Sn 및 Cu를 첨가한 치과 주조용 Co-Cr-Mo계 합금제조 및 용해과정 분석 (Manufactures of dental casting Co-Cr-Mo based alloys in addition to Sn, Cu and analysis of infrared thermal image for melting process of its alloys)

  • 강후원;박영식;황인;이창호;허용;원용관
    • 대한치과기공학회지
    • /
    • 제36권3호
    • /
    • pp.141-147
    • /
    • 2014
  • Purpose: Dental casting #Gr I (Co-25Cr-5Mo-3Sn-1Mn-1Si), #Gr II (Co-25Cr-5Mo-5Cu-1Mn -1Si) and #Gr III (Co-25Cr-5Mo-3Sn-5Cu-1Mn-1Si) master alloys of granule type were manufactured the same as manufacturing processes for dental casting Ni-Cr and Co-Cr-Mo based alloys of ingot type. These alloys were analyzed melting processes with heating time of high frequency induction centrifugal casting machine using infrared thermal image analyzer. Methods: These alloys were manufactured such as; alloy design, the first master alloy manufatured using vacuum arc casting machine, melting metal setting in crucible, melting in VIM, pouring in the mold of bar type, cutting the gate and runner bar and polishing. These alloys were put about 30g/charge in the ceramic crucible of high frequency induction centrifugal casting machine and heat, Infrared thermal image analyzer indicated alloys in the crucible were set and operated. Results: The melting temperatures of these alloys measuring infrared thermal image analyzer were decreased in comparison with remanium$^{(R)}$ GM 800+, vera PDI$^{TM}$, Biosil$^{(R)}$ f, WISIL$^{(R)}$ M type V, Ticonium 2000 alloys of ingot type and vera PDS$^{TM}$(Aabadent, USA), Regalloy alloys of shot type. Conclusion: Co-Cr-Mo based alloy in addition to Sn(#Gr I alloy) were decreased the melting temperature with heating time of high frequency induction centrifugal casting machine using infrared thermal image analyzer.

CoCrW와 CoCrMo 합금의 트라이볼로지 특성 평가 (Assessment of Tribological Characteristics of CoCrW and CoCrMo Alloys)

  • 권동균;오세진;정구현
    • Tribology and Lubricants
    • /
    • 제38권4호
    • /
    • pp.162-169
    • /
    • 2022
  • Cobalt-chromium (CoCr)-based alloys have been used for wear applications because of their excellent mechanical properties and wear resistance. With growing concern over environmental problems, CoCr alloys are expected to be used for various tribological applications in degraded lubrication states. To expand the applicability of the materials, data should be accumulated across a broad spectrum of experimental parameters. In this work, the friction and wear characteristics of cobalt-chromium-tungsten (CoCrW) and cobalt-chromium-molybdenum (CoCrMo) alloys are investigated experimentally. The tests are conducted using a pin-on-reciprocating-plate tribotester in dry lubrication. CoCrW and CoCrMo are used as pin and plate materials to investigate the effect of the counter material. The results show that the friction coefficients between CoCrW and CoCrMo generally range from 0.4 to 0.5. The friction coefficient between the CoCrW pin and plate is found to be slightly small. However, the total wear between the CoCrW pin and plate is found to be the largest. In contrast, the total wear between the CoCrW pin and plate is relatively small. Furthermore, CoCrW may cause a faster wear progression of CoCrMo, especially for the case in which CoCrMo is used as the pin material. The results of this work provide a better understanding of the tribological properties of CoCrW and CoCrMo alloys. In addition, this work provides a practical guideline for the use of CoCrW and CoCrMo from the tribological design viewpoint.

도재소부용 Ni-Cr-Mo계 치과용 합금의 미세조직 및 기계적성질 (Microstructure and Mechanical Properties of Ni-Cr-Mo Based Dental Cast Iron for Porcelain-Fused-to-Metal Firing)

  • 최답천
    • 한국주조공학회지
    • /
    • 제27권3호
    • /
    • pp.120-125
    • /
    • 2007
  • The microstructure, mechanical properties and melting range of Ni-Cr-Mo based alloys were investigated to develop Be-free Ni-Cr-Mo base dental alloys for Porcelain-Fused-to-Metal Firing(PFM). All as-cast alloys showed dendritic structure. Rockwell hardness of 20Cr7Mo was increased with addition of Si and Ti. On the contrary, it was decreased with addition of Co. The duplex alloying elemental addition such as 3Co + xTi, 2Si + xCo and 2Si + xTi to 20Cr7Mo resulted in much increase of hardness. Rockwell hardness and compressive strength for 20Cr3CoSiTi or 17Cr6CoSiTi alloy that add Si-Ti had similar values compared to the commercial alloys. Melting range for 20Cr3CoSiTi and 17Cr6CoSiTi alloy that add Si-Ti showed similar or lower than commercial alloys. In conclusion, 20Cr3CoSiTi and 17Cr6CoSiTi alloys can be applied for commercial use.

SH(shear horizontal) 초음파를 이용한 압력용기용 재료의 피로손상 예측 (The Prediction of Fatigue Damage for Pressure Vessel Materials using Shear Horizontal Ultrasonic Wave)

  • 강용호;정용근;송정일
    • 한국정밀공학회지
    • /
    • 제26권6호
    • /
    • pp.90-96
    • /
    • 2009
  • Ultrasonic method using SH(shear horizontal) wave has been developed to determine the surface damage in fatigued material. Fatigue damages based on propagation energy were analyzed by multi-regression analysis in interrupted fatigue test specimen including CrMoV and 12Cr alloy steel. From the test results, as the fatigue damage increased the propagation time of the launched waves increased and amplitude of wavelet decreased. Also, analysis for the waveform modulation showed a reliable estimation, with confidence limit of 97% for 12Cr steel and 95% for CrMoV steel, respectively. Therefore, It is thought that SH ultrasonic wave technique can be applied to determine fatigue damage of in-service component nondestructively.

치과용 고주파 주조기를 이용한 Co-Cr-Mo계 합금 용해과정의 적외선 열화상 분석 (Analysis of infrared thermal image for melting processes of Co-Cr-Mo based alloy using high frequency induction casting machine)

  • 강후원;박영식;황인;이창호;허용;원용관
    • 대한치과기공학회지
    • /
    • 제36권3호
    • /
    • pp.149-158
    • /
    • 2014
  • Purpose: Dental casting Co-Cr-Mo based alloys of five kinds of ingot type and two kinds of shot type were analyzed the melting processes with heating time of high frequency induction centrifugal casting machine using infrared thermal image analyzer. Methods: When Co-Cr-Mo based alloys were put about 30g/charge in the ceramic crucible of high frequency induction centrifugal casting machine and heat, Infrared thermal image analyzer and IR thermometer indicated these alloys in the crucible were set and operated. Results: The melting temperatures of alloys measuring infrared thermal image analyzer were deviated ${\pm}10^{\circ}C$ compared to those of manufacturing company. On the other hand, the melting time of alloys were differently appeared with the shape of alloys(ingot and shot type). Conclusion: The melting temperatures of dental Co-Cr-Mo based alloys were measured the degree of $1,360{\sim}1410^{\circ}C$ and the heating time with the alloys of ingot and shot type were deviated ${\pm}10sec$.

CoCr 기반 합금의 초기 마모 특성에 대한 정량적 평가 (Quantitative Assessment of Initial Wear Characteristics of CoCr-Based Alloys)

  • 차수빈;김회진;후인 옥-팟;정구현
    • Tribology and Lubricants
    • /
    • 제36권4호
    • /
    • pp.199-206
    • /
    • 2020
  • CoCr-based alloys have been developed as wear-resistant materials owing to their excellent mechanical properties and strong wear resistance. The purpose of this study is to experimentally assess the frictional and wear characteristics of CoCr-based alloys slid against two different counter materials subjected to various normal forces to determine the expansion applicability of CoCr-based alloys. CoCrMo and CoCr alloys were selected as the target materials and NiCr and NiCrB alloys as counter materials. Experimental tests were performed using a pin-on-reciprocating plate tribo-tester under dry lubrication. Before performing the tests, the surface of the specimens was observed through confocal microscopy and the hardness was measured using a micro-Vickers hardness tester. The wear volume of the plate was calculated at the end of the tests using confocal microscope data, and the wear rate was quantitatively obtained based on Archard's wear law. From the results, the wear rates of the CoCrMo specimens that slid against NiCr and NiCrB are 7.69 × 10-6 ㎣/Nm and 5.26 × 10-6 ㎣/Nm, respectively. The wear rates of the CoCr specimens that slid against NiCr and NiCrB were higher than those of the CoCrMo specimens by factors of approximately 4 and 8, respectively. The CoCrMo specimens further exhibited lower friction characteristics than the CoCr specimens. The findings of this study will be useful for expanded applications of CoCr-based alloys as wear-resistant materials for various mechanical parts.

베릴륨(Be)이 미 첨가된 치과도재소부용 Ni-Cr-Mo계 합금의 미세조직 및 기계적 성질 특성 (Microstructures and Mechanical Properties of Beryllium(Be)-free Ni-Cr-Mo based Alloys for Metal-Ceramic Crown)

  • 송경우;고은경;이정환;정종현;노학;한재익
    • 대한치과기공학회지
    • /
    • 제28권2호
    • /
    • pp.321-329
    • /
    • 2006
  • The popularity of Ni-Cr-Mo based metal alloys for metal-ceramic crown have increased recently because of low price, superior yield strength and rigidity. the use of these alloys give them the potential advantage of thinner copping with the required rigidity for long span bridges. The purpose of this study was to assess the microstructures and mechanical properties of Ni-Cr-Mo-(Si,Al,Nb,Zr,Ti.Cu,Mm) based Alloys not containing beryllium(Be) related toxic effects. The abtained results indicated that as-cast these specimen alloys showed compositional and microstructural differences, and mechanical properties values of Ni69Cr20Mo5Si2Al4 alloy among these specimen alloys was found to be superior to those of commercial Ni-Cr based alloy using in market place today.

  • PDF

Mechanical Properties and Microstructure of Aluminum Alloys with Dispersed Nanoscale Quasicrystalline Particles

  • Fujita, Masashi;Kimura, Hisamichi;Inoue, Akihisa
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.708-709
    • /
    • 2006
  • New Al-based alloys with very high ultimate tensile strength were developed in high Al concentration range of 91-95 at.% for Al-Fe-Cr-Ti-M (M: Co and Mo) systems and Al-Fe-Cr-Mo-Ti-Co system by the dispersion of nanoscale quasicrystalline particles in Al phase. The effect of adding elements, M was discussed in the viewpoint of stability of super-cooled liquid state and formation ability of quasicrystalline phase. The P/M Al-Fe-Cr-Ti-M alloys with dispersed nanoscale quasicrystalline particles exhibited ultimate tensile strength of 350MPa at 573K and 200MPa at 673K.

  • PDF

고강도 인바계 합금의 열팽창 및 인장 특성에 미치는 바나듐과 탄소 원소 첨가 영향 (Effects of V and C additions on the Thermal Expansion and Tensile Properties of a High Strength Invar Base Alloy)

  • 윤애천;윤신천;하태권;송진화;이기안
    • 소성∙가공
    • /
    • 제24권1호
    • /
    • pp.44-51
    • /
    • 2015
  • The current study seeks to examine the effects of V and C additions on the mechanical and low thermal expansion properties of a high strength invar base alloy. The base alloy (Fe-36%Ni-0.9%Co-2.75%Mo-0.7Cr-0.23Mn-0.17Si-0.3%C, wt.%) contains $Mo_2C$ carbides, which form as the main precipitate. In contrast, alloys with additions of 0.4%V+0.3%C (alloy A) or 0.4%V+0.45%C (alloy B) contain $Mo_2C$+[V, Mo]C carbides. The average thermal expansion coefficients of these high strength invar based alloys were measured in the range of $5.16{\sim}5.43{\mu}m/m{\cdot}^{\circ}C$ for temperatures of $15{\sim}230^{\circ}C$. Moreover, alloy B showed lower thermal expansion coefficient than the other alloys in this temperature range. For the mechanical properties, the [V, Mo]C improved hardness and strengths(Y.S. and T.S.) of the high strength invar base alloy. T.S.(tensile strength) and Y.S.(yield strength) of hot forged alloy B specimen were measured at 844.6MPa and 518.0MPa, respectively. The tensile fractography of alloy B exhibited a ductile transgranular fracture mode and voids were initiated between the [V, Mo]C particles and the matrix. Superior properties of high strength and low thermal expansion coefficient can be obtained by [V, Mo]C precipitation in alloy B with the addition of 0.4%V and 0.45%C.

기계적 합금화법에 의한 Ti-Fe-X계 수소 저장합금의 제조에 관한 연구 (Development of Ti-Fe-X metal hydride electrode by mechanical alloying)

  • 하창진;이경섭
    • 한국재료학회지
    • /
    • 제5권1호
    • /
    • pp.112-122
    • /
    • 1995
  • Metal hydride alloys of TiFe based system have been produced by mechanical alloying(MA) method and their electrochemical characteristics have been evaluated for application for Ni/MH battery electrode. These alloys became amorphous after 36hrs ball milling and easily activated electrochemically. All MA amorphous alloys reached at the first charge/discharge cycle the maximum capacity which was 2-3 times higher than the crystalline state. But their cyclic lives were much inferior to the crystalline state. Alloying elements such as Ni, Co, Cr, Mo substituting Fe greatly improved the capacity and 180 mAh/g capacity was obtained in an alloy of TiFe_{0.6}Ni_{0.1}Co_{0.1}Cr_{0.1}Mo_{0.1}$.