• Title/Summary/Keyword: Chloride migration

Search Result 88, Processing Time 0.024 seconds

Performance of self-compacting concrete with manufactured crushed sand

  • Benyamina, Smain;Menadi, Belkacem;Bernard, Siham Kamali;Kenai, Said
    • Advances in concrete construction
    • /
    • v.7 no.2
    • /
    • pp.87-96
    • /
    • 2019
  • Self-compacting concretes (SCC) are highly fluid concrete which can flow without any vibration. Their composition requires a large quantity of fines to limit the risk of bleeding and segregation. The use of crushed sand rich in limestone fines could be an adequate solution for both economic and environmental reasons. This paper investigates the influence of quarry limestone fines from manufactured crushed sand on rheological, mechanical and durability properties of SCC. For this purpose, five mixtures of SCC with different limestone fines content as substitution of crushed sand (0, 5, 10, 15 and 20%) were prepared at constant water-to-cement ratio of 0.40 and $490kg/m^3$ of cement content. Fresh SCC mixtures were tested by slump flow test, V-funnel flow time test, L-box height ratio, segregation resistance and rheological test using a rheometer. Compressive and flexural strengths of SCC mixtures were evaluated at 28 days. Regarding durability properties, total porosity, capillary water absorption and chloride-ion migration were studied at 180 days. For the two test modes in fresh state, the results indicated compatibility between slump flow/yield stress (${\tau}_0$) and V-funnel flow time/plastic viscosity (${\mu}$). Increasing the substitution level of limestone fines in SCC mixtures, contributes to the decrease of the slump flow and the yield stress. All SCC mixtures investigated achieved adequate filling, adequate passing ability and exhibit no segregation. Moreover, the inclusion of limestone fines as crushed sand substitution reduces the capillary water absorption, chloride-ion migration and consequently enhances the durability performance.

The Critical Flux in Microfiltration: Comparison between Theoretical and Experimental Values (정밀여과에서 임계플럭스(Critical flux)에 관한 이론 및 실험적 고찰)

  • 윤성훈;이정학
    • Membrane Journal
    • /
    • v.7 no.3
    • /
    • pp.150-156
    • /
    • 1997
  • The particle back transport velocity from the membrane surface were evaluated to determine the critical flux. Four kinds of back transport mechanisms were considered, i.e. back diffusion, shear induced migration, lateral migration, and interaction enhanced migration. The interaction enhanced migration caused by electrostatic repulsion between particles and membrane surface was found to be the most important mechanism of particle back transport for the charged particles of 0.1 ~10${\mu}{\textrm}{m}$ diameter with 20 to 40 mV of zeta potential. Hematite particles with different sizes were synthesized with ferric chloride (FeCl$_3$) and hydrochloric acid (HCl) at high temperature, and subsequently experimental critical fluxes for each sized particle were obtained. The experimental results were well coincident with the calculated critical fluxes based on back transport mechanisms.

  • PDF

Chloride Ion Penetration Resistance of Slag-replaced Concrete and Cementless Slag Concrete by Marine Environmental Exposure (해양환경 폭로에 의한 슬래그 치환 콘크리트 및 슬래그 콘크리트의 염화물 이온 침투 저항성)

  • Lee, Bo-Kyeong;Kim, Gyu-Yong;Kim, Gyeong-Tae;Shin, Kyoung-Su;Nam, Jeong-Soo
    • Journal of the Korea Concrete Institute
    • /
    • v.29 no.3
    • /
    • pp.299-306
    • /
    • 2017
  • In this research, it was examined chloride ion penetration resistance of slag-replaced concrete and cementless slag concrete considering marine environmental exposure conditions of splash zone, tidal zone and immersion zone. In the design strength of grade 24 MPa, the specimens were tested to determine their compressive strength, scanning electron microscopy images and chloride migration coefficient. Further, chloride ion penetration depth and carbonation depth of specimens exposed to marine environment were measured. Experimental results confirm that chloride migration coefficient of specimens tended to decrease with increasing the replacement ratio of ground granulated blast-furnace slag in accelerated laboratory test. In addition, the specimens exposed to the tidal zone were found to be the greatest chloride ion penetration depth compared to splash zone and immersion zone. On the other hand, the chloride ion penetration depth of the specimens exposed to splash zone tended to increase with increasing the replacement ratio of ground granulated blast-furnace slag in contrast with the results for the tidal zone and immersion zone.

The Effect of Entrained Air Contents on the Properties of Freeze-thaw Deterioration and Chloride Migration in Marine Concrete (연행 공기량이 해양콘크리트의 동결융해 및 염화물 확산특성에 미치는 영향)

  • Park, Sang-Joon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.12 no.5
    • /
    • pp.161-168
    • /
    • 2008
  • The freeze-thaw deterioration and chloride attack, which are the typical degradation factors for durability of marine concrete, are significantly affected by pore structures in terms of penetration and diffusion. These pore structures of concrete are closely related to the types and amount of AE agent, used to guarantee the resistance of freeze-thaw deterioration, and the elapsed time before concrete pouring. This paper evaluates the durability of concrete based on the results of tests on cylinder specimens and core specimens from mock-up members with different air content of 4~6% and 8~10%, respectively. According to the test results, the air content of hardened concrete is 2.5~5.2% at 7 days and 2.4~5.1% at 28 days. These air contents are about half of the initial values just after the concrete mixing. Judging from the amount of scale after the freeze-thaw test completed, air content of 8~10% is slightly more beneficial against the deterioration of concrete than air content of 4~6%. Meanwhile, the core specimens from mock-up members exhibit somewhat unfavorable freeze-thaw deterioration and chloride migration characteristic compared with the cylinder specimens tested in the laboratory under the same mixing condition, as to show 106% in freeze-thaw test and 160% in chloride diffusion coefficient test, respectively.

Root Bark extract of Morus alba L. Suppressed the Migration and Invasion of HCT116 Human Colorectal Carcinoma Cells (HCT116 인체 대장암 세포주에서 상백피 추출물에 의한 전이 억제 효과)

  • Park, Shin-Hyung;Park, Hyun-Ji
    • Journal of Physiology & Pathology in Korean Medicine
    • /
    • v.35 no.5
    • /
    • pp.177-184
    • /
    • 2021
  • The root bark of Morus alba L. (MA) used in traditional oriental medicine for the treatment of pulmonary diseases exerts various pharmacological activities including anticancer effects. In the current study, we investigated the effects of MA on the migration and invasion of colorectal carcinoma cells. Results from a transwell assay showed that the methylene chloride extract of MA (MEMA) suppressed the migration and invasion of HCT116 human colorectal carcinoma cells in a concentration-dependent manner. MEMA reduced both mRNA and protein levels of matrix metalloproteinase (MMP)-9, but did not suppress the expression of MMP-2 in HCT116 cells. As a molecular mechanism, MEMA inhibited the phosphorylation of mitogen-activated protein kinases (MAPKs), including ERK, JNK and p38, in a dose-dependent manner. In addition, MEMA dephosphorylated both Src and signal transducer and activator of transcription 3 (STAT3) in HCT116 cells. Taken together, we demonstrate that MEMA suppressed the migration and invasion capacity of HCT116 human colorectal cancer cells by downregulation of MMP-9 and inactivation of both MAPKs and Src/STAT3 signaling pathway.

Testing of the permeability of concrete box beam with ion transport method in service

  • Wang, Jia Chun
    • Computers and Concrete
    • /
    • v.15 no.3
    • /
    • pp.461-471
    • /
    • 2015
  • The permeability is the most direct indicator to reflect the durability of concrete, and the testing methods based on external electric field can be used to evaluate concrete permeability rapidly. This study aims to use an experiment method to accurately predict the permeability of concrete box beam during service. The ion migration experiments and concrete surface resistivity are measured to evaluate permeability of five concrete box beams, and the relations between these results in service concrete and electric flux after 6 hours by ASTM C1202 in the laboratory are analyzed. The chloride diffusion coefficient of concrete, concrete surface resistivity and concrete 6 hours charge have good correlation relationship, which denote that the chloride diffusion coefficient and the surface resistivity of concrete are effective for evaluating the durability of concrete structures. The chloride diffusion coefficient of concrete is directly evaluated permeability of concrete box beam in service and may be used to predict the service life, which is fit to engineering applications and the concrete box beam is non-destructive. The concrete surface resistivity is easier available than the chloride diffusion coefficient, but it is directly not used to calculate the service life. Therefore the mathematical relation of the concrete surface resistivity and the concrete chloride diffusion coefficient need to be found, which the service life of reinforced concrete is obtained by the concrete surface resistivity.

The Investigation of Crack widths for the Effect of Cracks on Chloride Penetration of Concrete (콘코리트 중의 염화물 침투에 영향을 미치는 균열폭에 대한 고찰)

  • Yoon, In-Seok;Erik, Schlangen;Breuged, Klaas Van
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.945-948
    • /
    • 2006
  • Chloride penetration into concrete is a hot issue of concern all over the world, notwithstanding, very few attempts have been conducted to explore the effect of cracks on choride penetration. Cracks provoke to lose a main function of watertightness of concrete and lead to reduce the service life of concrete. For this reason, it is necessary to define a critical crack width to prevent a quick chloride penetration through crack. In this study, experiment is focused on establishing a critical crack width in terms of chloride penetration. Concrete specimens with different crack widths I crack lengths have been subjected to rapid chloride migration testing. In a side of analytical solution, a simple approach to quantify the chloride diffusion coefficient of only crack zone excluding sound concrete was proposed. The result clearly showed a critical crack width of 0.03 mm. Based on the experimental results, a phenomenological model was proposed to explain the meaning of critical crack width in practical engineering. In this model, cracked concrete zone was divided into three zones. These zones corresponded to a wide crack, a zone with micro-cracks and an uncracked zone.

  • PDF

Effect of the Kinds and Replacement Ratios of Mineral Admixtures on the Development of Concrete Resistance against the Penetration of Chloride Ions (혼화재 종류 및 치환율이 콘크리트의 내염성능 향상에 미치는 영향에 관한 연구)

  • Kim Young-Jin;Lee Sang-Soo;Kim Dong-Seuk;Yoo Jae-Kang
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.3 s.81
    • /
    • pp.319-326
    • /
    • 2004
  • This paper investigates the effect of the concrete containing mineral admixtures(pozzolanic materials such as fly-ash, ground granulated blast-furnace slag, silica fume and meta kaolin) on the resistance properties to chloride ion invasion. The purposed testing procedure was applied to the concrete replaced mineral admixtures for 3${\~}$4 replacement ratios under water-binder ratios ranged from 0.40 to 0.55. For the electro-migration test, Tang and Nilsson's method was used to estimate the diffusion coefficient of chloride ion. As a results, the water-binder ratios, kinds of mineral admixtures and replacement ratios, water curing periods had a great effect on the diffusion coefficient of chloride ion, and the optimal replacement ratios had a limitation for each mineral admixtures. Also, the use of mineral admixtures by mass(replacement of OPC) enhance the resistance ability against chloride penetration compared with the plain concrete. The compressive strength was shown related to the diffusion coefficient of chloride ion, the compressive strength increases with the diffusion coefficient of chloride ion decreasing. Below the 50 MPa, the variation of diffusion coefficient of concrete replaced mineral admixtures was bigger than that of plain concrete.

Surface Segregation of Hydroniums and Chlorides in a Thick Ice Film at Higher Temperatures

  • Lee, Du Hyeong;Bang, Jaehyeock;Kang, Heon
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.263-263
    • /
    • 2013
  • This work examines the dynamic properties of ice surfaces in vacuum for the temperature range of 140~180 K, which extends over the onset temperatures for ice sublimation and the phase transition from amorphous to crystallization ice. In particular, the study focuses on the transport processes of excess protons and chloride ions in ice and their segregative behavior to the ice surface. These phenomena were studied by conducting experiments with a relatively thick (~100 BL) ice film constructed with a bottom $H_2O$ layer and an upper $D_2O$ layer, with excess hydronium and chloride ions trapped at the $H_2O$/$D_2O$ interface as they were generated by the ionization of hydrogen chloride. The migration of protons, chloride ions, and water molecules to the ice film surface and their H/D exchange reactions were measured as a function of temperature using the methods of low energy sputtering (LES) and Cs+ reactive ion scattering (RIS). Temperature programmed desorption (TPD) experiments monitored the desorption of water and hydrogen chloride from the surface. Our observations indicated that both hydronium and chloride ions migrated from the interfacial layer to segregate to the surface at high temperature. Hydrogen chloride gas desorbs via recombination reaction of hydronium and chloride ions floating on the surface. Surface segregation of these species is driven by thermodynamic potential gradient present near the ice surface, whereas in the bulk, their transport is facilitated by thermal diffusion process. The finding suggests that chlorine activation reactions of hydrogen chloride for polar stratospheric ice particles occur at the surface of ice within a depth of at most a few molecular layers, rather than in the bulk phase.