Ti(C,N)계 서메트 공구의 조성변화가 절삭성능에 미치는 영향 (Effect of Composition on Cutting Characteristics of Ti(C,N) Cermet Tool)

  • 박준석;김경재;김성원;권원태;강신후
    • 한국정밀공학회지
    • /
    • 제20권1호
    • /
    • pp.144-150
    • /
    • 2003
  • When WC and group IV elements are added to Ti(C,N)-Ni substrate, microstructures of the cermet is changed. The microstructure gives direct effect on the property of the material. In this study, the amount of WC and group W elements of Ti(C,N) cermet tool was investigated. The composition of WC was changed from 5 to 20wt% to determine the effect of WC on the cutting performance of cermet tool. The more WC was added, the longer the tool life of the cermet tool was. The cermet with 20wt% WC showed the best fracture toughness. The effect of group W elements; ZrC, ZrN and HfC was also investigated by adding each of them to manufacture the cermet tool with fixed l4wt% WC composition. The cermet with 1wt% ZrC and 14wt% WC showed the best cutting performance among the investigated cermet tools.

Ti(C,N)계 서메트 공구의 조성변화에 따른 절삭성능 및 신뢰도 분석 (Effect of Composition on Cutting Characteristics and Reliability Analysis of Ti(C,N) Cermet Tool)

  • 박준석;김성원;권원태;강신후
    • 대한기계학회논문집A
    • /
    • 제26권11호
    • /
    • pp.2336-2341
    • /
    • 2002
  • When WC and group IV elements are added to Ti(C,N)-Ni cermet, microstructures of the cermet is changed. The change effects directly on the property of the material. In this study, the amount of WC and group IV elements of Ti(C,N) cermet tool was investigated. The composition of WC was changed from 5 to 20wt% to determine the effect of WC on the cutting performance of cermet tool. The more WC was added, the longer the tool life of the cermet tool was. The cermet with lwt% ZrC and l4wt% WC showed the best cutting performance among the investigated cermet tools. The cutting performance of cermet cutting tools suggests the possibility in interrupted cutting for reliability test experimentation was performed repeatedly with $Ti(C_{0.7},N_{0.3})- l4WC-1ZrC-20Ni$ cermet tool machining SCM440. The flank wear of cermet cutting tool at given time condition is suitable for Normal distribution and Log normal distribution by Chi squared test.

폭발용사에 의한 내에로젼성 서멧 피막 코팅에 관한 연구 (A Study on the Erosion-Resistant Cermet Film Coating using the Detonation Spray Method)

  • 김현근;남인철;오재환
    • Journal of Welding and Joining
    • /
    • 제19권1호
    • /
    • pp.95-103
    • /
    • 2001
  • The properties of the detonation sprayed cermet coating are investigated through the mechanical, corrosion and erosion test. The test results are also compared with the properties of the substrate materials, STS 329J1, dual phase stainless steel and the plasma sprayed cermet coatings. The two kinds of carbide cermet power, WC+NiCr, Cr$_3$C$_2$+NiCr were used in this experiment. The experimental results showed that the anti-corrosive and anti-erosive properties of the detonation sprayed cermet coatings are superior to the plasma sprayed cermet coatings. The WC+NiCr cermet coating appears to be more effective than Cr$_3$C$_2$+NiCr cermet coating in abrasive erosion environment, whereas the Cr$_3$C$_2$+NiCr cermet coatings are more effective in cavitation erosion environment.

  • PDF

Ti(C,N)계 서메트 공구의 WC와 IV족 원소 첨가가 단속 절삭성능에 미치는 영향 (Effect of WC and group IV Elements of Ti(C,N) on the Intermittent Cutting Performance)

  • 박준석;김경재;권원태;강신후
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 추계학술대회 논문집
    • /
    • pp.919-922
    • /
    • 1997
  • In this study, the amount of WC and group N elements of Ti(C, N) cermet tool was investigated. The composition of WC was changed from 5 to 20% to determine the effect of WC on the cutting performance of cermet tool. The more WC was added, the longer the tool life of the cermet tool was. The cermet with 20% WC showed the best fracture toughness. The effect of group N elements ; ZrC, ZrN and HfC was also investigated by adding each of them to manufacture the cermet tool with fixed 14% WC composition. The cermet with 1% group N ZrC and 14% WC showed the best cutting performance among the investigated cermet tools.

  • PDF

선삭시 Ti(C,N)계 서메트 공구의 WC와 IV족 원소 첨가가 절삭성능에 미치는 영향 (Effect of WC and group IV Elements of Ti(C,N) on Cutting Performance in Turning)

  • 박준석;김경재;권원태;강신후
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2001년도 추계학술대회(한국공작기계학회)
    • /
    • pp.3-7
    • /
    • 2001
  • In this study, the effect of WC and group IV elements on the cutting performance in turning is investigated. The composition of WC was changed from 5 to 20% to determine the effect of WC on the cutting performance of cermet tool. The more WC was added, the longer the tool life of the cermet tool was. The cermet with 20% WC showed the best fracture toughness. The cermet tool with 20% WC showed the best cutting performance among the various WC composition. The effect of group IV elements ; ZrC, ZrN and HfC was also investigated by adding each of them to manufacture the cermet tool with fixed 14% WC composition. The cermet with 1% group IV HfC and 14% WC showed the best cutting performance among the investigated cermet tools.

  • PDF

초미립 서멧 절삭공구의 절삭성능과 기계적 특성 (Cutting Performance of Submicron Cermet Tools and Their Mechanical Properties)

  • 안동길
    • 한국정밀공학회지
    • /
    • 제18권4호
    • /
    • pp.182-189
    • /
    • 2001
  • TiCN based submicron cermet and similar ISO grad of the conventional cermets with TiCN of different particle size were produced by PM process, and their microstructure, mechanical properties and cutting performance were compared. The microstructure of submicron cermet was more homogeneous and showed much finer microstructure, resulting in better hardness and fracture toughness. The submicron cermet tools achieved excellent cutting performance such as wear resistance and toughness in comparison with two grades of the conventional cermets in millimg test. The relationship between microstrucure, mechanical properties and cutting performance of these cermet tools was discussed. The submicron cermet tools revealed for their potential to wide application range and interrupt cutting because of their superior wear resistance and toughness combinations.

  • PDF

선삭가공에서 서멧과 초경 및 코팅 초경공구의 절삭특성 비교 (Comparison of Cutting Characteristics between Cermet, Carbide and Coated Carbide Tools in Turning)

  • 안동길
    • 한국정밀공학회지
    • /
    • 제17권5호
    • /
    • pp.186-194
    • /
    • 2000
  • The purpose of this study is to investigate the difference in cutting characteristics of cermet, carbide and coated carbide tools in the similar application range via turning test of various conditions. The cermet and carbide tools in the range of ISO P10 grade were developed using optimum compositions with a view to obtaining a high toughness and hardness by PM process. First mechanical properties were characterized on these tools. Experimental results of wear behaviour and resistance to fracturing were presented and discussed in the turning of gray cast iron and alloy steels by cermet, carbide and coated carbide tools. The coated carbide tool shows similar cutting performance compared to the cermet, while the cermet has better combination of wear resistance and toughness of high speed (V=500m/min) cutting in comparison with carbide and coated carbide tools, and also shows a potentiality for cast iron cutting. Fe adhesive behaviour on the tools and surface roughness of workpieces were explained by chemical affinity between tools and workpieces.

  • PDF

TiB$_2$-Fe 서메트의 소결성 및 기계적성질에 미치는 Mo첨가의 영향 (Effect of Mo Addition on the Sinterability and Mechanical Properties of TiB$_2$-Fe Cermets)

  • 최덕순
    • 한국세라믹학회지
    • /
    • 제36권5호
    • /
    • pp.471-477
    • /
    • 1999
  • Fe and Fe-Mo binder were used to produce TiB2 based cermet by a pressureless sintering. The densification behaviour of TiB2-Fe-Mo cermet during liquid-phase sintering in argon was studied in relation to binder phase charactertics. The effects of Mo addition and sintering condition on the sintering behaviour and mechanical properties were also investigated. TiB2-based cermets with Fe-Mo binder composition showed a better sinterability than the cermets with only Fe binder. In TiB2-Fe-Mo cermet higher densities in the wide temperature range were obtained and also fully densified sintered cermet were obtained at 1873K The enhancement in the densification phenomenon of TiB2-Fe-Mo system can be explained by improved liquid phase wettability associated with the roles of Mo components as solute atoms. When Fe-Mo binders were used cermets with a finer grain size and enhanced mechanical properties wereproduced and new phases such as Fe2B and Mo2FeB2 were observed in the sintered cermet. The highest bending strength was obtained from the 20vol% Fe-Mo cermet and these hardness-fracture toughness combination in the wide binder compositions is better than that of TiB2-Fe cermet. In order to improve mechanical properties microstructure control with high purity powders is desirable because high purity powders prevent the formation of Fe2B and Mo2FeB2 phase which comsume the ductile binder phase.

  • PDF

고온용 서밋 태양선택흡수막의 증착 (Deposition of Cermet Solar Selective Coatings for High Temperature Applications)

  • 이길동
    • 한국태양에너지학회 논문집
    • /
    • 제26권1호
    • /
    • pp.57-64
    • /
    • 2006
  • Cr-CrO cermet solar selective coatings with a double cermets layer film structure were prepared using a special direct current (dc) magnetron sputtering technology. The typical films structures from surface to bottom substrate were measured to be an $Al_2O_3$ anti-reflection layer on a double Cr-CrO cermet layer on an Al metal infrared reflection layer. Optical properties of optimized Cr-CrO cermet solar selective coating were absorptance (${\alpha}$) = 0.95 and emittance (${\varepsilon}$) = 0.10 ($100^{\circ}C$). Atomic force microscopy (AFM) image showed that Cr-CrO cermet film was very smooth and their grain size was also very small The results of thermal stability test showed that the Cr-CrO cermet solar selective coatings were stable for use at temperature of $400^{\circ}C$.

절삭공구용 서멧의 자기적 특성과 기계적 성질의 관계 (Relationship between Magnetic and Mechanical Properties of Cermet Tools)

  • 안동길;이정희
    • 비파괴검사학회지
    • /
    • 제20권3호
    • /
    • pp.231-237
    • /
    • 2000
  • 공업용 서멧 절삭공구는 다성분계 탄화물과 강자성체(ferromagnetic material)인 철족의 Co, Ni 결합상 금속으로 구성 되어 있다. 본 연구에서는 새로운 시도로서 금속 결합상 량과 소결조건에 따른 TiCN계 서멧의 자기적 특성의 측정에 의한 기계적 성질의 평가방법을 연구하였다. 실험에서는 결합상이 다른 상용 서멧조성의 합금을 분말 야금법에 의해 제조하였다. 소결된 서멧의 자기적 특성은 합금의 조직과 탄소량에 따라 크게 변화하였다. 포화자화(magnetic saturation, $4{\pi}\;{\sigma}$)와 항자력(coercive force, Hc)은 비례하였으며, 고탄소 소결합금에 있어서는 Co-Ni 결합상에서의 W, Mo, Ti등의 용매원자의 농도가 낮아짐에 따라 포화자화는 증가하였다 항자력이 높을수록 경도는 증가하였고, 서멧의 강도 및 인성은 포화자화가 증가할수록 우수하였다. 서멧공구에서 자기적 특성을 측정하여 기계적 성질을 비파괴적으로 평가할 수 있었다.

  • PDF