezing and thawing 300 cycles, respectively. These eco-concrete can be used for environment-friendly side walk and farm road.