  • Purpose: The objective of this study was to investigate the effects of calcium phosphate coated titanium implant surface on bone response and implant stability at early stage of healing period of 3 weeks and later healing period of 6 weeks. Material and methods: A total of 24 machined, screw-shaped implants (Dentium Co., Ltd., Seoul, Korea) which dimensions were 3.3 mm in diameter and 5.0 mm in length, were used in this research. All implants (n = 24), made of commercially pure (grade IV) titanium, were divided into 2 groups. Twelve implants (n = 12) were machined without any surface modification (control). The test implants (n = 12) were anodized and coated with thin film (150nm) of calcium phosphate by electron-beam deposition. The implants were placed on the proximal surface of the rabbit tibiae. The bone to implant contact (BIC) ratios was evaluated after 3 and 6 weeks of implant insertion. Results: The BIC percentage of calcium phosphate coated implants ($70.8{\pm}18.9%$) was significantly higher than that of machined implants ($44.1{\pm}16.5%$) 3 weeks after implant insertion (P = 0.0264). However, there was no significant difference between the groups after 6 weeks of healing (P > .05). Conclusion: The histomorphometric evaluation of implant surface revealed that; 1. After 3 weeks early healing period, bone to implant contact (BIC) percentage of calcium phosphate coated implants (70.8%) was much greater than that of surface untreated machined implants (44.1%) with P = 0.0264. 2. After 6 weeks healing period, however, BIC percentage of calcium phosphate coated implants group (79.0%) was similar to the machined only implant group (78.6%). There was no statistical difference between two groups (P = 0.8074). 3. We found the significant deference between the control group and experimental group during the early healing period of 3 weeks. But no statistical difference was found between two groups during the later of 6 weeks.

Evaluation of buccal mucoadhesive [P(AA-co-PEGMM)] copolymer films containing butorphanol tartrate (Butolphanol tartrate 함유 구강점막 점착성 [P(AA-co-PEGMM)] 공중합체 필름의 평가)

  • Kim, Joun-Sik;Han, Kun
    • Journal of Pharmaceutical Investigation
    • /
    • v.32 no.1
    • /
    • pp.1-6
    • /
    • 2002
  • The mucoadhesive characteristics of [P(AA-co-PEGMM)] films by estimating the glass transition temperature $(T_g)$, analyzing surface energy and studying FT-IR was previously reported. In this study, the possibility of buccal mucoadhesive dosage form of [P(AA-co-PEGMM)] films by mucoadhesive force measurements and dissolution tests were also investigated. Mucoadhesiveness of [P(AA-co-PEGMM)] films was compared with cr-PAA and cr-PEGMM films crosslinked with 3% ethyleneglycol dimethacrylate (EGDMA). The buccal mucoadhesive force of [P(AA-co-PEGMM)] films increased with increasing content of PEGMM. [P{AA-co-PEGMM (18 mole%)}] films showed a significantly greater mucoadhesiveness than cr-PAA and cr-PEGMM films. The mucoadhesive force measured in normal saline (pH 5.0) was higher than that measured in phosphate buffer (pH 6.8) because of the pH dependence of hydrogels with carboxyl ions within the PAA. Moreover, the mucoadhesive force of [P{AA-co-PEGMM (18 mole%)}] films was at maximum after 2 hr attachment of buccal mocosa and it was maintained over $1\;N/cm^2$ for up to 10 hr. In dissolution studies, the release of butorphanol tartrate from [P(AA-co-PEGMM)] films increased with increasing PEGMM content, and films prepared with 18 mole% PEGMM gave almost zero order release kinetics.

Synergistic effect of phosphate solubilization by Burkholderia strains isolated from button mushroom bed (양송이배지로부터 분리한 Burkholderia균의 인산가용화 공조효과)

  • Park, Ji-Hoon;Han, Chang-Hoon;Yoon, Min-Ho
    • Journal of Mushroom
    • /
    • v.15 no.4
    • /
    • pp.183-189
    • /
    • 2017
  • This study investigated the synergistic effect of single inoculation and co-inoculation of phosphate-solubilizing bacteria (PSB) Burkholderia metallica JH-7 and Burkholderia contaminans JH-15. Phosphate-solubilizing abilities of these strains were assessed by measuring phosphorus content in culture media that were singly inoculated or co-inoculated with these strains for 7 days. B. metallica JH-7 was found to release the highest content of soluble phosphorus ($140.80{\mu}g\;mL^{-1}$ ) into the medium, followed by single inoculation of B. contaminans JH-15 ($135.95{\mu}g\;mL^{-1}$ ) and co-inoculation of two strains ($134.84{\mu}g\;mL^{-1}$ ). The highest pH reduction, organic acid production, and glucose consumption were observed in the medium inoculated with B. metallica JH-7 alone compared with that in the medium co-inoculated with both the strains. Results of a plant growth promotion bioassay showed 17.4% and 7.48% higher leaf and root growth, respectively, in romaine lettuce inoculated with B. metallica JH-7 alone than in romaine lettuce inoculated with a control strain. However, no significant difference was observed between single inoculation and co-inoculation of these strains with respect to phosphorus release and plant growth. Although the results of the present study did not show the synergistic effect of phosphate solubilization by the PSB strains examined, these results indicate that treatment with PSB exerts a beneficial effect on crop growth.

Study of the corrosion effect of CO2 stream with SO2 and NO2 on a phosphate coated steel tube (SO2 및 NO2 포함 고압 CO2 스트림이 인산염 코팅 CO2 수송관 부식에 미치는 영향)

  • Cho, Meang-Ik;Kang, Seong-Gil;Huh, Cheol;Baek, Jong-Hwa
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.15 no.12
    • /
    • pp.6973-6979
    • /
    • 2014
  • To mitigate global warming and climate change, many countries are investing massively on the development of CCS technology, which is assumed to be the key technology to reduce $CO_2$ emissions. CCS technology is comprised of the capture, transport, and storage processes. During the capture process, impurities other than $CO_2$ are inevitably flowed into the $CO_2$ stream. In the present study, corrosion characteristics of a phosphate coated tube for $CO_2$ transportation was investigated with a $CO_2$ stream composed of $CO_2$, $H_2O$, $SO_2$, and $NO_2$. The test specimen was a phosphate coated steel tube, which was filled with $CO_2$ stream with the impurities mentioned above. SEM-EDS analysis is conducted to investigate the corrosion behavior. The results showed that although the H2O concentration did not exceed the solubility limit, corrosion occurred in the specimen, which has an inflow of $SO_2$ or $NO_2$. This suggests that the $SO_2$, $NO_2$ and $H_2O$ concentration should be strictly controlled. These results suggest that the $SO_2$ and $NO_2$ concentration should be controlled below 175ppm and 65ppm, respectively.

The Current Problems of Chemical Fertilizer Supply and Consumption in Korea (비료수급정책(肥料需給政策)의 현황(現況)과 대책)

  • Kim, Dong-Hi
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.15 no.1
    • /
    • pp.16-33
    • /
    • 1982
  • The major problems of chemical fertilizer supply and consumption involved in price policies since the end of World War II in Korea and their solutions were extensively discussed. The period was divided into three sub-periods: 1946-1960, 1961-1967 and 1968 to present. Since 1968 when the operations of three large-scaled fertilizer plants: Yongnam Chemical Co., Chinhae Chemical Co. and Hankuk Fertilizer Co. were begun in full scale, the domestic supply of nitrogen and phosphate fertilizers were almost enough for the domestic demand. However, since 1976, when Namhae Chemical Co. was added to the production capacity, the fertilizer industry has been faced with the overproduction problem of nitrogen, and the high production cost due to high petroleum price, which gave financial difficulties. Several policy directions and alternative measures for solving the current problems were also suggested in this presentation.

  • PDF

Evaluation of Physical Properties of Mucosal Adhesive Tablets (II):-Dissolution Rate- (점막 부착정제의 물성평가(II):- 용출속도-)

  • Park, Kwang-Sin;Chung, Bee-Hwan;Cha, Bong-Jin;Kwon, Jong-Won
    • Journal of Pharmaceutical Investigation
    • /
    • v.23 no.1
    • /
    • pp.55-59
    • /
    • 1993
  • Dissolution of mucosal adhesive tablets prepared with two polymers using hydroxypropylcellulose-H (HPC) and carbopol 934 (CP) was tested. Adhesive tablets containing HPC/CP and brilliant blue FCF (BB) were prepared from direct compression. Three factors of polymer ratio (HPC:CP), BB content and compression force were chosen as important factors of preparation and factorial analysis for these factors was carried out. Eight kinds of formulations from different combinations of three factors were prepared and dissolution test in pH 6.8 phosphate buffer solution was performed. Dissolution rate was significantly affected by HPC:CP ratio and BB content, but was not affected by compression force.

  • PDF

Cell Performances of Surface-Treated $LiNi_{1/3}Mn_{1/3}Co_{1/3}O_2$ Material for Li Secondary Battery (리륨이차전지용 $LiNi_{1/3}Mn_{1/3}Co_{1/3}O_2$ 양극활물질의 표면개질에 따른 전지특성)

  • Kim, Hyun-Soo;Kong, Ming-Zhe;Kim, Ke-Tack;Moon, Seong-In
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.294-295
    • /
    • 2007
  • $LiNi_{1/3}Mn_{1/3}Co_{1/3}O_2$ material was surface modified with Zr-phosphate. Scanning electron microscope, energy dispersive spectroscopy and electrochemical studies indicate that surface modification improve the rate capability. Electrochemical studies were performed by assembling 2032 coin cells with lithium metal as an anode.

  • PDF

A Study on Phosphate Removal Characteristic of EAF Slag for Submarine Cover Material (EAF Slag의 해양복토제 활용을 위한$PO_4{^-}-P$ 제거특성에 관한 연구)

  • Kim, Jae-Won;Seo, Jong-Beom;Kang, Min-Gyeong;Kim, In-Deuk;Oh, Kwang-Joong
    • Clean Technology
    • /
    • v.16 no.4
    • /
    • pp.258-264
    • /
    • 2010
  • This study estimated the possibility of phosphate removal characteristics to utilize EAF(electric arc furnace) slag as submarine cover material. The major phosphate removal mechanism was a certain formation of HAP precipitation occurred by the ionization reaction between $Ca^{2+}$ and $OH^-$, which were leached from the EAF Slag. Another phosphate removal mechanism was the adsortion of EAF slag surface. As a result of $PO_4{^-}-P$ removal characteristics using continuous column reactor, $PO_4{^-}-P$ concentration decreased rapidly after 3 days and 10 days later, it show under 0.5 ppm. The result as applied in real sea water, shows that the phosphate removal effects were 93~98% by the subaqueous sediment removal using the EAF slag. In conclusion, EAF slag is useful in $PO_4{^-}-P$ removal and control and it is possible to use without additional process like crush and selection.

Catalytic properties of wheat phytase that favorably degrades long-chain inorganic polyphosphate

  • An, Jeongmin;Cho, Jaiesoon
    • Asian-Australasian Journal of Animal Sciences
    • /
    • v.33 no.1
    • /
    • pp.127-131
    • /
    • 2020
  • Objective: This study was conducted to determine catalytic properties of wheat phytase with exopolyphosphatase activity toward medium-chain and long-chain inorganic polyphosphate (polyP) substrates for comparative purpose. Methods: Exopolyphosphatase assay of wheat phytase toward polyP75 (medium-chain polyP with average 75 phosphate residues) and polyP1150 (long-chain polyP with average 1150 phosphate residues) was performed at pH 5.2 and pH 7.5. Its activity toward these substrates was investigated in the presence of Mg2+, Ni2+, Co2+, Mn2+, or ethylenediaminetetraacetic acid (EDTA). Michaelis constant (Km) and maximum reaction velocity (Vmax) were determined from Lineweaver-Burk plot with polyP75 or polyP1150. Monophosphate esterase activity toward p-nitrophenyl phosphate (pNPP) was assayed in the presence of polyP75 or polyP1150. Results: Wheat phytase dephosphorylated polyP75 and polyP1150 at pH 7.5 more effectively than that at pH 5.2. Its exopolyphosphatase activity toward polyP75 at pH 5.2 was 1.4-fold higher than that toward polyP1150 whereas its activity toward polyP75 at pH 7.5 was 1.4-fold lower than that toward polyP1150. Regarding enzyme kinetics, Km for polyP75 was 1.4-fold lower than that for polyP1150 while Vmax for polyP1150 was 2-fold higher than that for polyP75. The presence of Mg2+, Ni2+, Co2+, Mn2+, or EDTA (1 or 5 mM) exhibited no inhibitory effect on its activity toward polyP75. Its activity toward polyP1150 was inhibited by 1 mM of Ni2+ or Co2+ and 5 mM of Ni2+, Co2+, or Mg2+. Ni2+ inhibited its activity toward polyP1150 the most strongly among tested additives. Both polyP75 and polyP1150 inhibited the monophosphate esterase activity of wheat phytase toward pNPP in a dose-dependent manner. Conclusion: Wheat phytase with an unexpected exopolyphosphatase activity has potential as a therapeutic tool and a next-generational feed additive for controlling long-chain polyP-induced inappropriate inflammation from Campylobacter jejuni and Salmonella typhimurium infection in public health and animal husbandry.

Effect of Type I Collagen on Hydroxyapatite and Tricalcium Phosphate Mixtures in Rat Calvarial Bony Defects

  • Kim, Jung-Hwan;Kim, Soung-Min;Kim, Ji-Hyuck;Kwon, Kwang-Jun;Park, Young-Wook
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.34 no.1
    • /
    • pp.36-48
    • /
    • 2008
  • To repair bone defects in the oral and maxillofacial field, bone grafts including autografts, allografts, and artificial bone are used in clinical dentistry despite several disadvantages. The purpose of this study was to evaluate new bone formation and healing in rat calvarial bone defects using hydroxyapatite (HA, $Ca_{10}[PO_4]_6[OH]_2,\;Bongros^{(R)}$, Bio@ Co., KOREA) and tricalcium phosphate (${\beta}-TCP,\;Ca_3[PO_4]_2$, Sigma-Aldrich Co., USA) mixed at various ratios. Additionally, this study evaluated the effects of type I collagen (Rat tail, BD Biosciences Co., Sweden) as a basement membrane organic matrix. A total of twenty, 8-week-old, male Sprague-Dawley rats, weighing 250-300g, were divided equally into a control group (n=2) and nine experimental groups (n=2, each). Bilateral, standardized transosseous circular calvarial defects, 5.0 mm in diameter, were created. In each experimental group, the defect was filled with HA and TCP at a ratio of 100:0, 80:20, 70:30, 60:40, 50:50, 40:60, 30:70, 20:80, and 0:100 with or without type I collagen. Rats were sacrificed 4 and 8 weeks post-operation for radiographic (standardized plain film, Kodak Co., USA), histomorphologic (H&E [Hematoxylin and Eosin], MT [Masson Trichrome]), immunohistochemical staining (for BMP-2, -4, VEGF, and vWF), and elementary analysis (Atomic absorption spectrophotometer, Perkin Elmer AAnalyst $100^{(R)}$). As the HA proportion increased, denser radiopacity was seen in most groups at 4 and 8 weeks. In general radiopacity in type I collagen groups was greater than the non-collagen groups, especially in the 100% HA group at 8 weeks. No new bone formation was seen in calvarial defects in any group at 4 weeks. Bridging bone formation from the defect margin was marked at 8 weeks in most type I collagen groups. Although immunohistochemical findings with BMP-2, -4, and VEGF were not significantly different, marked vWF immunoreactivity was present. vWF staining was especially strong in endothelial cells in newly formed bone margins in the 100:0, 80:20, and 70:30 ratio type I collagen groups at 8 weeks. The calcium compositions from the elementary analysis were not statistically significant. Many types of artificial bone have been used as bone graft materials, but most of them can only be applied as an inorganic material. This study confirmed improved bony regeneration by adding organic type I collagen to inorganic HA and TCP mixtures. Therefore, these new artificial bone graft materials, which are under strict storage and distribution systems, will be suggested to be available to clinical dentistry demands.