폭발용사에 의한 내에로젼성 서멧 피막 코팅에 관한 연구 (A Study on the Erosion-Resistant Cermet Film Coating using the Detonation Spray Method)

  • 김현근;남인철;오재환
    • Journal of Welding and Joining
    • /
    • 제19권1호
    • /
    • pp.95-103
    • /
    • 2001
  • The properties of the detonation sprayed cermet coating are investigated through the mechanical, corrosion and erosion test. The test results are also compared with the properties of the substrate materials, STS 329J1, dual phase stainless steel and the plasma sprayed cermet coatings. The two kinds of carbide cermet power, WC+NiCr, Cr$_3$C$_2$+NiCr were used in this experiment. The experimental results showed that the anti-corrosive and anti-erosive properties of the detonation sprayed cermet coatings are superior to the plasma sprayed cermet coatings. The WC+NiCr cermet coating appears to be more effective than Cr$_3$C$_2$+NiCr cermet coating in abrasive erosion environment, whereas the Cr$_3$C$_2$+NiCr cermet coatings are more effective in cavitation erosion environment.

  • PDF

고속 화염 용사 공정으로 제조된 WC계 및 Cr3C2계 Cermet 코팅 소재의 미세조직 및 마모 특성 (Microstructural and Wear Properties of WC-based and Cr3C2-based Cermet Coating Materials Manufactured with High Velocity Oxygen Fuel Process)

  • 강연지;함기수;김형준;윤상훈;이기안
    • 한국분말재료학회지
    • /
    • 제25권5호
    • /
    • pp.408-414
    • /
    • 2018
  • This study investigates the microstructure and wear properties of cermet (ceramic + metal) coating materials manufactured using high velocity oxygen fuel (HVOF) process. Three types of HVOF coating layers are formed by depositing WC-12Co, WC-20Cr-7Ni, and Cr3C2-20NiCr (wt.%) powders on S45C steel substrate. The porosities of the coating layers are $1{\pm}0.5%$ for all three specimens. Microstructural analysis confirms the formation of second carbide phases of $W_2C$, $Co_6W_6C$, and $Cr_7C_3$ owing to decarburizing of WC phases on WC-based coating layers. In the case of WC-12Co coating, which has a high ratio of $W_2C$ phase with high brittleness, the interface property between the carbide and the metal binder slightly decreases. In the $Cr_3C_2-20CrNi$ coating layer, decarburizing almost does not occur, but fine cavities exist between the splats. The wear loss occurs in the descending order of $Cr_3C_2-20NiCr$, WC-12Co, and WC-20Cr-7Ni, where WC-20Cr-7Ni achieves the highest wear resistance property. It can be inferred that the ratio of the carbide and the binding properties between carbide-binder and binder-binder in a cermet coating material manufactured with HVOF as the primary factors determine the wear properties of the cermet coating material.

The In-situ Dressing of CMP Pad Conditioners with Novel Coating Protection

  • Sung, James-C.;Kan, Ming-Chi
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1142-1143
    • /
    • 2006
  • Kinik Company pioneered diamond pad conditioners protected by DLC barrier ($DiaShield^{(R)}$ Coating) back in 1999 (Sung & Lin, US Patent 6,368,198). Kink also evaluated Cermet Composite Coating (CCC or $C^3$, patent pending) with a composition that grades from a metallic (e.g. stainless steel) interlayer to a ceramic (e.g. $Al_2O_3$ or SiC) exterior. The metallic interlayer can form metallurgical bond with metallic matrix on the diamond pad conditioner. The ceramic exterior is both wear and corrosion resistant. The gradational design of $C^3$ coating will assure its strong adherence to the substrate because there is no weak boundary between coating and substrate.

  • PDF

고온용 서밋 태양선택흡수막의 증착 (Deposition of Cermet Solar Selective Coatings for High Temperature Applications)

  • 이길동
    • 한국태양에너지학회 논문집
    • /
    • 제26권1호
    • /
    • pp.57-64
    • /
    • 2006
  • Cr-CrO cermet solar selective coatings with a double cermets layer film structure were prepared using a special direct current (dc) magnetron sputtering technology. The typical films structures from surface to bottom substrate were measured to be an $Al_2O_3$ anti-reflection layer on a double Cr-CrO cermet layer on an Al metal infrared reflection layer. Optical properties of optimized Cr-CrO cermet solar selective coating were absorptance (${\alpha}$) = 0.95 and emittance (${\varepsilon}$) = 0.10 ($100^{\circ}C$). Atomic force microscopy (AFM) image showed that Cr-CrO cermet film was very smooth and their grain size was also very small The results of thermal stability test showed that the Cr-CrO cermet solar selective coatings were stable for use at temperature of $400^{\circ}C$.

Pd 코팅된 Ta/YSZ 수소분리막의 제조 및 안정성 (Fabrication and Stability of Pd Coated Ta/YSZ Cermet Membrane for Hydrogen Separation)

  • 이상진;전성일;박정훈
    • 멤브레인
    • /
    • 제20권1호
    • /
    • pp.69-75
    • /
    • 2010
  • 수소투과금속인 tantalum과 세라믹 지지체로 $Y_2O_3$-stabilized $ZrO_2$ (YSZ)를 이용하여 cermet 수소분리막을 제조하였다. Ta/YSZ cermet 분리막은 헬륨분위기에서의 예비소결과 고진공 하에서의 본소결을 통해 제조하였으며, 소결 및 밀봉 과정에서 발생하는 불순물은 연마를 통해 제거 가능하였다. 이렇게 제조된 분리막은 tantalum의 연속상이 잘 발달된 치밀구조를 보였다. 수소 해리를 위해 팔라듐 코팅을 한 Ta/YSZ 분리막을 이용하여 $200{\sim}350^{\circ}C$의 범위에서 수소투과실험을 수행하였다. $300^{\circ}C$에서 분리막에 균열이 형성되었고 Pd 코팅층은 몇 곳이 박리되었다. XRD 결과는 tantalum이 수소와 반응하여 $Ta_2H$가 생성되는 것을 보여주며, $Ta_2H$에 인한 격자 팽창이 분리막의 결함을 초래하였다.

HVOF용사 코팅한 SM490B 코팅층의 미시조직 특성 (The Micro Structure Characteristics of Coating Layer on SM490B with HVOF Coating)

  • 남기수;조원익;윤명진;김병문
    • 한국공작기계학회논문집
    • /
    • 제14권5호
    • /
    • pp.80-86
    • /
    • 2005
  • High velocity oxy-fuel thermally sprayed coating of the WC-Co cermet material is a well-established process for modifying the surface properties of the structural components exposed to the corrosive and wear attacks. The hard WC phase in the coating resists to the wear while the soft metallic Co increases the adhesive and cohesive bonding properties. The coating properties deposited by the HVOF process are greatly dependent on the feedstock materials and processing parameters. The effects of the feedstock material and process coating parameters including the in-flight particle parameters and resultant coating microstructures were observed in this paper.

아연-0.2%알루미늄합금 용융도금액 중에서 용사층의 내구성에 관한 연구 (A Study on Durability of Sprayed Coating Layer in the Molten Zn-0.2% Al Alloy Bath)

  • 강태영;임병문;최장현;김영식
    • Journal of Welding and Joining
    • /
    • 제19권5호
    • /
    • pp.512-519
    • /
    • 2001
  • Sink roll has been used in molten Zn-0.2%Al alloy bath of continuous galvanizing line in sinking and stabilizing process of the steel strip in molten metal bath. In this process, although the scraper scraps off the sink roll surface, the dross compounds is builded up on the sink roll surface and the life time of the sink roll is shorten by the dross compounds. The present study was investigated the application of the spray coating layer on sink roll body for improving durability In molten Zn-0.2%Al alloy. Through the durability tests in molten Zn-0.2%Al alloy with various ceramic and cermet coating layer, the optimum bond and top coating material was obtained. As the results, the system of STS430F base metal, WC-l7Co bond and $ZrO_2-SiO_2$ top coating was clarified to be the best quality of durability in molten Zn-0.2%Al alloy.

  • PDF

집전체에 따른 NI-YSZ Cermet 기반의 가역적 고체산화물 연료전지를 이용한 고온 수증기 전기분해 특성 (Current Collector Effects on High Temperature Electrolysis by NI-YSZ Cermet Supported Solid Oxide Cells)

  • 신의철;안평안;서현호;이종숙;유지행;우상국
    • 한국수소및신에너지학회논문집
    • /
    • 제21권6호
    • /
    • pp.533-539
    • /
    • 2010
  • Ni-YSZ supported button cells were prepared by spray-coating YSZ and screen-printing YSZ-LSM powder as an electrolyte and oxygen electrode on Ni-YSZ cermet disks. In order to identify the polarization loss mechanism in high temperature electrolysis current-voltage characteristics coupled with electrochemical impedance spectroscopy were investigated as a function of temperature, current load, and the humidity. The effects of the different current collectors of platinum and silver for oxygen electrodes were compared. With Ag current collector two polarization losses were distinguished. The high frequency component was attributed to the Ni-YSZ cermet which was less susceptible to temperature variation but increasing in loss with humidity. The lower frequency component was attributed to the LSM electrode. Platinum current collector led to a much lower polarization loss.